Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “nickel oxide”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 433 records · Page 24

Roles of Mn and Co in Ni-rich layered oxide cathodes synthesized utilizing a Taylor Vortex Reactor

It is reported that layered oxides, composed of nickel, manganese, and cobalt (NMC), are sought after as cathode materials which provide improved energy density, cycle life, and safety in commercial lithium ion batteries (LIBs). Increasing Ni contents higher than 80% can provide even higher practical discharge capacities >200 mAh/g and similar to ~4 V discharge potential vs Li/Li + , making them promising cathodes for next generation LIBs. However, rapid capacity fade during cycling and heat-related safety concerns are delaying their successful transition to industry. We report systematic performance optimization of LiNiO 2 , LiNi 0.9 Mn 0.1 O 2 , and LiNi 0.9 Co 0.1 O 2 high Ni layered oxide cathodes synthesized by utilizing a Taylor Vortex Reactor. Co-free LiNi 0.9 Mn 0.1 O 2 cathode showed 200 mAh/g highest discharge capacity at 0.1 C rate with 84% retention after 103 cycles at 0.3C rate while LiNi 0.9 Co 0.1 O 2 cathode showed higher initial but poor cycle life (225 mAh/g highest discharge capacity at 0.1C rate with only 56% capacity retention after 103 cycles at 0.3 C rate. Synchrotron based X-ray diffraction (SXRD), X-ray absorption spectroscopy (XAS) and focused ion beam (FIB) imaging of pristine and cycled cathodes after 103 cycles provided important information on degradation mechanism. The roles of Mn and Co on layered structure formation, charge balance, cationic mixing, and electrochemical performance were elucidated using the crystallographic information from XRD refinement and electronic state analysis from XAS providing valuable information to design future Ni-rich layered oxide cathodes.

25 ENERGY STORAGE↗

A technoeconomic analysis of poly- and single-crystalline NMCxyz from material synthesis to battery pack design

A process model was developed for estimating the cost of manufacturing lithium nickel manganese cobalt oxide (LiNi x Mn y Co z O 2 , NMCxyz), the main cathode active material in lithium-ion batteries used for electric vehicles in the United States. The model was used to estimate the prices of NMC622, NMC811, and NMC955 with poly- and single-crystalline morphologies. The Battery Performance and Cost Model (BatPaC) was used to translate the NMC prices into battery pack prices. A decrease in cobalt content from NMC622 (20% Co) to NMC955 (5% Ni) decreases the material price by $\$$0.85/kg (−3%) due to a decrease in the cost of battery materials, which account for >60% of the total price. NMC622 only produce cheaper packs if the nickel sulfate cost is > 4 × its baseline, indicating higher nickel materials will lower pack cost under normal market conditions. Single-crystalline materials are $\$$2/kg (+8%) more expensive than their polycrystalline counterparts due to higher manufacturing costs from longer, hotter calcinations in less densely packed saggars. This increases the pack price by ∼$\$$3/kWh, assuming identical electrochemical properties. In conclusion, the single-crystalline materials could yield cheaper packs if cycled to higher upper cutoff voltages (i.e., 4.35 to 4.43 V for the single-crystalline material vs. 4.25 V for their polycrystalline counterparts).

Cost modeling↗

The microscopic mechanisms of high temperature oxidation of Haynes 282

Nickel-based superalloy finds widespread applications in aerospace and extreme environments. They are known for their high temperature oxidation resistance under extended periods. However, the oxide formation and evolution which sets the stages for the later parabolic oxidation kinetics is not fully understood. This paper aims to provide new insights into the transient stage oxidation mechanism and kinetics of a typical Ni-based superalloy (Haynes 282). While tracking the chemical and microstructural evolution under micrometer scale at 800°C, we show that the oxide scale and its grain boundary species change significantly during the initial stages of oxidation and can have a profound impact on the oxidation kinetics. Cr 2 O 3 forms initially at the grain boundary along with minor amount of Al 2 O 3 . Then, the grain boundary region is enriched with copious amounts TiO 2 while Cr migrates away from the grain boundary. A noticeable change in the isothermal oxidation kinetics observed likely results from a mechanistic change from uniform surface oxidation to preferential outward diffusion of Ti 4+ ions through the grain boundary. Through first-principles calculations combined with energy dispersive spectroscopy, we confirmed the preferential outward diffusion of Ti 4+ ions as the diffusion barrier is lower for Ti than Cr along the grain boundaries. In conclusion, these findings highlight the critical role of early-stage grain boundary oxidation dynamics in dictating the long-term oxidation resistance of Ni-based superalloys and provide a foundation for future strategies to enhance their performance in extreme environments.

