Effect of processing on fracture toughness of silicon carbide as determined by Vickers indentations

Several alpha-SiC materials were processed by hot isostatic pressing (HIPing) and by sintering an alpha-SiC powder containing boron and carbon. Several beta-SiC materials were processed by HIPing a beta-SiC powder with boron and carbon additions. The fracture toughnesses K(sub 1c) of these beta- and alpha-SiC materials were estimated from measurements of Vickers indentations. The three formulas used to estimate K(sub 1c) from the indentation fracture patterns resulted in three ranges of K(sub 1c) estimates. Furthermore, each formula measured the effects of processing differently. All three estimates indicated that fine-grained HIPed alpha-SiC has a higher K(sub 1c) than coarsed-grained sintered alpha-SiC. Hot isostatically pressed beta-SiC, which had an ultrafine grain structure, exhibited a K(sub 1c) comparable to that of HIPed alpha-SiC.

Dannels, Christine M.↗

Effect of processing parameters on the characteristics of high-Tc superconductor YBa2Cu3Oy

SEM, thermogravimetric analysis, powder X-ray diffraction,and measurements of electrical resistivity and magnetic susceptibility, are presently used to characterize the influence of sintering temperature, sintering and annealing atmospheres, and quench-rate on the properties of the YBa2Cu3Oy superconducting oxide. It is established that annealing in oxygen, together with slow cooling rates, are required for preparation of high-Tc superconductors with sharp transitions; rapid quenching from high temperature does not yield good superconductors, due to low oxygen content.

Bansal, Narottam P.↗

Effects of various consolidation techniques on microstructure, strength, and reliability of alpha-SiC

The effects of slurry pressing, HIP, and sinter-HIP on the strength, microstructure, and critical processing flaws in alpha-SiC are examined. Also, the feasibility of glass encapsulation is determined. Baseline strength was improved by about 25 percent by using slurry pressing instead of dry pressing. HIP further improved average strength to as high as 655 MPa. Sinter-HIP did not noticeably improve average strength. Although process-related flaws such as shrinkage cracks and large voids were not seen in HIPed alpha-SiC, surface-related flaws were observed. It is suggested that surface finishing by lapping, polishing, and heat treating might reduce the effect of surface-related flaws, improving the Weibull modulus in HIPed alpha-SiC.

Dutta, Sunil↗

The chemistry of comets

Comets appear to represent a population of rather homogeneous objects. In particular, the original size distribution peaks at a mean diameter of the order of 10 km. Cometary dust grains appear to be made of clusters of extremely fine particles (0.1-1.0 micron) sintered by heat at a variable degree during their perihelion passages. The brightness laws of comets appear to be derived only by the sublimation of water ice or at least of gas hydrates of the clathrate type. Pristine nuclei are likely to be radially undifferentiated; only their crustal surface must be outgassed and sintered by the heat of perihelion passages. Comet Halley is confirmed to be in the same general class as the bright comets of the 1970s. With an organic fraction of 33 percent in the cometary dust, the carbon of Comet Halley is close to cosmic abundances.

Delsemme, A. H.↗

Copper Chloride Cathode For Liquid-Sodium Cell

Rechargeable liquid-sodium cell with copper chloride cathode offers substantial increase in energy density over cells made with other cathode materials. Unit has theoretical maximum energy density of 1135 W.h/kg. Generates electricity by electrochemical reaction of molten sodium and solid copper chloride immersed in molten electrolyte, sodium tetrachloroaluminate at temperature of equal to or greater than 200 degrees C. Wall of alumina tube separates molten electrolyte from molten sodium anode. Copper chloride cathode embedded in pores of sintered nickel cylinder or directly sintered.

Bugga, Ratnakumar V.↗

Millimeter wave surface resistance of RBa2Cu3O(7-delta) (R=Y,Eu,Dy,Sm,Er) superconductors

The measurements are reported of the millimeter wave surface resistance R(sub s) at 58.6 GHz of bulk samples of RBa2Cu3O(7-delta) (R = Y,Eu,Dy,Sm,Er) and of YBa2Cu3O(7-delta) superconducting films, in the temperature range from 20 to 300 K. The bulk samples were prepared by cold pressing the powders of RBa2Cu3O(7-delta) into one in. disks. The powders were prepared by several sinterings in one atmosphere of oxygen at 925 C, with grindings between sinterings, to obtain the superconducting phase. The thin films were deposited on SrTiO3 and LaGaO3 substrates by pulsed laser ablation. Each sample was measured by replacing the end wall of a gold-plated Te sub 013 circular mode copper cavity with the sample and determining the cavity quality factor . From the difference in the Q-factor of the cavity, with and without the sample, the R(sub s) of the sample was determined.

Miranda, F. A.↗

Microstructural changes in beta-silicon nitride grains upon crystallizing the grain-boundary glass

Crystallizing the grain-boundary glass of a liquid-phase-sintered Si3N4 ceramic for 2 h or less at 1500 C led to formation of delta-Y2Si2O7. After 5 h at 1500 C, the delta-Y2Si2O7 had transformed to beta-Y2Si2O7 with a concurrent dramatic increase in dislocation density within beta-Si3N4 grains. Reasons for the increased dislocation density are discussed. Annealing for 20 h at 1500 C reduced dislocation densities to the levels found in as-sintered material.

