Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Anode”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 451 records · Page 25

Stabilizing Graphite Anode in Electrolytes with Nanoscale Anion Networking for High-Rate Lithium Storage

Graphite is the preferred anode material in commercial lithium-ion batteries (LIBs), but its limited compatibility with various organic molecules restricts the electrolyte solvent options. The primary challenge is solvent co-intercalation with Li ions, leading to graphite layer exfoliation. As a result, electrolyte selection often relies on ethylene carbonate (EC)-based solvents. Here, in this study, we introduce electrolytes featuring a nanoscale anion network ordering that hinders the liquid-phase exfoliation of graphite. This network, formed from concentrated long-chain lithium salts, traps free dioxolane (DOL) molecules, reducing the interactions between graphite particles and solvents during Li intercalation. Our findings reveal a mechanism that stabilizes graphite in otherwise unstable solvents with concentrated salts like LiTFSI, providing key insights for improving LIB performance by addressing electrolyte limitations on graphite anodes.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Pressure-Tolerant 3D Anodes Enable Short-Circuit Prevention and Low Heat Generation in Argyrodite Solid-State Batteries

Solid-state batteries (SSBs) offer a safer, higher-energy-density alternative to lithium-ion batteries, yet commercialization is hindered by incompatibility with lithium metal. Here, to overcome these challenges, we developed a cost-effective, commercially available prelithiated micro carbon fiber framework (Li-Cf) anode featuring a high-pressure-tolerance, for use with argyrodite solid-state electrolytes (SSEs). This 3D structure accommodates uniform lithium deposition, simplifies cell assembly under elevated pressure, inhibits dendrite growth toward SSEs, reduces heat generation, and enhances overall compatibility. Notably, our architecture enables the cell to tolerate pressures up to 400 MPa without short-circuiting during assembly. Meanwhile, the 3D framework serves as a preferential pathway for lithium deposition, thereby reducing lithium growth toward the SSEs and mitigating the risk of dendrite formation in SSEs. Operando calorimetry and distribution of relaxation times analysis reveal that lithium morphology degradation at the interface with the SSEs is a key failure mechanism in lithium metal argyrodite SSBs, leading to increased diffusion resistance and heat generation. In contrast, the Li-Cf anode mitigates these issues by reducing both heat flux and charge transfer resistance. Full cells with LiNi 0.8 Co 0.1 Mn 0.1 O 2 /Li 6 PS 5 Cl/Li-Cf retain ~79% capacity after 600 cycles, demonstrating significantly improved cycling stability and strong potential for practical energy storage applications.

25 ENERGY STORAGE↗

Texture Evolution of Plated Lithium in Anode-Free Solid-State Batteries

Here, this study investigates lithium plating texture in anode-free solid-state batteries using synchrotron-based X-ray diffraction. Conventional methods are limited by lithium’s low electron density and softness, which hinders direct interrogation in anode-free solid-state batteries. Results reveal that lithium plating texture is influenced by temperature and current density. Under mild conditions, lithium exhibited a ⟨110⟩ fiber texture. However, higher current densities and elevated temperatures led to a more randomized orientation, suggesting a dependence on plating conditions. The results highlight how the operating and processing conditions for lithium metal can influence the texture of lithium metal and reversible operation.

36 MATERIALS SCIENCE↗

Anode-less Solid-State Li–S Batteries Enabled by Fe-Stabilized Polysulfides

Anode-less solid-state lithium-sulfur batteries (SSLSBs) with lithium sulfide (Li 2 S) as the cathode promise a high energy density and ease of manufacturing. However, Li 2 S is plagued by poor conductivity, sluggish activation kinetics, and a poor cycle life. Here, in this study, we report an FeCl 3 -activated Li 2 S (FLS) cathode with solid-state polysulfide intermediates generated through a redox reaction between FeCl 3 and Li 2 S. This strategy is shown to boost the electrical conductivity of Li 2 S by 7 orders of magnitude and lower the activation barrier. During cycling, Fe plays a significant role in stabilizing the highly active polysulfide species, contributing to the exceptional electrochemical performance. The FLS cathode achieves 80% capacity retention over 500 cycles with >99% Li 2 S utilization. Furthermore, a Li-metal-free (anode-less) full cell retained over 80% of its initial capacity after 240 cycles. This work underscores the promise of leveraging Fe-stabilized polysulfides in enabling high-energy, long-lasting, solid-state Li-S batteries.

