Phase Transfer‐Mediated Degradation of Ether‐Based Localized High‐Concentration Electrolytes in Alkali Metal Batteries

Abstract Localized high‐concentration electrolytes (LHCEs) have attracted interest in alkali metal batteries due to the advantages of forming stable solid‐electrolyte interphases (SEIs) on anodes and good chemical/electrochemical stability. Herein, a new degradation mechanism is revealed for ether‐based LHCEs that questions their compatibility with alkali metal anodes (Li, Na, and K). Specifically, the ether solvent reacts with alkali metals to generate solvated electrons (e s − ) that attack hydrofluoroether co‐solvents to form a series of byproducts. The ether solvent essentially acts as a phase‐transfer reagent that continuously transfers electrons from solid‐phase metals into the solution phase, thus inhibiting the formation of stable SEI and leading to continuous alkali metal corrosion. Switching to an ester‐based solvating solvent or intercalation anodes such as graphite or molybdenum disulfide has been shown to avoid such a degradation mechanism due to the absence of e s − .

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Degradation Mechanisms of High Capacity 18650 Cells Containing Si-Graphite Anode and Nickel-Rich NMC Cathode

Application of advanced anode and cathode materials in commercial lithium-ion batteries is attracting attention due to their high capacity. Silicon (Si)/graphite anodes and nickel (Ni)-rich lithium nickel manganese cobalt oxide with layered structures have been paired in commercial 18650 high energy density cells (~270 Wh/kg). It is crucial to investigate the cell performance and the aging behavior of this commercial cell. In this study, we present commercial cell degradation mechanisms by comparing fresh and aged electrodes, including changes of crystal structure, morphology, elemental composition, and electrochemical properties. The quantitative analysis was done based on dV/dQ incremental capacity analysis of 18650 cells. To determine the amount of cyclable lithium ions (Li + ) and active material loss, the lithiation and delithiation capacity were compared for fresh and aged electrodes in half coin cells. Results showed that even with 5% (by mass) of Si added in the anode, cracks occurred across the anode leading to contact loss and thickening of the solid electrolyte interphase (SEI) layer. Additionally, the average fluorine (F) ratio of the aged anodes was higher compared to that of the fresh anodes. More severely, the F content on the Si aggregations on aged anodes increased to as high as 5 times that of the fresh anode, indicating SEI growth, especially on Si particles. Solid 7 Li nuclear magnetic resonance results showed no detectable Li metal deposition on the aged anode. On the cathode side, cracks on the primary particle interfaces contributed to cathode material loss, contact loss, and impedance rise. Furthermore, Li + loss into the thickened SEI layer, particle cracking, and impedance rise are the main reasons behind cell degradation.

25 ENERGY STORAGE↗

Effects of fluorinated solvents on electrolyte solvation structures and electrode/electrolyte interphases for lithium metal batteries

Electrolyte is very critical to the performance of the high-voltage lithium (Li) metal battery (LMB), which is one of the most attractive candidates for the next generation high-density energy storage systems. Electrolyte formulation and structure determine the physical properties of the electrolytes and their interfacial chemistries on the electrode surfaces. Localized high-concentration electrolytes (LHCEs) outperform state-of-the-art carbonate electrolytes in many aspects in LMBs due to their unique solvation structure. Types of fluorinated co-solvents used in LHCEs are investigated here in searching for the most suitable diluent for high concentration electrolytes (HCEs). Non-solvating solvents (including fluorinated ethers, fluorinated borate and fluorinated orthoformate) added in HCEs enable the formation of LHCEs with high-concentration solvation structures. However, low solvating fluorinated carbonate will coordinate with Li+ ions and form a second solvation shell or a pseudo-LHCE which diminishes the benefits of LHCE. In addition, it is evident that the diluent has significant influence on the electrode/electrolyte interphases (EEIs) beyond retaining the high-concentration solvation structures. Diluent molecules surrounding the high-concentration clusters could accelerate or decelerate the anion decomposition through co-participation of diluent decomposition in the EEI formation. The varied interphase features lead to significantly different battery-performance. This study points out the importance of diluents and their synergetic effects with the conductive salt and the solvating solvent in designing LHCEs. These systematic comparisons and fundamental insights into LHCEs using different types of fluorinated solvents can guide further development of advanced electrolytes for high-voltage LMBs.

