At least 451 records · Page 25

Morphology and Evolution of 14Cr Powder During Mechanical Alloying for Oxide Dispersion Strengthened Ferritic Alloys

Oxide Dispersion Strengthened (ODS) Ferritic steel alloys are candidate materials for Generation IV and Fusion reactor concepts due to their high temperature material properties and their irradiation stability. However, these material properties are strongly influenced by nanocluster dispersion and grain size distributions, which are directly correlated to mechanical alloying methodologies and parameters. Current powder processing strategies use ball milling times greater than or equal to 40 hrs to achieve sufficient dispersoid, i.e Y{sub 2}O{sub 3}, incorporation within the metal matrix, but these time intensive milling cycles are neither practical nor economical. This work aims to investigate how the particle morphology evolves during mechanical alloying during the processing of a 14Cr ODS ferritic alloy, and if higher-intensity milling, shorter milling cycles can still achieve sufficient mixing of yttria in comparison to the dispersion and incorporation observed in conventional lower-intensity milling methodologies. Comparisons of milled particle size distributions are presented for low and high intensity milling cycles, while microscopy and high-temperature tensile data are presented for consolidated samples using higher-intensity milling parameters. (authors)

36 MATERIALS SCIENCE↗

Morphological Evolution of Oxide Scales Grown on Ferritic Steels in Steam

This study is concerned with the thermally-grown oxide scales formed inside tubes in a steam boiler during normal operation, and the influence of the morphological evolution of those scales on how strains are developed and accommodated. Understanding such details is an important consideration in modeling the tendency for scale spallation or exfoliation. Overall, the scales formed on ferritic steels in steam can be simplistically described as a layer of essentially pure magnetite in contact with the steam, and a second layer of magnetite containing alloying elements (especially Cr) next to the alloy. Hematite also can develop as a third, outermost oxide layer that may be non-uniform in thickness, and penetrate inwards along grain boundaries in the magnetite layer. A peculiar variant of this morphology often reported on low-alloy ferritic steels after boiler service (but not on laboratory-oxidized specimens) has a relatively thick outer magnetite layer and multiple inner layers described as decreasing in thickness as the alloy surface is approached. These inner layers appear to be repeating sets of double layers of pure magnetite and magnetite containing alloying elements. The results of detailed examination of such multi-layered morphology and the implications for the mode of scale growth and failure are discussed.

36 MATERIALS SCIENCE↗

Mechanical and Electrochemical Behavior of Dual-Phase Steels Having Varying Ferrite–Martensite Volume Fractions

Dual-phase (DP) steels behave differently under corrosive environment depending upon the volume fractions of phases, mainly martensite, ferrite and bainite. The mechanical behavior and corrosion resistance of DP steels with varying martensite (from 32 to 100%) are investigated. The increase in martensite volume fraction of DP steel results in significant improvement in tensile strength and hardness with a subsequent reduction in elongation. Unlike the mechanical behavior, the increase in martensite volume fraction in steel does not exhibit a direct relationship with their corrosion resistance behavior. The corrosion mechanism in DP steels having different martensite and ferrite volume fractions depends on the self-corrosion resistance behavior of both the phases as well as the occurrence of galvanic corrosion between them.

36 MATERIALS SCIENCE↗

Oxidation Kinetics of Ferritic Alloys in High-Temperature Steam Environments

High-temperature isothermal steam oxidation kinetic parameters of several ferritic alloys were determined by thermogravimetric analysis. We measured the oxidation kinetic constant (k) as a function of temperature from 900°C to 1200°C. The results show a marked increase in oxidation resistance compared to reference Zircaloy-2, with kinetic constants 3–5 orders of magnitude lower across the experimental temperature range. Our results of this investigation supplement previous findings on the properties of ferritic alloys for use as candidate cladding materials and extend kinetic parameter measurements to high-temperature steam environments suitable for assessing accident tolerance for light water reactor applications.

