Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “TRANSMUTATION”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 433 records · Page 24

Neutron energy spectrum influence on irradiation hardening and microstructural development of tungsten

We performed a neutron irradiation to single crystal pure tungsten in the mixed spectrum High Flux Isotope Reactor (HFIR). In order to investigate the influences of neutron energy spectrum, the microstructure and irradiation hardening were compared with previous data obtained from the irradiation campaigns in the mixed spectrum Japan Material Testing Reactor (JMTR) and the sodium-cooled fast reactor Joyo. The irradiation temperatures were in the range of ~90–~800 °C and fast neutron fluences were 0.02–9.00 × 10 25 n/m 2 (E > 0.1 MeV). Post irradiation evaluation included Vickers hardness measurements and transmission electron microscopy. Moreover, the hardness and microstructure changes exhibited a clear dependence on the neutron energy spectrum. The hardness appeared to increase with increasing thermal neutron flux when fast fluence exceeds 1 × 10 25 n/m 2 (E > 0.1 MeV). Finally, irradiation induced precipitates considered to be χ- and σ-phases were observed in samples irradiated to >1 × 10 25 n/m 2 (E > 0.1 MeV), which were pronounced at high dose and due to the very high thermal neutron flux of HFIR. Although the irradiation hardening mainly caused by defects clusters in a low dose regime, the transmutation-induced precipitation appeared to impose additional significant hardening of the tungsten.

36 MATERIALS SCIENCE↗

Irradiation hardening of pure tungsten exposed to neutron irradiation

In this paper, pure tungsten samples have been neutron irradiated in HFIR at 90–850 °C to 0.03–2.2 dpa. A dispersed barrier hardening model informed by the available microstructure data has been used to predict the hardness. Comparison of the model predictions and the measured Vickers hardness reveals the dominant hardening contribution at various irradiation conditions. For tungsten samples irradiated in HFIR, the results indicate that voids and dislocation loops contributed to the hardness increase in the low dose region (<0.3 dpa), while the formation of intermetallic second phase precipitation, resulting from transmutation, dominates the radiation-induced strengthening beginning with a relatively modest dose (>0.6 dpa). Finally, the precipitate contribution is most pronounced for the HFIR irradiations, whereas the radiation-induced defect cluster microstructure can rationalize the entirety of the hardness increase observed in tungsten irradiated in the fast neutron spectrum of Joyo and the mixed neutron spectrum of JMTR.

36 MATERIALS SCIENCE↗

Microstructural evolution of pure tungsten neutron irradiated with a mixed energy spectrum

Here, microstructures of single-crystal bulk tungsten (W) and polycrystalline W foil with a strong grain texture were investigated using transmission electron microscopy following neutron irradiation at ~90–800 °C to 0.03–4.6 displacements per atom (dpa) in the High Flux Isotope Reactor with a mixed energy spectrum. The dominant irradiation defects were dislocation loops and small clusters at ~90 °C. Additional voids were formed in W irradiated at above 460 °C. Voids and precipitates involving transmutation rhenium and osmium were the dominant defects at more than ~1 dpa. We found a new phenomenon of microstructural evolution in irradiated polycrystalline W: Re- and Os-rich precipitation along grain boundaries. Comparison of results between this study and previous studies using different irradiation facilities revealed that the microstructural evolution of pure W is highly dependent on the neutron energy spectrum in addition to the irradiation temperature and dose.

