At least 433 records · Page 24

Microstructure Evolution of Gas Atomized Iron Based ODS Alloys

In a simplified process to produce precursor powders for oxide dispersion-strength- ened (ODS) alloys, gas-atomization reaction synthesis (GARS) was used to induce a surface oxide layer on molten droplets of three differing erritic stainless steel alloys during break-up and rapid solidification. The chemistry of the surface oxide was identified using auger electron spectroscopy (AES) and scanning electron microscopy (SEM) with energy dispersive spectroscopy (EDS). The precursor iron-base powders were consolidated at 850 C and 1,300 C using hot isostatic pressing (HIPing). Consolidation at the lower temperature resulted in a fully dense microstructure, while preventing substantial prior particle-boundary-oxide dissociation. Microstructural analysis of the alloys consolidated at the higher temperature confirmed a significant reduction in prior-particle-boundary-oxide volume fraction, in comparison with the lower-temperature-consolidated sample. This provided evidence that a high-temperature internal oxygen-exchange reaction occurred between the metastable prior particle-boundary-oxide phase (chromium oxide) and the yttrium contained within each prior particle. This internal oxygen-exchange reaction is shown to result in the formation of yttrium-enriched oxide dispersoids throughout the alloy microstructure. The evolving microstructure was characterized using transmission electron microscopy (TEM) and high-energy X-ray diffraction (HE-XRD).

36 MATERIALS SCIENCE↗

Microstructural evolution during transient liquid phase bonding of Inconel 738LC using AMS 4777 filler alloy

IN-738LC nickel-based superalloy was joined by transient liquid phase diffusion bonding using AMS 4777 filler alloy. The bonding process was carried out at 1050 Degree-Sign C under vacuum atmosphere for various hold times. Microstructures of the joints were studied by optical and scanning electron microscopy. Continuous centerline eutectic phases, characterized as nickel-rich boride, chromium-rich boride and nickel-rich silicide were observed at the bonds with incomplete isothermal solidification. In addition to the centerline eutectic products, precipitation of boron-rich particles was observed in the diffusion affected zone. The results showed that, as the bonding time was increased to 75 min, the width of the eutectic zone was completely removed and the joint was isothermally solidified. Homogenization of isothermally solidified joints at 1120 Degree-Sign C for 300 min resulted in the elimination of intermetallic phases formed at the diffusion affected zone and the formation of significant {gamma} Prime precipitates in the joint region. - Highlights: Black-Right-Pointing-Pointer TLP bonding of IN-738LC superalloy was performed using AMS 4777 filler alloy. Black-Right-Pointing-Pointer Insufficient diffusion time resulted in the formation of eutectic product. Black-Right-Pointing-Pointer Precipitation of B-rich particles was observed within the DAZ. Black-Right-Pointing-Pointer The extent of isothermal solidification increased with increasing holding time. Black-Right-Pointing-Pointer Homogenizing of joints resulted in the dissolution of DAZ intermetallics.

36 MATERIALS SCIENCE↗

Microstructure and mechanical behavior of hot-work tool steels processed by Selective Laser Melting

Highlights: • H11 and a modified H11 hot work tool steels have been produced by SLM. • As-built alloys are characterized by α-Fe cells surrounded by C-rich γ-Fe regions. • Rapidly solidified structures revealed able to respond to precipitation hardening. • Mechanical behavior of AM H11 is similar to that obtained by conventional processes. - Abstract: The present study is aimed at identifying and testing high-strength alloys for tooling applications featuring suitable processability for laser-based additive manufacturing technologies. The microstructure and mechanical properties of the H11 hot-work tool steel and a leaner version of the same alloy (L-H11) processed by Selective Laser Melting were assessed as a function of specific microstructural conditions obtained by performing different heat treatments. Tempering was performed on quenched alloys or simply from as built material. The rapidly solidified microstructures revealed able to respond directly to precipitation hardening treatment without performing any prior solution annealing. The microstructure of the as-built alloys revealed characterized by α-Fe dendritic cells decorated at boundaries by C-rich γ-Fe regions. Air quenching was responsible for the transformation of the solidification cells into lath martensitic structures and for the formation of the M{sub 3}C phase, which transformed into more complex carbide species on tempering. The hardness of quenched and tempered H11 steel is similar to that obtained by processing the alloy with conventional routes, and the final hardness gap between the two SLM processed H11 and L-H11 alloys treated according to optimal tempered condition was limited to 62 HV.

