Processing and crystallographic structure of non-equilibrium Si-doped HfO[subscript 2]
Abstract not provided
SEARCH · Engineering Papers
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Abstract not provided
Nanostructured titania have been successfully synthesized by hydrolysis of alkoxide at calcination temperatures 500 °C, 600 °C and 700 °C. As the calcination temperature increases, alcohol washed samples show lesser rutile content as compared to water washed samples. Morphology and Particle sizes was determined by field emission scanning electron microscopy (FESEM), while thermogravimetric-differential scanning calorimetry (TG-DSC) was used to determine thermal stability. Alcohol washed samples undergo 30% weight loss whereas 16% in water washed samples was observed. The mean particle sizes were found to be increase from 37 nm to 100.9 nm and 35.3 nm to 55.2 nm for water and alcohol washed samples respectively. Hydrolysis of alkoxide was shown to be an effective means to prepare thermally stable titania by using alcohol washed samples as a precursor.
We investigate the ionization and displacement effects of an electron-beam (e-beam) on amorphous Gd{sub 2}Zr{sub 2}O{sub 7} synthesized by the co-precipitation and calcination methods. The as-received amorphous specimens were irradiated under electron beams at different energies (80 keV, 120 keV, and 2 MeV) and then characterized by X-ray diffraction and transmission electron microscopy. A metastable fluorite phase was observed in nanocrystalline Gd{sub 2}Zr{sub 2}O{sub 7} and is proposed to arise from the relatively lower surface and interface energy compared with the pyrochlore phase. Fast crystallization could be induced by 120 keV e-beam irradiation (beam current = 0.47 mA/cm{sup 2}). The crystallization occurred on the nanoscale upon ionization irradiation at 400 °C after a dose of less than 10{sup 17} electrons/cm{sup 2}. Under e-beam irradiation, the activation energy for the grain growth process was approximately 10 kJ/mol, but the activation energy was 135 kJ/mol by calcination in a furnace. The thermally activated ionization process was considered the fast crystallization mechanism.
Nanostructure anatase and rutile type TiO{sub 2} were synthesized from dissolution roasted ilmenite from natural ilmenite sand as the starting materials. Anatase TiO{sub 2} and rutile TiO{sub 2} (high crystallinity) with the diameters of 20–100 nm were obtained by calcined soluble ilmenite sand produced by leaching process. Calcinations of the xerogel TiO{sub 2} from liquor products were conducted for 4 hours at temperature of 450 °C. The samples were characterized by XRD (X-ray diffraction), STA (simultant thermal analysis), TEM (Transmission Electron Microscopy), and BET surface area. Titania Anatase-Rutile form as a mixture were produced by titania slag with the hydrolysis product. While, in another route, complete titania anatase phase was produced through hydrolysis and condensation steps of leach liquors. This synthesis methods provide a simple route to fabricate nanostructure TiO{sub 2} from low cost material.
In this present work, CaCu{sub 3}Ti{sub 4}O{sub 12} (CCTO) was synthesized by conventional solid-state reaction technique. The synthesis process was carried out in two phases; by conventional process (calcination and sintering at 1080°C for 10 hours) and phase II involves the micro assisted pre sintering of conventionally calcined CCTO for very short soaking time of 30 min at 1080°C in a microwave furnace followed by sintering at 1080°C for 10 hours in conventional furnace. X-ray diffraction (XRD) patterns confirmed the formation of single phase ceramic. Dielectric properties were studied over the frequency range from 50Hz -5MHz at temperatures (273K-343K). It was observed that pre- microwave sintering enhance the dielectric constant values from 10900 to 11893 and respectively reduces the dielectric loss values from 0.49 to 0.34 at room temperature(1 KHz). CCTO ceramics which are found desirable for many technological applications. The effect is more pronounced at low frequencies of applied electric field.
