Poly(cyclohexadiene)-Based Polymer Electrolyte Membranes for Fuel Cell Applications

The goal of this research project was to create and develop fuel cell membranes having high proton conductivity at high temperatures and high chemical and mechanical durability. Poly(1,3-cyclohexadiene) (PCHD) is of interest as an alternative polymer electrolyte membrane (PEM) material due to its ring-like structure which is expected to impart superior mechanical and thermal properties, and due to the fact that PCHD can readily be incorporated into a range of homopolymer and copolymer structures. PCHD can be aromatized, sulfonated, or fluorinated, allowing for tuning of key performance structure and properties. These factors include good proton transport, hydrophilicity, permeability (including fuel gas impermeability), good mechanical properties, morphology, thermal stability, crystallinity, and cost. The basic building block, 1,3-cyclohexadiene, is a hydrocarbon monomer that could be inexpensively produced on a commercial scale (pricing typical of other hydrocarbon monomers). Optimal material properties will result in novel low cost PEM membranes engineered for high conductivity at elevated temperatures and low relative humidities, as well as good performance and durability. The primary objectives of this project were: (1) To design, synthesize and characterize new non-Nafion PEM materials that conduct protons at low (25-50%) RH and at temperatures ranging from room temperature to 120 C; and (2) To achieve these objectives, a range of homopolymer and copolymer materials incorporating poly(cyclohexadiene) (PCHD) will be synthesized, derivatized, and characterized. These two objectives have been achieved. Sulfonated and crosslinked PCHD homopolymer membranes exhibit proton conductivities similar to Nafion in the mid-RH range, are superior to Nafion at higher RH, but are poorer than Nafion at RH < 50%. Thus to further improve proton conductivity, particularly at low RH, poly(ethylene glycol) (PEG) was incorporated into the membrane by blending and by copolymerization. Conductivity measurements at 120 C over RH ranging from 20 to 100% using the BekkTech protocol showed much improved proton conductivities. Conductivities for the best of these new membranes exceed the DOE Year 3 milestone of 100 mS/cm at 50% RH at 120 C. Further optimization of these very promising low cost membranes could be pursued in the future.

08 HYDROGEN↗

Electrophilic Metal Alkyl Chemistry in New Ligand Environments

The goals of this project were to design new electrophilic metal alkyl complexes and to exploit these systems in fundamental studies of olefin polymerization and other important and new catalytic reactions. A key target reaction is insertion copolymerization of olefins and polar CH 2 =CHX vinyl monomers such as vinyl halides and vinyl ethers. During the period covered by this report we (i) investigated the properties of ortho-alkoxy-arylphosphine ligands in Ni-based olefin polymerization catalysts, (ii) studied the synthesis of double-end-capped polyethylene using group 4 metal catalysts that contain tris-pyrazolylborate ligands, (iii) explored the ethylene insertion reactivity of group 4 metal tris-pyrazolyl-borate complexes, (iv) showed that (α- diimine)PdMe + species undergo multiple insertion of silyl vinyl ethers, (v) synthesized and explored the reactivity of base-free Ni benzyl complexes that contain ortho-phosphino-arene sulfonate ligands, (vi) established the mechanism of the reaction of vinyl chloride with (α- diimine)PdMe + catalysts, (vii) explored the role of cationic polymerization and insertion chemistry in the reactions of vinyl ethers with (α-diimine)PdMe + species, (viii) discovered a new class of self-assembled tetranuclear Pd catalysts that produce high molecular weight linear polyethylene and copolymerize ethylene and vinyl fluoride, and (ix) developed model systems that enabled investigation of cis-trans isomerization of {phosphine-sulfonate}Pd(II) complexes.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

NMED Correspondence Related to Notice of Intent for Chromium Project

Two methods of injection using a solution containing 50 kilograms (kg) of tracer are proposed for each well. Half of the tracer (25 kg) may be mixed with 3,000 gallons of potable water and delivered into a scheduled injection stream of treated groundwater as permitted in OP-1835 over a five to seven-hour period. This procedure would then be repeated on a consecutive second day. Alternatively, 5 kg of tracer may be added to each of ten 3,000-gallon tanks for a total of 30,000 gallons of tracer solution that may be injected independently of other injection flow over a period of up to five days. The permittees request that the types and masses of tracers that may be utilized per each injection well remain flexible enough to allow for one or more of the naphthalene sulfonate tracers to be substituted with a different naphthalene sulfonate. This need for flexibility is due to the availability of the tracers and any tracer listed that is designated for a given CrIN well may be interchanged with a tracer that is designated for another CrIN well, pending final NMED approval. The permittees are not allowed to introduce any new tracers and will submit a final work plan prior to each injection for each CrIN well.