36 MATERIALS SCIENCE↗

Considering interplay between multiple physical phenomena to elucidate single crystal-like texture, phase transformations, and mechanical behavior of directed energy deposited SS316L

A widespread implementation of large scale additive manufacturing (AM) processes, such as wire arc-directed energy deposition (WA-DED) AM can transform the current manufacturing supply chain networks. Naturally, such implementation requires control of the microstructural attributes, such as texture and phase evolution in the processed alloys. Currently, the texture evolution in fusion-based AM (F-BAM) processes is majorly rationalized by the phenomena occurring only during solidification. However, such rationalization is insufficient for understanding the evolution of primary and secondary crystallographic orientations, and consequently, fails to offer a comprehensive understanding and control of overall texture in F-BAM processed alloys. To this end, we report a single crystal (SX)-like texture in WA-DED processed SS316L for the first time. Furthermore, we assess the physical phenomena that may lead to such unique microstructural evolution during WA-DED AM. Subsequently, using microstructural characterization spanning the build height and thermomechanical simulations we investigate the effect of competitive growth and epitaxial growth occurring during solidification and thermally induced plastic deformation occurring post solidification on the overall texture of WA-DED processed SS316L. A spatial variation in solidification pathway is also established and correlated with variation in undercoolings across the build. Tensile tests revealed a strong orientation dependence of deformation mechanisms with over 110% elongation to failure of specimens deformed along <011>. Such anisotropy is rationalized using Schmid's analysis of dislocation slip and deformation twinning. Importantly, overall, the mechanisms outlined in this work will facilitate an enhanced understanding and subsequent control of texture evolution, solidification behavior and mechanical behavior of WA-DED processed steels.

36 MATERIALS SCIENCE↗

Microstructural development of diffusion-brazed austenitic stainless steel to magnesium alloy using a nickel interlayer

The differences in physical and metallurgical properties of stainless steels and magnesium alloys make them difficult to join using conventional fusion welding processes. Therefore, the diffusion brazing of 316L steel to magnesium alloy (AZ31) was performed using a double stage bonding process. To join these dissimilar alloys, the solid-state diffusion bonding of 316L steel to a Ni interlayer was carried out at 900 deg. C followed by diffusion brazing to AZ31 at 510 deg. C. Metallographic and compositional analyses show that a metallurgical bond was achieved with a shear strength of 54 MPa. However, during the diffusion brazing stage B{sub 2} intermetallic compounds form within the joint and these intermetallics are pushed ahead of the solid/liquid interface during isothermal solidification of the joint. These intermetallics had a detrimental effect on joint strengths when the joint was held at the diffusion brazing temperature for longer than 20 min.

36 MATERIALS SCIENCE↗

Microstructures, Martensitic Transformation, and Mechanical Behavior of Rapidly Solidified Ti-Ni-Hf and Ti-Ni-Si Shape Memory Alloys

In this work, the microstructure and mechanical properties of rapidly solidified Ti{sub 50−x/2}Ni{sub 50−x/2}Hf{sub x} (x = 0, 2, 4, 6, 8, 10, and 12 at.%) and Ti{sub 50−y/2}Ni{sub 50−y/2}Si{sub y} (y = 1, 2, 3, 5, 7, and 10 at.%) shape memory alloys (SMAs) were investigated. The sequence of the phase formation and transformations in dependence on the chemical composition is established. Rapidly solidified Ti-Ni-Hf or Ti-Ni-Si SMAs are found to show relatively high yield strength and large ductility for specific Hf or Si concentrations, which is due to the gradual disappearance of the phase transformation from austenite to twinned martensite and the predominance of the phase transformation from twinned martensite to detwinned martensite during deformation as well as to the refinement of dendrites and the precipitation of brittle intermetallic compounds.

36 MATERIALS SCIENCE↗

Investigation of the swelling behavior of cationic exchange resins saturated with Na{sup +} ions in a C{sub 3}S paste

Ion exchange resins (IERs) are widely used by the nuclear industry to decontaminate radioactive effluents. Spent products are usually encapsulated in cementitious materials. However, the solidified waste form can exhibit strong expansion, possibly leading to cracking, if the appropriate binder is not used. In this work, the interactions between cationic resins in the Na{sup +} form and tricalcium silicate are investigated during the early stages of hydration in order to gain a better understanding of the expansion process. It is shown that the IERs exhibit a transient swelling of small magnitude due to the decrease in the osmotic pressure of the external solution. This expansion, which occurs just after setting, is sufficient to damage the material which is poorly consolidated for several reasons: low degree of hydration, precipitation of poorly cohesive sodium-bearing C–S–H, and very heterogeneous microstructure with zones of high porosity.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Microstructural evolution during solution treatment of Co-Cr-Mo-C biocompatible alloys