Polycrystalline samples of La{sub 0.67}Sr{sub 0.33}Mn{sub 0.65}Fe{sub 0.35}O{sub 3} (LSMFO) were synthesized using the standard ball mill method with different calcination temperatures ranging from 800 to 1100°C for 7 h. The phase purity of these samples was confirmed using X-ray diffraction (XRD) patterns. All samples were found to have rhombohedral crystal structure with R 3-bar c space group. The lattice parameters, cell volume, bond angle and bond length have been obtained using the Rietveld refinement by FullProf software. The average crystallite size calculated using the Debye-Scherrer formula was found between 27 and 60 nm. Surface morphology of the prepared samples has been examined using a scanning electron microscope (SEM). SEM images show the formation of well-arranged grain sizes distributed from 240 to 400 nm, much larger than one estimated using the Scherrer formula. All tiny particles are highly agglomerated with the increasing temperature and porosity decreases with increasing temperature. An analysis of the frequency and peak broadening of Raman modes as a function of temperature clearly shows the significant temperature effect on the A{sub 1g} and E{sub g} modes of LSMFO. The shifts and broadening of the A{sub 1g} and E{sub g} modes are discussed in light of the oxygen sublattice distortion. Our study shows the reduction in distortion with increasing calcination temperature, which suggests a decrease in the JT effect.
These are a set of slides intended for an information session as part of recruiting activities at Brigham Young University. It gives an overview of aqueous chloride operations, specifically on plutonium and americium purification/recovery. This presentation details the steps taken perform these processes, from plutonium size reduction, dissolution, solvent extraction, oxalate precipitation, to calcination. For americium recovery, it details the CLEAR (chloride extraction and actinide recovery) Line, oxalate precipitation and calcination.
The project objective was to demonstrate scaled production of high purity rare earth oxides (REO), nominally exceeding 90% grade, from coal refuse sources using innovative technologies that reduce cost and improve environmental outcomes relative to traditional rare earth processing technologies. The project utilized a critical material pilot plant constructed and tested as part of a previous U.S. Department of Energy project. Target performance criteria was a 50% reduction in production cost based on previous optimum values, 150% increase in recovery and greater than 2% concentrates of rare earth oxides, cobalt and manganese. Concentrate production goals were to produce a rare earth mix oxide product at a rate of 200 grams per day having a minimum purity of 50% as well as products of cobalt and manganese having a minimum purity of 2%. A previous pilot plant investigation identified acid cost as the major contributor to an operating cost that made the recovery of rare earth and other critical metals from bituminous coal sources economically challenging. As such, acid cost reduction was a major target using bio-oxidation reactors to produce sulfuric acid from naturally occurring coal pyrite. Based on laboratory data, a bio-oxidation circuit was designed for the pilot plant to produce 7.5 l/min of acid using two 11-m3 (3000 gallon) reactors equipped with 40 hp aerators for air dispersion. The pilot-scale tests revealed that acid concentration equivalent to as high as 1.0 M sulfuric acid could be continuously produced. However, the bio-acid contained exceptionally high iron concentrations, which complicated downstream processing of the pregnant leach solution (PLS). A TEA of the bio-oxidation circuit showed that production cost was approximately $0.13 per kg acid equivalent if produced using a four-day retention time in the reactors. This value represents a 48% reduction from that of purchased bulk sulfuric acid. Calcination (or roasting) studies were conducted on coarse refuse from West Kentucky No. 13 and Fire Clay coal seam sources. The test results revealed the potential to increase recovery by nearly 100% using temperatures between 500°C to 700°C with light REE recovery value being the most improved. Acid baking of the calcined products using sulfuric acid at 250°C increased heavy rare earth recovery from around 40% to 80% while decreasing the acid requirements by over 50%. The existing pilot plant was upgraded for the pilot scale demonstration of REE and CM recovery. The primary feedstocks were West Kentucky No.13 and heap leach pregnant leach solution (PLS) while a secondary feedstock was a lignite waste material from a construction sand operation. The pilot scale operation started with PLS generation through leaching followed