54 ENVIRONMENTAL SCIENCES↗

PILBCP-IL Composite Ionomers for High Current Density Performance

Wide-spread commercialization of fuel cell electric vehicles using proton exchange membrane fuel cell (PEMFC) power sources requires that several existing limitations be addressed. These include: (1) a reduction in platinum (Pt) loading in the catalytic electrodes, (2) improvements in reactant and electronic mobility throughout the catalytic electrodes, (3) reduction in the reliance on materials derived from polluting “forever chemicals”, and (4) a significant improvement in the operational longevity of catalytic electrode components. In this project, a team of two universities, Drexel University and Texas A&M University, one national lab, National Renewable Energy Laboratory, and one company, General Motors, collaborated to develop a new cathode ionomer chemistry that would address these limitations and result in an improvement in performance over existing ionomer materials. The key technology developed through this collaborative project was a composite cathode ionomer encompassing an ionic liquid interlayer between Pt catalysts and a sulfonated polymerized ionic liquid block co-polymer (S-PILBCP) that possess the orthogonal properties of protonic conductivity and ionic liquid enhanced kinetics and durability (see schematic in Figure 1). The composite S-PILBCP ionomer eliminates many of the existing issues with perfluorosulfonic acid-based ionomers including active site blocking by sulfonate specific adsorption, restricted O 2 transport through ionomer films, limited humidity tolerance and active area loss for carbon pore confined catalyst particles, and use of polluting “forever chemicals”. Following successful integration of the developed composite ionic liquid into a PEMFC cathode catalyst layer, we demonstrate enhanced performance over Nafion containing cathodes with Pt/C and PtCo/C at both low and high current density. The performance with our composite S-PILBCP ionomer meets the Department of Energy (DOE) targets for light duty vehicle applications

08 HYDROGEN↗

Relative toxicity of pyrolysis products of some synthetic polymers

Nineteen samples of synthetic polymers were evaluated for relative toxicity in the course of characterizing materials intended for aircraft interior applications. The generic polymers included ABS, chlorinated PVC, polycarbonate, polyphenylene oxide, polyphenylene sulfide, polysulfone, polyaryl sulfone, polyether sulfone, polybismaleimide, and polyvinyl fluoride. Test results are presented, and compared in relative rankings with similar results on cellulosic materials and other synthetic polymers. Under these test conditions, the samples of synthetic polymers were either comparable to or significantly less toxic than the samples of commercial cellulosic materials.

Hilado, C. J.↗

Thermoplastic polymers for improved fire safety

The thermochemical and flammability characteristics of some typical thermoplastic materials currently in use and others being considered for use in aircraft interiors are described. The properties studied included (1) thermomechanical properties such as glass transition and melt temperature, (2) changes in polymer enthalpy by differential scanning calorimetry, (3) thermogravimetric analysis in anaerobic and oxidative environments, (4) oxygen index, (5) smoke evolution, (6) relative toxicity of the volatile products of pyrolysis, and (7) selected physical properties. The generic polymers that were evaluated included: acrylonitrile butadiene styrene, bisphenol A polycarbonate, 9,9 bis (4-hydroxyphenyl) fluorene polycarbonatepoly (dimethyl siloxane) block polymer, phenolphthalein bisphenol A polycarbonate, phenolphthalein polycarbonate, polyether sulfone, polyphenylene oxide, polyphenylene sulfide, polyaryl sulfone, chlorinated polyvinyl chloride homopolymer, polyvinyl fluoride, and polyvinylidene fluoride. Processing parameters, including molding characteristics of some of the advanced polymers, are described. Test results and relative ranking of some of the flammability, smoke, and toxicity properties are presented.