36 MATERIALS SCIENCE↗

Iron phosphate glasses: Bulk properties and atomic scale structure

Bulk properties such as glass transition temperature, density and thermal expansion of iron phosphate glass compositions, with replacement of Cs by Ba, are investigated as a surrogate for the transmutation of 137Cs to 137Ba, relevant to the immobilisation of Cs in glass. These studies are required to establish the appropriate incorporation rate of 137Cs in iron phosphate glass. Density and glass transition temperature increases with the addition of BaO indicating the shrinkage and reticulation of the iron phosphate glass network. The average thermal expansion coefficient reduces from 19.8 × 10-6 K-1 to 13.4 × 10-6 K-1, when 25 wt. % of Cs2O was replaced by 25 wt. % of BaO in caesium loaded iron phosphate glass. In addition to the above bulk properties, the role of Ba as a network modifier in the structure of iron phosphate glass is examined using various spectroscopic techniques. The FeII content and average coordination number of iron in the glass network was estimated using Mössbauer spectroscopy. The FeII content in the un-doped iron phosphate glass and barium doped iron phosphate glasses was 20, 21 and 22 ± 1% respectively and the average Fe coordination varied from 5.3 ± 0.2 to 5.7 ± 0.2 with increasing Ba content. The atomic scale structure was further probed by Fe K-edge X-ray absorption spectroscopy. The average coordination number provided by extended X-ray absorption fine structure spectroscopy and X-ray absorption near edge structure was in good agreement with that given by the Mössbauer data.

36 MATERIALS SCIENCE↗

Recent progress in the development of SiC composites for nuclear fusion applications

Silicon carbide (SiC) fiber reinforced SiC matrix composites continue to undergo development for fusion applications worldwide because of inherent advantages of the material including low activation, high temperature capability, relatively low neutron absorption, and radiation resistance. This work presents an international overview of recent achievements in SiC-based composites for fusion applications. Key subjects include applications in fusion reactors, high-dose radiation effects, transmutation effects, material lifetime assessment, and development of joining technology (processing, test method development, irradiation resistance, and modeling capability). This paper also discusses synergy among research for fusion materials and non-fusion materials (for fission and aerospace applications). Finally, future research directions and opportunities are proposed.

36 MATERIALS SCIENCE↗

Microstructural evolution of 3C-SiC exposed to simultaneous neutron irradiation and helium implantation

The synergism of transmutant helium and irradiation defects is critically important to understand the performance of SiC when in service in nuclear environments. In this study, we exposed 3C-SiC in contact with a 2 μm Ni foil to neutron irradiation at 500 °C to 29 dpa in the high flux isotope reactor to simulate the simultaneous introduction of helium and irradiation defects into SiC. The combination of TEM observations and thermal desorption measurements helps to elucidate the impact of helium on the microstructural evolution in 3C-SiC. Thermal helium desorption spectra from ion-implanted and neutron-irradiated SiC showed a completely different desorption behavior in terms of the peak position and helium desorption flux. The identification of possible helium trapping sites was attempted by applying the first order dissociation model to the measured thermal helium desorption spectra. TEM observations of the neutron-irradiated samples showed that the presence of helium facilitated the stabilization of the defect clusters and promoted the formation of visible helium bubbles in SiC subject to simultaneous neutron irradiation and in-situ He implantation. Following the subsequent heat treatment during the thermal desorption measurements, large faceted helium bubbles were found along grain boundaries in the neutron-irradiated SiC with in-situ He implantation, while the helium bubbles in the grain interior were relatively smaller than those found in the neutron-irradiated sample without in-situ He implantation due to the reduced mobility of He-defect clusters. In conclusion, the He contents contained in the neutron-irradiated samples were quantified based on the experimental data from TEM and thermal desorption measurements.

36 MATERIALS SCIENCE↗

Mechanical properties of single-crystal tungsten irradiated in a mixed spectrum fission reactor

To collect data for fusion applications and understand the basic properties of tungsten, single-crystal tungsten was neutron irradiated in the mixed-spectrum High Flux Isotope Reactor at the Oak Ridge National Laboratory at temperatures of 90–830 °C to fast fluences of 0.01–9 × 10 25 n/m 2 (E > 0.1 MeV). For tensile tests at room temperature of the irradiated material in both orientations, <110> and <100> tensile orientation, initially there was strengthening that peaked at 0.02 dpa and was followed by progressive modulus of toughness reduction, approaching zero at higher doses. For all irradiation temperatures, in elevated temperature tensile tests there was a distinct transition from ductile-to-brittle behavior between 0.1 and 0.4 dpa, accompanied by an increase in indentation hardness. The ductile-to-brittle transition with increasing dose was particularly critical because it presented as a total loss in elongation and modulus of toughness. The critical transition dose was well below the dose (~1 dpa) where irradiation-induced precipitates are visible in the TEM. The extent of Vickers microhardness increase was significant at higher doses and did not depend on irradiation temperature or crystal orientation, reaching 12.9 GPa after 2.8 dpa. Furthermore, the significant mechanical property degradation above 0.1 dpa is believed to have been caused by the accumulation of irradiation-induced clusters and eventually precipitates of the transmutation elements Re and Os.