Cao, Xia↗

Highly efficient interface stabilization for ambient-temperature quasi-solid-state sodium metal batteries

Solid-state sodium (Na) batteries (SSSBs) using sulfide-based solid electrolytes (SSEs) hold tremendous promise due to their high theoretical specific capacity, enhanced safety and abundant resources. However, detrimental interfacial issues between SSEs and Na metal present a major challenge to the advancement of sulfide-based SSSBs. To address interfacial issues, we demonstrate an efficient approach by incorporating an ionic liquid electrolyte ((PYR/Na)TFSI) as interlayer to stabilize the Na metal/SSE interface. The presence of the (PYR/Na)TFSI interlayer enables the formation of a stable solid electrolyte interphase (SEI) to prevent the harmful reactions and inhibit Na dendrites. Combination of ab initio molecular dynamics simulations and X-ray photoelectron spectroscopy revealed that this stable SEI is largely composed of reduced products of TFSI -, such as NaF and CF 3 . As a result, the symmetric cells exhibited stable Na plating/striping cycling for 300 h at 0.1 mA cm -2 . In addition, FeS2||Na quasi-solid-state batteries delivered an impressive specific capacity of over 300 mAh g -1 under the current density of 20 mA g -1 at room temperature. Under a higher current density (100 mA g -1 ), such batteries performed with long-term cycling stability and maintained a specific capacity of around 103 mAh g -1 after 330 cycles. This work demonstrates the novel perspective of using an ionic liquid interlayer to address interfacial issues, contributing to the advancement of high-performance SSSBs for the next-generation energy storage systems.

25 ENERGY STORAGE↗

Trace LiBF 4 Enabling Robust LiF-Rich Interphase for Durable Low-Temperature Lithium-Ion Pouch Cells

Lithium-ion batteries (LIBs) with electrolytes containing lithium tetrafluoroborate (LiBF 4 ) can achieve large capacity retention under low temperature, but the accompanying rapid capacity decay inhibits commercialization. Here, in this study, the impact of LiBF 4 as a supplemental salt to LiPF 6 is systematically investigated using low ethylene carbonate (EC)-content electrolytes, along with a low-melting-point cosolvent. It is found that rational adjustment of the amount of LiBF 4 could not only regulate the interactions of anions and solvents in Li + solvation sheaths but also tune the composition and morphology of solid electrolyte interphase (SEI). It is worth noting that electrolytes with trace amount of LiBF 4 (0.05 M) show synergetic interaction between PF 6 - and Li + and decreased interaction between EC and Li + , achieving a dense and LiF-rich SEI, which enables a 200 mAh pouch cell with less gas generation, long-lived cycling, and higher low-temperature capacity, simultaneously. This work provides new insight into utilizing trace LiBF 4 for stable interface construction of durable low-temperature LIBs.

25 ENERGY STORAGE↗

AlF 3 Surface-Coated Li[Li 0.2 Ni 0.17 Co 0.07 Mn 0.56 ]O 2 Nanoparticles with Superior Electrochemical Performance for Lithium-Ion Batteries

For Li-rich layered cathode materials considerable attention has been paid owing to their high capacity performance for Li-ion batteries (LIBs). In our work, layered Li-rich Li[Li 0.2 Ni 0.17 Co 0.07 Mn 0.56 ]O 2 nanoparticles are surface-modified with AlF 3 through a facile chemical deposition method. The AlF 3 surface layers have little impact on the structure of the material and act as buffers to prevent the direct contact of the electrode with the electrolyte; thus, they enhance the electrochemical performance significantly. The 3 wt% AlF 3 -coated Li-rich electrode exhibits the best cycling capability and has a considerably enhanced capacity retention of 83.1% after 50 cycles. Moreover, the rate performance and thermal stability of the 3 wt% AlF3-coated electrode are also clearly improved. Finally, surface analysis indicates that the AlF 3 coating layer can largely suppress the undesirable growth of solid electrolyte interphase (SEI) film and, therefore, stabilizes the structure upon cycling.

