High Temperature Photovoltaics Silicone Adhesives for Venus Surface

The harsh environment at the surface of Venus, with a low solar intensity, red-rich solar spectrum, high temperatures, and a corrosive acid environment, makes it a challenging location to use photovoltaics. For the design of photovoltaic power generation for future missions to Venus, solar arrays that can function at high temperatures under low light intensity must be developed, and a significant difficulty in this is achieving a long lifetime without degradation under Venus conditions. One issue that must be addressed is the encapsulation to protect the solar cells from the environment, and most particularly the transparent adhesive affixing the coverglass to the cells. In this paper the factors affecting the reliability and degradation of transparent silicone adhesives under Venus conditions are discussed.

Katampe, Ibrahim↗

Oxidation of Alumina-Forming MAX Phases in Turbine Environments

Protective coatings for high temperature turbine components are based on YSZ thermal barriers and oxidation resistant, alumina-forming NiAl or NiCoCrAlY bond coats. Ti2AlC and Cr2AlC MAX phases are thus of special interest because of good oxidation resistance and CTE that can match Al2O3 and YSZ. Their alumina scales grow according to cubic kinetics due to grain growth in the scale, with initial heating dominated by fast TiO2 growth. Protective cubic kinetics are also found in high pressure burner rig tests of MAXthal 211 Ti2AlC, but with reduced rates due to volatile TiO(OH)2 formation in water vapor. YSZ-coatings on bulk Ti2AlC exhibit remarkable durability up to 1300C in furnace tests and at least a 25x life advantage compared to superalloys. At another extreme, Cr2AlC is resistant to low temperature Na2SO4 hot corrosion and exhibits thermal cycling stability bonded to a superalloy disk material. Accordingly, sputtered Cr2AlC coatings on disk specimens prevented hot corrosion detriments on LCF. Breakaway oxidation (Ti2AlC), scale spallation (Cr2AlC), interdiffusion, and processing as coatings still present serious challenges. However the basic properties of MAX phases provide some unusual opportunities for use in high temperature turbines.

ceramics↗

Sandblasting nozzle

A nozzle for use with abrasive and/or corrosive materials is formed of sintered ceramic compositions having high temperature oxidation resistance, high hardness and high abrasion and corrosion resistance. The ceramic may be a binary solid solution of a ceramic oxide and silicon nitride, and preferably a ternary solid solution of a ceramic oxide, silicon nitride and aluminum nitride. The ceramic oxide is selected from a group consisting of Al2O3, Y2O3 and Cr2O3, or mixtures of those compounds. Titanium carbide particles are dispersed in the ceramic mixture before sintering. The nozzles are encased for protection from external forces while in use by a metal or plastic casing.

Perkins, G. S.↗

Wrapped Wire Detects Rupture Of Pressure Vessel

Simple, inexpensive technique helps protect against damage caused by continuing operation of equipment after rupture or burnout of pressure vessel. Wire wrapped over area on outside of vessel where breakthrough most likely. If wall breaks or burns, so does wire. Current passing through wire ceases, triggering cutoff mechanism stopping flow in vessel to prevent further damage. Applied in other situations in which pipes or vessels fail due to overpressure, overheating, or corrosion.

Hunt, James B.↗

Scattering defects in silver mirror coatings

Scatter centers common to protected silver have been investigated on a variety of space flight quality mirrors. The defects have been characterized as to number density, size, location within the film layer structure, and dependence on illumination angle. In addition the total integrated scatter values as a function of wavelength, humidity test soak time, and temperature have been determined for some mirrors. These submicrometer sized defects are believed to be the precursors of silver corrosion spots. A mechanism for their generation is proposed, and measures to reduce their occurrence are suggested.

Pellicori, S. F.↗

Novel Environmental Barrier Coatings for the Protection of SiC Components

Greater gas turbine engine efficiency is a major goal in aeronautics research often pursued through increased engine operating temperatures. However, it is necessary to replace the current hot-stage alloy components with more thermally robust parts, such as Silicon-based ceramics and composites. Unfortunately, these materials are still susceptible to the effects of oxidation, water vapor, and (Calcium-Magnesium-Alumino-Silicate) CMAS interaction, among other issues at high temperature. To mitigate these effects, environmental barrier coating (EBC) materials are employed to help control the rate of degradation to the underlying composite, but must also survive the corrosive environment. The current study explores new design space in Mg-based EBC materials with respect to microstructure, high temperature phase stability, volatilization in water vapor, as well as structure-property relationships at high temperature.