by iron and aluminum removal, nominally at 3.3 and 4.5 pH, respectively. Leaching lixiviants used for the test were industrial grade sulfuric acid or bio-acid generated at the pilot scale facility. For most of the tests, the solid feed rate was 200 lb/hr whereas lixiviant was added at 2 gpm to provide an optimal residence time of 45 minutes. Following the contaminant removal step, several different process schematics were tested with the goal of maximizing REE recovery and purity. In the first test, direct processing of aluminum precipitation raffinate for REE recovery using oxalic acid at pH 1.5 was investigated. Overall REE recovery was approximately 45%. Unfortunately, elevated calcium content in the PLS significantly impacted the RE-Oxide product grade. Similarly, high calcium content decreased both the product purity and grades of CM products. As such, a new flowsheet was tested with the same initial process schematic but different precipitation stages for REEs and CMs at pH 6.0 and 9.0, respectively. It was noted that the overlapping precipitation behavior of Co, Ni and Zn with REEs limited the applicability of this process schematic. While this change increased the RE-Oxide grade from 36% in the first test to 87%, the loss of critical metals to the REE cake and bypass of the REEs to the CM cake significantly impacted the recovery of both REEs and CMs. Therefore, the modified process flowsheet combined oxalic acid precipitation stage raffinate and redissolved CM cake filtrate to maximize both the recovery and purity of the products. Consequently, a RE-Oxide product with 85% purity and CM cakes with over 19% Co, 38% Ni, 14% Zn and 9% Mn content were generated with significantly higher recoveries. While the modified process flowsheet improved recoveries and grades, elemental losses observed in separate precipitation and redissolution losses inspired the adaptation of a single precipitation stage at pH 9.0 for both REEs and CMs. This change was anticipated to maximize the REE recovery while minimizing the costs associated with separated redissolution and processing stages. As expected, REE recovery in this new circuit arrangement was over 56% with a product grade of over 87% RE-Oxide content. Similarly, Co, Ni, Mn, and Zn recoveries of 54%, 40%, 67%, and 66%, respectively, were achieved. Unfortunately, the elevated calcium content present in the solution due to its precipitation at pH 9.0 caused a decrease in the CM cake quality. Therefore, the final process flowsheet involved the addition of calcium oxalate precipitation following the oxalic acid precipitation stage, which effectively eliminated calcium contamination of the CM products. Finally, the pilot scale experiments conducted using bio-acid achieved comparable REE leaching recoveries to the conventional sulfuric acid leaching. Elevated iron concentration in the solution caused the co-precipitation of REEs with the iron and aluminum cake, resulting in the REE losses. Furthermore, elevated iron content bypassing the iron and aluminum precipitation stages contaminated the metal sulfide and manganese cake, respectively. A techno-economic analysis was performed based on a commercial facility capable of treating 500 tph of coal-based material. The production cost for West Kentucky No. 13 coarse refuse material ranged from approximately $500-$700/kg of total rare earth oxide whereas the lignite source had significantly lower production cost of $100-$300/kg. The significant difference in cost was due to the easier leaching characteristics of the lignite material and the higher feed concentrations. All process scenarios resulted in a negative net present value (NPV). For the lignite feedstock, laboratory REE leach recovery values were about 30% higher than the pilot plant data. Using the lab leach results, a positive net present value was achieved and the production cost decreased from $100-$300 $/kg to less than $150/kg of total REO.
The thermal analysis of Fe{sub 8}(OOH){sub 16}Cl{sub 1.3} (Akaganeite-M) nanospindles prepared by the hydrolysis of FeCl{sub 3} solutions are determined by thermogravimetric analyses and differential scanning calorimetry (TG/DSC), in conjunction with field-emission scanning electron microscopy (FE-SEM), and X-ray diffraction (XRD). Different products are formed after Fe{sub 8}(OOH){sub 16}Cl{sub 1.3} nanospindles are calcined at different temperatures for 30 min in N{sub 2} atmosphere: Fe{sub 1.833}(OH){sub 0.5}O{sub 2.5} and magnetite obtained at 250 deg. C; pure magnetite (Fe{sub 3}O{sub 4}) obtained at 630 deg. C; and magnetite containing some iron nitrides (Fe{sub 2}N and Fe{sub 4}N) obtained at 800 deg. C. The calcination of Fe{sub 8}(OOH){sub 16}Cl{sub 1.3} provides a new method to prepare pure magnetite.