25 ENERGY STORAGE↗

Challenges in Lithium Metal Anodes for Solid-State Batteries

In this Perspective, we highlight recent progress and challenges related to the integration of lithium metal anodes in solid-state batteries. While prior reports have suggested that solid electrolytes may be impermeable to lithium metal, this hypothesis has been disproven under a variety of electrolyte compositions and cycling conditions. Herein, we describe the mechanistic origins and importance of lithium filament growth and interphase formation in inorganic and organic solid electrolytes. Multimodal techniques that combine real and reciprocal space imaging and modeling will be necessary to fully understand nonequilibrium dynamics at these buried interfaces. Currently, most studies on lithium electrode kinetics at solid electrolyte interfaces are completed in symmetric Li–Li configurations. To fully understand the challenges and opportunities afforded by Li-metal anodes, full-cell experiments are necessary. Lastly, the impacts of operating conditions on solid-state batteries are largely unknown with respect to pressure, geometry, and break-in protocols. Given the rapid growth of this community and the diverse portfolio of solid electrolytes, we highlight the need for detailed reporting of experimental conditions and standardization of protocols across the community.

25 ENERGY STORAGE↗

Synthesizing Highly Crystalline Graphite Powder from Bulk Polyethylene Waste for Lithium-Ion Battery Anodes

Upcycling plastic waste into graphite can potentially be used, in conjunction with other methods, to manage existing waste materials and diversify graphite supply chains. However, synthesizing large quantities of crystalline graphite powder from plastic waste, particularly polyethylene (PE), remains a challenge because PE decomposes into light gases during thermal processing and simple methods do not exist at any appreciable size scale to address this challenge. In this work, a method is developed for air processing bulk forms of PE waste to create stable carbon char that does not readily decompose during high-temperature processing. This method employs solid additives in the form of salts, which are combined with the PE melt during air processing to increase the effective surface area of the melt and improve the oxygen-driven chemistry that stabilizes PE for high-temperature processing. After removal of the solid salt additives from the PE-derived char, it is converted into a highly crystalline bulk graphite powder using an Fe-based catalytic process. The PE-derived graphite anode in a lithium-ion coin cell showed a specific capacity of 345 mAh/g at 0.05C with an initial Coulombic efficiency of 87% and reversible capacity retention of ~100% at different current rates. It also showed a specific capacity of up to 313 mAh/g at 0.5 discharge/charge cycles per hour (0.5C) and Coulombic efficiency of 99.9% after 250 cycles, indicating excellent electrochemical performance as an anode material for lithium-ion batteries. This method illustrates that there are opportunities for upcycling large quantities of PE waste to produce graphite powders suitable for use in LIBs.

25 ENERGY STORAGE↗

Metallicity, Atomic Disorder, and Li-Ion Storage in Fast-Charging Anodes

Oxides of Nb with Wadsley-Roth shear structures comprise a family of stable, high-rate anode materials for Li-ion batteries. A particular pair of them offers the unusual opportunity to test how important metallic conduction of the starting electrode is for electrode performance. The selected pair of compounds with similar 4 × 3 Wadsley-Roth block structures are insulating Ti 2 Nb 10 O 29 and metallic Nb 12 O 29 . A combination of diffraction, electrochemistry, magnetic measurements, and entropic potential measurements is employed to establish key findings for these two anode materials. We find that starting with a metallic oxide is not especially advantageous over a comparable material that readily transitions into a metallic state upon lithiation. Second, the rate performance appears to be dictated by ion mobility, and atomic Ti/Nb disorder in Ti 2 Nb 10 O 29 contributes to improved capacity retention at high rates by suppressing Li-ion ordering. However, subtle details in the nature of redox processes make Nb 12 O 29 a slightly better electrode material for long-term cycling at slower rates.

crystal structure↗

Mechanical rolling formation of interpenetrated lithium metal/lithium tin alloy foil for ultrahigh-rate battery anode

To achieve good rate capability of lithium metal anodes for high-energy-density batteries, one fundamental challenge is the slow lithium diffusion at the interface. Here we report an interpenetrated, three-dimensional lithium metal/lithium tin alloy nanocomposite foil realized by a simple calendering and folding process of lithium and tin foils, and spontaneous alloying reactions. The strong affinity between the metallic lithium and lithium tin alloy as mixed electronic and ionic conducting networks, and their abundant interfaces enable ultrafast charger diffusion across the entire electrode. Furthermore, we demonstrate that a lithium/lithium tin alloy foil electrode sustains stable lithium stripping/plating under 30 mA cm -2 and 5 mAh cm -2 with a very low overpotential of 20 mV for 200 cycles in a commercial carbonate electrolyte. Cycled under 6 C (6.6 mA cm -2 ), a 1.0 mAh cm -2 LiNi 0.6 Co 0.2 Mn 0.2 O 2 electrode maintains a substantial 74% of its capacity by pairing with such anode.

