The ternary antimonide CeIrSb absorbs hydrogen under moderate temperature and pressure conditions (4 MPa and 573 K), leading to the hydride CeIrSbH{sub 0.8}. The crystal structures of both compounds have been investigated by X-ray diffraction on powders and single crystals: TiNiSi type, space group Pnma, a=735.07(7), b=456.93(4), c=792.8(1) pm, R1/wR2=0.0206/0.0395, 601 F{sup 2} values for CeIrSb and a=728.16(14), b=460.35(6), c=825.87(2) pm, R1/wR2=0.0322/0.0735, 528 F{sup 2} values for CeIrSbH{sub 0.8} with 20 variables per refinement. Hydrogenation induces both an increase of the cell volume V (+4%) and a strongly anisotropic expansion of the unit cell with a maximum of 4.3% in the c direction, leading to a significant increase of the Ce-Ir and Ce-Ce distances in this direction. The H-insertion into CeIrSb leads to a magnetic transition from intermediate valence to antiferromagnetic behavior (T{sub N}=7.0 K) evidenced by magnetization, electrical resistivity and specific heat measurements. This transition can be explained on the basis of the Doniach diagram considering the J{sub cf} interaction between the 4f(Ce) and conduction electrons. - Graphical Abstract: Cerium coordination in CeIrSb and CeIrSbH{sub 0.8}.
37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