Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “test matrix”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 451 records · Page 25

The effect of low energy protons on silicon solar cells with simulated coverglass cracks

Results of a series of low-energy proton (LEP) tests are presented. The purpose of the tests was to investigate the effect of low-energy protons on the electrical performance of solar cells with simulated cracked covers. The results of the tests were then related to the space environment. A matrix of LEP tests was set up using solar cells with simulated cracks to determine the effect on electrical performance as a function of fluence, energy, crack width, coverglass adhesive shielding, crack location, and solar cell size. The results of the test were, for the most part, logical, and consistent.

Gasner, S.↗

Improved procedures for mass matrix-reductions in eigenvalue solutions

Analytical models of three structures were used to test mass matrix-reduction schemes. Accuracy of four mode shapes and frequencies was tracked through successive mass matrix-reductions with diminishing numbers of indicator degrees of freedom. Results were consistently disappointing. Two new procedures were developed in attempt to improve accuracy.

Levy, R.↗

Characterization of Ceramic Matrix Composite Vane Subelements Subjected to Rig Testing in a Gas Turbine Environment

Vane subelements were fabricated from a silicon carbide fiber-reinforced silicon carbide matrix (SiC/SiC) composite. A cross-sectional slice of an aircraft engine metal vane was the basis of the vane subelement geometry. To fabricate the small radius of the vane's trailing edge using stiff Sylramic SiC fibers, a unique SiC fiber architecture was developed. A test configuration for the vanes in a high pressure gas turbine environment was designed and fabricated. Testing was conducted using a pressure of 6 atm and combustion flow rate of 0.5 kg/sec, and consisted of fifty hours of steady state operation followed by 102 2-minute thermal cycles. A surface temperature of 1320 C was obtained for the EBC-coated SiC/SiC vane subelement. This paper will briefly discuss the vane fabrication, test configuration, and results of the vane testing. The emphasis of the paper is on characterization of the post-test condition of the vanes.

Verrilli, Michael↗

Knowledge Discovery Process for Characterization of Materials Failure Mechanism

It is the intent of this project to provide a platform to visualize the various data collected from stress-strain testing of composite ceramic matrix materials. The data collected from the stress-strain tests are acoustic emissions (AE). As a material is subjected to a stress-strain test, various failure mechanisms occur in the material. The recorded sounds emitted during the test may correspond to various failure mechanisms. This project, thus, will give a possible way to visualize the data and data derived from the recorded AE. The stress-strain testing was performed on several composite matrix material combinations. Each of these tests produced anywhere from 1000 to 10,000+ AE events. For each AE event recorded, several characteristics in both the time and frequency domains are created. This project has two goals. First, this project will provide a summation page for a selected waveform. This page will include all of the characteristics determined from the AE event waveform along with graphs of the AE event waveform and its corresponding Power Spectrum. The other function of this project is to retrieve and display selected AE event waveforms for comparison.

Cios, Krzysztof J.↗

Failure analysis of nuclear transient-tested UN tristructural isotropic fuel particles in a 3D printed SiC matrix

Fully ceramic microencapsulated fuel elements containing UN tristructural isotropic (TRISO) fuel particles within a 3D printed SiC matrix were subjected to transient testing with varying energy depositions. Detailed post-irradiation examinations were performed, including leaching in hot HNO3 and post-leaching X-ray computed tomography, to quantify the percentage of failed TRISO particles and crack propagation within the particles and surrounding fuel matrix. In parallel, detailed finite element analyses were performed for comparison with experimental findings and to better evaluate transient failure modes. The lowest transient energy deposition—which still exceeded bounding values for high-temperature gas-cooled reactor applications—resulted in no detectable TRISO particle failures or matrix cracking, which was consistent with the simulations. Simulations of the higher-energy transients for which significant TRISO particle failure was expected were generally able to reproduce the transient temperatures and matrix cracking. Thus, the TRISO particle failures were explained based on the effects of local SiC matrix thickness and porosity. Results generally confirmed the high strength of the additively manufactured SiC matrix but also affirmed the need for a modified UN TRISO architecture to prevent SiC matrix cracks from propagating through TRISO layers. This unique failure mode has not historically been considered for TRISO fuels contained in weaker graphite matrices.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Estimation of full modal damping matrices from complex test modes

This paper describes the refinements of a previously published method for estimating a full modal damping matrix from complex test modes. It also documents application of the refined method to a structure where complex test modes were derived by the ERA method from multi-input random vibration test data. A numerical example based on simulated test data is presented to demonstrate the validity of the method. The application using real data was not successful, presumably because of noise in the small phase angles of the measured complex modes. Alternative test and data reduction procedures are suggested as possible remedies to the problem. A careful analysis of measurement and data processing errors should be made to examine basic feasibility before implementing the alternative procedures. The ability to estimate a full modal damping matrix is considered important for the preflight estimation of on-orbit damping, and for the synthesis of structural damping from substructure tests.