25 ENERGY STORAGE↗

Hierarchical porous silicon structures with extraordinary mechanical strength as high-performance lithium-ion battery anodes

Abstract Porous structured silicon has been regarded as a promising candidate to overcome pulverization of silicon-based anodes. However, poor mechanical strength of these porous particles has limited their volumetric energy density towards practical applications. Here we design and synthesize hierarchical carbon-nanotube@silicon@carbon microspheres with both high porosity and extraordinary mechanical strength (>200 MPa) and a low apparent particle expansion of ~40% upon full lithiation. The composite electrodes of carbon-nanotube@silicon@carbon-graphite with a practical loading (3 mAh cm −2 ) deliver ~750 mAh g −1 specific capacity, <20% initial swelling at 100% state-of-charge, and ~92% capacity retention over 500 cycles. Calendered electrodes achieve ~980 mAh cm −3 volumetric capacity density and <50% end-of-life swell after 120 cycles. Full cells with LiNi 1/3 Mn 1/3 Co 1/3 O 2 cathodes demonstrate >92% capacity retention over 500 cycles. This work is a leap in silicon anode development and provides insights into the design of electrode materials for other batteries.

25 ENERGY STORAGE↗

In-situ anodic precipitation process for highly efficient separation of aluminum alloys

Electrorefining process has been widely used to separate and purify metals, but it is limited by deposition potential of the metal itself. Here we report in-situ anodic precipitation (IAP), a modified electrorefining process, to purify aluminium from contaminants that are more reactive. During IAP, the target metals that are more cathodic than aluminium are oxidized at the anode and forced to precipitate out in a low oxidation state. This strategy is fundamentally based on different solubilities of target metal chlorides in the NaAlCl4 molten salt rather than deposition potential of metals. The results suggest that IAP is able to efficiently and simply separate components of aluminum alloys with fast kinetics and high recovery yields, and it is also a valuable synthetic approach for metal chlorides in low oxidation states.

36 MATERIALS SCIENCE↗

Three-dimensional hierarchically porous MoS 2 foam as high-rate and stable lithium-ion battery anode

Architected materials that actively respond to external stimuli hold tantalizing prospects for applications in energy storage, wearable electronics, and bioengineering. Molybdenum disulfide, an excellent two-dimensional building block, is a promising candidate for lithium-ion battery anode. However, the stacked and brittle two-dimensional layered structure limits its rate capability and electrochemical stability. Here we report the dewetting-induced manufacturing of two-dimensional molybdenum disulfide nanosheets into a three-dimensional foam with a structural hierarchy across seven orders of magnitude. Our molybdenum disulfide foam provides an interpenetrating network for efficient charge transport, rapid ion diffusion, and mechanically resilient and chemically stable support for electrochemical reactions. These features induce a pseudocapacitive energy storage mechanism involving molybdenum redox reactions, confirmed by in-situ X-ray absorption near edge structure. The extraordinary electrochemical performance of molybdenum disulfide foam outperforms most reported molybdenum disulfide-based Lithium-ion battery anodes and state-of-the-art materials. This work opens promising inroads for various applications where special properties arise from hierarchical architecture.

25 ENERGY STORAGE↗

Mechanistic Understanding of Interphase-driven Aging in Silicon Anodes

Conventional solid electrolyte interphases (SEIs) strongly adhere to micro-silicon (µ-Si) and crack under volume changes, causing poor cycling performance. Nano-silicon improves cycling performance but remains costly with limited calendar life. Here potentiostatic ageing tests demonstrate that both calendar and cycle ageing are governed by SEI cracking and dissolution with different relative contributions. When the system is not dominated by SEI dissolution, the relative calendar life of Si anodes could correlates positively with their cycle life. LiF-rich SEI that enables long cycle life in µ-Si is therefore expected to enhance calendar life as well. Using this framework, we screened electrolytes, SEIs and electrodes and validated them with full-cell storage. LiF-rich SEI minimizes cracking and dissolution, enabling μ-Si to achieve excellent calendar life, whereas nano-silicon suffers from SEI dissolution and needs reduced electrolyte–electrode contact for better calendar life. This work clarifies calendar-ageing behaviour and accelerates electrolytes and SEI development for long-life Si anodes.