DFT↗

Long-term high-velocity oxidation and hot corrosion testing of several NiCrAl and FeCrAl base oxide dispersion strengthened alloys

Several oxide dispersion strengthened (ODS) alloys have been tested for cyclic, long-term, high gas-velocity resistance to oxidation at 1100 C and hot corrosion at 900 C. Both nominally Ni-16Cr-4Al and Fe-20Cr-4.5Al ODS alloys were subjected up to about 2500 cycles, where each cycle consisted of 1 hr in a hot, Mach 0.3 combusted gas stream followed by a 3-min quench in an ambient temperature, Mach 0.3 air blast. For comparison to existing technology, a coated superalloy was simultaneously tested. The ODS iron alloy exhibited clearly superior behavior, surviving 3800 oxidation and 2300 hot corrosion cycles essentially unscathed. While the ODS nickel alloys exhibited adequate oxidation resistance, the long-term hot corrosion resistance could be marginal, since the best life for such alloys under these conditions was only about 1100 cycles. However, the hot corrosion resistance of the ODS Ni-base alloys is excellent in comparison to that of traditional superalloys.

Lowell, C. E.↗

A High Energy–Density, Cobalt–Free, Low–Nickel LiNi 0.7 Mn 0.25 Al 0.05 O 2 Cathode with a High–Voltage Electrolyte for Lithium–Metal Batteries

Cobalt-free cathode materials have garnered increased attention for applications in next-generation batteries for electric vehicles, as cobalt is considered to have at a high supply chain risk. Here, the use of a localized saturated electrolyte (LSE) to enable stable cycling of a cobalt-free, low-nickel layered-oxide cathode LiNi 0.7 Mn 0.25 Al 0.05 O 2 (NMA-70) to higher voltages (4.6 V) in a lithium-metal battery is demonstrated. Compared to the baseline LP57 electrolyte, the LSE extends the cycle life from ≈100 cycles to ≈400 cycles before reaching 80% capacity retention. Visual indicators of cell degradation, such as product deposition, are observed on electrodes cycled in LP57. It is shown that cycling NMA-70 in LSE reduces the overall active material loss and overpotential growth during extended cycling. This is attributed to the formation of a beneficial fluorinated interphase layer, a lower degree of rock-salt phase formation, and a reduction in the gas evolution from the cathode surface. The decrease in gas evolution from the cathode cycled in LSE reflects a lower degree of electrolyte reactivity and an overall improvement in the safety characteristics of the cell. Furthermore, this study highlights the importance of a stable electrolyte to enable the high-voltage cycling of alternative, lower nickel, and cobalt-free cathodes.

25 ENERGY STORAGE↗

Isothermal and cyclic oxidation at 1000 and 1100 deg C of four nickel-base alloys: NASA-TRW VIA, B-1900, 713C, and 738X

The isothermal and cyclic oxidation resistance of four cast Ni-base gamma + gamma prime alloys, NASA-TRW Via, B-1900, 713C, and 738X, was determined in still air at 1000 and 1100 C. The oxidation process was evaluated by specific sample weight change with time, sample thickness change, X-ray diffraction of the scales, and sample metallography. The behavior is discussed in terms of the Cr, Al, and refractory metal contents of the alloys.

