Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “BRITTLENESS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 451 records · Page 25

Effect of Zinc Interlayer in Microstructure Evolution and Mechanical Properties in Dissimilar Friction Stir Welding of Aluminum to Titanium

The welding of aluminum (Al) and titanium (Ti) is difficult and challenging due to the differences in their chemical and physical properties, and the formation of brittle intermetallic phases. In the present experiment, a zinc (Zn) interlayer was used during friction stir welding of Al to Ti. The weld was characterized in detail to understand the mechanisms associated with microstructural evolution and improvement in mechanical properties of the weld. X-ray computed tomography results reveal three-dimensional distribution of particles and flakes of titanium in the weld nugget. It was also observed that Ti particles are inhomogeneously distributed in the weld and the distribution depends on their morphology. Such a distribution of Ti was informative in understanding material flow. In addition, the consolidation of Zn in the Al matrix reveals the nature of material flow in the weld nugget as well. The importance of the Zn interlayer and mechanism of phase formation was explored in this study. It was characterized that the mechanical mixing of Zn with Al and Ti alters phase evolution and restricts the formation of conventional Al{sub 3}Ti intermetallic phase. The presence of zinc homogenizes elemental distribution and inhibits the formation of brittle intermetallic phases, which leads to a substantial improvement in mechanical properties of the weld.

36 MATERIALS SCIENCE↗

Role of Si in the Surface Damage Mechanism of RB-SiC/Si Under Mechanical Loading

Indentation test (Nanoindentation and Vickers indentation), diamond scratching and high spindle speed grinding are conducted to investigate the role of silicon (Si) in the surface damage behavior of reaction-bonded SiC/Si composites (RB-SiC/Si). Even though the addition of Si contributes to densifying the bulk materials and improving the toughness, the indentation and diamond scratching results firstly indicate that the cracks initiate at the SiC/Si interfaces due to the non-uniform deformation caused by the existence of Si, and the phase transformation of Si also leads to the pop-out effect during the nanoindentation and the diamond scratching test. The ground surface of RB-SiC/Si is characterized by scratching grooves and brittle fracture, indicating the ductile material removal mode and brittle material removal mode for RB-SiC/Si, respectively, and the surface reliefs form on the ground surface due to the different hardness between Si and SiC phases. Moreover, the phase transformation of Si contributes to the easy fracture of phase boundaries under the mechanical loading, and the accompanied volume change also results in the dislodgement of hard particles and the generation of surface burs on the ground surface.

36 MATERIALS SCIENCE↗

Dry Sliding Wear Resistance of Cobalt Boride Coatings Formed on ASTM F1537 Alloy

New results about the wear resistance of CoB-Co{sub 2}B coatings under dry sliding conditions were estimated in this work. The cobalt boride coatings were developed at the surface of the ASTM F1537 alloy by means of the powder-pack boriding process using two experimental conditions: 1223 K with 6 h of exposure and 1273 K with 10 h of exposure. Before the sliding wear tests, Vickers depth-sensing microindentation tests were conducted on the cross section of the cobalt boride coatings to estimate the distribution of hardness, Young’s modulus, and residual stresses. Otherwise, the sliding wear tests were performed on both boriding conditions and on the untreated material, using a ball-on-flat configuration comprised of an alumina ball as a counterpart with applied loads between 5 and 20 N. The wear rates of the borided ASTM F1537 alloy were ranged between 4.02 and 8.91 × 10{sup −6} mm{sup 3} N{sup −1} m{sup −1} compared with the values of the untreated material (13.90 and 15.78 × 10{sup −6} mm{sup 3} N{sup −1} m{sup −1}) for the overall set of experimental conditions; nevertheless, the influence of boriding conditions (1273 K with 10 h of exposure) tended to increase the CoB coating thickness, developing a more brittle layer that decreased the sliding wear resistance at the surface of the borided ASTM F1537 alloy. Finally, the presence of failure mechanisms on the surface of the wear tracks was analyzed for both borided ASTM F1537 alloy and untreated material.