Johnson, Christopher S.↗

Spontaneous and reversible hollowing of alloy anode nanocrystals for stable battery cycling

High-capacity alloy anode materials for Li-ion batteries have long been held back by limited cyclability caused by the large volume changes during lithium insertion and removal. Hollow and yolk-shell nanostructures have been used to increase the cycling stability by providing an inner void space to accommodate volume changes and a mechanically and dimensionally stable outer surface. These materials, however, require complex synthesis procedures. Here, using in situ transmission electron microscopy, we show that sufficiently small antimony nanocrystals spontaneously form uniform voids on the removal of lithium, which are then reversibly filled and vacated during cycling. This behaviour is found to arise from a resilient native oxide layer that allows for an initial expansion during lithiation but mechanically prevents shrinkage as antimony forms voids during delithiation. In this work, we developed a chemomechanical model that explains these observations, and we demonstrate that this behaviour is size dependent. Thus, antimony naturally evolves to form optimal nanostructures for alloy anodes, as we show through electrochemical experiments in a half-cell configuration in which 15-nm antimony nanocrystals have a consistently higher Coulombic efficiency than larger nanoparticles.

25 ENERGY STORAGE↗

Phase engineering of layered anode materials during ion-intercalation in Van der Waal heterostructures

Transition metal dichalcogenides (TMDs) are a class of 2D materials demonstrating promising properties, such as high capacities and cycling stabilities, making them strong candidates to replace graphitic anodes in lithium-ion batteries. However, certain TMDs, for instance, MoS 2 , undergo a phase transformation from 2H to 1T during intercalation that can affect the mobility of the intercalating ions, the anode voltage, and the reversible capacity. In contrast, select TMDs, for instance, NbS 2 and VS 2 , resist this type of phase transformation during Li-ion intercalation. This manuscript uses density functional theory simulations to investigate the phase transformation of TMD heterostructures during Li-, Na-, and K-ion intercalation. The simulations suggest that while stacking MoS 2 layers with NbS 2 layers is unable to limit this 2H → 1T transformation in MoS 2 during Li-ion intercalation, the interfaces effectively stabilize the 2H phase of MoS 2 during Na- and K-ion intercalation. However, stacking MoS 2 layers with VS 2 is able to suppress the 2H → 1T transformation of MoS 2 during the intercalation of Li, Na, and K-ions. The creation of TMD heterostructures by stacking MoS 2 with layers of non-transforming TMDs also renders theoretical capacities and electrical conductivities that are higher than that of bulk MoS 2 .

25 ENERGY STORAGE↗

Tutorial review on structure – dendrite growth relations in metal battery anode supports

This tutorial review explains the emerging understanding of the surface and bulk chemistry – electrochemical performance relations in anode supports (aka secondary current collectors, substrates, templates, hosts) for lithium, sodium and potassium metal batteries (LMBs, SMBs or NMBs, and KMBs or PMBs). In relation to each section, the possible future research directions that may yield both new insight and improved cycling behavior are explored. Representative case studies from Li, Na and K metal anode literature are discussed. The tutorial starts with an overview of the solid electrolyte interphase (SEI), covering both the “classic” understanding of the SEI structure and the “modern” insights obtained by site-specific cryogenic stage TEM analysis. Next, the multiple roles of supports in promoting cycling stability are detailed. Without an optimized support architecture, the metal–electrolyte interface becomes geometrically unstable at a lower current density and cycle number. Taking into consideration the available literature on LMBs, SMBs and KMBs, it is concluded that effective architectures are geometrically complex and electrochemically lithiophilic, sodiophilic or potassiophilic, so as to promote conformal electrochemical wetting of the metal during plating/stripping. One way that philicity is achieved is through support oxygen surface chemistry, which yields a reversibly reactive metal–support interface. Examples of this include the well-known oxygen–carbon moieties in reduced graphene oxide (rGO), as well as classic ion battery reversible conversion reaction oxides such as SnO 2 . Unreactive surfaces lead to dewetted island growth of the metal, which is a precursor to dendrites, and possibly to non-uniform dissolution. Surveying the literature on various Li, Na and K metal supports, it is concluded that the key bulk thermodynamic property that will predict electrochemical wetting behavior is the enthalpy of infinite solution (Δ sol H ∞ ) of the metal (solute) into the support (solvent). Large and negative Δ sol H ∞ promotes uniform metal wetting on the support surface, corresponding to relatively low plating overpotential. Positive Δ sol H ∞ promotes dewetted islands and a relatively high overpotential. This simple rule explains a broad range of studies on Li, Na and K metal – support interactions, including the previously reported correlation between mutual solubility and wetting.

