SEARCH · Engineering Papers
Results for “Solid state electrolyte”
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Innovative Approaches to Li-Argyrodite Solid Electrolytes for All-Solid-State Lithium Batteries
Explore the source record for details and available documents.
Ionic Liquid (IL) Laden Metal–Organic Framework (IL-MOF) Electrolyte for Quasi-Solid-State Sodium Batteries
Not provided.
Revealing unprecedented cathode interface behavior in all-solid-state batteries with oxychloride solid electrolytes
The superionic conductor, lithium tantalum oxychloride (LTOC), exhibits unprecedented stability with Co-lean and Ni-rich cathodes, while lowering the working temperature proves effective in regulating the Co-rich cathode interface with LTOC.
Lithium Dendrite-Free Li 7 N 2 I-LiOH Solid Electrolytes for High Energy Lithium Batteries
All-solid-state lithium batteries (ASSLBs) hold great potential to improve the safety and energy density of today’s lithium-ion batteries by using non-flammable inorganic solid electrolytes. Solid electrolytes (SEs) are believed to prevent Li dendrite growth because of high mechanical strength and high Li+ transference numbers. Significant advances in SE have been achieved, among which, Li7La3Zr2O12 (LLZO) and Li2S–P2S5 (LPS) are the most promising SEs for bulk-type solid-state lithium batteries because of high ionic conductivities (>10-4 S/cm2). However, in contrast to our expectations, the growth of lithium dendrites is not suppressed but is facilitated in LLZOs and LPSs regardless of dopants, porosity, and crystallinity of the electrolytes. Despite the unity Li transference number and over two-times of shear modulus than that of Li metal, the critical current densities for Li plating and stripping in these SEs are less than 1.0 mA cm-2, which is one-fourth to one-tenth of that in liquid electrolytes at room temperature. The incompatibility between LLZO and LPS with Li metal seriously limits the energy density of all-solid-state batteries. The mechanism for lithium dendrite formation and growth in SEs are still disputable. Lack of understanding of the Li dendrite formation mechanism seriously impeded the development of solid-state lithium batteries. The development of the criterion for Li dendrite suppression is essential for the success of solid electrolyte lithium batteries. In this project, a criterion for Li dendrite suppression will be developed through thermodynamics and kinetics analysis of lithium dendrite nucleation/growth, which will guide the solid-state electrolyte design. Li7N2I-LiOH, Li5NI2-LiOH and Li3YCl6 solid electrolyte with high ionic conductivity and low electronic conductivity were used to validate the criterion for lithium dendrite suppression. Different surface modifications were also explored to enhance the dendrite suppression capability of SSEs.
Stable Anode–Free All–Solid–State Lithium Battery through Tuned Metal Wetting on the Copper Current Collector
A stable anode-free all-solid-state battery (AF-ASSB) with sulfide-based solid-electrolyte (SE) (argyrodite Li 6 PS 5 Cl) is achieved by tuning wetting of lithium metal on “empty” copper current-collector. Lithiophilic 1 µm Li 2 Te is synthesized by exposing the collector to tellurium vapor, followed by in situ Li activation during the first charge. The Li 2 Te significantly reduces the electrodeposition/electrodissolution overpotentials and improves Coulombic efficiency (CE). During continuous electrodeposition experiments using half-cells (1 mA cm –2 ), the accumulated thickness of electrodeposited Li on Li 2 Te–Cu is more than 70 µm, which is the thickness of the Li foil counter-electrode. Full AF-ASSB with NMC811 cathode delivers an initial CE of 83% at 0.2C, with a cycling CE above 99%. Additionally, cryogenic focused ion beam (Cryo-FIB) sectioning demonstrates uniform electrodeposited metal microstructure, with no signs of voids or dendrites at the collector-SE interface. Electrodissolution is uniform and complete, with Li 2 Te remaining structurally stable and adherent. By contrast, an unmodified Cu current-collector promotes inhomogeneous Li electrodeposition/electrodissolution, electrochemically inactive “dead metal,” dendrites that extend into SE, and thick non-uniform solid electrolyte interphase (SEI) interspersed with pores. Density functional theory (DFT) and mesoscale calculations provide complementary insight regarding nucleation-growth behavior. Unlike conventional liquid-electrolyte metal batteries, the role of current collector/support lithiophilicity has not been explored for emerging AF-ASSBs.