36 MATERIALS SCIENCE↗

Modeling and simulation of oxygen transport in high burnup LWR fuel

We have developed a formulation for oxygen transport in uranium dioxide nuclear fuel that accounts for the effects of irradiation. The overall simulation combines the evolving isotopic composition, thermochemistry, and oxygen transport in irradiated fuel. The driving forces for oxygen transport are computed from local thermodynamic equilibrium calculations and account for the effects of temperature gradients and composition, including fission products. The proposed method provides a mechanism for including complex thermodynamic models of nuclear fuel in modeling of mass redistribution, and alleviates difficulties associated with the common thermodiffusion formulation. Here, the transport model has been implemented within the nuclear fuel performance code BISON utilizing the thermochemistry code Thermochimica, with burnup calculations provided by the ORIGEN isotopic transmutation code.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Microstructural characterization of cold-worked 316 stainless steel flux thimble tubes irradiated up to 100 dpa in a commercial Pressurized Water Reactor

Two flux thimble tubes (FTT) made of 15% cold-worked 316 stainless steel (SS) were harvested from Ringhals Pressurized Water Reactor (PWR) Unit 2, with peak damages of 76 and 100 displacements per atom (dpa) after 29 and 34 years’ service, respectively. Specimens sectioned from parent tubes were comprehensively characterized with nominal damage levels of ~0, ~41, ~74, 76, and 100 dpa at a nominal temperature range of 285-323 °C. Both FTTs contained helium and hydrogen gases as transmutation products. The helium follows a production rate of ~9.8 appm/dpa, while environmental factors complicate hydrogen production obscuring an exact H/dpa ratio. Irradiation-induced dislocation loops, nano-cavities, solute clusters, and microsegregation were all observed. The dislocation loops and nano-cavities indicated saturation at 41 dpa. The solute clusters continued to evolve with Ni-Si clusters formed at 41 dpa, and Ni-Si-Mn-P clusters formed at 74 and 100 dpa, but neither clusters exhibited distinct diffraction patterns at any damage levels. Solute clusters were observed to frequently be co-located with dislocation loops, but fully decorated loops were rarely detected. Significant radiation-induced segregation (RIS) was observed around grain boundaries at all damage levels. The modified inverse Kirkendall (MIK) model captured the RIS behavior of major elements. Large cavities within or around an Mn-S rich region were observed for the first time. Through all the damage levels, void swelling is always below 0.05%, making significant dimensional change unlikely in core internals when used at similar conditions. Meanwhile, the role of overwhelming nanocavities, presumably helium bubbles, should be considered in other potential degradation mechanisms, including irradiation-assisted stress corrosion cracking, embrittlement, and loss of fracture toughness, which remain the concerns for extended operation of nuclear power plants.

Post Irradiation Examination, Isotope Dilution Mas↗

Effects of helium on irradiation response of reduced-activation ferritic-martensitic steels: Using nickel isotopes to simulate fusion neutron response

Understanding the effects of helium on microstructures and mechanical properties of reduced-activation ferritic-martensitic steels is important to use of these steels in fusion reactor structures. The 9Cr-2WVTa steels were doped with 58Ni and 60Ni isotopes at 2 weight percent to control the rate of transmutation helium generation. The samples were irradiated in the High Flux Isotope Reactor to ~24 displacements per atom at nominal temperatures of 300, 400, and 500°C, producing 228 and 7 atomic parts-per-million helium in the 58 Ni- and 60 Ni-doped samples, respectively. Transmission electron microscopy revealed a variety of precipitates and the radiation-induced dislocation loops and cavities (voids or helium bubbles). Tensile tests of the irradiated samples at the irradiation temperatures showed radiation-induced hardening at 300°C and radiation-induced softening at 400°C. Analysis indicates that the hardening primarily originated from the loops and cavities. The 58 Ni-doped samples had greater strengthening contributions from loops and cavities, leading to higher hardening with lower ductility than the 60 Ni-doped samples. The greater helium production of 58 Ni did not show pronounced reductions in ductility of the samples.