Three different Co-Cr-Mo-C alloys conforming to ASTM F75 standard were poured in an industrial environment and subjected to a conventional solution treatment at 1225 Degree-Sign C for several time intervals. The microstructural changes and transformations were studied in each case in order to evaluate the way in which treatment time influences the secondary phase fraction and clarify the microstructural changes that could occur. To assess how treatment time affects microstructure, optical microscopy and image analyzer software, scanning electron microscopy and energy dispersion spectrometry analysis were employed. The main phases detected in the as-cast state were: {sigma}-phase, M{sub 6}C, and M{sub 23}C{sub 6} carbides. The latter presented two different morphologies, blocky type and lamellar type. Despite being considered the most detrimental feature to mechanical properties, {sigma}-phase and lamellar carbides dissolution took place in the early stages of solution treatment. M{sub 23}C{sub 6} carbides featured two different behaviors. In the alloy obtained by melting an appropriate quantity of alloyed commercial materials, a decrease in size, spheroidization and transformation into M{sub 6}C carbides were simultaneously observed. In the commercial ASTM F75 alloy, in turn, despite being the same phase, only a marked decrease in precipitates size was noticed. These different behaviors could be ascribed to the initial presence of other phases in the alloy obtained from alloyed materials, such as {sigma}-phase and 'pearlitic' carbides, or to the initial precipitate size which was much larger in the first than in the commercial ASTM F75 alloy studied. M{sub 6}C carbides dissolved directly in the matrix as they could not be detected in samples solution-treated for 15 min. - Highlights: Black-Right-Pointing-Pointer Three different Co-Cr-Mo alloys were poured under an industrial environment. Black-Right-Pointing-Pointer Transformation of existing phases followed during conventional solution treatment. Black-Right-Pointing-Pointer In as-cast/treated samples, phases were identified by color metallography, SEM and EDS. Black-Right-Pointing-Pointer M{sub 23}C{sub 6} {yields} M{sub 6}C transformation was corroborated by SEM and EDS analysis. Black-Right-Pointing-Pointer Carbide spheroidization was also detected prior a noticeably carbide size decreasing.

36 MATERIALS SCIENCE↗

MEMPHIS (Mesoscle Multiphysics Phase Field Simulator v.0

SAND2024-01427O Mesoscale Multiphysics Phase Field Simulator (MEMPHIS) is used for solving interfacial problems and can be applied to many evolutionary problems. Some examples are solidification dynamics, viscous fingering, fracture mechanics, hydrogen embrittlement, vesicle dynamics, electro-mechanical degradation of batteries, aging of microstructures, and segregation. MEMPHIS is written in Fortran 90 in a modular fashion, where model and numerical solvers are decoupled from one another. Sandia National Laboratories is a multimission laboratory managed and operated by National Technology & Engineering Solutions of Sandia, LLC, a wholly owned subsidiary of Honeywell International Inc., for the U.S. Department of Energy’s National Nuclear Security Administration under contract DE-NA0003525.

Dingreville, Remi↗

Microstructure and XRD analysis of brazing joint for duplex stainless steel using a Ni-Si-B filler metal

Brazing of a nitrogen-containing duplex stainless steel was preformed using a nickel-based filler metal (Ni-4.5wt.%, Si-3.2wt.%, B). The microstructure of the brazed joint was investigated using scanning electron microscopy, energy dispersive spectrometry, electron probe microanalyzer, and layer-by-layer X-ray diffraction analysis. The results indicated that before completion of isothermal solidification, BN, Ni{sub 3}B and Ni{sub 3}Si precipitates formed at the interface, in the athermally solidified zone and isothermally solidified zone, respectively. After isothermal solidification, only {gamma}-Ni phase appeared in the brazed interlayer. The appearance of hardness peak values in the athermally solidified zone and the interface most probably corresponded to the formation of Ni{sub 3}B and BN, respectively.