With 10 vitrification lines in operation (3 on WVP in Sellafield, 1 on AVM in Marcoule and 6 on AVH in La Hague), Sellafield Ltd and Areva NC benefit from the most in-depth experience worldwide in the vitrification of highly active liquors within a framework of commercial operations. Based on the two-step process design, using a calciner and an induction-heated hot melter, which was initially deployed in Marcoule in 1978, core vitrification equipment has been continuously improved by the independent development programmes of the two companies. In March 2005, Sellafield Ltd and Areva NC signed the Vitrification Assistance Program (hereafter referred to as VAP); a co-operative project lasting 4 years during which Areva NC is to share some areas of their experience and expertise with Sellafield Ltd. Now at the halfway point of this project, this paper summarises the work performed by the VAP team to date, highlighting the early benefits and lessons learned. The following points will be developed: - Equipment delivery and preparation for implementation on WVP - Training organization and dissemination to WVP teams - Lessons learned from the early changes implemented in operations (Calciner, Melter, Dust Scrubber and Primary off gas system), and initial feedback from the first campaign using a VAP equipped line. In conclusion: The vitrification process and technology implemented at Sellafield and at La Hague, based on the two-step process, have proved to be efficient in treating high active liquor of various types. Ten lines based on this principle have been successfully operated for more than 15 years in France and in the UK. The process has also been demonstrated to be sufficiently versatile to benefit from continuous improvement and development programmes. VAP, as a complete package to support vitrification technology and knowledge transfer from AREVA NC to Sellafield Ltd, has provided the framework for fruitful technical exchanges and discussions between the two companies. From equipment delivery to knowledge embedding within the WVP teams, both companies have worked hard together to respect the tight schedule of the contract, despite growing external constraints. This has been closely managed in order to achieve the best results for the VAP without jeopardizing the continuing production operations on both the Sellafield and La Hague sites. For future campaigns, WVP1 will be equipped with an automatic heating control system similar to the one used at La Hague (i.e. based on 4 kHz). This will facilitate the work of the WVP operators and finalise the conversion of WVP melter control systems from manual to automatic, meaning that the melters on all 3 lines will be automatically controlled. Further implementation of VAP equipment is also planned on the other lines. (authors)
The one-dimensional W-doped VO{sub 2} (M) solid solutions with a various doped content were successfully synthesized under hydrothermal condition and subsequent calcination for the first time, and physical-chemical and phase transformation character were explored, subsequently. DSC analyses displayed that the phase-transition temperature of VO{sub 2} (M) solid solution could be linearly tuned with the doped content. Promisingly, the one-dimensional W-doped VO{sub 2} (M) had a good thermochromic property. - Graphical Abstract: One-dimensional W-doped VO{sub 2} (M) solid solutions with a various doped content were synthesized under hydrothermal condition and subsequent calcination. The physical-chemical and phase transformation character were explored, subsequently.
We developed a facile synthetic route of porous cobalt oxide (Co{sub 3}O{sub 4}) nanorods via a microemulsion-based method in combination with subsequent calcination process. The porous structure was formed by controlled decomposition of the microemulsion-synthesized precursor CoC{sub 2}O{sub 4} nanorods without destruction of the original morphology. The as-prepared Co{sub 3}O{sub 4} nanorods, consisting of small nanoparticles with diameter of 80-150 nm, had an average diameter of 200 nm and a length of 3-5 {mu}m. The morphology and structure of synthesized samples were characterized by transmission electron microscopy and scanning electron microscopy. The phase and composition were investigated by X-ray powder diffraction and X-ray photoelectron spectroscopy. The optical property of Co{sub 3}O{sub 4} nanorods was investigated. Moreover, the porous Co{sub 3}O{sub 4} nanorods exhibited high electrochemical performance when applied as cathode materials for lithium-ion batteries, which gives them good potential applications. - Graphical abstract: The porous Co{sub 3}O{sub 4} nanorods synthesized via a microemulsion-based method in combination with subsequent calcination were applied in the negative electrode materials for lithium-ion batteries and exhibited high electrochemical performance.
Perovskite-type KTaO{sub 3} powder was synthesized by an alternative solid-state method at low temperature. Stoichiometric ammonium tantalum hydroxide, K{sub 2}C{sub 2}O{sub 4} and KF were mixed in water and then dried at room temperature. The crude product was formed by calcining the dried mixture at different temperatures. Pyrochlore-free KTaO{sub 3} powder was successfully synthesized after treating the crude product with water. KF plays an important role to inhibit the formation of pyrochlore K{sub 2}Ta{sub 2}O{sub 6} during the calcination process of ammonium tantalum hydroxide/K{sub 2}C{sub 2}O{sub 4}/KF mixture. X-ray diffraction (XRD), scanning electron microscopy (SEM), Fourier-transform infrared (FTIR) spectroscopy, UV-vis diffuse reflectance (UV-vis) spectroscopy and thermogravimetric (TG) analysis were used to characterize the precursor compound and as-prepared samples. XRD results show that pyrochlore-free KTaO{sub 3} powder can be obtained at 600 deg. C. SEM results reveal that the as-prepared products are agglomerated and each of the agglomerations consists of many small grains with 10-30 nm in diameter. - Graphical abstract: Pyrochlore-free KTaO{sub 3} powder was prepared at 600 deg. C using tantalum hydroxide/K{sub 2}C{sub 2}O{sub 4}/KF raw materials. Pyrochlore K{sub 2}Ta{sub 2}O{sub 6} and perovskite KTaO{sub 3} coexist at 600 deg. C using tantalum hydroxide/K{sub 2}C{sub 2}O{sub 4} raw materials. Highlights: > In-situ degradation of TaO{sub x}(OH){sub 5-x}(NH{sub 4}){sub x}, K{sub 2}C{sub 2}O{sub 4} and KF promotes the reaction. > Synthesis of KTaO{sub 3} displayed a two-step reaction path with the intermediate formation of K{sub 2}TaO{sub 3}F. > Formation of intermediate K{sub 2}TaO{sub 3}F benefits to prepare pyrochlore-free KTaO{sub 3} at low temperature. > Pyrochlore-free KTaO{sub 3} is prepared at 600 deg. C, which is the lowest temperature reported so far by hard chemistry method. > Synthetic method is a facile, rapid, low price and environment friendly route.