Lee, William E.↗

Radiographic Detection Of Voids In SiC And SiN Ceramics

Two reports describe experimental studies of efficacy of radiographic detection of voids in "green" (unfired) and sintered SiC and SiN ceramics. Projection radiography provides greater sensitivity of detection. Studies motivated by need for nondestructive technique to detect flaws limiting strengths of sintered structural ceramic components.

Baaklini, George Y.↗

Making Three-Layer Solid Electrolyte/Electrode Sandwiches

Tape-casting-and-sintering process joins two ceramic materials having widely different sintering temperatures into integral sandwich structure. Layers retain their identities, without migration of constituents. Used to make three-layer structure composed of outer porous layers of strontium-doped lanthanum manganite and inner dense layer of yttria-stabilized zirconia. Structures used to make electrolytic and fuels cells with solid electrolytes for use at high temperatures. Other potential applications include oxygen pumps and oxygen sensors.

Schroeder, James E.↗

Semiconductor structural damage attendant to contact formation in III-V solar cells

In order to keep the resistive losses in solar cells to a minimum, it is often necessary for the ohmic contacts to be heat treated to lower the metal-semiconductor contact resistivity to acceptable values. Sintering of the contacts, however can result in extensive mechanical damage of the semiconductor surface under the metallization. An investigation of the detailed mechanisms involved in the process of contact formation during heat treatment may control the structural damage incurred by the semiconductor surface to acceptable levels, while achieving the desired values of contact resistivity for the ohmic contacts. The reaction kinetics of sintered gold contacts to InP were determined. It was found that the Au-InP interaction involves three consecutive stages marked by distinct color changes observed on the surface of the Au, and that each stage is governed by a different mechanism. A detailed description of these mechanisms and options to control them are presented.

Fatemi, Navid S.↗

Crystallization and properties of Sr-Ba aluminosilicate glass-ceramic matrices

Powders of roller quenched (Sr,Ba)O-Al2O3-2SiO2 glasses of various compositions were uniaxially pressed into bars and hot isostatically pressed at 1350 C for 4 hours or cold isostatically pressed and sintered at different temperatures between 800 to 1500 C for 10 or 20 hours. Densities, flexural strengths, and linear thermal expansion were measured for three compositions. The glasss transition and crystallization temperatures were determined by Differential Scanning Calorimetry (DSC). The liquidus and crystallization temperature from the melt were measured using high temperature Differential Thermal Analysis (DTA). Crystalline phases formed on heat treatment of the glasses were identified by powder x ray diffraction. In Sr containing glasses, the monoclinic celsian phase always crystallized at temperatures above 1000 C. At lower temperatures, the hexagonal analog formed. The temperature for orthorhombic to hexagonal structure transformation increased monotonically with SrO content, from 327 C for BaO-Al2O3-2SiO2 to 758 C for SrO-Al2O3-2SiO2. These glass powders can be sintered to almost full densities and monoclinic celsian phase at a relatively low temperature of 1100 C.

Bansal, Narottam P.↗

Improved silicon carbide for advanced heat engines

The development of high strength, high reliability silicon carbide parts with complex shapes suitable for use in advanced heat engines is studied. Injection molding was the forming method selected for the program because it is capable of forming complex parts adaptable for mass production on an economically sound basis. The goals were to reach a Weibull characteristic strength of 550 MPa (80 ksi) and a Weibull modulus of 16 for bars tested in four-point loading. Statistically designed experiments were performed throughout the program and a fluid mixing process employing an attritor mixer was developed. Compositional improvements in the amounts and sources of boron and carbon used and a pressureless sintering cycle were developed which provided samples of about 99 percent of theoretical density. Strengths were found to improve significantly by annealing in air. Strengths in excess of 550 MPa (80 ksi) with Weibull modulus of about 9 were obtained. Further improvements in Weibull modulus to about 16 were realized by proof testing. This is an increase of 86 percent in strength and 100 percent in Weibull modulus over the baseline data generated at the beginning of the program. Molding yields were improved and flaw distributions were observed to follow a Poisson process. Magic angle spinning nuclear magnetic resonance spectra were found to be useful in characterizing the SiC powder and the sintered samples. Turbocharger rotors were molded and examined as an indication of the moldability of the mixes which were developed in this program.

Whalen, Thomas J.↗

FNAS materials processing and characterization

Research on melt-sintered high temperature superconducting materials is presented. The vibrating sample magnetometer has become a useful characterization tool for the study of high temperature superconductors. Important information regarding the superconducting properties of a sample can be obtained without actually making contact with the sample itself. A step toward microgravity processing of high temperature superconductors was taken. In the future, the samples need to be optimized prior to this processing of the sample before the specific effects of the microgravity environment can be isolated. A series of melt-sintered samples show that bulk processing of high temperature superconductors is getting better.