Hasselman, T. K.↗

Performance and Safety Tests of Lithium-Ion Cells Arranged in a Matrix Design Configuration

Matrix Packs display large variations in cell bank voltages at the charge and discharge current (C/2) used in this test program. The voltage difference is larger at the end of discharge than at the end of charge under the conditions studied. Disconnection of a cell from the pack leads to a larger voltage difference during discharge (greater than 2.0 V) between the bank that has one less cell and the other banks. Thermal profile does not show any significant changes or increase in temperature after one cell was disconnected from the bank in spite of falling to very low voltages at the end of discharge. All tests on the matrix pack with the HAM displayed lower max in general due to the placement of thermocouple on the outside of the HAM rather than on the cells. Disconnection of cells has almost no influence on the performance of the packs and does not show any abnormal thermal changes for the 100 cycles obtained in this test program. Longer cycle life may influence the performance especially if the low voltage cell goes into reversal. Overcharge leads to CID activation of cells. If the matrix configuration has a larger number of cells in series, (more than 5 S configuration), the limitations of protective devices may manifest itself irrespective of it being in a matrix configuration. External short circuit causes a fire with expulsion of content from some cells. The fire does not propagate itself laterally, but if there was cell module stacking, then the fire would cause the cells above it to also go into flames/thermal runaway. Limitations of protective devices are observed in this case as the PTCs in the cells did not protect under this abusive condition. Matrix configurations seem to provide protection against lateral propagation of fire and flame. Matrix pack configuration seems to provide good performance in spite of losing cell connections; at least for the configuration tested under this program.

Jeevarajan, Judith↗

Device for quick changeover between wind tunnel force and pressure testing

This device allows for expeditious and repeated changeovers between pressure and force testing and which uses a minimum internal volume of a wind tunnel test structure. A matrix configuration of holes is located on the outer surface of the structure. Pressure tubes lead through the internal cavity of the structure from test sites to this outer surface matrix configuration. A pressure tube connector with a corresponding matrix of holes is connected to the surface of the structure. Pressure tubes leading from remotely located transducers are joined to the connector, thus forming pressure passageways from the test sites to the transducers to allow for pressure testing. When force testing is required, the pressure tube connector is disconnected and a cover plate is connected. The cover plate seals the exposed internal pressure tubes. Also, the outer surface of the cover plate conforms to the exterior of the structure, providing the necessary smooth surface for force testing. If further pressure testing is required, the cover plate can be disconnected and the pressure tube connector reconnected.

Wood, Richard M.↗

Fabrication and Characterization of SMA Hybrid Composites

Results from an effort to fabrication shape memory alloy hybrid composite (SMAHC) test specimens and characterize the material system are presented in this study. The SMAHC specimens are conventional composite structures with an embedded SMA constituent. The fabrication and characterization work was undertaken to better understand the mechanics of the material system, address fabrication issues cited in the literature, and provide specimens for experimental validation of a recently developed thermomechanical model for SMAHC structures. Processes and hardware developed for fabrication of the SMAHC specimens are described. Fabrication of a SMA14C laminate with quasi-isotropic lamination and ribbon-type Nitinol actuators embedded in the 0' layers is presented. Beam specimens are machined from the laminate and are the focus of recent work, but the processes and hardware are readily extensible to more practical structures. Results of thermomechanical property testing on the composite matrix and Nitinol ribbon are presented. Test results from the Nitinol include stress-strain behavior, modulus versus temperature. and constrained recovery stress versus temperature and thermal cycle. Complex thermomechanical behaviors of the Nitinol and composite matrix are demonstrated, which have significant implications for modeling of SMAHC structures.