The development of effective treatment and disposal methods is very urgent and important subject. Tohoku University and UNION SHOWA have developed various selective adsorbents (zeolites, zeolite sheets and composites loaded with insoluble ferrocyanides) for the effective decontamination of radioactive Cs{sup +} and Sr{sup 2+} As for Cs{sup +} adsorption, CST, chabazite and insoluble ferrocyanides composites had relatively large distribution coefficients (K{sub d}) above 10{sup 3} cm{sup 3}/g and excellent adsorption kinetics in seawater. Even after high temperature calcination at 1,100 deg. C, cesium was still immobilized in the calcined products of Cs{sup +}-zeolites, suggesting high immobilization ability of zeolites for Cs{sup +}. As for Sr{sup 2+} adsorption, A and X zeolites had relatively large K{sub d} values around 10{sup 2} cm{sup 3}/g, and zeolite sheet (A zeolite) exhibited excellent adsorption kinetics in seawater. Considering the decontamination of radioactive Sr{sup 2+} in groundwater, the effects of Ca{sup 2+} and Mg{sup 2+} ions on the K{sub d} value of Sr{sup 2+} were further examined by batch method. The K{sub d} value of Sr{sup 2+} was almost independent of Mg{sup 2+} concentration up to 2,500 ppm, while gradually lowered in the presence of Ca{sup 2+} above 200 ppm, due to the differences in the ionic radius of hydrated ion. The Cs{sup +} and Sr{sup 2+} adsorption ability for KNiFC-A (composite of A zeolite loaded with insoluble ferrocyanides) was examined by batch method. Here the matrix of composite (A zeolite) and loaded ferrocyanides (KNiFC) have high selectivity towards Sr{sup 2+} and Cs{sup +}, respectively. The K{sub d} values of Sr{sup 2+} and Cs{sup +} in seawater were estimated to be above 10{sup 2} and 10{sup 3} cm{sup 3}/g, respectively, indicating the effectiveness for the decontamination of both Sr{sup 2+} and Cs{sup +}. The basic data on the Cs{sup +} and Sr{sup 2+} adsorption properties for selective adsorbents are effective for the practical decontamination processes of these metal ions in seawater and groundwater. (authors)
Created technological scheme for treatment of liquid radioactive waste generated while uranium and plutonium chemical and metallurgical manufacturing consists of: - Liquid radioactive waste (LRW) purification from radionuclides and its transfer into category of manufacturing waste; - Concentration of suspensions containing alpha-nuclides and their further conversion to safe dry state (calcinate) and moving to long controlled storage. The following technologies are implemented in LRW treatment complex: - Settling and filtering technology for treatment of liquid intermediate-level waste (ILW) with volume about 1500m{sup 3}/year and alpha-activity from 10{sup 6} to 10{sup 8} Bq/dm{sup 3} - Membrane and sorption technology for processing of low-level waste (LLW) of radioactive drain waters with volume about 150 000 m{sup 3}/year and alpha-activity from 10{sup 3} to 10{sup 4} Bq/dm{sup 3}. Settling and filtering technology includes two stages of ILW immobilization accompanied with primary settling of radionuclides on transition metal hydroxides with the following flushing and drying of the pulp generated; secondary deep after settling of radionuclides on transition metal hydroxides with the following solid phase concentration by the method of tangential flow ultrafiltration. Besides, the installation capacity on permeate is not less than 3 m{sup 3}/h. Concentrates generated are sent to calcination on microwave drying (MW drying) unit. Membrane and sorption technology includes processing of averaged sewage flux by the method of tangential flow ultrafiltration with total capacity of installations on permeate not less than 18 m{sup 3}/h and sorption extraction of uranium from permeate on anionite. According to radionuclide contamination level purified solution refers to general industrial waste. Concentrates generated during suspension filtering are evaporated in rotary film evaporator (RFE) in order to remove excess water, thereafter they are dried on infrared heating facility. Solid concentrate produced is sent for long controlled storage. Complex of the procedures carried out makes it possible to solve problems on treatment of LRW generated while uranium and plutonium chemical and metallurgical manufacturing in Federal State Unitary Enterprise (FSUE) Mayak and cease its discharge into open water reservoirs. (authors)
