Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “ULTIMATE STRENGTH”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 433 records · Page 24

Investigation of Microstructures and Tensile Properties of 316L Stainless Steel Fabricated via Laser Powder Bed Fusion

In this study, a thorough investigation of the microstructures and tensile properties of 316L stainless steel fabricated via laser powder bed fusion (L-PBF) was done. 316L stainless steel specimens with two different thicknesses of 1.5 mm and 4.0 mm fabricated under similar conditions were utilized. Microstructural characterization was performed using optical microscopy (OM) and scanning electron microscopy (SEM) equipped with electron backscatter diffraction (EBSD). Melt pools and cellular structures were observed using OM, whereas EBSD was utilized to obtain the grain size, grain boundary characteristics, and crystallographic texture. The 1.5 mm thick sample demonstrated a yield strength (YS) of 538.42 MPa, ultimate tensile strength (UTS) of 606.47 MPa, and elongation to failure of 69.88%, whereas the 4.0 mm thick sample had a YS of 551.21 MPa, UTS of 619.58 MPa, and elongation to failure of 73.66%. These results demonstrated a slight decrease in mechanical properties with decreasing thickness, with a 2.4% reduction in YS, 2.1% reduction in UTS, and 5.8% reduction in elongation to failure. In addition to other microstructural features, the cellular structures were observed to be the major contributors to the high mechanical properties. Using the inverse pole figure (IPF) maps, both thicknesses depicted a crystallographic texture of {001} <101> in their as-built state. However, when subjected to tensile loads, texture transitions to {111} <001> and {111} <011> were observed for the 1.5 mm and 4.0 mm samples, respectively. Additionally, EBSD analysis revealed the pre-existence of high-density dislocation networks and a high fraction of low-angle grain boundaries. Interestingly, twinning was observed, suggesting that the plastic deformation occurred through dislocation gliding and deformation twinning.

316L stainless steel↗

Alloys For Corrosive, Hydrogen-Rich Environments

"NASA-23" denotes class of alloys resisting both embrittlement by hydrogen and corrosion. Weldable and castable and formed by such standard processes as rolling, forging, and wire drawing. Heat-treated to obtain desired combinations of strength and ductility in ranges of 100 to 180 kpsi yield strength, 120 to 200 kpsi ultimate tensile strength, and 10 to 30 percent elongation at break. Used in place of most common aerospace structural alloy, Inconel(R) 718.

Mcpherson, William B.↗

Oxidation resistant high-entropy alloys

Disclosed herein are new face-centered cubic (f.c.c.) high-entropy alloys with compositions (in atomic %) of Fe.sub.aNi.sub.bMn.sub.cAl.sub.dCr.sub.eC.sub.f where a is between 37-43 atomic %, b is between 8-14 atomic %, c is between 32-38 atomic %, d is 4.5-10.5 atomic %, e is between 2.5-9 atomic % and f is between 0-2 atomic %. The undoped alloy has strength of 159 MPa and 40% elongation to failure, but the doped, carbon-containing alloy having 1.1 atomic percent carbon has yield strength of 360 MPa, an ultimate tensile strength (UTS) of 1200 MPa and 50% elongation to failure at room temperature. At 700.degree. C., the yield strength is 214 MPa with 24% elongation to failure. Thus, the present alloy may replace austenitic stainless steels in applications where better strength is needed at both room temperature and elevated temperature in an oxidation resistant alloy.

Baker, Ian↗

Scaled-Up Fabrication of Thin-Walled ZK60 Tubing using Shear Assisted Processing and Extrusion (ShAPE)

Shear Assisted Processing and Extrusion (ShAPE) has been scaled-up and applied to direct extrusion of thin-walled magnesium tubing. Using ShAPE, billets of ZK60A-T5 were directly extruded into round tubes having an outer diameter of 50.8 mm and wall thickness of 1.52 mm. The severe shearing conditions inherent to ShAPE resulted in microstructural refinement with an average grain size of 3.8μm measured at the midpoint of the tube wall. Tensile testing per ATSM E-8 on specimens oriented parallel to the extrusion direction gave an ultimate tensile strength of 254.4 MPa and elongation of 20.1%. Specimens tested perpendicular to the extrusion direction had an ultimate tensile strength of 297.2 MPa and elongation of 25.0%. Due to material flow effects resulting from the simultaneous linear and rotational shear intrinsic to ShAPE, ram force and electrical power consumption during extrusion were just 40 kN and 11.5 kW respectively. This represents a significant reduction in ram force and power consumption compared to conventional extrusion. As such, there is potential for ShAPE to offer a scalable, lower cost extrusion option with potentially improved bulk mechanical properties.