Turner, Travis L.↗

Thermomechanical Properties of Neutron Irradiated Al 3 Hf-Al Thermal Neutron Absorber Materials

A thermal neutron absorber material composed of Al 3 Hf particles in an aluminum matrix is under development for the Advanced Test Reactor. This metal matrix composite was fabricated via hot pressing of high-purity aluminum and micrometer-size Al 3 Hf powders at volume fractions of 20.0, 28.4, and 36.5%. Room temperature tensile and hardness testing of unirradiated specimens revealed a linear relationship between volume fraction and strength, while the tensile data showed a strong decrease in elongation between the 20 and 36.5% volume fraction materials. Tensile tests conducted at 200 °C on unirradiated material revealed similar trends. Evaluations were then conducted on specimens irradiated at 66 to 75 °C to four dose levels ranging from approximately 1 to 4 dpa. Tensile properties exhibited the typical increase in strength and decrease in ductility with dose that are common for metallic materials irradiated at ≤0.4T m . Hardness also increased with neutron dose. The difference in strength between the three different volume fraction materials was roughly constant as the dose increased. Nanoindentation measurements of Al 3 Hf particles in the 28.4 vol% material showed the expected trend of increased hardness with irradiation dose. Transmission electron microscopy revealed oxygen at the interface between the Al 3 Hf particles and aluminum matrix in the irradiated material. Scanning electron microscopy of the exterior surface of tensile tested specimens revealed that deformation of the material occurs via plastic deformation of the Al matrix, cracking of the Al 3 Hf particles, and to a lesser extent, tearing of the matrix away from the particles. The fracture surface of an irradiated 28.4 vol% specimen showed failure by brittle fracture in the particles and ductile tearing of the aluminum matrix with no loss of cohesion between the particles and matrix. The coefficient of thermal expansion decreased upon irradiation, with a maximum change of –6.3% for the annealed irradiated 36.5 vol% specimen.

36 MATERIALS SCIENCE↗

Evaluation of Additively Manufactured Monolithic SiC and SiC Ceramic Matrix Composites for CSP- Fabrication and Testing of Receiver Design Feature Specimens in a Simulating Lab Test via Laser Heating

Critical to the creation of a multi-component SiC receiver design concept capable of meeting the SETO CST cost goal objectives of <$150/kWth is the optimal utilization of material for solar absorption and heat transfer to transport fluid. This is to maximize the solar-thermal efficiency in the techno-economic analysis of derived use case. As a first step in preparation of sub-component design for on-sun test evaluations we use different proposed SiC absorber element in a customized laser heat flux test to assess an effective heat transfer coefficient characteristic of the design. The test results are analyzed to extract the effective heat transfer coefficient, thus enable optimization of the geometry of receiver components for heat transfer, efficiency attributes and the thermo-structural management of the components. High intensity CO2 laser is used in combination with air flow through the test specimen to assess the effective heat transfer coefficient under heat flux conditions corresponding to high solar concentrations in the range of 1000-2000 suns.

14 SOLAR ENERGY↗

Thermal-structural panel buckling tests

A titanium-matrix-composite (TMC) hat-stiffened panel of 61 cm sq area and 3.175 cm thick was nondestructively tested to 649 C to examine its buckling characteristics. Compressive loads were applied to the panel in a 978.6 kN uniaxial load frame system. High-temperature testing was performed using quartz lamp heating. A single-strain-age force/stiffness buckling prediction technique was developed to predict panel buckling loads. For the monolithic panel, these test predictions correlated within 10 percent with a finite-element buckling analyses performed elsewhere. Comparisons between force/stiffness predictions and analyses for the TMC panel are in progress.

Thompson, Randolph C.↗

Catalytic combustion of heavy partially-vaporized fuels

An experimental program to demonstrate efficient catalytic combustion of fuel-lean and fuel-rich mixtures of residual fuel and air, and to assess the influence of incomplete fuel vaporization on the performance of a catalytic reactor is being conducted. A 7.5-cm diameter catalytic reactor was designed and will be tested over a matrix of conditions representative of a gas turbine combustor inlet. For each of three test phases, two series of tests with a uniform but poorly vaporized (less than 50 percent) mixture of No. 6 fuel oil and air will be performed. In the first series, the non-vaporized fuel will be contained in a spray of droplets with a Sauter Mean Diameter (SMD) less than 30 microns. In the second series, the non-vaporized fuel will be characterized by a spray SMD approximately equal to 100 microns. The designs of the fuel injection system and the catalytic reactor are described in this paper.