Kourtides, D. A.↗

Effect of temperature and heating rate on apparent lethal concentrations of pyrolysis products

The apparent lethal concentrations for 50 percent of the test animals of the pyrolysis products from twelve polymeric materials were studied as a function of temperature and heating rate. The materials were polyethylene, nylon 6, ABS, polycarbonate, polyether sulfone, polyaryl sulfone, wool fabric, aromatic polyamide fabric, polychloroprene foam, polyvinyl fluoride film, Douglas fir, and red oak. The apparent lethal concentration values of most materials vary significantly with temperature and heating rate. The apparent lethal concentration values, based on weight of sample charged, appears to effectively integrate the thermophysical, thermochemical, and physiological responses from a known quantity of material under specified imposed conditions.

Hilado, C. J.↗

Thermochemical characterization of some thermoplastic materials

The thermochemical and flammability characteristics of some typical thermoplastic materials currently in use or being considered for use in aircraft interiors are described. The properties studied included thermomechanical properties such as glass-transition and melt temperature, changes in polymer enthalpy, thermogravimetric analysis in anerobic and oxidative environments, oxygen index, smoke evolution, relative toxicity of the volatile products of pyrolysis, and selected physical properties. The generic polymers evaluated included acrylonitrile butadiene styrene, bisphenol A polycarbonate, 9,9 bis (4-hydroxyphenyl) fluorene polycarbonate-poly (dimethylsiloxane) block polymer, phenolphthalein-bisphenol A polycarbonate, phenolphthalein polycarbonate, polyether sulfone, polyphenylene oxide, polyphenylene sulfide, polyaryl sulfone, chlorinated polyvinyl chloride homopolymer, polyvinyl fluoride, and polyvinylidene fluoride. Processing parameters, including molding characteristics of some of the advanced polymers, are described. Test results and relative rankings of some of the flammability, smoke, and toxicity properties are presented. Under these test conditions, some of the advanced polymers evaluated were significantly less flammable and toxic than or equivalent to polymers in current use.

Kourtides, D. A.↗

Effect of heating rate on toxicity of pyrolysis gases from some synthetic polymers

The effect of heating rate on the toxicity of the pyrolysis gases from some synthetic polymers was investigate, using a screening test method. The synthetic polymers were polyethylene, polystyrene, polymethyl methacrylate, polycarbonate, ABS, polyaryl sulfone, polyether sulfone, and polyphenylene sulfide. The toxicants from the sulfur-containing polymers appeared to act more rapidly than the toxicants from the other polymers. It is not known whether this effect is due primarily to differences in concentration or in the nature of the toxicants. The carbon monoxide concentrations found do not account for the observed results.

Hilado, C. J.↗

Assessment of relative flammability and thermochemical properties of some thermoplastic materials

The thermochemical and flammability characteristics of some typical thermoplastic materials currently in use and others being considered for use in aircraft interiors are described. The properties studied included (1) thermal mechanical properties such as glass transition and melt temperature, (2) changes in polymer enthalpy by differential scanning calorimetry, (3) thermogravimetric analysis in an anaerobic and oxidative environment, (4) oxygen index, (5) smoke evolution, (6) relative toxicity of the volatile products of pyrolysis, and (7) selected physical properties. The generic polymers which were evaluated included: acrylonitrile-butadiene-styrene, bisphenol A polycarbonate, bisphenol fluorenone carbonatedimethylsiloxane block polymer, phenolphthalein-bisphenol A polycarbonate, phenolphthalein polycarbonate, polyether sulfone, polyphenylene oxide, polyphenylene sulfide, polyaryl sulfone, chlorinated polyvinyl chloride homopolymer, polyvinyl fluoride, and polyvinylidene fluoride. Processing parameters including molding characteristics of some of the advanced polymers are described. Test results and relative rankings of some of the flammability, smoke and toxicity properties are presented.

Kourtides, D. A.↗

Two-week studies of survivors from exposures to pyrolysis gases

Swiss Webster male mice which had survived near-lethal concentrations of pyrolysis gases from a variety of polymeric materials were killed two weeks after exposure, and the lungs, heart, liver, kidney, and spleen were examined. Microscopic examination revealed no significant effects on the liver, kidney, and spleen, while the effect on lungs could not be determined because of the high level of pathology in both experimental and control animals. The polymeric materials which were pyrolyzed were polyethylene, ABS, polycarbonate, polyaryl sulfone, polyether sulfone, polyphenylene sulfide, modified polyphenylene oxide, chlorinated polyvinyl chloride, polyvinylidene fluoride, and fluorene polycarbonate. It is suggested that tissue specimens should be examined 24 or 48 hr after exposure rather than 2 wks after exposure, since the 2 wk period permits healing to occur.