36 MATERIALS SCIENCE↗

Radiation Effects Related to Repaired BWR Core Shrouds

The material properties of the core shroud and supporting tie rod components are important factors for Boiling Water Reactor (BWR) life extension considerations. Given the variability of nickel and boron content found in 304 stainless steel shroud plates, and XM-19 and Inconel X-750 tie rod materials, this paper combines the latest spectral information in the vicinity of the core shroud to calculate hydrogen and helium gas production limits as well as atomic displacement damage spanning 80 full-power years (FPY) using the SPECTER code. Results indicate that, whereas boron has little effect on the atomic displacement damage, helium production from boron can be important and must be included in weldability assessments. Since the boron concentration is uncertain, helium generation is calculated assuming a composition range based on specifications and reported measurements. The results show that helium production caused by transmutations in the 304 SS shroud material are dominated by the concentration of boron and will have a significant impact on weldability after only a few years of service. For tie rods, the susceptibility to irradiation-assisted stress corrosion cracking (IASCC) has been assessed by determining helium production in Inconel X-750 IASCC specimens irradiated in the Advanced Test Reactor (ATR) reactor and correlating with the helium produced in a BWR. As a tie rod material in a high thermal neutron flux environment, Inconel X-750 is more likely to be IASCC sensitive during service in a BWR due to helium than the XM-19 stainless steel alloy because of a greater nickel content and boron concentration. Weldability of the core shroud plate material, IASCC of the tie rod materials, and the gamma photon contribution to radiation damage are discussed.

radiation damage in materials, BWR↗

Post-irradiation characterization of a high burnup mixed oxide fuel rod with minor actinides

The Advanced Fuels Campaign performed a series of irradiation tests of minor actinide-bearing mixed oxide fuel (MA-MOX), the so-called AFC-2C&D experiments, to investigate the transmutation of long-lived transuranic actinide isotopes contained in spent nuclear fuel via fast reactor technology at burnups exceeding 10 % fission of initial metallic atoms. This manuscript reports the test results derived from one of the five MA-MOX rodlets taken to higher burnup in the AFC-2D irradiation. This includes both non-destructive investigations, such as gamma and neutron spectrometry, and destructive investigations, such as fission gas release, ceramography, and chemical burnup analysis. In addition, the microstructure of the fuel was investigated using advanced electron microscopy techniques including electron backscatter diffraction (EBSD) and transmission electron microscopy (TEM). Here, it was observed with EBSD that the pellet had subdivision of the grains and the TEM observed migration of cladding material into the 5 metal precipitates in the fuel which could have been from the higher than desired oxygen/metal ratio. The TEM also showed an enrichment of Cr in fuel clad chemical interaction (FCCI) layer.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Helium interaction with solutes and impurities in neutron-irradiated nanostructured ferritic alloys: A first principles study