36 MATERIALS SCIENCE↗

Cu Interlayer-Induced High-Strength Laser-Welded AISI 304 Steel-Niobium Joint

Joining niobium to austenitic stainless steel is necessary for the fabrication of particle accelerators. However, the brittle iron-niobium intermetallics formed in the joint significantly reduce the joint strength. Copper was used as an interlayer to prevent the brittle phase formation while joining niobium to AISI 304 steel. The laser beam was first focused on the Cu-steel faying surface and then on the Cu-Nb faying surface. The tensile strength of the joint is greater than that of the Nb. The weld microstructure consists of austenite with Cu-rich precipitates along with the austenitic grain boundaries and Cu-rich phase embedded with Nb-rich particles and dendrites. Solid solution strengthening of Cu by Fe and second-phase strengthening of Cu by Nb play a critical role in improving the mechanical properties of the joint. These results highlight new possibilities for the joining of niobium to steel.

36 MATERIALS SCIENCE↗

Effect of Tungsten Inert Gas Arc Remelting on Microstructure and Wear Properties of Plasma-Sprayed NiCr-Cr{sub 3}C{sub 2} Coating

In this work, a NiCr-Cr{sub 3}C{sub 2} coating was prepared on an AISI 1045 steel substrate by plasma spraying and then remelted with the tungsten inert gas (TIG) arc method. The purpose was to study the effects of TIG remelting treatment on the microstructure, mechanical properties and wear properties of a plasma-sprayed NiCr-Cr{sub 3}C{sub 2} coating. The results show that after TIG remelting, the density of the coating increased, the internal porosity decreased from 8.1 to 0.2%, and the number of cracks and inclusions greatly reduced. The hardness of the coating also became uniform and increased from 1007 to 1141 HV{sub 0.1}, with an obvious increase of 13.3%, and the fracture toughness increased by 321.3%. The wear volume after TIG remelting at room temperature was reduced by 59.5%, and the wear pattern changed from brittle fracture and abrasive wear to abrasive wear and adhesive wear. The wear loss at 700 °C was also reduced by 43.6%, and the wear pattern was transformed from brittle fracture and fatigue wear caused by oxidation to oxidative wear and adhesive wear. Therefore, TIG remelting treatment can effectively improve the microstructure, mechanical properties and wear resistance of a plasma-sprayed NiCr-Cr{sub 3}C{sub 2} coating.

36 MATERIALS SCIENCE↗

Integrative Materials Design of Three-Phase Mo-Si-B Alloys

Mo-Si-B alloys can offer higher temperature capability than Ni-base superalloys with proper balancing of the creep, ductility, and oxidation resistance through microstructure optimization. Mo-Si-B alloys are heterogeneous, containing both brittle and ductile phases and interfaces. Therefore, the phase fractions, their distributions, and their constitutive properties over the range of room temperature to maximum use temperature must be considered. This work addresses here the optimization of mechanical properties for three-phase Mo-Si-B alloys. Three modeling tools are employed: microstructure generators to re-create statistically realistic microstructures, crystal viscoplasticity constitutive equations implemented for use with finite element solvers to capture microplasticity, and reduced-order models for evaluating important mechanical properties. In particular, the effects of microstructure on elastic modulus, yield strength, fatigue resistance, and susceptibility to brittle microcracking are considered. A novel reduced-order model is introduced for the evaluation of susceptibility to microcracking at phase interfaces. It is found that the Si content of the α-Mo phase is much more significant to the alloy’s balance of mechanical properties than the α-Mo volume fraction.