36 MATERIALS SCIENCE↗

Effects of Mn partitioning on nanoscale precipitation and mechanical properties of ferritic steels strengthened by NiAl nanoparticles

The critical role of Mn partitioning in the formation of ordered NiAl nanoparticles in ferritic steels has been examined through a combination of atom probe tomography (APT) and thermodynamic and first-principles calculations. Our APT study reveals that Mn partitions to the NiAl nanoparticles, and dramatically increases the particle number density by more than an order of magnitude, leading to a threefold enhancement in strengthening. Atomistic structural analyses reveal that Mn is energetically favored to partition to the NiAl nanoparticles by preferentially occupying the Al sublattice, which not only increases the driving force, but also reduces the strain energy for nucleation, thereby significantly decreasing the critical energy for formation of the NiAl nanoparticles in ferritic steels. In addition, the effects of Mn on the precipitation strengthening mechanisms were quantitatively evaluated in terms of chemical strengthening, coherency strengthening, modulus strengthening and order strengthening.

36 MATERIALS SCIENCE↗

Temperature-dependent cavity swelling in dual-ion irradiated Fe and Fe-Cr ferritic alloys

Fe-Cr ferritic-martensitic (FM) steels are promising structural material candidates for fusion and advanced fission reactors due to their attractive mechanical properties and volumetric swelling resistance. However, significant discrepancies exist regarding the effect of solutes and irradiation temperature on cavity swelling under ion versus neutron irradiation conditions. In this study, simultaneous dual ion irradiations (8 MeV Ni 3+ ions and energy-degraded 3.5 MeV He 2+ ions) were used to quantify the cavity swelling behavior in ultra-high purity Fe and Fe-Cr alloys (3-14 wt.% Cr), Fe-10 wt.% Cr-780 wt.ppm C, and Eurofer97 FM steel. The irradiations were conducted over a wide temperature range (400-550°C) with a mid-range dose of ~30 displacements per atom (dpa) and 0.1 appm/dpa He implantation rate. Here, using state-of-the-art transmission electron microscopy (TEM), we reveal that pure Fe has a ~50°C lower peak swelling temperature difference than Fe-Cr alloys, which is attributed to higher vacancy mobility in pure Fe. Chromium solute appears to strongly suppress cavity swelling in Fe-Cr alloys for temperatures below ~470°C, but seems to have little effect or slightly enhances swelling above ~470°C. Cavities were observed in all the irradiated samples between 400-550°C. This indicates that the narrow temperature range of observable cavities reported in prior ion irradiated Fe-Cr ferritic alloy studies is likely an artifact associated with the use of low ion energies (<5 MeV), which leads to pronounced near-surface and implanted ion effects that suppress cavity swelling even at midrange depths (particularly at high temperatures).

36 MATERIALS SCIENCE↗

Kinetic analysis of the interactions between calcium ferrite and coal char for chemical looping gasification applications: Identifying reduction routes and modes of oxygen transfer

Chemical Looping Gasification (CLG) is an emerging technology that shows promise for efficient coal gasification by eliminating the need for energy intensive gas separations to achieve a non-nitrogen diluted syngas stream. Oxygen from oxygen carriers, such as CaFe 2 O 4 , are used for coal gasification in place of conventionally produced gaseous oxygen from cryogenic separation of air. These oxygen carriers are unique for their ability to selectively oxidize coal to form syngas and show limited reactivity with syngas components (H 2 , CO). To gain a deeper understanding of how these unique oxygen carriers perform and to offer a first attempt at the reaction modeling of solid mediated interactions of this nature, this study was carried out to determine the kinetic parameters associated with the selective oxidation of coal derived char (Wyodak and Illinois #6) with a metal ferrite, CaFe 2 O 4 . Using thermogravimetric analysis (TGA) coupled with mass spectrometry, the selective oxygen release of metal ferrite in the presence of char by proximal contact was examined. The application of combinatory model fitting approaches was used to describe controlling resistances during oxygen release. A combination of the modified shrinking core model (SCM) with planar oxygen ion diffusion control and reaction order based models was used for kinetic parameter determination. CaFe 2 O 4 particle size plays a major role in the prevailing mode of oxygen release. Particle sizes on the order of 40–50 μm tend to favor first order kinetically controlled regimes independent of geometric and diffusion controls. The probability for oxygen ion diffusion controlling regimes increased when the particle size range of the oxygen carrier was increased up to 350 μm. Char type also impacted the prevalence of the controlling regime. Higher ranked chars react in a slower manner, limiting the gradient for oxygen ion release from the oxygen carrier. Activation energies determined for this process range from 120–200kJ/mol and oxygen ion diffusion coefficients are on the order of 10-8 cm 2 /s. It is suggested that oxygen ion movement is regulated by lattice diffusion out of partially reduced phases (Ca 2 Fe 2 O 5 ) and through reduced outer layers composed of CaO and Fe. The controlled movement of oxygen ions influences the rate of carbon oxidation in the char and therefore the selectivity towards partial oxidation products, which are desirable in CLG applications.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