Density functional theory calculations are performed to explore the binding between He and alloying solutes, impurities, and transmutation products expected in neutron irradiated nanostructured ferritic alloys (NFAs), here 14YWT is taken as an example. Elements that exhibit significant binding (attraction) with an interstitial He are Y (binding energy = 0.46 eV), Mg (0.32), O (0.33), Ti (0.16), and C (0.15). Those that provide significant binding to a substitutional He are O (1.44), Y (1.24), N (0.73), H (0.56), Mg (0.52), Ti (0.34), Si (0.34), C (0.33), Al (0.32), Ni (0.26), Ta (0.23), and Mn (0.16). The presence of these elements in Fe matrix could reduce the transport of He towards oxide particles, dislocations, and internal boundaries, and could promote He bubble nucleation in the matrix. For convenience, we compile existing binding energy data of He with He n and He n V (He-vacancy) clusters. Dissociation pathway analysis reveals that, in general, the most likely dissociation of a He n V cluster is by a sequential emission of individual He atoms. Furthermore, larger bubbles are more prone to dissociation than smaller ones. In addition, we estimate the binding energy (segregation energy) of He in bulk Y 2 Ti 2 O 7 (YTO) single crystal, YTO/Fe interface, and YTO particle embedded in Fe, with respect to interstitial He in Fe, from existing formation energies of He in these structures. We also compile available data of He binding with Fe self-interstitial atom (SIA), SIA clusters, and edge and screw dislocations. Note that given the absence of DFT data, the binding with SIA clusters and dislocations are gathered from simulations with empirical potentials. Finally, the data presented in this paper is important to inform multiscale simulations of He bubble accumulation.

36 MATERIALS SCIENCE↗

The effect of helium on cavity swelling in dual-ion irradiated Fe and Fe-10Cr ferritic alloys

We report Ferritic-martensitic (FM) steels for in-vessel components in proposed fusion reactors are expected to suffer from high levels of displacement damage and helium (He) generation by neutron transmutation. However, a thorough understanding of the He synergistic effects on the cavity swelling in FM steels is still not well established. To gain fundamental insights into the He effect on cavity swelling, high purity Fe and Fe-10 wt.% Cr ferritic model alloys were irradiated with 8 MeV Ni ions and co-implanted He ions at 400 to 550 °C up to 30 displacements per atom (dpa) with He implantation rates of 0.1, 10 and 50 appm He/dpa. The current study focuses on the 50 appm He/dpa, 500 °C behavior vs. 0.1 and 10 appm He/dpa. Irradiation-induced defects, including cavities, dislocation loops, and dislocation networks were characterized using transmission electron microscopy (TEM). In the grain interior, a bimodal cavity size distribution was observed in the 10 and 50 appm He/dpa samples, but not for 0.1 appm He/dpa. Cavity swelling was maximized at intermediate He implantation rates of ~10 appm He/dpa for both ion-irradiated Fe and Fe-10Cr alloys. The cavity swelling behavior as a function of He implantation rate appears to be controlled by the He/dpa-dependent variation of cavity sink strengths. Treating small bubbles as biased sinks for interstitial absorption can significantly increase the ratio of biased to unbiased sink strengths (Q) and results in maximized cavity swelling for a Q ratio close to one.

36 MATERIALS SCIENCE↗

A fusion relevant data-driven engineering void swelling model for 9Cr tempered martensitic steels

The UCSB database on cavity evolution in 9-12Cr tempered martensitic steels (TMS), includes the results for both dual heavy and helium ion (DII), and High Flux Isotope Reactor (HFIR) in situ helium injection (ISHI) neutron irradiations at 500°C. These results were combined with literature single ion and fission neutron irradiation data to derive a model for the void volume fraction, f v , as a function of displacements per atom (dpa) and transmutant helium concentrations in atomic parts per million (appm). The scientific foundation for the paper is described in a companion paper entitled “Cavity Evolution and Void Swelling in Dual Ion Irradiated Tempered Martensitic Steels”. Here, in this study, we show that f v (dpa, He/dpa) is described by the incubation dose, dpa i , for the onset of void growth, and the post-incubation growth rate, f v ’(%/dpa). Both dpa i and f v ’ decrease with increasing He/dpa at > ~ 5. The dpa i is also lower for the ISHI neutron irradiations at the same He/dpa. Single heavy ion and fission reactor neutron irradiations, with low He/dpa ratios, have a much larger dpa i . Based on a combined analysis of DII, single ion, ISHI and fission neutron data, we further show that the post-incubation f v data analyzed here have a common empirical curve shape, with f v ’ reaching up to ~ 0.2%/dpa at very high dpa. We also show that f v ’ can be predicted based on a physical model of defect partitioning between evolving sinks. At 500°C and fusion relevant He/dpa ≈ 10, the best-fit model predicts nominal swelling, S = f v /(1-f v ), of ~ 1.1, 4.9 and 16% at 50, 100 and 200 dpa, respectively. The physically motivated, data-driven model includes estimated uncertainties for both dpa i and f v ’.