All‐Solid‐State Batteries With Mechanically Stable Interfaces Consisting of a Zero‐Strain Cation‐Disordered Rocksalt Cathode
Interface stabilization is critical to the development of working all‐solid‐state batteries. Rigid cathode/solid electrolyte interfaces often disintegrate due to anisotropic volume change of cathode‐active materials, resulting in irreversible capacity loss. Herein, we demonstrate that Li 1.211 Mo 0.467 Cr 0.3 O 2 (LMCO), a pioneering cation‐disordered rocksalt oxide (DRX) cathode that has intrinsically small volume change upon lithium intercalation, can be integrated with a thiophosphate‐based solid electrolyte for all‐solid‐state batteries. Interface stability of the all‐solid LMCO cell was investigated by electrochemical impedance spectroscopy, X‐ray micro‐computed tomography, and electron microscopy. Since LMCO was initially synthesized as a layered phase exhibiting a large volume change, interface disintegration can be observable in the early cycles. As layered LMCO phase‐transformed into DRX LMCO in subsequent cycles, reintegration of the interfaces occurs within a pressurized cell as a result of its zero‐stain behavior. Consequently, the DRX LMCO cathode maintains interface integrity, and thus electrical wiring, over an extended number of cycles, leading to improved capacity retention with small internal cell resistance.
A three-dimensional interconnected polymer/ceramic composite as a thin film solid electrolyte
In this work we introduce an approach to fabricate a solid composite electrolyte film that is thin, ionically conductive, and mechanically robust with good potential for manufacturability, in the application of lithium metal batteries. First a doped-lithium aluminum titanium phosphate ceramic thin film with thickness of ~25 μm is formed by aqueous spray coating, a scalable process. The film is partially sintered to form a three-dimensionally interconnected structure with a dense backbone. It is then backfilled with a crosslinkable poly(ethylene oxide) (PEO)-based polymer electrolyte. We report the composite has very high ceramic loading of 77 wt% (61 vol%) and an ionic conductivity of 3.5 × 10 -5 S/cm at 20 °C with an activation energy of 0.43 eV. The main ion transport pathway is through the ceramic network, predicted by modelling and verified by experiments. Owing to the interconnected structure of the ceramic, the composite electrolyte exhibits much improved mechanical strength.
Machinable, high‐conductivity NaSICON through mitigation of humidity effects during solid‐state synthesis
The Na + super ion conductor (NaSICON, Na 1+x Zr 2 Si x P 3-x O 12 ) is a solid electrolyte well-known for fast, selective Na + transport at low temperatures, uniquely enabling sodium-based batteries. Producing high-quality NaSICON from solid-state methods, especially when cost-effective, potentially hygroscopic precursors are used, is not trivial. To understand and eliminate the influence of humidity during processing, a scheme was developed to reproducibly yield a high Na + conductivity (3.75 mS/cm at 25°C, 81.7 mS/cm at 150°C), high density (97%), and machinable NaSICON without the use of binders, sintering aids, or dopants. Controlled humidity studies over 20%–50% RH coupled with thermal, structural, and electrical analysis reveal that calcination temperatures < 1000°C leave NaSICON processing susceptible to water absorption at > 20% RH due to the presence of hygroscopic Na 3 PO 4 and Na 2 CO 3 during shaping, pressing, and sintering. Water absorption results in NaSICON with lower densities, machinability, and Na+ conductivity, due to impaired intergranular Na+ transport. At the other extreme, fully converting precursor to the NaSICON phase at 1230°C before pressing and sintering leads to poor conductivity and density. By calcining at 1000°C, excellent quality NaSICON may be produced under a range of laboratory environments, enabling low-cost production of high-conductivity, machinable NaSICON necessary the ever-growing energy storage market.
Role of Intradomain Heterogeneity on Ion and Polymer Dynamics in Block Polymer Electrolytes: Investigating Interfacial Mobility and Ion-Specific Dynamics and Transport
Block polymers show promise as solid-state battery electrolytes due to the optimization of conductive and mechanical properties enabled via tuning of block chemistry and length. We investigate a polystyrene-block-poly(oligo-oxyethylene methacrylate) (PS-b-POEM) electrolyte doped with various lithium salts to investigate the role of molecular structure on ion transport properties and on local ion dynamics and associations. Anion charge becomes more delocalized with increasing size, reducing the coupling between salt ions while increasing coupling between ion and polymer chain motions and creating a more mobile overall environment. We observe support for this ion-polymer coupling via 1 H, 7 Li and 19 F NMR spectroscopy, from which we obtain ion-specific mobility transition temperatures that differ from the polymer glass transition temperature. We also note faster transport and weaker local energetic interactions with anion size using temperature-dependent NMR diffusometry. 1 H NMR spectroscopy further elucidates polymer chain dynamics and enables quantification of the temperature-dependent fraction of the conducting block that is immobile near the PS-POEM domain interface. As a result, NMR thus represents a species-specific and timescale-specific platform to quantify phase and interface behavior, and to correlate ion-specific transport with polymer chain dynamics.