Kowalski, Benjamin A.↗

Extreme Environment Technologies for Space and Terrestrial Applications

Over the next decades, NASA's planned solar system exploration missions are targeting planets, moons and small bodies, where spacecraft would be expected to encounter diverse extreme environmental (EE) conditions throughout their mission phases. These EE conditions are often coupled. For instance, near the surface of Venus and in the deep atmospheres of giant planets, probes would experience high temperatures and pressures. In the Jovian system low temperatures are coupled with high radiation. Other environments include thermal cycling, and corrosion. Mission operations could also introduce extreme conditions, due to atmospheric entry heat flux and deceleration. Some of these EE conditions are not unique to space missions; they can be encountered by terrestrial assets from the fields of defense,oil and gas, aerospace, and automotive industries. In this paper we outline the findings of NASA's Extreme Environments Study Team, including discussions on state of the art and emerging capabilities related to environmental protection, tolerance and operations in EEs. We will also highlight cross cutting EE mitigation technologies, for example, between high g-load tolerant impactors for Europa and instrumented projectiles on Earth; high temperature electronics sensors on Jupiter deep probes and sensors inside jet engines; and pressure vessel technologies for Venus probes and sea bottom monitors. We will argue that synergistic development programs between these fields could be highly beneficial and cost effective for the various agencies and industries. Some of these environments, however, are specific to space and thus the related technology developments should be spear headed by NASA with collaboration from industry and academia.

extreme environments↗

Molten Silicate Reactivity with Environmental Barrier Coating Materials for Gas Turbine Engine Applications

Rare earth (RE) disilicates are utilized in environmental barrier coatings (EBCs) to protect SiC-based ceramic matrix composites (CMCs) from destructive reactions with water vapor and other combustion species. These coating materials, however, degrade when exposed to molten silicate deposits primarily composed of calcium-magnesium aluminosilicates (CMAS). Coating materials are exposed to CMAS by engine ingestion of dust particulates from terrestrial sources during operation. Due to continual increases in engine operating temperature, it is important to understand the high temperature thermochemical mechanisms that drive corrosion of these materials. This work focuses on characterizing reaction products between disilicates and CMAS and optimizing coating chemistries to mitigate damage.

Stokes, Jamesa L.↗

Space Shuttle Program Dual Docked Operations

Due to the ever-increasing visiting vehicle traffic to and from the International Space Station (ISS) during mated Orbiter/ISS missions, it became apparent to both the ISS Program (ISSP) and the Space Shuttle program (SSP) that there would arise occasions where a visiting vehicle docking and/or undocking could overlap when the Space Shuttle Orbiter was docked to the ISS, referred to as Dual Docked Operations (DDO). The primary concerns were that plumes from the visiting vehicles would cause contamination, corrosion, and erosion to Space Shuttle surfaces and present a toxicity hazard to ground personnel when processing the Space Shuttle after landing. This potential conflict provided the genesis for evaluating risk mitigations to gain maximum flexibility for managing potential visiting vehicle traffic to and from the ISS and to maximize launch and landing opportunities for all visiting vehicles. The overarching goal of this effort was to assess the viability and readiness of the SSP to protect for DDO on any given mission. To assess the viability of performing DDO, the ISSP delivered plume particle fluence (i.e., number of particles per unit area) and contamination deposition based on the visiting vehicle’s proximity operations to the SSP for evaluation. This paper summarizes the concept definition, studies, and analysis results generated by the SSP, ISSP, and Mission Operations Directorate (MOD) for implementing DDO involving the Orbiter and Russian vehicles (RVs). Discussion and results presented herein represent a generic assessment of the SSP and ISSP integrated safety and technical evaluations of DDO involving the Orbiter and RVs. Mission-specific analysis and operational impacts were conducted flight-by-flight as they arose.

Launch vehicles↗

Advanced Polymer

In the mid-1980's, Langley developed a polyimide sulfone, combining desirable properties of two classes of polymers. Composites and other products made from polyimide sulfone can be used with solvents and corrosive fluids, are light weight, low cost and can be easily fabricated for a wide range of industrial uses. High Technology Systems, Inc. obtained a license for the polymer and was awarded a Small Business Innovation Research (SBIR) contract for development in a powder form. Although its principal use is as a matrix resin for composites, the material can also be used as a high temperature structural adhesive for aircraft structures and as a coating for protection from heat and radiation for electronic components.

Source record↗

Electrodeposited Zinc-Nickel as an Alternative to Cadmium Plating for Aerospace Application

Corrosion evaluation studies were conducted on 4130 alloy steel samples coated with electrodeposited zinc-nickel and samples coated with electrodeposited cadmium. The zinc nickel was deposited by the selection electrochemical metallizing process. These coated samples were exposed to a 5-percent salt fog environment at 35 plus or minus 2 C for a period ranging from 96 to 240 hours. An evaluation of the effect of dichromate coatings on the performance of each plating was conducted. The protection afforded by platings with a dichromate seal was compared to platings without the seal. During the later stages of testing, deposit adhesion and the potential for hydrogen entrapment were also evaluated.