Bucci, T. J.↗

Characterization of flammability properties of some thermoplastic and thermoset resins

The thermochemical and flammability properties of some thermally stable polymers considered for use in aircraft interiors are described. The properties studied include: (1) thermomechanical properties such as glass transition and melt temperature; (2) dynamic thermogravimetric analysis in anaerobic environment; (3) flammability properties such as oxygen index, flame spread, and smoke evolution; and (4) selected physical properties. The thermoplastic polymers evaluated included polyphenylene sulfide, polyaryl sulfone, 9,9-bis(4-hydroxyphenyl)-fluorene polycarbonate-poly(dimethylsiloxane) and polyether sulfone. The thermoset polymers evaluated included epoxy, bismaleimide, a modified phenolic and polyaromatic melamine resin. These resins were primarily used in the fabrication of glass reinforced prepregs for the construction of experimental panels. Test results and relative rankings of some of the flammability parameters are presented and the relationship of the molecular structure, char yield, and flammability properties of these polymers are discussed.

Kourtides, D. A.↗

Thermochemical characterization of some thermally stable thermoplastic and thermoset polymers

The thermochemical and flammability properties of some thermally stable polymers considered for use in aircraft interiors are described. The properties studied include: (1) thermomechanical properties such as glass transition and melt temperature; (2) dynamic thermogravimetric analysis in anaerobic environment; (3) flammability properties such as oxygen index, flame spread, and smoke evolution; and (4) selected physical properties. The thermoplastic polymers evaluated include polyphenylene sulfide, polyaryl sulfone, 9,9-bis(4-hydroxyphenyl)-fluorene polycarbonate-poly(dimethylsiloxane) and polyether sulfone. The thermoset polymers evaluated include epoxy, bismaleimide, a modified phenolic, and polyaromatic melamine resin. These resins were primarily used in the fabrication of glass-reinforced prepregs for the construction of experimental panels. Test results and relative rankings of some of the flammability parameters are presented, and the relationship of the molecular structure, char yield, and flammability properties of these polymers are discussed.

Kourtides, D. A.↗

Imide modified epoxy matrix resins

Results of a program designed to develop tough imide modified epoxy (IME) resins cured by bisimide amine (BIA) hardeners are presented. State of the art epoxy resin, MY720, was used. Three aromatic bisimide amines and one aromatic aliphatic BIA were evaluated. BIA's derived from 6F anhydride (3,3 prime 4,4 prime-(hexafluoro isopropyl idene) bis (phthalic anhydride) and diamines, 3,3 prime-diam nodiphenyl sulfone (3,3 prime-DDS), 4,4 prime-diamino diphenyl sulfone (4,4 prime-DDS), 1.12-dodecane diamine (1,12-DDA) were used. BIA's were abbreviated 6F-3,3 prime-DDS, 6F-4,4 prime-DDS, 6F-3,3 prime-DDS-4,4 prime DDS, and 6F-3,3 prime-DDS-1,12-DDA corresponding to 6F anhydride and diamines mentioned. Epoxy resin and BIA's (MY720/6F-3,3 prime-DDS, MY720/6F-3,3 prime-DDS-4,4 prime-DDS, MY720/6F-3,3 prime-DDS-1,12-DDA and a 50:50 mixture of a BIA and parent diamine, MY720/6F-3,3 prime-DDS/3,3 prime-DDS, MY720/6F-3,3 prime-DDS-4,4 prime-DDS/3,3 prime-DDS, MY720/6F-3,3 prime-DDS-1,12-DDA/3,3 prime-DDS were studied to determine effect of structure and composition. Effect of the addition of two commercial epoxies, glyamine 200 and glyamine 100 on the properties of several formulations was evaluated. Bisimide amine cured epoxies were designated IME's (imide modified epoxy). Physical, thermal and mechanical properties of these resins were determined. Moisture absorption in boiling water exhibited by several of the IME's was considerably lower than the state of the art epoxies (from 3.2% for the control and state of the art to 2.0 wt% moisture absorption). Char yields are increased from 20% for control and state of the art epoxies to 40% for IME resins. Relative toughness characteristics of IME resins were measured by 10 deg off axis tensile tests of Celion 6000/IME composites. Results show that IME's containing 6F-3,3 prime-DDS or 6F-3,3 prime-DDS-1,12-DDA improved the "toughness" characteristics of composites by about 35% (tensile strength), about 35% (intralaminar shear strength), and about 78% (shear strain to failure) relative to the control composite.