Direct Extrusion↗

Optimization of matrix viscosity improves polypropylene fiber dispersion and properties of engineered cementitious composites

Engineered cementitious composites (ECC) is a durable cementitious material with high tensile ductility and strain-hardening characteristics. Although considered as a cost-effective fiber for ECC, polypropylene (PP) fiber is reportedly difficult to disperse in mortar matrix due to its high aspect ratio and hydrophobicity. In this study, the matrix viscosity of a low-carbon ECC based on limestone calcined clay cement was tailored as a variable to improve PP fiber dispersion under a pre-determined mixing protocol. The effect of matrix viscosity on the composite fresh and hardened properties was investigated experimentally. Results suggested an optimal range of matrix viscosity (10.3–11.5 Pa . s) favors the composite tensile strength and strain capacity at 28 days. At the optimal state with a 0.1 % viscosity modifying admixture (VMA)-to-binder mass ratio, PP-ECC achieved 7.0 % tensile strain capacity and 3.5 MPa ultimate tensile strength. When matrix viscosity falls outside the desired range, both ultimate tensile strength and strain capacity were diminished. By tailoring the VMA dosage, the matrix viscosity can be adjusted for desired fiber dispersion, workability, and mechanical properties. Finally, the findings of this study provide a technical reference for the practical design and application of PP-ECC.

36 MATERIALS SCIENCE↗

Thermal degradation of the tensile strength of unidirectional boron/aluminum composites

The variation of ultimate tensile strength with thermal treatment of B-Al composite materials and of boron fibers chemically removed from these composites in an attempt to determine the mechanism of the resulting strength degradation was studied. Findings indicate that thermally cycling B-Al represents a more severe condition than equivalent time at temperature. Degradation of composite tensile strength from about 1.3 GN/m squared to as low as 0.34 GN/m squared was observed after 3,000 cycles to 420 C for 203 micrometers B-1100 Al composite. In general, the 1100 Al matrix composites degraded somewhat more than the 6061 matrix material studied. Measurement of fiber strengths confirmed a composite strength loss due to the degradation of fiber strength. Microscopy indicated a highly flawed fiber surface.

Grimes, H. H.↗

Thermal degradation of the tensile strength of unidirectional boron/aluminum composites

The variation of ultimate tensile strength with thermal treatment of B-Al composite materials and of boron fibers chemically removed from these composites is studied systematically in an attempt to determine the mechanism of the resulting strength degradation. The results indicate that thermally cycling of B-Al represents a more severe condition than equivalent time at temperature. Degradation of composite tensile strength from about 1.3 GN/sq m to as low as 0.34 GN/sq m was observed after 3000 cycles to 420 C for 203-micron B-1100 Al composite. In general, the 1100 Al-matrix composites degraded somewhat more than the 6061 matrix material studied. Measurement of fiber strengths confirmed a composite strength loss due to the degradation of fiber strength. Microscopy indicated a highly flawed fiber surface. On the basis of various thermal-cycling studies and electron diffraction analysis, a mechanism is favored in which B reacts with Al, freshly exposed by cold working during cycling, to form AlB2. The nonuniform interface reaction leads to a highly flawed and weakened B fiber.

Grimes, H. H.↗

A Discussion of Strength Reduction Factor Development for Thermal Aging Effect on Nuclear Structural Alloys

In consideration of structural alloy property deterioration during long-term exposure to elevated temperatures, the yield and ultimate tensile strength reduction factors are provided in the Boiler and Pressure Vessel Code Section III for nuclear reactor component design and operation analysis. Because the Gen IV reactor requirement of 40 ~ 60 years of service life makes it difficult to acquire such long exposure test data for developing the reduction factors, they must be derived from test data with relatively short exposure by predictive methods considered to be reasonably reliable. A novel approach with a physically-based model has recently been proposed for application to development of reduction factors for 9Cr-1Mo-V. In the model, contributors to the tensile strength are first identified and related to definite microstructural features of the alloy, then some physically-based methods are employed to simulate the microstructural evolution, and finally the model is assembled with test-data-calibrated parameters to generate the yield and ultimate tensile strength reduction factors covering elevated temperature exposure for up to 57 years. The approach is undoubtedly a trailblazing development that will, if proven reliable, lead to a paradigm shift in predicting thermal aging behavior of many other alloys. Its debut application to Section III, however, concerns nuclear safety and naturally warrants objective, impartial, and thorough technical scrutiny. In the present paper, the novel and conventional approaches are discussed. Necessary improvements to the novel approach are recommended for its application to nuclear structural component design and analysis, and for its potential expanded use to other alloys.