36 MATERIALS SCIENCE↗

Comparative characterization of mixed spectra and thermal neutron shielded irradiated tungsten

The effect of mixed spectra and thermal neutron shielded irradiation on tungsten was evaluated with plasma exposure in the tritium plasma experiment followed by thermal desorption spectroscopy, X-ray photoelectron spectroscopy, and transmission electron microscopy. The two different irradiation campaigns were performed at the High Flux Isotope Reactor to 0.39–0.74 displacement per atom (dpa) in the 894–1379 K temperature range. A neutron spectrum influence on the void size and void number density was not observed. However, a strong correlation was found between void size and void number density with temperature, but not with dpa in the limited dpa range of this study. Thermal neutron shielding significantly reduced the transmutation to Re+Os. Higher irradiation temperature will lead to larger voids with lower number density, which reduces deuterium retention. In conclusion, grain growth was also observed for high-temperature irradiation of over ~1300 K within the limited grains visible in the transmission electron microscopy specimens.

36 MATERIALS SCIENCE↗

Transmission Electron Microscopy Characterization of Fuel Cladding Chemical Interaction between Minor Actinides bearing U-Pu-Zr Fuel and AIM1 Cladding

Minor actinides (MA) significantly contribute to the long-term radiotoxicity of spent nuclear fuel (SNF). Separating MA from SNF and incorporating it into metallic fuels for fast reactor transmutation is a potential method to reduce this radiotoxicity. Here, this study focuses on transmission electron microscopy characterization of two samples from the fuel cladding chemical interaction (FCCI) region of an americium (Am) and neptunium (Np)-bearing (MA-bearing) uranium-plutonium-zirconium (U-Pu-Zr) fuel irradiated in the Phenix fast reactor to 9.5 % FIMA burnup at approximately 550 °C cladding temperature. The results show that despite the complex chemical interactions between MA and AIM1 cladding elements, excessive FCCI was not induced, and Am penetration depth in the cladding limited to less than 4 µm. Np remained mostly inside fuel. The Zr-rich compounds layer effectively limited the accumulation of lanthanide on the inner cladding surface. Overall, the FCCI behavior between investigated MA-bearing U-Pu-Zr fuel and AIM1 cladding is benign.

Chemical interaction↗

Microstructurally informed synchrotron x-ray analysis revealing helium defect transitions in ultrafine grained tungsten

The formation of insoluble gaseous defects in materials due to nuclear transmutation or ion implantation involves the diffusion of impurity atoms to form atomic defect clusters that coalesce into bubbles or cavities and ultimately degrade the material properties. Transmission electron microscopy (TEM) is limited in its ability to resolve sub-nanometer gas clusters whereas X-ray diffraction (XRD) provides information pertaining to local atomic changes. Here, in this study, helium (He) implanted ultrafine grained tungsten is explored through a multimodal defect characterization campaign combining TEM-informed Small Angle X-ray Scattering (SAXS) analysis, XRD lattice parameter measurements, and nanoscale He cluster quantification from a region of reciprocal space accessible via Wide Angle X-ray Scattering (WAXS). Moderate elevated temperature implantations are shown to produce high concentrations of sub-nanoscale He clusters and small, homogeneously distributed cavities, which collectively are linked to lattice expansion and further substantiated through complementary atomistic simulations. Increased implantation temperatures encourage the diffusion of these defects to the grain boundaries (GBs), leading to lattice relaxation and the growth of large GB cavities manifesting as bimodal size distributions in the SAXS analysis. Overall, our results demonstrate the utility of multimodal synchrotron X-ray analysis in bridging the gap between microscale He cavity quantification and atomic-scale defect analysis.

36 MATERIALS SCIENCE↗