36 MATERIALS SCIENCE↗

Solidification and crystallographic texture modeling of laser powder bed fusion Ti-6Al-4V using finite difference-monte carlo method

Laser powder bed fusion (LPBF) additive manufacturing makes near-net-shaped parts with reduced material cost and time, rising as a promising technology to fabricate Ti-6Al-4V, a widely used titanium alloy in aerospace and medical industries. However, LPBF Ti-6Al-4V parts produced with 67° rotation between layers, a scan strategy commonly used to reduce microstructure and property inhomogeneity, have varying grain morphologies and weak crystallographic textures that change depending on processing parameters. Here, this study predicts LPBF Ti-6Al-4V solidification at three energy levels using a finite difference-Monte Carlo method and validates the simulations with large-area electron backscatter diffraction (EBSD) scans. The developed model accurately shows that a <001> texture forms at low energy and a <111> texture occurs at higher energies parallel to the build direction but with a lower strength than the textures observed from EBSD. A validated and well-established method of combining spatial correlation and general spherical harmonics representation of texture is developed to calculate a difference score between simulations and experiments. The quantitative comparison enables effective fine-tuning of nucleation density (N 0 ) input, which shows a nonlinear relationship with increasing energy level. Future improvements in texture prediction code and a more comprehensive study of N 0 with different energy levels will further advance the optimization of LPBF Ti-6Al-4V components. These developments contribute a novel understanding of crystallographic texture formation in LPBF Ti-6Al-4V, the development of robust model validation and calibration pipeline methodologies, and provide a platform for mechanical property prediction and process parameter optimization.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Toward Process-Based Quality through a Fundamental Understanding of Weld Microstructural Evolution

Here, in this overview paper, the possibility of qualifying welded components by integrating software and hardware tools that are capable of describing physical processes that occur during welding is explored. The existing and emerging tools to define geometrical boundary conditions, process parameters, heat and mass transfer, solidification, solid-state transformation, plastic deformation, distortion, residual stress, and performance of welded components are reviewed. Existing challenges relevant to the fundamental understanding of complex alloying, processing environment, and transients in energy deposition are discussed with reference to microstructure evolution. Finally, approaches to address these challenges were articulated with published case studies relevant to welding and additive manufacturing.

36 MATERIALS SCIENCE↗

Characterization, Mechanism and Control Measures of V Segregation in Continuous Casting Billet of C-Mn Steel

To eliminate V segregation, which significantly deteriorates the homogeneity of continuous casting steel billets, V segregation in the C-Mn steel billet was observed by microscope, SEM and EDS. The formation mechanism and control measures for V segregation were proposed. Results show that many slim V segregation strips are distributed on an inverted conical surface and that most segregation strips start from the vertex of the inverted conical surface. A series of inverted conical surfaces containing V segregation strips periodically appears along the longitudinal direction of the billet. The microstructures in the V segregation strip are fine granular structures, while the microstructures outside the V segregation strip are coarse Widmanstätten. The V segregation strip also contains many inclusions and porosities. The formation mechanism for V segregation, which is illuminated by a physical simulation of Al-5wt pctCu alloy, is attributed to the fissure in the equiaxed dendritic network torn by solidification contraction. By controlling the percentage and distribution of equiaxed grains, the V segregation in the billet of C-Mn steel is completely eliminated.

36 MATERIALS SCIENCE↗

Growth mechanism of in situ synthesized TiB{sub w} in titanium matrix composites prepared by common casting technique

Titanium matrix composites reinforced with TiB and RE{sub 2}O{sub 3} (RE = rare earth metal) were fabricated by a non-consumable arc-melting technology utilizing chemical reaction between titanium, B{sub 2}O{sub 3} and RE. Microstructural characterization of in situ synthesized TiB was performed by scanning electron microscopy (SEM) and transmission electron microscopy (TEM). When the volume percentage is relatively low, the TiB shows a typical fine needle-shape due to the solidification process. The TiB whiskers have a B27 crystal structure and grow along the B27 [010] direction. Based on Density Functional Theory (DFT), the surface energies of B27 (100), (101), (101-bar ) and (001) planes were calculated. The results show that the cross sections of TiB whiskers are hexagonal and consist of (100), (101), (101-bar ) planes.

36 MATERIALS SCIENCE↗

High-temperature electrochemical performance of low-cost La–Ni–Fe based hydrogen storage alloys with different preparation methods