Ren, Weiju↗

Cryogenic Treatment of CoCrFeMnNi(NbC) High-Entropy Alloys

The effect of cryogenic treatment on the microstructure and mechanical properties of CoCrFeMnNi and CoCrFeMnNi(NbC) high-entropy alloys was investigated during annealing. The heat-treated samples were characterized by optical microscopy, scanning electron microscopy–wavelength-dispersive x-ray spectroscopy, x-ray diffraction technique, differential scanning calorimetry, Vickers hardness testing and tensile testing. The results showed a single-phase FCC crystal structure matrix in both alloys during cryogenic treatment and annealing. Cryogenic treatment altered the recrystallization behavior of CoCrFeMnNi high-entropy alloy, while it did not influence the recrystallization of CoCrFeMnNi(NbC) high-entropy alloy. It was also found that cryogenic treatment changed the precipitation behavior of CoCrFeMnNi(NbC) high-entropy alloy during annealing. In both studied high-entropy alloys, the mechanical testing indicated that the cryogenic treatment can effectively reduce the yield strength of cold-rolled samples after annealing. This was primarily attributed to the effect of cryogenic treatment in enhancing crystalline defects annihilation. Furthermore, the cryogenic treatment increased the ultimate tensile strength of CoCrFeMnNi(NbC). A lager plastic deformation and precipitates were considered as the main reasons for the higher ultimate tensile strength.

36 MATERIALS SCIENCE↗

Effect of Decarburization on Notch Sensitivity and Fatigue-Crack-Propagation Rates in 12 MoV Stainless-Steel Sheet

Tests were conducted in order to determine the effect of surface decarburization on the notch sensitivity and rate of fatigue crack propagation in 12 MoV stainless-steel sheet at room temperature. Three specimen configurations were utilized in the course of the investigation: standard tensile specimen, 9-inch-wide specimens containing fatigue cracks or thread-cut notches of 0.005-inch radius, and 2-inch-wide specimens containing fatigue cracks. The 12 MoV stainless-steel sheet in the normal condition was found to have an ultimate tensile strength of 251 ksi and to be extremely notch sensitive. The material in the decarburized condition was found to have an ultimate tensile strength of 210 ksi and to be considerably stronger than the normal material in the presence of fatigue cracks. Decarburization did not appear to have any significant influence on the rate of fatigue crack propagation in the 2-inch-wide specimens at the stress levels considered. In addition to the tests, two methods for predicting residual static strength and their application to the material are discussed.

Herrnstein, William H., III↗

Effects of porosity on weld-joint tensile strength of aluminum alloys

Tensile properties in defect-free weldments of aluminum alloys 2014-T6 and 2219-T87 (sheet and plate) are shown to be related to the level or concentration of induced simulated porosity. The scatter diagram shows that the ultimate tensile strength of the weldments displays the most pronounced linear relationship with the level of porosity. The relationships between yield strength or elongation and porosity are either trivial or inconsequential in the lower and intermediate levels of porosity content. In highly concentrated levels of porosity, both yield strength and elongation values decrease markedly. Correlation coefficients were obtained by simple straight line regression analysis between the variables of ultimate tensile strength and pore level. The coefficients were greater, indicating a better correlation, using a pore area accumulation concept or pore volume accumulation than the accumulation of the pore diameters. These relationships provide a useful tool for assessing the existing aerospace radiographic acceptance standards with respect to permissible porosity. In addition, these relationships, in combination with known design load requirements, will serve as an engineering guideline in determining when a weld repair is necessary based on accumulative pore level as detected by radiographic techniques.