Barrett, C. A.↗

A Study on Advanced Lithium-Based Battery Cell Chemistries to Enhance Lunar Exploration Missions

NASA's Exploration Technology Development Program (ETDP) Energy Storage Project conducted an advanced lithium-based battery chemistry feasibility study to determine the best advanced chemistry to develop for the Altair lunar lander and the Extravehicular Activities (EVA) advanced lunar surface spacesuit. These customers require safe, reliable energy storage systems with extremely high specific energy as compared to today's state-of-the-art batteries. Based on customer requirements, the specific energy goals for the development project are 220 watt-hours per kilogram (Wh/kg) delivered at the battery level at 0 degrees Celsius (degrees Celcius) at a C/10 discharge rate. Continuous discharge rates between C/5 and C/2, operation over 0 to 30 degrees C, and 200 cycles are targeted. The team, consisting of members from NASA Glenn Research Center, Johnson Space Center, and Jet Propulsion laboratory, surveyed the literature, compiled information on recent materials developments, and consulted with other battery experts in the community to identify advanced battery materials that might be capable of achieving the desired results with further development. A variety of electrode materials were considered, including layered metal oxides, spinel oxides, and olivine-type cathode materials, and lithium metal, lithium alloy, and silicon-based composite anode materials. lithium-sulfur systems were also considered. Hypothetical cell constructs that combined compatible anode and cathode materials with suitable electrolytes, separators, current collectors, headers, and cell enclosures were modeled. While some of these advanced materials are projected to obtain the desired electrical performance, there are risks that also factored into the decision making process. The risks include uncertainties due to issues such as safety of a system containing some of these materials, ease of scaling-up of large batches of raw materials, adaptability of the materials to processing using established or reasonable cost manufacturing techniques, manufacturability of the materials in dimensions required for integration into battery cells of practical capacities, low Technology Readiness levels (TRl), and the ability to achieve the desired performance by the customer need dates. The advanced cell chemistry options were evaluated with respect to multiple quantitative and qualitative attributes while considering their projected performance at the end of the available development timeframe. Following a rigorous ranking process, a chemistry that combines a lithiated nickel manganese cobalt oxide (lithium NMC) cathode with a silicon-based composite anode was selected as the technology that can offer the best combination of safety, specific energy, energy density, and likelihood of success. Tasks over the next three years will focus on development of electrode materials, compatible electrolytes, and separator materials, and integration of promising components to assess their combined performance in working cells. Cells of the chosen chemistry will be developed to TRl 6 by 2014 and will then be transferred to the customers for infusion into their mission paths.

Reid, Concha↗

Interfacial Chemistry Involved in Selective Separation of NMC/LMO and LCO/LMO Binary Cathode Materials by Froth Flotation Using Oleic Acid

The variability in cathode compositions within recycled lithium-ion battery (LIB) feedstocks poses a significant challenge to efficient downstream refining processes. This study demonstrates the feasibility of using froth flotation with oleic acid as a collector to selectively separate lithium nickel-manganese-cobalt oxide (NMC) and lithium cobalt oxide (LCO) from lithium manganese oxide (LMO) materials. Laboratory-scale flotation tests achieved an 80% separation efficiency in a single stage, producing a froth product with >90% purity of NMC/LCO at approximately 90% yield. Concurrently, the LMO materials were enriched in the sink product with ∼90% purity and ∼90% yield. This approach was further validated using recycled cathode materials, confirming its applicability to realistic feedstocks. The underlying mechanism governing the selective separation of NMC/LCO from LMO was investigated using ζ-potential measurements, contact angle measurements, bubble-particle attachment experiments, and X-ray photoelectron spectroscopy (XPS) analysis. Both contact angle and bubble-particle attachment results confirmed that oleic acid adsorption rendered NMC and LCO surfaces hydrophobic, thereby enhancing flotation recovery. At pH 5, oleic acid adsorbed preferentially onto NMC and LCO surfaces via electrostatic interactions, while exhibiting minimal adsorption on LMO surfaces. However, separation efficiency deteriorated at higher pH, which was attributed to the co-flotation of LMO materials caused by oleate chemisorption on MnOH + species. This work establishes froth flotation as a viable cathode/cathode separation strategy, providing a low-cost, scalable pathway to preconcentrate and enrich nickel-rich and cobalt-rich cathode active materials from incompatible cathode chemistries for direct recycling or hydrometallurgical processing. Furthermore, this study reveals, for the first time, the mechanism of oleate adsorption on the surface of different cathode materials.

