Hydrogen Diffusion Coefficient Measures on Thin Film Uranium Oxide
Thin films of uranium oxides, putatively UO 2 and U 3 O 8 , were deposited on palladium/silver (75/25) foil discs (10 μm thick, 10 mm diameter). Methodology for sealing these foils, applying a hydrogen pressure (~ 1 atm) to the oxide side, and measuring the pressure on the permeate side (opposite side of foil) is reported. The experimental apparatus is held at 100 °C to speed diffusion, aided by the pressure differential across the foil (~1 atm (750 torr) on oxide side, initially low vacuum on permeate side, ~1x 10 -4 torr). Early results indicate an effective diffusion coefficient of roughly 7.66 x 10 -17 +/- 2.22 x 10 -17 cm 2 /sec for UO 2 . These values are in line with expectations and prior measures relative to large lag times for system baseline (substrate only). Evaluation of the technique for U 3 O 8 thin films suggests further development will be needed to extend the technique to more oxidized films (U 3 O 8 , UO 3 ). Characterization of the foils (thickness and speciation) post diffusion experiments will be carried out by SIGMA (Eric Tegtmeier and Andy Richards) in FY24 which will sharpen the uncertainty quantification for UO 2 diffusion coefficients, aiding the nucleation model for DRACO.