Lovoy, C. V.↗

Investigation on Microstructural Evolutions and Mechanical Properties of P92 Steel During Thermal Processing

The evolution of the microstructure of P92 steel during heat processing has a significant effect on the final performance of steel products and is thus an area of critical interest. Accordingly, the grain growth behavior of austenite and δ-ferrite changes in P92 steel is comprehensively investigated in this study through thermodynamic calculations and physical simulation. The results show that the A{sub C1}, A{sub C3} and γ–δ transformation temperatures of P92 steel are 841 °C, 878 °C and 1095 °C, respectively, which are comparable to the measured values of 850 °C, 879 °C and 1175 °C, respectively. When the temperature exceeds the A{sub C1} temperature, the austenite grain size increases with increasing temperature and longer holding times, and the growth rate of austenite grains increases with higher temperatures but decreases with holding time at a certain temperature. A model that shows the austenite grain growth kinetics is established: D{sup n} − D{sub 0}{sup n} = 2.03 × 10{sup 16}exp(− 498,770/RT)t, in which the time exponent n decreases from 4.52 to 2.11 with an increase in temperature from 1000 °C to 1200 °C due to the reduced pinning effect resultant of the dissolution of precipitates, M{sub 23}C{sub 6}, VX and NbX at 887 °C, 1073 °C and 1200 °C, respectively. The formation of δ-ferrite at 1200 °C when held for 600 s and 1300 °C when held for 60 ~ 600 s causes a smaller austenite grain size. The relationship between the evolution of the microstructure of P92 steel and the mechanical properties is also studied. The results show that the prior austenite grain size has an inverse relationship with impact energy and ultimate tensile strength at 620 °C, while the presence of soft δ-ferrite leads to a reduction in the microhardness, impact energy and ultimate tensile strength at 620 °C.

36 MATERIALS SCIENCE↗

Tempering and Austempering of Double Soaked Medium Manganese Steels

The addition of a tempering or austempering step to the double soaking of a 0.14C–7.17Mn (wt pct) steel was investigated in the present contribution. The double soaking heat treatment is a two-step intercritical annealing heat treatment, which generates microstructures of athermal martensite, retained austenite and ferrite when applied to medium manganese steels. Microstructures following double soaking and (aus)tempering contained a combination of retained austenite, athermal or tempered martensite, and blocky or bainitic ferrite. X-ray diffraction, dilatometry and transmission Kikuchi diffraction were utilized to investigate microstructural changes which occurred during tempering or austempering. The resulting mechanical properties were measured using uniaxial tensile testing. The double soaking plus tempering heat treatment was shown to generate an ultimate tensile strength of 1,340 MPa in combination with 28 pct total elongation while the double soaking plus austempering heat treatment resulted in an ultimate tensile strength of 1,675 MPa and total elongation of 22 pct. Overall, both novel heat treatments produced a combination of strength and ductility desired for the third generation of advanced high strength steels.

36 MATERIALS SCIENCE↗

Effects of Nd Addition on the Microstructure and Mechanical Properties of Extruded Mg-6Gd-2.5Y-0.5Zr Alloy

The microstructure, age-hardening behavior, mechanical properties and texture of extruded Mg-6Gd-2.5Y-0.5Zr alloys with various additions of Nd have been investigated through optical microscopy, x-ray diffraction, scanning electron microscopy, transmission electron microscopy, electron back-scattered diffraction, hardness and tensile tests. The results indicate that the number of second-phase particles in the as-extruded alloys increases (especially with the addition of 1.5 wt.% Nd), and the amount of the strengthening β′ phase in the peak-aged sample initially increases, and then decreases when the content of Nd increases above 1.0 wt.%. The precipitation of second-phase particles in the extrusion process weakens the age strengthening. The peak-aged Mg-6Gd-2.5Y-1Nd-0.5Zr alloy shows a maximum yield strength of 259 MPa and an ultimate tensile strength of 350 MPa, which can be attributed to the finely dispersed strengthening β′ phase. All as-extruded alloys exhibit that (0001) planes are aligned perpendicular to the extrusion direction, and the maximum intensity of the texture increases gradually with Nd addition.