The Influence of Charge Correlation and Ion Solvation on the Phase Behavior of Single-Ion Conducting Polymer Blend Electrolytes Using SAXS/SANS
Single-ion conducting polymer blends (SICPBs) have demonstrated exceptional electrochemical performance as solid-state battery electrolytes; however, their nanoscale morphology and thermodynamic behavior remain unexplored. In this work, we investigate blends composed of deuterated poly(ethylene oxide) and poly[lithium sulfonyl(trifluoromethane sulfonyl)imide methacrylate], dPEO/P(LiMTFSI), and report the first experimental study of the nanostructures of charge-neutral polymer blends using small-angle neutron scattering (SANS) and small-angle X-ray scattering (SAXS). Despite the macroscopic miscibility indicated by a single glass-transition temperature, SANS and SAXS results reveal disordered, charge-correlated nanostructures that are strongly influenced by blend composition and temperature. At low concentrations of charge polymer, the scattering is dominated by concentration fluctuations, and the random phase approximation is applied to extract values of the Flory–Huggins interaction parameter, χ SC . At higher charged polymer content, concentration fluctuations are suppressed, and a correlation model is used to characterize the nanostructures of the charge correlations. We find that the structures of the charge correlations are highly dependent on blend composition─consistent with predictions from Sing’s self-consistent field theory-liquid state models. Understanding these features is essential for uncovering the ion transport mechanism that leads to improved electrochemical performance previously reported in SICPB systems.
PGM-Free Oxygen-Reduction Catalyst Development for Proton-Exchange Membrane Fuel Cells: Challenges, Solutions, and Promises
Proton-exchange membrane fuel cells (PEMFCs) are efficient and clean hydrogen energy technologies for transportation and stationary applications. Highly active and durable low-cost cathode catalysts for the oxygen-reduction reaction (ORR) under challenging acidic environments are desperately needed to address the cost and durability issues of PEMFCs. The most promising platinum group metal (PGM)-free catalysts for the ORR in acidic media are atomically dispersed and nitrogen-coordinated metal site catalysts denoted as M–N–C, M = Fe, Co, or Mn. Due to significant efforts in the past few decades, these catalysts have demonstrated much-improved ORR activity and promising initial fuel cell performance approaching traditional Pt/C catalysts. However, the insufficient long-term stability (up to 5000 h) under PEMFC operation represents a primary technical barrier to making current PGM-free catalysts less viable yet in PEMFCs. In this Account, we highlight recent advances in synthesizing efficient PGM-free catalysts for the ORR in PEMFCs, emphasizing effective strategies to improve mass and intrinsic activity and the possible degradation mechanisms. In particular, a chemical doping method based on the zeolitic imidazolate framework (ZIF)-8 represents the key to developing efficient M–N–C catalysts containing atomically dispersed and nitrogen-coordinated single metal active sites (i.e., MN 4 ). The newly acquired understanding of the formation mechanism of MN 4 active sites during the thermal activation and its correlation to catalytic properties guide the rational catalyst design rather than relying on current trial-and-error approaches. Considerable efforts have further been invested in increasing the active site density and enhancing intrinsic activity by regulating carbon-phase structures and the local coordination environment. Furthermore, these highly active catalysts usually suffer from significant activity loss during the ORR. Therefore, breaking the activity–stability trade-off is the key to simultaneously achieving activity and stability in one catalyst, which is discussed on the basis of our recent successes in regulating local carbon structures surrounding active single metal sites. Significant research efforts toward understanding the degradation mechanisms and improving the lifetime of PGM-free catalysts are still crucial for viable applications in the future. Novel electrode designing strategies are needed to translate the PGM-free catalysts’ ORR activity to solid-state electrolyte-based membrane electrode assemblies (MEAs) with robust three-phase (i.e., gas–liquid–solid) interfaces for efficient charge and mass transports for performance improvement. On the basis of our effort at the University at Buffalo supported by ElectroCat Consortium associated with U.S. DOE’s Hydrogen and Fuel Cell Technologies Office, we provide a perspective on PGM-free cathode catalysts concerning remaining bottlenecks and future opportunities, aiming to inspire the community in both mechanistic understanding and technological development.
Solid-state polymer magnesium supercapacitor
Here, the present article focuses on the development of a highly ion-conductive, solvent-free, solid-state polymer electrolyte membrane (PEM) via photopolymerization of polyethylene glycol diacrylate (PEGDA) network from its homogeneous melt mixtures containing succinonitrile (SCN) plasticizer and magnesium bis(trifluoromethane sulfonyl) imide Mg(TFSI) 2 salt. The above solid-state Mg-PEM exhibits a Helmholtz electric double-layer capacitor (EDLC) behavior in its supercapacitive symmetric carbonaceous electrode configuration. The electrochemical stability for this PEM membrane (20/40/40 PEGDA/SCN/Mg (TFSI) 2 ) was found to be approximately 3 V from linear sweep voltammetry with a specific capacitance of about 44 F/g from cyclic voltammetry and an energy density of approximately 17 Wh/kg in the 0–2 V range from the constant current density (CCD) experiment. Of particular interest is its excellent capacity retention of over 11,200 cycles, thus tested with the Coulombic efficiency of over 87%. Moreover, the energy density after extensive cycling for 11,200 has increased to approximately 56 Wh/kg at 10 mV/s in the potential range of 0–3 V relative to 17 Wh/kg in the potential range of 0–2 V at the same scan rate, attesting the excellent electrochemical stability and long life of the present Mg-PEM supercapacitor.