Rosfjord, T. J.↗

Fatigue Life Methodology for Bonded Composite Skin/Stringer Configurations

A methodology is presented for determining the fatigue life of composite structures based on fatigue characterization data and geometric nonlinear finite element (FE) analyses. To demonstrate the approach, predicted results were compared to fatigue tests performed on specimens which represented a tapered composite flange bonded onto a composite skin. In a first step, tension tests were performed to evaluate the debonding mechanisms between the flange and the skin. In a second step, a 2D FE model was developed to analyze the tests. To predict matrix cracking onset, the relationship between the tension load and the maximum principal stresses transverse to the fiber direction was determined through FE analysis. Transverse tension fatigue life data were used to -enerate an onset fatigue life P-N curve for matrix cracking. The resulting prediction was in good agreement with data from the fatigue tests. In a third step, a fracture mechanics approach based on FE analysis was used to determine the relationship between the tension load and the critical energy release rate. Mixed mode energy release rate fatigue life data were used to create a fatigue life onset G-N curve for delamination. The resulting prediction was in good agreement with data from the fatigue tests. Further, the prediction curve for cumulative life to failure was generated from the previous onset fatigue life curves. The results showed that the methodology offers a significant potential to Predict cumulative fatigue life of composite structures.

Krueger, Ronald↗

Fibre-matrix bond strength studies of glass, ceramic, and metal matrix composites

An indentation test technique for compressively loading the ends of individual fibers to produce debonding has been applied to metal, glass, and glass-ceramic matrix composites; bond strength values at debond initiation are calculated using a finite-element model. Results are correlated with composite longitudinal and interlaminar shear behavior for carbon and Nicalon fiber-reinforced glasses and glass-ceramics including the effects of matrix modifications, processing conditions, and high-temperature oxidation embrittlement. The data indicate that significant bonding to improve off-axis and shear properties can be tolerated before the longitudinal behavior becomes brittle. Residual stress and other mechanical bonding effects are important, but improved analyses and multiaxial interfacial failure criteria are needed to adequately interpret bond strength data in terms of composite performance.

Grande, D. H.↗

Pendulum impact resistance of tungsten fiber/metal matrix composites.

The impact properties of copper, copper-10 nickel, and a superalloy matrix reinforced with tungsten fibers were studied. In most cases the following increased composite impact strength: increased fiber or matrix toughness, decreased fiber-matrix reaction, increased test temperature, hot working and heat treatment. Notch sensitivity was reduced by increasing fiber or matrix toughness. The effect of fiber content depended on the relative toughness of the fibers and matrix. Above 530 K a 60 volume per cent superalloy matrix composite had a greater impact strength than a turbine blade superalloy, whereas below 530 K a hot worked 56 volume per cent composite had a greater impact strength than the superalloy.

Winsa, E. A.↗

Compression creep of graphite/epoxy laminates monitored using moire interferometry

Uniaxial compressive creep loadings were applied for ten hours to various graphite/epoxy laminates with a hole. All tests were performed at room temperatures. In-plane displacements were monitored using moire interferometry. Moire fringe patterns were reduced to in-plane strain fields numerically. The fiber-dominated laminates tested exhibited little or no viscoelastic behavior during the ten hour period. Conversely, the matrix-dominated laminates tested did exhibit viscoelastic behavior during the ten hour test time.

Tuttle, M. E.↗

Fatigue behavior of continuous fiber silicon-carbide-aluminum composites

Four lay-ups of continuous fiber silicon carbide (SCS2) fiber/aluminum matrix composites were tested to assess fatigue mechanisms including stiffness loss when cycled below their respective fatigue limits. The lay-ups were 0 (sub 8), 0(sub 2)/ + or - 45 (sub 2s), 0/90 (sub 2s),and 0/ + or 45/90 (subs). The data were compared with predictions from the author's previously published shakedown model which predicts fatigue-induced stiffness loss in metal matrix composites. A fifth lay-up, + or - 45 (sub 2s), was tested to compare shakedown and fatigue limits. The particular batch of silicon-carbide fibers tested in this program had a somewhat lower modulus (340 GPa) than expected and displayed poor bonding to the aluminum matrix. Good agreement was obtained between the stiffness loss model and the test data. The fatigue damage below the fatigue limit was primarily in the form of matrix cracking. The fatigue limit corresponded to the laminate shakedown for the + or - 45 (sub 2s) laminate.

Johnson, W. S.↗