Mcmillan, V. C.↗

Stress corrosion cracking of a titanium alloy in chloride-containing liquid environments

Ti-8 Al-1 Mo-1 V was tested in solvents containing chloride, bromide or iodide ions. It was found that the region II plateau velocity could be correlated with the inverse of the viscosity for several solvents. It seems most likely that this reflects the influence of the viscosity on the diffusion coefficient of some species involved in a mass transfer process which limits the crack growth. Associated tests were performed in which the potential, pH and concentration of Cl- were varied, in some of the same solutions as used for the viscosity tests. It is concluded from these tests that the absence of cathodic protection against cracking in solutions of low pH arises from an ohmic effect which isolates the crack tip from external potential control.

Smyrl, W. H.↗

Chromium and reactive element modified aluminide diffusion coatings on superalloys - Environmental testing

The high temperature performance of reactive element (RE)-doped and Cr/RE-modified aluminide diffusion coatings on commercial Ni-base alloy substrates was determined. In isothermal oxidation at 1100 C in air, RE-doped aluminide coatings on IN 713LC substrates formed a continuous slow-growing n-Al2O3 scale after 44 hrs of exposure. The coatings were protected by either an outer ridge Al2O3 scale with an inner compact Al2O3 scale rich in RE or by a continuous compact scale without any noticeable cracks or flaws. The cyclic oxidation behavior of Cr/RE-modified aluminide coatings on Rene 80 and IN 713LC alloys and of RE-doped aluminide coatings on IN 713LC alloys at 1100 C in static air was determined. Pack powder entrapment from the powder contacting (PC) process detracted significantly from the overall cyclic oxidation performance. Type I hot corrosion behavior of Cr/RE-modified aluminide coatings on Rene 80 and Mar-M247 alloy substrates at 900 C in a catalyzed 0.1 percent SO3/O3 gas mixture was determined. The modified coatings produced from the PC arrangement provided significantly better resistance to hot corrosion attack than commercial low-activity aluminide coatings produced by the above pack arrangement.

Bianco, Robert↗

Conversion Coatings for Aluminum Alloys by Chemical Vapor Deposition Mechanisms

With the rise of environmental awareness and the renewed importance of environmentally friendly processes, the United States Environmental Protection Agency has targeted surface pre-treatment processes based on chromates. Indeed, this process has been subject to regulations under the Clean Water Act as well as other environmental initiatives, and there is today a marked movement to phase the process out in the near future. Therefore, there is a clear need for new advances in coating technology that could provide practical options for replacing present industrial practices. Depending on the final application, such coatings might be required to be resistant to corrosion, act as chemically resistant coatings, or both. This research examined a chemical vapor deposition (CVD) mechanism to deposit uniform conversion coatings onto aluminum alloy substrates. Robust protocols based on solutions of aryl phosphate ester and multi-oxide conversion coating (submicron) films were successfully grown onto the aluminum alloy samples. These films were characterized by X-ray Photoelectron Spectroscopy (XPS). Preliminary results indicate the potential of this technology to replace aqueous-based chromate processes.

Reye, John T.↗

External Tank - The Structure Backbone

The External Tank forms the structural backbone of the Space Shuttle in the launch configuration. Because the tank flies to orbital velocity with the Space Shuttle Orbiter, minimization of weight is mandatory, to maximize payload performance. Choice of lightweight materials both for structure and thermal conditioning was necessary. The tank is large, and unique manufacturing facilities, tooling, handling, and transportation operations were required. Weld processes and tooling evolved with the design as it matured through several block changes, to reduce weight. Non Destructive Evaluation methods were used to assure integrity of welds and thermal protection system materials. The aluminum-lithium alloy was used near the end of the program and weld processes and weld repair techniques had to be refined. Development and implementation of friction stir welding was a substantial technology development incorporated during the Program. Automated thermal protection system application processes were developed for the majority of the tank surface. Material obsolescence was an issue throughout the 40 year program. The final configuration and tank weight enabled international space station assembly in a high inclination orbit allowing international cooperation with the Russian Federal Space Agency. Numerous process controls were implemented to assure product quality, and innovative proof testing was accomplished prior to delivery. Process controls were implemented to assure cleanliness in the production environment, to control contaminants, and to preclude corrosion. Each tank was accepted via rigorous inspections, including non-destructive evaluation techniques, proof testing, and all systems testing. In the post STS-107 era, the project focused on ascent debris risk reduction. This was accomplished via stringent process controls, post flight assessment using substantially improved imagery, and selective redesigns. These efforts were supported with a number of test programs to simulate combined environments. Processing improvements included development and use of low spray guns for foam application, additional human factors considerations for production, use of high fidelity mockups during hardware processing with video review, improved tank access, extensive use of non destructive evaluation, and producibility enhancements. Design improvements included redesigned bipod fittings, a bellows heater, a feedline camera active during ascent flight, removal of the protuberance airload ramps, redesigned ice frost ramps, and titanium brackets replaced aluminum brackets on the liquid oxygen feedline. Post flight assessment improved due to significant addition of imagery assets, greatly improving situational awareness. The debris risk was reduced by two orders of magnitude. During this time a major natural disaster was overcome when Katrina damaged the manufacturing facility. Numerous lessons from these efforts are documented within the paper.