CO 2 utilization potential of a novel calcium ferrite based looping process fueled with coal: Experimental evaluation of various coal feedstocks and thermodynamic integrated process analysis

Here, conversion of CO 2 to CO was performed at 800-850C via reduction of calcium ferrite (CaFe 2 O 4 ) with coal followed by oxidation of reduced CaFe 2 O 4 with CO 2 to produce CO and partially oxidized Ca ferrite. The process was evaluated with several types of coals which included lignite, sub-bituminous, bituminous, anthracite and pet-coke. Reduction of CaFe 2 O 4 with sub-bituminous coal and lignite coal was more favorable than that with higher rank coals. Stable reactivity performance was demonstrated for 35-cycle test conducted with lignite coal/CaFe 2 O 4 at 800°C and with high conversion of CO 2 to CO. The rate of conversion of CO 2 to CO with reduced CaFe 2 O 4 was found to be 1st order with respect to CO 2 and had a low activation energy of 7.4 kJ/mol. Thermodynamic integrated process assessments suggest that two and three reactor process concepts can be realized and net CO 2 utilization achievable. The two reactor configuration shows the highest potential for CO 2 utilization while generating a value-added CO rich syngas stream.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Unusual Thermal Stability of Nano-structured Ferritic alloys

A scientific question vitally important to the materials community is whether there exist self-assembled nanoclusters that are thermodynamically stable at elevated temperatures. Using in-situ neutron scattering, we characterized the structure and thermal stability of a nano-structured ferritic (NSF) alloy. Nanometer sized clusters were found to persist up to ~1400 C, providing direct evidence of a thermodynamically stable alloying state for the nanoclusters. Cluster formation requires the coexistence of Y, Ti, and O without the precipitation of oxide phases. The presence of thermally stable nanoclusters at grain boundaries limits the diffusion of Fe atoms, thereby stabilizing the microstructure of the ferritic matrix at high temperatures. Our experimental results provide physical insights of the dramatically improved high-temperature mechanical properties in NSF alloy and point to a new direction in alloy design.

72 PHYSICS OF ELEMENTARY PARTICLES AND FIELDS↗

A review of advantages of high-efficiency X-ray spectrum imaging for analysis of nanostructured ferritic alloys

Nanostructured ferritic alloys (NFAs) exhibit complex microstructures consisting of 100-500 nm ferrite grains, grain boundary solute enrichment, and multiple populations of precipitates and nanoclusters (NCs). Understanding these materials' excellent creep and radiation-tolerance properties requires a combination of multiple atomic-scale experimental techniques. Recent advances in scanning transmission electron microscopy (STEM) hardware and data analysis methods have the potential to revolutionize nanometer to micrometer scale materials analysis. The application of these methods is applied to NFAs as a test case and is compared to both conventional STEM methods as well as complementary methods such as scanning electron microscopy and atom probe tomography. In this paper, we review past results and present new results illustrating the effectiveness of latest-generation STEM instrumentation and data analysis.

36 MATERIALS SCIENCE↗

Helium sequestration at nanoparticle-matrix interfaces in helium + heavy ion irradiated nanostructured ferritic alloys

Here we irradiated four ferritic alloys with energetic Fe and He ions: one castable nanostructured alloy (CNA) containing Ti-W-Ta-carbides, and three nanostructured ferritic alloys (NFAs). The NFAs were: 9Cr containing Y-Ti-O nanoclusters, and two Fe-12Cr-5Al NFAs containing Y-Zr-O or Y-Hf-O clusters. All four were subjected to simultaneous dual-beam Fe + He ion implantation (650 °C, ~50 dpa, ~15 appm He/dpa), simulating fusion-reactor conditions. Examination using scanning/transmission electron microscopy (STEM) revealed high-number-density helium bubbles of ~8 nm, ~10 21 m -3 (CNA), and of ~3 nm, 10 23 m -3 (NFAs). STEM combined with multivariate statistical analysis data mining suggests that the precipitate-matrix interfaces in all alloys survived ~50 dpa at 650 °C and serve as effective helium trapping sites. All alloys appear viable structural material candidates for fusion or advanced fission energy systems. Finally, among these developmental alloys the NFAs appear to sequester the helium into smaller bubbles and away from the grain boundaries more effectively than the early-generation CNA.