36 MATERIALS SCIENCE↗

Fabrication, structure and mechanical properties of indium nanopillars

Solid and hollow cylindrical indium pillars with nanoscale diameters were prepared using electron beam lithography followed by the electroplating fabrication method. The microstructure of the solid-core indium pillars was characterized by scanning micro-X-ray diffraction, which shows that the indium pillars were annealed at room temperature with very few dislocations remaining in the samples. The mechanical properties of the solid pillars were characterized using a uniaxial microcompression technique, which demonstrated that the engineering yield stress is {approx}9 times greater than bulk and is {approx}1/28 of the indium shear modulus, suggesting that the attained stresses are close to theoretical strength. Microcompression of hollow indium nanopillars showed evidence of brittle fracture. This may suggest that the failure mode for one of the most ductile metals can become brittle when the feature size is sufficiently small.

36 MATERIALS SCIENCE↗

An investigation of the microstructure and ductility of annealed cold-rolled tungsten

Tungsten is notoriously brittle metal at room temperature. Furthermore, contrary to most metals, plastic deformation increases ductility and recrystallization decreases ductility of tungsten. The fundamentals that govern this behavior have challenged academia and industry for decades. This paper focuses on understanding the controlling factors of ductility through a systematic investigation of the changes in microstructure and mechanical properties of cold-rolled tungsten that occur during annealing. Cold-rolled tungsten samples were annealed at temperatures up to 1400 °C, and mechanical testing and microstructural analysis was performed before and after annealing. Furthermore, a dislocation mobility model based on the Orowan equation was applied. The mechanisms of deformation are discussed within the context of deformed and annealed microstructures. The high fraction of low angle grain boundaries and high density of edge dislocations were found to be the most important factors for ductility. Although there were gradual changes in microstructure and mechanical properties, the ductility of cold-rolled tungsten was maintained up to 1300 °C. The material recrystallized when annealed above this temperature, had no ductility, and suffered brittle fracture. Microstructural characterizations of the as-rolled material revealed a typical BCC texture, with grains elongated in rolling direction and a large amount of edge dislocations and low angle grain boundaries. The level of texturing and the fraction of low angle grain boundaries diminished after recrystallization. It was found that, compared to the recrystallized material, as-rolled tungsten can accommodate over 7 orders of magnitude higher deformation velocity due to the high density of edge dislocations.

36 MATERIALS SCIENCE↗

A eutectic dual-phase design towards superior mechanical properties of heusler-type ferromagnetic shape memory alloys

Heusler-type ferromagnetic shape memory alloys possess attractive multifunctional properties, including magnetic field induced shape memory effect, magnetoresistance and magnetocaloric effect, owing to the unique concurrent magnetic and martensitic transformations. However, these intermetallics generally exhibit intrinsic high brittleness and low strength, which severely impede their workability for processing and applicability in real use. In this study, we demonstrate a new grain refining strategy by means of eutectic solidification to improve the mechanical properties in Ni-Mn-Sn-Fe alloys. In a fully eutectic microstructure, the average γ lamellae thickness was refined to ~170 nm and the composite showed a compressive strength of 1950 MPa, ductility of 19.5%, Young’s Modulus of 38 GPa, pseudoelasticity of 3.2% and high mechanical cyclic stability. The high mechanical performance is attributed to the effect of departmentalization of the brittle Heusler alloy by the densely distributed γ phase fine lamellae in resisting crack propagation. The eutectic Heusler composite exhibited a metamagnetic phase transformation, with a magnetic entropy change of 10.2 J/kg·K and a refrigeration capacity of 168 J/kg in a field change of 5 T.

36 MATERIALS SCIENCE↗

Hierarchically-structured large superelastic deformation in ferroelastic-ferroelectrics

Large superelastic deformation in ferroelastic-ferroelectrics (FMs) is a complex phenomenon involving multiple mechanisms operating simultaneously. Understanding how these mechanisms contribute corporately is critical to apply this useful property to the intrinsically brittle FMs, which can therefore display both excellent functional and mechanical performance. Here, we have directly observed and quantitatively analyzed in situ in a transmission electron microscope the three main mechanisms of twinning domain, phase transformation and mobile point defect contributing to extremely large superelastic deformation in single-crystal BaTiO 3 (5.0% strain) and Pb(Mg 1/3 Nb 2/3 )O 3 -PbTiO 3 (10.1% strain). Finally, our results reveal the hierarchical origin of large recoverable strain in “brittle” FMs.