ANSTO's Synroc technology has been developed to provide a safe, secure matrix for the immobilization and final disposal of radioactive waste. Synroc technology will be used to manage radioactive wastes from the production of the radioisotope Molybdenum-99 (Mo-99). This paper shall outline various stages of the process development with specific reference to the thermal treatment technology of calcination. Calcination is a key step in the Synroc process [1-2].The rotary thermal processing system includes: an advanced heating element design for increased robustness and ease of remote operation and maintenance, an enhanced modular design of components for ease of remote maintenance in a hot cell and in compliance with hot cell radioactive environment requirements for safety, reliability and maintainability. In addition to thermal treatment of waste from nuclear medicine production, this technology provides solutions for a variety of nuclear materials processing applications including sintering UO{sub 2} pellets for reactor fuel rods, oxidation of UO{sub 2} pellets, swarf, and powder to U{sub 3}O{sub 8}, de-nitration of Uranyl nitrate and hydrofluorination of UO{sub 2} pellets. The paper will also discuss thermal processing solutions for a range of nuclear applications. (authors)
Spent nuclear fuel of pressurized water reactors mainly consists of uranium, plutonium, minor actinides and fission products. The long term radiotoxicity of wastes is mainly due to plutonium and minor actinides such as neptunium, americium and curium. So, in order both to reduce the radiotoxicity of the ultimate wastes and to save uranium resources, researches for current and new generations of nuclear plants focus on the recycling of plutonium and minor actinides, to fabricate new mixed oxides nuclear fuel pellets (MOX) or transmutation targets. In this aim, production of actinide oxides is necessary. Currently, according to the Purex process, the spent fuel is dissolved in nitric acid and then valuable actinides (uranium and plutonium) are separated and purified from fission products and minor actinides in the Areva plant 'La Hague'. The resulting plutonium nitric solution is converted into a solid phase by oxalic conversion: the oxalic precipitation is followed by the calcination of the obtained oxalate into plutonium oxide. Considering either the MOX fuel or the transmutation targets fabrication from actinide oxides, the control of the particle structure and microstructure is a key factor related to the ability of oxide powder to sinter and shape as pellets. In the oxalic conversion process, the morphology of the precipitated oxalate is strongly influenced by the precipitation conditions and is kept during the calcination from oxalate into oxide. In this context, the aim of this work is to control the morphology of the final actinide oxide by changing the oxalic precipitation conditions. A lot of possibilities can be considered to modulate the morphology of actinide oxalates. Numerous parameters such as temperature, pressure, the presence of a magnetic field, the operating process (seeding, emulsions)... can modify the precipitated particles shape. Additives are also able to play a major role at the precipitation stage by means of different mechanisms involving either complexation, surface covering or structure insertion. This study focuses on this way to modify the morphology of actinides oxalates.
Solid-state reaction of appropriate amounts of Y 2 O 3 , BaCOs, and CuO for 2 h at 800°C in flowing oxygen with a total pressure of 2.7 x 10 2 Pa (2 mm Hg), followed by cooling and annealing at 750°C for 10 h in oxygen at ambient pressure, has produced orthorhombic YBa 2 Cu 4 O 8 (124) as the main phase with YBa 2 Cu 3 O x (123) as an impurity phase. After the as-calcined powder was annealed in oxygen at 800°C for 24 h under ambient pressure, the phase purity improved considerably. Calcined 124 powder was pressed into pellets and rapidly annealed at temperatures from 870°C to 935°C. At these temperatures, the 124 decomposed into 123. The superconducting transition temperature, T c , of the annealed samples depended upon the annealing temperature and atmosphere. The decomposed samples have been characterized by low field RF SQUID magnetometer and high resolution transmission electron microscopy.