Golben, John P.↗

Microstructural changes in Beta-silicon nitride grains upon crystallizing the grain-boundary glass

Crystallizing the grain boundary glass of a liquid phase sintered Si3N4 ceramic for 2 h or less at 1500 C led to formation of gamma Y2Si2O7. After 5 h at 1500 C, the gamma Y2Si2O7 had transformed to beta Y2Si2O7 with a concurrent dramatic increase in dislocation density within beta Si3N4 grains. Reasons for the increased dislocation density is discussed. Annealing for 20 h at 1500 C reduced dislocation densities to the levels found in as-sintered materials.

Lee, William E.↗

Lifetime studies of high power rhodium/tungsten and molybdenum electrodes for application to AMTEC (alkali metal thermal-to-electric converter)

A detailed and fundamental model for the electrochemical behavior of AMTEC electrodes is developed which can aid in interpreting the processes which occur during prolonged operation of these electrodes. Because the sintering and grain growth of metal particles is also a well-understood phenomenon, the changes in electrode performance which accompany its morphological evolution may be anticipated and modeled. The grain growth rate observed for porous Mo AMTEC electrodes is significantly higher than that predicted from surface diffusion data obtained at higher temperatures and incorporated into the grain growth model. The grain growth observed under AMTEC conditions is also somewhat higher than that measured for Mo films on BASE (beta-alumina solid electrolyte) substrates in vacuum or at similar temperatures. Results of modeling indicate that thin Mo electrodes may show significant performance degradation for extended operation (greater than 10,000 h) at higher operating temperatures (greater than 1150 K), whereas W/Rh and W/Pt electrodes are expected to show adequate performance at 1200 K for lifetimes greater than 10,000 h. It is pointed out that current collection grids and leads must consist of refractory metals such as Mo and W which do not accelerate sintering or metal migration.

Williams, R. M.↗

Pool boiler heat transport system for a 25 kWe advanced Stirling conversion system

Experiments to determine alkali metal/enhanced surface combinations that have stable boiling at the temperatures and heat fluxes that occur in the Stirling engine are reported. Two enhanced surfaces and two alkali metal working fluids were evaluated. The enhanced surfaces were an EDM hole covered surface and a sintered-powder-metal porous layer surface. The working fluids tested were potassium and eutectic sodium-potasium alloy (NaK), both with and without undissolved noncondensible gas. Noncondensible gas (He and Xe) was added to the system to provide gas in the nucleation sites, preventing quenching of the sites. The experiments demonstrated the potential of an alkali metal pool boiler heat transport system for use in a solar-powered Stirling engine. The most favorable fluid/surface combination tested was NaK boiling on a -100 +140 mesh 304L stainless steel sintered porous layer with no undissolved noncondensible gas. This combination provided stable, high-performance boiling at the operating temperature of 700 C. Heat fluxes into the system ranged from 10 to 50 W/sq cm. The transition from free convection to nucleate boiling occurred at temperatures near 540 C. Based on these experiments, a pool boiler was designed for a full-scale 25-kWe Stirling system.

Anderson, W. G.↗

Crystallization and properties of Sr-Ba aluminosilicate glass-ceramic matrices

Powders of roller quenched (Sr,Ba)O-Al2O3-2SiO2 glasses of various compositions were uniaxially pressed into bars and hot isostatically pressed at 1350 C for 4 hours or cold isostatically pressed and sintered at different temperatures between 800 to 1500 C for 10 or 20 hours. Densities, flexural strengths, and linear thermal expansion were measured for three compositions. The glass transition and crystallization temperatures were determined by Differential Scanning Calorimetry (DSC). The liquidus and crystallization temperature from the melt were measured using high temperature Differential Thermal Analysis (DTA). Crystalline phases formed on heat treatment of the glasses were identified by powder X ray diffraction. In Sr containing glasses, the monoclinic celsian phase always crystallized at temperatures above 1000 C. At lower temperatures, the hexagonal analog formed. The temperature for orthorhombic to hexagonal structural transformation increased monotonically with SrO content, from 327 C for BaO-Al2O3-2SiO2 to 758 C for SrO-Al2O3-2SiO2. These glass powders can be sintered to almost full densities and monoclinic celsian phase at a relatively low temperature of 1100 C.

Bansal, Narottam P.↗

Thermochemical analysis of chemical processes relevant to the stability and processing of SiC-reinforced Si3N4 composite

Chemical processes relevant to the stability and processing of SiC-reinforced Si3N4 composites have been examined from thermochemical considerations. The thermodynamic stabilities of various interfaces, such as SiC-Si3N4, SiC-Si3N4-Si2ON2, and SiC-Si3N4-SiO2, have been examined as a function of temperature, and the temperatures above which these interfaces become unstable have been calculated. The degradation of SiC during the processing of the composite has been examined. The processing routes considered in this study include the reaction bonded silicon nitride (RBSN) process and the pressure-assisted sintering processes with suitable sintering additives.

Misra, Ajay K.↗