36 MATERIALS SCIENCE↗

Mechanical Characteristics of Additively Manufactured ODS 316L and 316H Alloys with and Without Post-build Processing

This research aims to explore an accelerated development path for oxide dispersion-strengthened (ODS) alloys by integrating additive manufacturing (AM) technologies with recent advances in ODS materials and traditional manufacturing methods. Novel AM and post-build processing routes have been developed for ODS austenitic alloys, specifically Fe-Cr-Ni alloys like 316L and 316H. Electron microscopy and mechanical characterizations were conducted to evaluate the effects of process variables on microstructure and properties, aiming for an economically feasible route property optimization. Traditionally, ODS alloy production involves multi-day high-energy mechanical milling of alloy powder with yttria (Y 2 O 3 ) followed by powder consolidation via extrusion or other methods and additional thermomechanical processing (TMP) for property control. Here, to address these challenges associated with this complex and costly approach, we propose exploring alternative, cost-effective processing routes focusing on AM and traditional TMP methods. The new ODS alloy processing routes have achieved up to a 400% increase in yield strength and a 60% increase in ultimate tensile strength compared to wrought stainless steels while still maintaining significant ductility and fracture toughness. This paper details the novel and economical AM-based processing routes for ODS austenitic alloys, combined with post-build TMPs, and discusses the mechanical and microstructural characteristics of the developed materials.

Byun, Thak Sang [Oak Ridge National Laboratory (OR↗

Enhanced high-temperature tensile property by gradient twin structure of duplex high-Nb-containing TiAl alloy

A pre-deformation process was employed for a TiAl alloy via high-temperature torsion, in which the stability of the constituent phases was tailored, resulting in enhanced hardening capability and ductility via a gradient microstructure. A sample with a pre-torsion of 360° exhibited a yield strength of 475 MPa and an ultimate tensile strength of 592 MPa, with a tensile ductility of 47% at 850 °C. The tensile properties were significantly enhanced compared with the as-forged sample, which exhibited values of 395 MPa, 494 MPa, and 4.6%, respectively. The physical mechanisms for the significant enhancement of the mechanical property of the TiAl alloys were studied in-depth via of transmission electron microscopy, electron-backscattered diffraction, and high-energy X-ray diffraction techniques. The high strength is mainly attributed to the twin structure formed during torsion, while high fracture elongation correlates to the recrystallization of the γ phase at twin-twin sections and the load partitioning regulated by a hierarchical microstructure. When the tensile micro-strains along the loading direction and transverse direction in the γ phase of the pre-deformed TiAl alloy, a higher mechanical performance was obtained. Moreover, the fracture mode of the pre-torsional tensile sample is a combination of pores and cleavage facets which resulted from the microstructure after torsion. Finally, the gradient twin structure approach in this study provides a strategy for developing TiAl alloys with exceptionally high-temperature tensile property, and the results of the micromechanical behavior-microstructure-property relationship may improve the understanding of the plastic deformation of TiAl alloys.

36 MATERIALS SCIENCE↗

Progress Report of Alloy 709 Performance in Liquid Sodium

With improved high-temperature properties, Alloy 709 shows great potential for advanced reactor applications. To understand the effects of sodium on A709, small tensile specimens were machined from two commercial heats and subject to sodium exposure in two forced convection loops operated by Argonne. Thermal aging experiments were also conducted in parallel to isolate any sodium-specific effects. An increasing trend in yield strength and a decrease trend in ultimate tensile strength can be seen with the increasing exposure time, suggesting microstructural changes at these temperatures. Nonetheless, the thermally aged and sodium exposed samples behaved similarly, implying no sodium-specific effect at these temperatures. In contrast, 316H SS exposed to sodium at 650°C showed a strong sodium effect. The different responses of A709 and 316H SS to sodium exposure is of interest and requires additional effort to understand. The cold traps of the sodium loop were replaced early in FY23. During a maintenance operation, an unexpected sodium leak incident occurred at one of the sodium loops, triggering an emergency response. An investigation into the incident revealed that the leak happened at a VCR fitting on the recently replaced cold trap. The metal gasket of the leaked VCR fitting was not compressed sufficiently. A dimensional mismatch between the new component and old piping configuration was responsible for a significant misalignment. A new cold trap with improved design is in production. The new design provides additional flexibility and an access point for post-installation helium leak check and for venting of trapped gas. These design features will make the system more error-tolerant and the installation quality verifiable. A thermodynamic analysis was performed to understand the carburization-decarburization behavior of A709 in sodium environment. The equilibrium carbon activity in the alloy was evaluated with M 23 C 6 , TiC, and NbC. The carburization-decarburization boundary was calculated with different methods developed previously. The results suggests that A709 will be carburized in SMT-1 and SMT-2, and can be decarburized in low-carbon-activity environments such as EBR-II at temperatures above 620-650°C. Nonetheless, A709 should be less likely to be decarburized than 316H SS when exposed to the same low-carbon-activity environment.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