36 MATERIALS SCIENCE↗

Creep and failure at metal-oxide interfaces

Small-scale bicrystal creep experiments were performed on contacts formed via in situ high-temperature diffusion bonding of metal-oxide interfaces including Ag-ZrO 2 , Pd-ZrO 2 , Pt-ZrO 2 , and Ag-high entropy oxide. This work characterizes deformation and failure at metal-oxide interfaces during mechanical loading. Interfacial sliding can be activated easily, while tensile interfacial creep was not observed at any condition of stress or temperature measured. Plastic strain, instead, localizes within the metal under tensile loading. A variety of mechanisms for plastic strain occur in the metal including lattice dislocation-mediated plasticity, twinning, low-angle grain boundary formation, and low-angle grain boundary creep. Surface and low-angle grain boundary diffusion occur under conditions where no metal-oxide tensile creep is observed, highlighting the significant differences in their interfacial mechanical response. High-temperature interfacial failure occurs when the mean curvature at the contact neck is approximately zero and the applied stresses comparable to brittle fracture stresses. The brittle fracture stresses were measured to be σ ƒ = 180 ± 90 MPa at the Ag-ZrO 2 interface at 225 °C, σ ƒ = 460 ± 160 MPa at the Pd-ZrO 2 interface at 680 °C, and σ ƒ = 640 ± 440 MPa at the Pt-ZrO 2 interface at 1010 °C.

Creep↗

Phase-field modeling and experiments of dynamic fracture in single crystal quartz

Predicting the onset and characteristics of brittle fracture is important for a wide range of engineering and geological material applications. In this paper, we study important aspects of brittle fracture in α-quartz by phase-field modeling and experiments using a top-down approach. In the modeling framework, the work term in the Griffith energy balance is replaced with internal energy contributions that represent surface energy, thermal energy, and elastic strain energy stored in defects. This allows parametrization of individual energy contributions in terms of internal state variables and keeps track of energy partitioning after the onset of fracture. The path and history dependence of fracture is included in evolution laws for internal state variables, e.g., entropy evolution, while the energy remains a true potential. In the experimental part, dynamic compression experiments coupled with X-ray phase contrast imaging are performed on cube-like samples with a hole. In the top-down analysis, dynamic compression and three point bending experiments from the literature are simulated with the developed phase-field damage model. In conclusion, the fitted model highlights the strain rate, size, and stress state dependence of damage nucleation and evolution in single crystal α-quartz.

36 MATERIALS SCIENCE↗

Fatigue performance of laser powder bed fusion hydride-dehydride Ti-6Al-4V powder

We report hydride-dehydride (HDH) Ti-6Al-4V alloy with particle size distribution of 50–120 µm is laser powder bed fusion (L-PBF) processed using optimum processing parameters and a near-fully dense structure with a density of 99.9 % is achieved. Microstructural observations and phase analyses indicate formation of columnar β grains with acicular α/α' phases in as-built condition. The roughness of the as-fabricated samples is significant with an average roughness of R a = 15.71 ± 3.96 µm and a root mean square roughness of R rms = 108.4 ± 24.9 µm, however, both values are reduced to R a = 0.19 ± 0.04 µm and R rms = 4.9 ± 0.6 µm after mechanical grinding. Mechanical tests are carried out on as-fabricated specimens followed by stress relief treatment. All samples are tested to failure in fatigue, under fully-reversed tension-compression conditions of R = –1. The as-built samples failed from the surface with crack initiation mainly at micro-notches, whereas after mechanically grinding, crack initiation changed to subsurface defects such as pores. Minimizing surface roughness by mechanically grinding eliminates surface micro-notches which improves fatigue strength in the high cycle fatigue region. Fatigue notch factor calculations showed that the effect of surface roughness was significantly lower when HDH powder is used compared to standard spherical powder. X-ray diffraction analysis revealed an in-plane compressive stress, micro-strain and grain refinement on the surface of the mechanically ground samples. Fractography observations (macroscale) revealed a fully brittle fracture in the first stage of crack growth with a transition to a dominantly ductile fracture in the third stage of crack growth. On the other hand, at the micro scale, even the brittle fracture regions showed evidence of ductile fracture within the α' martensite laths.