PH↗

Enhancing Cycling Stability of Lithium Metal Batteries by a Bifunctional Fluorinated Ether

Abstract The lifespan of lithium (Li) metal batteries (LMBs) can be greatly improved by the formation of inorganic‐rich electrode‐electrolyte interphases (EEIs) (including solid‐electrolyte interphase on anode and cathode‐electrolyte interphase on cathode). In this work, a localized high‐concentration electrolyte containing lithium bis(fluorosulfonyl)imide (LiFSI) salt, 1,2‐dimethoxyethane (DME) solvent and 1,2‐bis(1,1,2,2‐tetrafluoroethoxy)ethane (BTFEE) diluent is optimized. BTFEE is a fluorinated ether with weakly‐solvating ability for LiFSI so it also acts as a co‐solvent in this electrolyte. It can facilitate anion decomposition at electrode surfaces and promote the formation of more inorganic‐rich EEI layers. With an optimized molar ratio of LiFSI:DME:BTFEE = 1:1.15:3, LMBs with a high loading (4 mAh cm −2 ) lithium nickel manganese cobalt oxide (LiNi 0.8 Mn 0.1 Co 0.1 ) cathode can retain 80% capacity in 470 cycles when cycled in a voltage range of 2.8–4.4 V. The fundamental understanding on the functionality of BTFEE revealed in this work provides new perspectives on the design of practical high‐energy density battery systems.

25 ENERGY STORAGE↗

Layered Heterostructure Ionogel Electrolytes for High‐Performance Solid‐State Lithium‐Ion Batteries

Abstract Ionogel electrolytes based on ionic liquids and gelling matrices offer several advantages for solid‐state lithium‐ion batteries, including nonflammability, wide processing compatibility, and favorable electrochemical and thermal properties. However, the absence of ionic liquids that are concurrently stable at low and high potentials constrains the electrochemical windows of ionogel electrolytes and thus their high‐energy‐density applications. Here, ionogel electrolytes with a layered heterostructure are introduced, combining high‐potential (anodic stability: >5 V vs Li/Li + ) and low‐potential (cathodic stability: <0 V vs Li/Li + ) imidazolium ionic liquids in a hexagonal boron nitride nanoplatelet matrix. These layered heterostructure ionogel electrolytes lead to extended electrochemical windows, while preserving high ionic conductivity (>1 mS cm −1 at room temperature). Using the layered heterostructure ionogel electrolytes, full‐cell solid‐state lithium‐ion batteries with a nickel manganese cobalt oxide cathode and a graphite anode are demonstrated, exhibiting voltages that are unachievable with either the high‐potential or low‐potential ionic liquid alone. Compared to ionogel electrolytes based on mixed ionic liquids, the layered heterostructure ionogel electrolytes enable higher stability operation of full‐cell lithium‐ion batteries, resulting in significantly enhanced cycling performance.

Hyun, Woo Jin↗

Tailoring Binder Molecular Weight to Enhance Slurry-Cast NMC Cathodes for Sulfide Solid-State Batteries

We demonstrate for the first time the critical influence of binder molecular weight on the performance of slurry-cast lithium nickel manganese cobalt oxide (NMC) cathodes in sulfide-based all-solid-state batteries (SSBs). SSBs are increasingly recognized as a safer and potentially more efficient alternative to traditional Li-ion batteries, owing to the superior ionic conductivities and inherent safety features of sulfide solid electrolytes. However, the integration of high-voltage NMC cathodes with sheet-type sulfide solid electrolytes presents significant fabrication challenges. Our findings reveal that higher molecular weight binders not only enhance the discharge capacity and cycle life of these cathodes but also ensure robust adhesion and structural integrity. By optimizing binder molecular weights, we effectively shield the active materials from degradation and mechanical stress, significantly boosting the functionality and longevity of SSBs. These results underscore the paramount importance of binder properties in advancing the practical application of high-performance all-solid-state batteries.