36 MATERIALS SCIENCE↗

Evolution of B2 and laves phases in a ferritic steel under Fe 2+ ion irradiation at 475 °C

Microstructural evolution in a novel ferritic steel (Fe–12Cr–3W–3Ni–3Al–1Nb, in wt.%) computationally designed to contain B2 and Laves phases after 4 MeV Fe 2+ ion irradiation up to 220 dpa at 475 °C was characterized using transmission electron microscopy in conjunction with x-ray energy dispersive spectroscopy. The ferritic matrix phase exhibited dislocation loops and tangled dislocations, but our focus was on stability of two types of intermetallic precipitates. The B2–NiAl precipitates ~13 nm in size remained crystalline and appeared to have slightly lower Al concentration after irradiation. The Laves phase, (Fe,Cr) 2 (Nb,W), were present in two size ranges: coarse micron-scale precipitates which were amorphized with a slight composition change at irradiation doses above~30 dpa, while the finer precipitate particles~100 nm in size were partially disintegrated with a noticeable composition change at doses above~70 dpa. Meanwhile, many Nb/Cr-enriched particles ~8 nm in size formed within a few hundreds of nanometers from the disintegrated particles. The understanding of the phase stability would help design advanced steels and engineer microstructures that are stable against high irradiation doses, while retaining good high temperature strength.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

High-temperature nanoindentation creep studies on castable and sintered nanostructured low-activation ferritic-martensitic alloys

In this article, we present the creep characteristics of two reduced activation ferritic-martensitic steels of identical starting compositions formed by different fabrication routes: a nanostructured ferritic alloy commonly referred to as a castable nanostructured alloy (CNA) and a sintered nanostructured alloy (SNA) variant. Through a series of nanoindentation experiments spanning a temperature range of 25 °C to 650 °C, with a maximum load of 100 mN, we find creep behaviors in the cast and sintered materials to be remarkably similar. The creep stress exponent (n) for CNA and SNA were found to be in the range of 8–35 and the activation volume was ∼14–42b 3 , underscoring a dominance of dislocation-mediated mechanisms in both alloys. Notably, we observed a decline in the creep stress exponent with increasing temperature, attributable to the heightened influence of thermally activated dislocations. This phenomenon suggests a potential transition in the deformation mechanism towards a thermally activated dislocation climb process, significantly impacting the observed creep behavior.

36 MATERIALS SCIENCE↗

Long-term oxidation behavior of spinel-coated ferritic stainless steel for solid oxide fuel cell interconnect applications

Long-term tests (>8,000 hours) indicate that AISI 441 ferritic stainless steel coated with a Mn-Co spinel protection layer is a promising candidate material system for IT-SOFC interconnect applications. While uncoated AISI 441 showed a substantial increase in area-specific electrical resistance (ASR), spinel-coated AISI 441 exhibited much lower ASR values (11-13 mOhm-cm2). Formation of an insulating silica sublayer beneath the native chromia-based scale was not observed, and the spinel coatings reduced the oxide scale growth rate and blocked outward diffusion of Cr from the alloy substrate. The structure of the scale formed under the spinel coatings during the long term tests differed from that typically observed on ferritic stainless steels after short term oxidation tests. While short term tests typically indicate a dual layer scale structure consisting of a chromia layer covered by a layer of Mn-Cr spinel, the scale grown during the long term tests consisted of a chromia matrix with discrete regions of Mn-Cr spinel distributed throughout the matrix. The presence of Ti in the chromia scale matrix and/or the presence of regions of Mn-Cr spinel within the scale may have increased the scale electrical conductivity, which would explain the fact that the observed ASR in the tests was lower than would be expected if the scale consisted of pure chromia.