25 ENERGY STORAGE↗

Failure modes of protection layers produced by atomic layer deposition of amorphous TiO 2 on GaAs anodes

Amorphous titanium dioxide (a-TiO 2 ) films formed by atomic layer deposition can serve as protective coatings for semiconducting photoanodes in water-splitting cells using strongly alkaline aqueous electrolytes. Herein, we experimentally examine the mechanisms of failure for p + -GaAs anodes coated with a-TiO 2 films (GaAs/a-TiO 2 ). Galvanic displacement of exposed GaAs by Au allowed imaging of pinholes in the a-TiO 2 coatings, and enabled collection of quantitative and statistical data associated with pinhole defects. A combination of imaging, electrochemical measurements, and quantitative analyses of corrosion products indicated that extrinsic pinholes were present in the a-TiO 2 films before electrochemical operation. During electrochemical operation these pinholes led to pitting corrosion of the underlying GaAs substrate. The dominant source of pinholes was the presence of atmospheric particulate matter on the GaAs surface during deposition of the a-TiO 2 layer. The pinhole density decreased substantially when the thickness of the a-TiO 2 coating increased beyond 45 nm, and approached zero when the thickness of the film exceeded 112 nm. The density of pinholes in films thinner than 45 nm decreased when the a-TiO 2 coating was deposited in an environmentally controlled cleanroom. Pinhole-free GaAs/a-TiO 2 devices were also tested via chronoamperometry to quantify the rate of pinhole formation during electrochemistry. The time-to-failure increased with thickness, suggesting that the failure mechanism may involve diffusion or migration through the film. However, other mechanisms may also contribute to the degradation of thicker films (>112 nm). Nevertheless, as previously hypothesized, extrinsic pinhole defects formed during deposition and testing control the short-term protective performance of the a-TiO 2 film for GaAs anodes evolving O 2 from water.

25 ENERGY STORAGE↗

Hierarchical assembly of ZnO nanowire trunks decorated with ZnO nanosheets for lithium ion battery anodes

Hierarchical architectures composed of nanomaterials in different forms are essential to improve the performance of lithium-ion battery (LIB) anodes. Here, we systematically studied the effects of hierarchical ZnO nanostructures on the electrochemical performance of LIBs. ZnO nanowire (NW) trunks were decorated with ZnO NWs or ZnO nanosheets (NSs) by successive hydrothermal synthesis to create hierarchical three-dimensional nanostructures. The branched ZnO NSs on the ZnO NW trunk exhibited a two-fold higher specific gravimetric capacity compared to ZnO NWs and branched ZnO NWs on ZnO NW trunks after 100 cycles of charging–discharging at 0.2C (197.4 mA g –1 ). The improvement in battery anode performance is attributable to the increased interfacial area between the electrodes and electrolyte, and the void space of the branched NSs that facilitates lithium ion transport and volume changes during cycling.

25 ENERGY STORAGE↗

Encapsulated Sb and Sb 2 O 3 particles in waste-tire derived carbon as stable composite anodes for sodium-ion batteries

A conductive network of waste-tire derived carbon (WTC) was used to produce homogeneous Sb/WTC and Sb 2 O 3 /WTC composite materials via ball milling as promising anodes for sodium-ion batteries (SIBs). Highly reversible redox peaks at 0.81/0.71, 0.25 V for Sb/WTC and 0.80/0.76, 0.21/0.26 V for Sb 2 O 3 /WTC anodes have been observed related to Na + intercalation and deintercalation in carbon and Na–Sb and Na 3 Sb as plausible conversion/alloy reactions. Sodium half-cells delivered reversible discharge capacities of 206 mA h g -1 and 207 mA h g -1 at a current density of 37 mA g -1 for the composite Sb/WTC and Sb 2 O 3 /WTC materials, respectively. Both the Sb/WTC and Sb 2 O 3 /WTC composite materials showed impressive capacity retention with 85% and 88%, respectively after 100 cycles. Furthermore, rate capability studies at 60 °C yielded an enhanced capacity of 240 mA h g -1 for Sb/WTC and 300 mA h g -1 for Sb 2 O 3 /WTC at 37 mA g -1 .

25 ENERGY STORAGE↗