36 MATERIALS SCIENCE↗

Green co-solvent-assisted one-pot synthesis of high-performance flexible lignin polyurethane foam

Although lignin is a promising candidate as a source of polyol for producing eco-friendly polyurethane foam (PUF), its direct application has limitations, primarily stemming from the brittleness of the resulting products and poor processibility at high lignin loadings. To address these technical challenges, we introduced an effective co-solvent for the lignin-based polyurethane foams (LPUFs) with up to 80wt% of lignin substitution for petroleum polyols. As a green co-solvent that involves carbon dioxide fixation during its production, propylene carbonate (PC), was blended with lignin and improved the distribution of lignin by decreasing the viscosity, providing a room-temperature reaction. The LPUFs demonstrated a comparable thermal insulation performance (R-values greater than 5 in -1 ) with commercially available PUF with a uniform size of closed-cell structure induced by the reduced viscosity of lignin-based polyol. LPUFs also showed enhanced fire retardancy and moisture resistance compared to the control PUFs, benefiting from lignin’s intrinsic fire-resistant and hydrophobic properties. To mitigate the brittleness issue at high lignin loadings, flexible polyethylene glycols (PEGs) with a high molecular weight (i.e., PEG-1000) were dissolved in PC at room temperature to further improve the mechanical strength of LPUFs. The compressive strength of LPUFs with 80 wt% lignin substitution content was remarkably improved to 226 kPa by the employment of co-solvent and PEG-1000 compared to the control PUF (<140 kPa). Moreover, the flexibility of the LPUFs was successfully controlled by simply adjusting the PEG-400/PEG-1000 ratio. In conclusion, the results of this study provide valuable insights for accelerating and broadening the utilization of lignin in sustainable materials and manufacturing areas.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Novel processing route for design and manufacturing of metal toughened nanoceramics: Al–Al 2 O 3 nanocermets

Monolithic alumina is a highly brittle ceramic with a very low fracture toughness, making it an unreliable material for mechanical and structural applications. Ceramic-metal composites (cermets) are the subject of intensive interest to obtain materials which can address the intrinsic brittleness of ceramics without compromising their high strength and light weight. In the present investigation, aluminium-alumina (Al–Al 2 O 3 ) nanocermets were developed. The nanocermets possessed the toughness of Al phase and the strength of reinforced nano Al 2 O 3 particles. Here, the nanocermets green bodies were prepared such that upon sintering each adjacent Al 2 O 3 grain was conformally coated with a continuous Al film. Mechanical milling via a combination of cryo-milling and ball-milling was used to prepare Al–Al 2 O 3 nano-powder mixture. Spark plasma sintering was used to consolidate the green nanocermets. Results show that specimens prepared from 35 h milled powders exhibited superior mechanical properties as compared to other nanocermets, with an improvement in microhardness, elastic modulus, compressive strength, and flexural strength by 88%, 78%, 69% and 40% with respect to sintered pure Al. The indentation toughness of 35 h milled nanocermet showed an increment of 12.5% with respect to sintered pure Al 2 O 3 . Characterization techniques such as XRD, SEM, HR-TEM, X-ray tomography were employed to investigate the phase evolution and structural morphology, while FEM simulations were performed for understanding the crack propagation mechanisms in nanocermets.