25 ENERGY STORAGE↗

Electrolyte materials - Issues and challenges

Electrolytes are vital components of an electrochemical energy storage device. They are usually composed of a solvent or mixture of solvents and a salt or a mixture of salts which provide the appropriate environment for ionic conduction. One of the main issues associated with the selection of a proper electrolyte is that its electronic properties have to be such that allow a wide electrochemical window - defined as the voltage range in which the electrolyte is not oxidized or reduced - suitable to the battery operating voltage. In addition, electrolytes must have high ionic conductivity and negligible electronic conductivity, be chemically stable with respect to the other battery components, have low flammability, and low cost. Weak stability of the electrolyte against oxidation or reduction leads to the formation of a solid-electrolyte interphase (SEI) layer at the surface of the cathode and anode respectively. Depending on the materials of the electrolyte and those of the electrode, the SEI layer may be composed by combinations of organic and inorganic species, and it may exert a passivating role. In this paper we discuss the current status of knowledge about electrolyte materials, including non-aqueous liquids, ionic liquids, solid ceramic and polymer electrolytes. We also review the basic knowledge about the SEI layer formation, and challenges for a rational design of stable electrolytes.

25 ENERGY STORAGE↗

Multimodal quantification of degradation pathways during extreme fast charging of lithium-ion batteries

Enabling fast charging of Li-ion batteries will be a key step towards realizing the technology's full potential in electric vehicles. Currently, fast charging is limited by a variety of processes that reduce cell capacity upon extended cycling. Using a multimodal approach combining incremental capacity analysis (dQ/dV), high energy X-ray diffraction (HEXRD), and mass spectrometry titration (MST), we identify specific degradation mechanisms—including Li plating, dead Li x C 6 formation, Li 2 C 2 formation, solid carbonate solid-electrolyte interphase (SEI) deposition, and loss of positive electrode active material (LAM PE )—that occur during extended fast charge cycling. We find that Li plating is the major source of capacity loss in cells cycled at 6C, while non-carbonate SEI species deposition on the graphite anode is the main source of capacity loss when cycled at 4C. We also study local degradative phenomena by examining specific ~1–5 cm 2 regions of the cells using HEXRD and MST. Here, we find that plated Li is often collocated with dead Li x C 6 , Li 2 C 2 , and solid carbonate SEI species, and these additional species cumulatively account for ~20% of the capacity lost during 6C cycling. Finally, in a cell with an anomalously high amount of LAM PE (quantified via dQ/dV), we find that regions of cathode degradation were accompanied by non-carbonate SEI products on the adjacent region of the anode. We postulate that this phenomenon arises due to crosstalk between the electrodes, wherein soluble electrolyte oxidation products formed at the delithiated cathode migrate to the graphite anode and are ultimately deposited on the graphite surface. This work demonstrates the utility of combining multiple characterization techniques to reveal a more holistic understanding of degradative phenomena that occur across multiple length scales during fast charge.

25 ENERGY STORAGE↗

Uniform High Ionic Conducting Lithium Sulfide Protection Layer for Stable Lithium Metal Anode

Artificial solid-electrolyte interphase (SEI) is one of the key approaches in addressing the low reversibility and dendritic growth problems of lithium metal anode, yet its current effect is still insufficient due to insufficient stability. Here, a new principle of “simultaneous high ionic conductivity and homogeneity” is proposed for stabilizing SEI and lithium metal anodes. Fabricated by a facile, environmentally friendly, and low-cost lithium solid-sulfur vapor reaction at elevated temperature, a designed lithium sulfide protective layer successfully maintains its protection function during cycling, which is confirmed by both simulations and experiments. Stable dendrite-free cycling of lithium metal anode is realized even at a high areal capacity of 5 mAh cm -2 , and prototype Li–Li 4 Ti 5 O 12 cell with limited lithium also achieves 900 stable cycles. These findings give new insight into the ideal SEI composition and structure and provide new design strategies for stable lithium metal batteries.