Welzyn, Kenneth↗

Lightning Protection System for Space Shuttle

The suitability and cost effectiveness of using a lightning mast for the shuttle service and access tower (SSAT) similar to the type used for the Apollo Soyuz Test Project (ASTP) mobile launcher (ML) was evaluated. Topics covered include: (1) ASTP launch damage to mast, mast supports, grounded overhead wires, and the instrumentation system; (2) modifications required to permit reusing the ASTP mast on the SSAT; (3) comparative costing factors per launch over a 10 year period in repetitive maintenance and refurbishment of the existing and modified masts, mast supports, grounded overhead wires, and ground instrumentation required to sustain mechanical and electrical integrity of the masts; (4) effects of blast testing samples of the ASTP ML type mast (corrosion and electrical flashover); (5) comparison of damages from ASTP launch and from blast testing.

Source record↗

Corrosion on Mars: Effect of the Mars Environment on Spacecraft Materials

This report presents the results of a one-year project, funded by NASA’s Kennedy Space Center Innovation Fund in FY18, to conduct a theoretical study on the effect of the Mars environment on spacecraft materials. Corrosion resistance is one of the most important properties in selecting materials for landed spacecraft and structures that will support surface operations for the human exploration of Mars. Currently, the selection of materials is done by assuming that the corrosion behavior of a material on Mars will be the same as that on Earth. This is understandable since there is no data on the corrosion resistance of materials in the Mars environment. However, given that corrosion is defined as the degradation of a metal that results from its chemical interaction with the environment, it cannot be assumed that corrosion is going to be the same in both environments since they are significantly different. The goal of this research was to develop a systematic approach to understand corrosion of spacecraft materials on Mars by conducting a literature search of available data, relevant to corrosion in the Mars environment. This project was motivated by the suggestion, by a team of researchers, that some of the structural degradation observed on Curiosity's wheels may have been caused by corrosive interactions with the transient liquid brines, reported to be present on Mars, while the most significant damage was attributed to rock scratching. An extensive literature search, on data relevant to corrosion on Mars, confirmed the need to investigate the interaction between materials, used for spacecraft and structures designed to support long-term surface operations on Mars, and the Mars environment. Previous preliminary experiments, designed to look at the interaction between aerospace aluminum alloy (AA7075-T73) and the gases present in the Mars atmosphere, at 20 degC and a pressure of 700 Pa, showed that there is an interaction between the small amount of oxygen present in the Mars gas and the alloy, when there is a scratch that removes the protective aluminum oxide film. Further studies are needed to consider many other important components of the Mars environment that can affect this interaction such as: the presence of brines, the interaction between these brines and materials, the effect of radiation on these interactions, and the possible catalytic effects of the clays present in the Martian regolith. This theoretical study provides strong justification to conduct experimental work to investigate the interaction between spacecraft materials with simulated Martian environments to reduce Mars exploration costs.

Calle, Luz M.↗

Surface effects of corrosive media on hardness, friction, and wear of materials

Hardness, friction, and wear experiments were conducted with magnesium oxide exposed to various corrosive media and also with elemental iron and nickel exposed to water and NaOH. Chlorides such as MgCl2 and sodium containing films were formed on cleaved magnesium oxide surfaces. The MgCl2 films softened the magnesium oxide surfaces and caused high friction and great deformation. Hardness was strongly influenced by the pH value of the HCl-containing solution. The lower the pH, the lower the microhardness. Neither the pH value of nor the immersion time in NaOH containing, NaCl containing, and HNO3 containing solutions influenced the microhardness of magnesium oxide. NaOH formed a protective and low friction film on iron surfaces. The coefficient of friction and the wear for iron were low at concentrations of NaOH higher than 0.01 N. An increase in NaOH concentration resulted in a decrease in the concentration of ferric oxide on the iron surface. It took less NaOH to form a protective, low friction film on nickel than on iron.

Miyoshi, K.↗