36 MATERIALS SCIENCE↗

A mixed-mode phase field fracture model in anisotropic rocks with consistent kinematics

Under a pure tensile loading, cracks in brittle, isotropic, and homogeneous materials often propagate such that pure mode I kinematics are maintained at the crack tip. However, experiments performed on geo-materials, such as sedimentary rock, shale, mudstone, concrete and gypsum, often lead to the conclusion that the mode I and mode II critical fracture energies/surface energy release rates are distinctive. This distinction has great influence on the formation and propagation of wing cracks and secondary cracks from pre-existing flaws under a combination of shear and tensile or shear and compressive loadings. To capture the mixed-mode fracture propagation, a mixed-mode I/II fracture model that employs multiple critical energy release rates based on Shen and Stephansson, IJRMMS, 1993 is reformulated in a regularized phase field fracture framework. Here we obtain the mixed-mode driving force of the damage phase field by balancing the microforce. Meanwhile, the crack propagation direction and the corresponding kinematics modes are determined via a local fracture dissipation maximization problem. Several numerical examples that demonstrate mode II and mixed-mode crack propagation in brittle materials are presented. Possible extensions of the model capturing degradation related to shear/compressive damage, as commonly observed in sub-surface applications and triaxial compression tests, are also discussed.

42 ENGINEERING↗

A chain stretch-based gradient-enhanced model for damage and fracture in elastomers

Similar to quasi-brittle materials, it has been recently shown that elastomers can exhibit a macroscopically diffuse damage zone that accompanies the fracture process. In this study, we introduce a stretch-based gradient-enhanced damage (GED) model that allows the fracture to localize and also captures the development of a physically diffuse damage zone. This capability contrasts with the paradigm of the phase field method for fracture, where a sharp crack is numerically approximated in a diffuse manner. Capturing fracture localization and diffuse damage in our approach is achieved by considering nonlocal effects that encompass network topology, heterogeneity, and imperfections. These considerations motivate the use of a statistical damage function dependent upon the nonlocal deformation state. From this model, fracture toughness is realized as an output. While GED models have been classically utilized for damage modeling of structural engineering materials (e.g., concrete), they face challenges when trying to capture the cascade from damage to fracture, often leading to damage zone broadening (de Borst and Verhoosel, 2016). This deficiency contributed to the popularity of the phase-field method over the GED model for elastomers and other quasi-brittle materials. Other groups have proceeded with damage-based GED formulations that prove identical to the phase-field method (Lorentz et al., 2012), but these inherit the aforementioned limitations. To address this issue in a thermodynamically consistent framework, we implement two modeling features (a nonlocal driving force bound and a simple relaxation function) specifically designed to capture the evolution of a physically meaningful damage field and the simultaneous localization of fracture, thereby overcoming a longstanding obstacle in the development of these nonlocal strain- or stretch-based approaches. Here, we discuss several numerical examples to understand the features of the approach at the limit of incompressibility, and compare them to the phase-field method as a benchmark for the macroscopic response and fracture energy predictions.

Elastomers↗

Anisotropic thermal-conductivity degradation in the phase-field method accounting for crack directionality

Dynamic loads applied to metals may lead to brittle or ductile fracture depending on the imposed strain rates, material properties, and specimen geometry. With an increase in the applied velocity, brittle to ductile failure mode transition may also be observed. Furthermore, at high strain rates, ductile fracture may be preceded by shear bands, which are narrow bands of intense plastic deformation, typically accompanied by a significant rise in temperature. Reliable models are needed to predict the response of metals subject to dynamic loads. In particular, capturing the interplay between heat conduction and crack propagation using the phase-field fracture method is still an open research field. To accurately capture the heat transfer physics across crack surfaces, damage models degrading thermal-conductivity are necessary. While isotropic thermal-conductivity degradation models were proposed, they may lead to errors as they are indifferent to crack directionality. In our current work, a new anisotropic approach is proposed in which thermal-conductivity, which depends on the phase-field gradient, is degraded solely across the crack. Here, it is shown that this approach improves the near-field approximation of temperature and heat flux compared with isotropic degradation, when taking the discontinuous crack solutions as reference. Additionally, the anisotropic degradation approach is implemented in a unified dynamic fracture model and a couple of examples demonstrate the viability of this approach.

42 ENGINEERING↗