25 ENERGY STORAGE↗

Composite Solid Ion Conductor with Engineered Lithium Interface

Successful widespread commercialization of electric vehicles is contingent upon development of safe high energy density batteries capable of long cycle life. Lithium metal affords the highest theoretical capacity (3,860 mAh/g) and lowest electrochemical potential (-3.04V vs SHE), which offers the highest specific energy density of anode materials today. While Li-ion batteries are capable of delivering energy densities of 400-600 Wh/kg, the development of lithium metal batteries such as Li-S and Li-air may boost this number up to 650 and 950 Wh/kg, respectively. However, significant progress towards the passivation of lithium metal must occur before the energy density benefit can be realized. Issues with lithium dendrite formation, anode volume expansion, and continuous solid electrolyte interphase (SEI) build-up often result in significant safety concerns, high cell resistance, and poor cycle life. The intrinsic high reactivity between lithium metal with conventional lithium ion electrolytes (organic carbonate-based solvents) makes it extremely difficult to overcome these problems. In this project, Wildcat performed focused, fundamental research and development on composite polymer/ceramic electrolytes and protected lithium metal anodes to develop an all solid state lithium metal battery targeting the DOE requirements to enable commercialization. Wildcat successfully leveraged its high throughput battery platform and explored a broad composite electrolyte compositional space. Additionally, Wildcat screened large numbers of inorganic and organic coatings for lithium metal protection using in situ liquid methods and translated the best results to all solid cells. The proposed composite polymer/ceramic electrolyte and a protected lithium metal anode enabled a solid-state lithium metal battery. The ultimate targets from this effort will deliver a safe all solid-state lithium metal pouch cell with over 350 Wh/kg and over 1,000 cycles (C/3) with the cost estimate below $100/kWh. During the course of the project, we demonstrated stable cycling of 10’s of cycles with the composite SSE and our protected lithium. The work has continued after the conclusion of the DOE funding, demonstrating further improvements in catholyte composition and thinner composite solid electrolytes.

25 ENERGY STORAGE↗

Insights into Reactivity of Silicon Negative Electrodes: Analysis Using Isothermal Microcalorimetry

Silicon offers high theoretical capacity as a negative electrode material for lithium-ion batteries; however, high irreversible capacity upon initial cycling and poor cycle life have limited commercial adoption. Herein, we report an operando isothermal microcalorimetry (IMC) study of a model system containing lithium metal and silicon composite film electrodes during the first two cycles of (de)lithiation. The total heat flow data are analyzed in terms of polarization, entropic, and parasitic heat flow contributions to quantify and determine the onset of parasitic reactions. These parasitic reactions, which include solid–electrolyte interphase formation, contribute to electrochemical irreversibility. Cycle 1 lithiation demonstrates the highest thermal energy output at 1509 mWh/g, compared to cycle 1 delithiation and cycle 2. To complement the calorimetry, operando X-ray diffraction is used to track the phase evolution of silicon. During cycle 1 lithiation, crystalline Si undergoes transformation to amorphous lithiated silicon and ultimately to crystalline Li 15 Si 4 . The solid-state amorphization process is correlated to a decrease in entropic heat flow, suggesting that heat associated with the amorphization contributes significantly to the entropic heat flow term. In conclusion, this study effectively uses IMC to probe the parasitic reactions that occur during lithiation of a silicon electrode, demonstrating an approach that can be broadly applied to quantify parasitic reactions in other complex systems.

25 ENERGY STORAGE↗

Isothermal Microcalorimetry: Insight into the Impact of Crystallite Size and Agglomeration on the Lithiation of Magnetite, Fe 3 O 4

Magnetite, Fe 3 O 4 , holds significant interest as a Li-ion anode material because of its high theoretical capacity (926 mAh/g) associated with multiple electron transfers per cation center. Notably, both crystallite size and agglomeration influence ion transport. This report probes the effects of crystallite size (12 and 29 nm) and agglomeration on the reactions involved with the formation of the surface electrolyte interphase on Fe 3 O 4 . Isothermal microcalorimetry (IMC) was used here to determine the parasitic heat evolved during lithiation by considering the total heat measured, cell polarization, and entropic contributions. Interestingly, the 29 nm Fe 3 O 4 -based electrodes produced more parasitic heat than the 12 nm samples (1346 vs 1155 J/g). This observation was explored using scanning electron microscopy (SEM) and X-ray fluorescence (XRF) mapping in conjunction with spatially resolved X-ray absorption spectroscopy (XAS). SEM imaging of the electrodes revealed more agglomerates for the 12 nm material, affirmed by XRF maps. Further, XAS results suggest that Li + transport is more restricted for the smaller crystallite size (12 nm) material, attributed to its greater degree of agglomeration. These results rationalize the IMC data, where agglomerates of the 12 nm material limit solid electrolyte interphase formation and parasitic heat generation during lithiation of Fe 3 O 4 .