Scola, D. A.↗

Ultrasonic mixing of epoxy curing agents

A new technique for mixing solid curing agents into liquid epoxy resins using ultrasonic energy was developed. This procedure allows standard curing agents such as 4,4 prime-diaminodiphenyl sulfone (4,4 prime-DDS) and its 3,3 prime-isomer, (3,3 prime-DDS) to be mixed without prior melting of the curing agent. It also allows curing agents such as 4,4 prime-diaminodiphenyl sulfone (4,4 prime-DDS) and its 3,3 prime-isomer, (3,3 prime-DDS) to be mixed without prior melting of the curing agent. It also allows curing agents with very high melt temperatures such as 4,4 prime-diaminobenzophenone (4,4 prime-DABP) (242 C) to be mixed without premature curing. Four aromatic diamines were ultrasonically blended into MY-720 epoxy resin. These were 4,4 prime-DDS; 3,3 prime-DDA; 4,4 prime-DABP and 3,3 prime-DABP. Unfilled moldings were cast and cured for each system and their physical and mechanical properties compared.

Hodges, W. T.↗

Solvent resistant thermoplastic aromatic poly(imidesulfone) and process for preparing same

A process for preparing a thermoplastic poly(imidesulfone) is disclosed. This resulting material has thermoplastic properties which are generally associated with polysulfones but not polyimides, and solvent resistance which is generally associated with polyimides but not polysulfones. This system is processable in the 250 to 350 C range for molding, adhesive and laminating applications. This unique thermoplastic poly(imidesulfone) is obtained by incorporating an aromatic sulfone moiety into the backbone of an aromatic linear polyimide by dissolving a quantity of a 3,3',4,4'-benzophenonetetracarboxylic dianhydride (BTDA) in a solution of 3,3'-diaminodiphenylsulfone and bis(2-methoxyethyl)ether, precipitating the reactant product in water, filtering and drying the recovered poly(amide-acid sulfone) and converting it to the poly(imidesulfone) by heating.

St.clair, T. L.↗

Polyaryl ethers and related polysiloxane copolymer molecular coatings preparation and radiation degrdation

Poly(arylene ether sulfones) comprise a class of materials known as engineering thermoplastics which have a variety of important applications. These polymers are tough, rigid materials with good mechanical properties over a wide temperature range, and they are processed by conventional methods into products typically having excellent hydrolytic, thermal, oxidative and dimensional stability. Wholly aromatic random copolymers of hydroquinone and biphenol with 4.4 prime dichlorodiphenyl sulfone were synthesized via mechanical nucleophilic displacement. Their structures were characterized and mechanical behavior studied. These tough, ductile copolymers show excellent radiation resistance to electron beam treatment and retain much of the mechanical properties up to at least 700 Mrads under argon.

Mcgrath, J. E.↗

Ultrasonic mixing of epoxy curing agents

A new technique for mixing solid curing agents into liquid epoxy resins using ultrasonic energy was developed. This procedure allows standard curing agents such as 4,4 prime-diaminodiphenyl sulfone (4,4 prime-DDS) and its 3,3 prime-isomer, (3,3 prime-DDS) to be mixed without prior melting of the curing agent. It also allows curing agents with very high melt temperatures such as 4,4 prime-diaminodiphenyl sulfone (4,4 prime-DDS) and its 3,3 prime-isomer, (3,3 prime-DDS) to be mixed without prior melting of the curing agent. It also allows curing agents with very high melt temperatures such as 4,4 prime-diaminobenzophenone (4,4 prime-DABP) (242 C) to be mixed without premature curing. Four aromatic diamines were ultrasonically blended into MY-720 epoxy resin. These were 4, 4 prime-DDS; 3,3 prime-DDA; 4, 4 prime-DABP and 3,3 prime-DABP. Unfilled moldings were cast and cured for each system and their physical and mechanical properties compared. Previously announced in STAR as N83-27018