Stevenson, Jeffry W.↗

Magnetic and electric modulus properties of In substituted Mg–Mn–Cu ferrites

Highlights: • Ferrite of composition Mg{sub 1−y}Cu{sub y}Mn{sub 0.1}In{sub x}Fe{sub 1.9−x}O{sub 4} with (0.0 ≤ x ≤ 0.4; y = 0.0; 0.1) has been synthesized. • Electric, magnetic and Mössbauer studies have been investigated. • The real and imaginary parts of electric modulus follow the Arrhenius law. • Saturation magnetization increases up to x = 0.2 and thereafter it decreases. • Good agreement between the magnetic and Mössbauer effect studies. - Abstract: Ferrite of composition Mg{sub (1−y)}Cu{sub (y)}Mn{sub (0.1)}In{sub (x)}Fe{sub (1.9−x)}O{sub 4} with (0.0 ≤ x ≤ 0.4; y = 0.0 and y = 0.1) has been synthesized by solid state reaction technique. X-ray diffraction (XRD) patterns of the samples indicated the formation of single-phase cubic spinel structure up to 0.2 and mixed phase for samples x ≥ 0.3. Vibrating sample magnetometer (VSM) measurements indicated that the saturation magnetization increases up to x = 0.2 and thereafter it decreases. Electric modulus analysis was used as a tool to analyze the electrical behavior of the samples. The activation energies extracted from real M′ (ω) and imaginary M″ (ω) peaks were found to follow the Arrhenius law. The area ratio of Fe{sup 3+} at the tetrahedral A- and octahedral B-sites was deduced from the spectral analysis of Mössbauer measurements. The results give evidence that In{sup 3+} replaces Fe{sup 3+} at A-site in the range (0.0 < x ≤ 0.2). As the In{sup 3+} content increases; it replaces Fe at B-site.

36 MATERIALS SCIENCE↗

Effect of chromium substitution on the dielectric properties of mixed Ni-Zn ferrite prepared by WOWS sol–gel technique

Graphical abstract: Variation of AC conductivity (σ{sub AC}) as a function of natural log of angular frequency (lnω) for Ni{sub 0.5}Zn{sub 0.5}Fe{sub 2-x}Cr{sub x}O{sub 4} nanoferrites at room temperature. - Highlights: • Cr doped mixed Ni-Zn ferrites were successfully synthesized by a newly developed WOWS sol gel technique. • The specific surface area and specific surface area to volume ratio increased with decrease in particle size. • The resonance peaks appeared in dielectric loss graphs, shifting towards low frequency with the increase in Cr concentration. • The prepared samples have the lowest values of the dielectric constant. • The dielectric constant were observed to be inversely proportional to square root of the AC resistivity. - Abstract: Cr{sup +3} doped Ni-Zn nanoferrite samples with composition Ni{sub 0.5}Zn{sub 0.5}Fe{sub 2-x}Cr{sub x}O{sub 4}(x = 0.1, 0.2, 0.3, 0.4) were synthesized With Out Water and Surfactant (WOWS) sol-gel technique. The structural, morphological and dielectric properties of the samples were investigated. The lattice constant, crystallite size, theoretical density and porosity of each sample were obtained from X-ray diffraction (XRD) data. The specific surface area and specific surface area to volume ratio increased with the decrease in the size of Cr{sup +3} doped Ni-Zn ferrite nanoparticles, as the concentration of Cr{sup +3} increased. The SEM analysis revealed that the particles were of nano size and of spherical shape. The dielectric parameters such as dielectric constant (ε′) and dielectric loss (tanδ) of all the samples as a function of frequency at room temperature were measured. The AC conductivity (σ{sub AC}) was determined from the dielectric parameters, which showed increasing trend with the rise in frequency.

36 MATERIALS SCIENCE↗

High-temperature strengthening mechanisms of Laves and B2 precipitates in a novel ferritic alloy

Precipitates of the Laves and B2 phases were engineered in a newly-designed advanced ferritic alloy. Under creep test at 650 °C with 120 MPa, the material showed a steady-state minimum creep rate of 1 × 10 –4 h –1 , about one order of magnitude lower than T91. Microstructural characterization of the ferritic alloy revealed primarily ductile and partially brittle fractures after the creep test. Coarse Laves phase (~ 1 µm) was observed associating with the brittle fracture, resulting in reduced creep ductility. However, fine Laves phase precipitates (~ 100 nm) helped the dimple-ductile fracture and strengthened the material through impeding the motion of dislocations and boundaries. Unlike the B2 precipitates remained coherent exerting the classic Orowan bypassing mechanism at the brittle location, some of the B2 precipitates at the ductile location became incoherent and can develop an attractive interaction with dislocations. In conclusion, this coherency change of B2 precipitates, together with the nucleation of ultrafine (~ 40 nm) Laves phase precipitates during the creep test, would compensate for the coarsening-induced loss of Orowan strengthening of coherent B2 precipitates.