25 ENERGY STORAGE↗

Phase Transfer‐Mediated Degradation of Ether‐Based Localized High‐Concentration Electrolytes in Alkali Metal Batteries

Abstract Localized high‐concentration electrolytes (LHCEs) have attracted interest in alkali metal batteries due to the advantages of forming stable solid‐electrolyte interphases (SEIs) on anodes and good chemical/electrochemical stability. Herein, a new degradation mechanism is revealed for ether‐based LHCEs that questions their compatibility with alkali metal anodes (Li, Na, and K). Specifically, the ether solvent reacts with alkali metals to generate solvated electrons (e s − ) that attack hydrofluoroether co‐solvents to form a series of byproducts. The ether solvent essentially acts as a phase‐transfer reagent that continuously transfers electrons from solid‐phase metals into the solution phase, thus inhibiting the formation of stable SEI and leading to continuous alkali metal corrosion. Switching to an ester‐based solvating solvent or intercalation anodes such as graphite or molybdenum disulfide has been shown to avoid such a degradation mechanism due to the absence of e s − .

Chen, Xiaojuan↗

Stabilized Electrode/Electrolyte Interphase by a Saturated Ionic Liquid Electrolyte for High-Voltage NMC532/Si-Graphite Cells

Nonaqueous electrolyte has become one of the technical barriers in enabling Li-ion battery comprising of a high voltage cathode and high capacity anode. Here, we demonstrate a saturated piperidinum bis(fluorosulfonyl)imide ionic liquid (IL) with a LiFSI salt not only supports the redox reaction on the cathode at high voltages, but also shows exceptional kinetic stability on the lithiated anode as evidenced by its improved cycling performance in a NMC532/Si-graphite full cells cycled between 4.6 and 3.0 V. On the basis of the spectroscopic/microscopic analysis and molecular dynamics (MD) simulations, the superior performance of the cells is attributed to the formation of solid-electrolyte-interphase on both electrode as well as unique solvation structure where a deadlocked coordination network is established at the saturated state, which prevents transition metal dissolution into the electrolyte via a solvation process.

25 ENERGY STORAGE↗

Designer interphases for the lithium-oxygen electrochemical cell

An electrochemical cell based on the reversible oxygen reduction reaction: 2Li+ + 2e- + O2 ↔ Li2O2, provides among the most energy dense platforms for portable electrical energy storage. Such Lithium-Oxygen (Li-O2) cells offer specific energies competitive with fossil fuels and are considered promising for electrified transportation. Multiple, fundamental challenges with the cathode, anode, and electrolyte have limited practical interest in Li-O2 cells because these problems lead to as many practical shortcomings, including poor rechargeability, high overpotentials, and specific energies well below theoretical expectations. We create and study in-situ formation of solid-electrolyte interphases (SEIs) based on bromide ionomers tethered to a Li anode that take advantage of three powerful processes for overcoming the most stubborn of these challenges. The ionomer SEIs are shown to protect the Li anode against parasitic reactions and also stabilize Li electrodeposition during cell recharge. Bromine species liberated during the anchoring reaction also function as redox mediators at the cathode, reducing the charge overpotential. Finally, the ionomer SEI forms a stable interphase with Li, which protects the metal in high Gutmann donor number liquid electrolytes. Such electrolytes have been reported to exhibit rare stability against nucleophilic attack by Li2O2 and other cathode reaction intermediates, but also react spontaneously with Li metal anodes. We conclude that rationally designed SEIs able to regulate transport of matter and ions at the electrolyte/anode interface provide a promising platform for addressing three major technical barriers to practical Li-O2 cells.

25 ENERGY STORAGE↗

Polar polymer–solvent interaction derived favorable interphase for stable lithium metal batteries

Lithium metal has long been regarded as one of the most promising anode materials for future rechargeable batteries. However, the severe reaction of Li with carbonate electrolytes and the rapid growth of Li-dendrites at high current densities hinder its practical application in Li-metal batteries. In this work, we report a polar polymer protective layer to suppress highly corrosive cyclic carbonates by tuning polymer–solvent interactions. The C≡N groups of polyacrylonitrile (PAN) polymer chains in the polar polymer network can effectively reduce high reactivity of the C=O groups of carbonate solvents leading to a stable solid electrolyte interphase (SEI) layer with higher inorganic components. In situ optical and electron microscopes demonstrate that the polar polymer network effectively restrained the formation and growth of Li-dendrites, which helps to stabilize the plating/stripping behavior of Li in a symmetric Li|Li cell and a Li|LiNi 1/3 Co 1/3 Mn 1/3 O 2 cell. This study provides a useful perspective of controlling electrolyte coordination to form a stable SEI layer in carbonate electrolytes for Li-metal batteries.

25 ENERGY STORAGE↗