25 ENERGY STORAGE↗

Direct Recycling of Blended Cathode Materials by Froth Flotation

We report that direct Li-ion battery recycling involves separating cathode active materials in the solid phase while preserving their electrochemical performance. To reuse the recycled ones in new batteries, it is necessary to separate individual cathode components, which would typically occur prior to the rejuvenation and any compositional reformulation processes. Herein, a froth flotation process is developed to separate pristine lithium nickel-manganese-cobalt oxide (LiNi 0.333 Mn 0.333 Co 0.333 O 2 , NMC111) and lithium manganese oxide (LMO) materials. The flotation results show that with multiple stages of the separation processes, a satisfactory separation is achieved with 95% grade or above of NMC111 in the froth product and 95% grade of LMO in the tailing product. The electrochemistry results show that the flotation chemicals have negligible impact on the electrochemical performance of recycled active materials, whereas the NMC111 exhibits a minor capacity fade after being in contact with deionized water at 2% solid concentration. An improvement in both the rate and cycling performance is achieved at 10% solid concentration or higher. It is found that there is little compositional and structural change to the aqueous recycled NMC111 powders. An effective and low-cost separation method for direct recycling mixed cathode compositions is demonstrated.

25 ENERGY STORAGE↗

Impact of heating and cooling loads on battery energy storage system sizing in extreme cold climates

Efficient operation of battery energy storage systems requires that battery temperature remains within a specific range. Current techno-economic models neglect the parasitic loads heating and cooling operations have on these devices, assuming they operate at constant temperature. In this work, these effects are investigated considering the optimal sizing of battery energy storage systems when deployed in cold environments. Here, a peak shaving application is presented as a linear programming problem which is then formulated in the PYOMO optimization programming language. The building energy simulation software EnergyPlus is used to model the heating, ventilation, and air conditioning load of the battery energy storage system enclosure. Case studies are conducted for eight locations in the United States considering a nickel manganese cobalt oxide lithium ion battery type and whether the power conversion system is inside or outside the enclosure. The results show an increase of 42% to 300% in energy capacity size, 43% to 217% in power rating, and 43% to 296% increase in capital cost dependent on location. This analysis shows that the heating, ventilation, and air conditioning load can have a large impact on the optimal sizes and cost of a battery energy storage system and merit consideration in techno-economic studies.

25 ENERGY STORAGE↗

Promising performance of sulfide catholytes compared to halide alternatives in NMC811 cathodes for sheet-type sulfide solid-state batteries

Sulfide-based solid-state batteries (SSBs) show promise in achieving energy densities over 350 Wh/kg, yet challenges persist with their incorporation of high-voltage, nickel-rich layered oxide cathodes, such as LiNi₀.₈Mn₀.₁Co₀.₁O₂ (NMC811), due to the poor oxidation stability of sulfide solid-state electrolytes (SSEs) like Li₆PS₅Cl (LPSCl). Although halide SSEs such as Li₃InCl₆ (LIC) and Li₃YCl₆ (LYC) have previously shown promise in stabilizing high-voltage NMC cathodes, our research reveals that sulfide SSE catholytes, particularly when combined with surface-coated NMC cathodes, deliver superior performance. Here, this investigation assesses the cycling stability of various catholytes—LPSCl, LIC, Li₁₀GeP₂S₁₂ (LGPS), combined LIC-LPSCl, and LYC-LPSCl—in SSBs with LiNbO₃-coated NMC811 cathodes against sheet-type LPSCl separators. Findings indicate that while LGPS-based cathodes maintain higher capacity retention, they yield lower deliverable capacity, and LIC cathodes experience significant electrochemical degradation. Importantly, our results underscore that sulfide SSE catholytes, in conjunction with LiNbO₃-coated cathodes, optimize the cathode-electrolyte interphase (CEI), enhancing both kinetics and mass transport. These insights provide a strategic direction for optimizing catholyte composition in the development of sheet-type sulfide-based SSBs.