Highlights: • Effects of four different preparation processes were studied at 20/60 °C. • All NS + HT, RS and RS + HT processes can optimize the thermodynamic performance. • The HT process can provoke the precipitation of A{sub 2}B{sub 7} and leads to a poor cycling life. • Al exhibits the most remarkable dissolution for all the alloys, especially at 60 °C. - Abstract: In order to optimize the microstructure and high temperature electrochemical performances of low-cost AB{sub 5}-type Ml(NiMnAl){sub 4.2}Co{sub 0.3}Fe{sub 0.5} hydrogen storage electrode alloys, four different preparation methods including normal solidification (NS), normal solidification and 900 °C heat treatment (NS + HT), rapid solidification (RS), rapid solidification and 900 °C heat treatment (RS + HT) were adopted in this work. All alloys exhibit CaCu{sub 5} type hexagonal structure and there is a small amount of A{sub 2}B{sub 7} phase in NS + HT and RS + HT alloys. It is found the using of HT process can decrease the hydrogen equilibrium plateau pressure, the plateau slope and hysteresis at 40, 60 and 80 °C. The NS + HT and RS + HT alloys also possess better activation, high rate discharge performance, larger discharge capacity, but poor cycling performance due to the existence of A{sub 2}B{sub 7} phase which can accelerate dissolution of Ni, Mn and Fe elements in KOH alkaline electrolyte. The RS process can make alloy exhibit the best cycling performance especially at 60 °C.

36 MATERIALS SCIENCE↗

Wear behavior of the surface alloyed AISI 1020 steel with Fe-Nb-B by TIG welding technique

Weld overlay coatings also known as hardfacing is a method which involves melting of the alloys and solidification for applied coatings. Recently hardfacing by welding has become a commonly used technique for improvement of material performance in extreme (high temperature, impact/abrasion, erosion, etc.) conditions.In the present study, the coatings were produced from a mixture of ferrous niobium, ferrous boron and iron powders in the ranges of -45µm particle size with different ratio. Fe{sub 12}Nb{sub 5}B{sub 3} and Fe{sub 2}NbBalloys were coated on the AISI 1020 steel surface by TIG welding. The phases formed in the coated layer are Fe{sub 2}B, NbB{sub 2}, NbFeB and Fe0,2 Nb{sub 0,8} phases. The hardness of the presence phases are changing between 1689±85 HV{sub 0.01}, and 181±7 HV{sub 0.1}. Microstructural examinations were realized by optical and scanning electron microscopy. The wear and friction behaviors of Fe{sub 12}Nb{sub 5}B{sub 3} and Fe2NbB realized on the AISI 1020 steel were investigated by the technique of TIG welding by using ball-on-disk arrangement against alumina ball.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Microsegregation Measurement: Methods and Applications

Microsegregation is chemical variation at the microstructural level in a solidified ingot, which can cause undesirable effects on material properties. Its formation is driven by different levels of solute elemental solubility between solid and liquid phases, resulting in solute buildup or depletion in the liquid phase during solidification. Characterization of microsegregation can be essential for understanding its formation and removing it through heat treatment. Measurement is frequently carried out via scanning electron microscope (SEM), though metallographic analysis, mechanical testing and optical radiography have been used. SEM analysis can consist of point measurements on single dendrites, line scans across or along dendrites, elemental maps, and extended line-based or grid-based analyses extending over many dendrites, which can generate large amounts of data. Line-based or grid-based data can be analyzed using scatterplots of element concentrations to visualize segregation behavior and sorting/ranking of data by a single element or a combination of elements, to give compositional profiles as a function of extent of solidification. For both qualitative and quantitative analyses, effects of phase transformations and secondary phases need to be considered as well as sorting of measurement errors when generating compositional profiles. Applications of analysis include determination of partition ratios, examination of solute–element interactions, determination of effects of cooling rate and back diffusion, applications to freckling studies, validations of modeling, and development of heat-treatment profiles.

36 MATERIALS SCIENCE↗

Morphological characteristic of the conventional and melt-spun Al-10Ni-5.6Cu (in wt.%) alloy

The Al-10Ni-5.6Cu alloy was prepared by conventional casting and further processed melt-spinning technique. The resulting conventional cast and melt-spun ribbons were characterized using X-ray diffraction, optical microscopy, scanning electron microscopy together with energy dispersive spectroscopy, differential scanning calorimetry and microhardness techniques. The X-ray diffraction analysis indicated that ingot samples were {alpha}-Al, intermetallic Al{sub 3}Ni and Al{sub 2}Cu phases. The optical microscopy and scanning electron microscopy results show that the microstructures of rapidly solidified ribbons are clearly different from their ingot alloy. Al-10Ni-5.6Cu ribbons reveal a very fine cellular structure with intermetallic Al{sub 3}Ni particles. Moreover, at high solidification rates the melt-spun ribbons have a polygonal structure dispersed in a supersaturated aluminum matrix. The differential scanning calorimetry measurements revealed that exothermic reaction was between 290 deg. C and 440 deg. C which are more pronounced in the ternary Al-10Ni-5.6Cu alloy.

36 MATERIALS SCIENCE↗