Catholyte↗

Degradation and Modeling of Large-Format Commercial Lithium-Ion Cells as a Function of Chemistry, Design, and Aging Conditions

Demand for large-format (>10 Ah) lithium-ion batteries has increased substantially in recent years, due to the growth of both electric vehicle and stationary energy storage markets. The economics of these applications is sensitive to the lifetime of the batteries, and end-of-life can either be due to energy or power limitations. Despite this, there is little information from cell manufacturers on the sensitivity of cell degradation to environmental conditions or battery use. This work reports accelerated aging test data from four commercial large-format lithium-ion batteries from three manufacturers, with varying design (thickness, casings, ...), chemistry (lithium-iron-phosphate (LFP) or lithium-nickel-manganese-cobalt-oxide positive electrodes (NMC), with graphite (Gr) negative electrodes), and capacity (50 to 250 Amp hours). The tested LFP|Gr cell is found to be relatively insensitive to cycling conditions like temperature or voltage window, while NMC|Gr cells have varying sensitivity. Degradation trends are further investigated by training predictive models: simple polynomial trend lines, a semi-empirical reduced-order model, and an empirical reduced-order model identified using machine-learning based on symbolic regression. Calendar and cycle life are simulated over a variety of conditions to directly compare the various batteries. Cell size and thickness are found to substantially impact sensitivity to temperature during cycle aging, while electrode chemistry impacts depth-of-discharge sensitivity. Real-world battery lifetime is evaluated by simulating residential energy storage and commercial frequency containment reserve systems in several U.S. climate regions. Predicted lifetime across cell types varies from 7 years to 20+ years, though all cells are predicted to have at least 10 year life in certain conditions.

battery lifetime↗

A control oriented comprehensive degradation model for battery energy storage system life prediction

In order to ensure that stationary battery energy storage systems (BESSs) provide reliable energy buffering, both for power quality and economic purposes, the degradation must be considered. Cell degradation involves various side reactions and is highly dependent on its operating conditions. To accurately track cell degradation and predict its impact on battery behavior, a comprehensive physics-based degradation model based on an electrolyte phase-enhanced single particle (SP) model is developed. Key degradation physics, namely solid electrolyte interphase (SEI) layer formation and growth, Li plating on the graphite anode, and Mn dissolution on cathode of nickel-cobalt-manganese oxide (NMC622) are considered. The model is validated against experimental capacity data. The results reveal that the deposition rate of both SEI layer and Li metal increase as the charge voltage increases. At the cathode side, the solvent oxidation rate determines the Mn dissolution rate. As a result, the volume fraction of NMC622 in the cathode continually decreases at a gradually increasing rate.

25 ENERGY STORAGE↗

Fast charging of Li-ion cells: Effect of separator membranes and mapping of “safe lines” to avoid Li plating

An experimental method is introduced that uses microprobe Li/Cu reference electrodes to map "safe" charging regimes to avoid Li metal plating on graphite anodes at rates to 8C. With this method, a Li-ion cell closely approaches the Li plating condition but avoids descending into this regime. This "safe" approach is used to demonstrate effects of the microporous separator on Li plating in cells consisting of a layered nickel-manganese -cobalt oxide cathode and graphite anode. We argue that most of the difference in behaviors for different separators arises from time delayed Li + ion percolation through the membrane. In conclusion, our study suggests that explicitly treating kinetics of phase transitions in the lithiated graphite anode is essential for electrochemical models predicting "safe" lines for fast charging cells.

25 ENERGY STORAGE↗

Mitigating Calendar Aging in Si-NMC Batteries with Advanced Dual-Salt Glyme Electrolytes

In addressing the critical challenge of calendar aging in silicon (Si)-based lithium-ion batteries, this study introduces a groundbreaking strategy utilizing glyme-type dual-salt electrolytes (lithium bis(trifluoromethanesulfonyl)imide [LiTFSI] and lithium difluoro(oxalato)borate [LiDFOB]). These electrolytes are demonstrated to significantly mitigate parasitic reactions and capacity loss in Si-NMC (lithium nickel manganese cobalt oxide) full cells, especially when compared with traditional carbonate-based electrolytes. Further, our exhaustive mechanistic analysis reveals that such electrolytes not only preserve the integrity of the Si anode but also improve the cathode/electrolyte interphases (CEI) through the formation of a conformal coating on the high-voltage cathode surface. This dual-salt approach, enhanced by the addition of a phosphate additive, effectively decelerates calendar aging, marking a substantial advance in the quest for durable and reliable Si-based energy storage technologies. The findings underscore the vital role of electrolyte composition in extending the calendar life of Si batteries, offering an alternative avenue toward maximizing the performance and longevity of next-generation Li-Si batteries.

36 MATERIALS SCIENCE↗