Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Lithiation”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 433 records · Page 24

Insights into ionic transport and structural changes in magnetite during multiple-electron transfer reactions

Metal oxides, such as Fe 3 O 4 , hold promise for future battery applications due to their abundance, low cost, and opportunity for high lithium storage capacity. In order to better understand the mechanisms of multiple-electron transfer reactions leading to high capacity in Fe 3 O 4 , a comprehensive investigation on local ionic transport and ordering is made by probing site occupancies of anions (O 2– ) and cations (Li + , Fe 3+ /Fe 2+ ) using multiple synchrotron X-ray and electron-beam techniques, in combination with ab-initio calculations. Results from this study provide the first experimental evidence that the cubic-close-packed (ccp) O-anion array in Fe 3 O 4 is sustained throughout the lithiation and delithiation processes, thereby enabling multiple lithium intercalation and conversion reactions. Cation displacement/reordering occurs within the ccp O-anion framework, which leads to a series of phase transformations, starting from the inverse spinel phase and turning into intermediate rock-salt-like phases (Li x Fe 3 O 4 ; 0 < x < 2), then into a cation-segregated phase (Li 2 O•FeO), and finally converting into metallic Fe and Li 2 O. Subsequent delithiation and lithiation processes involve interconversion between metallic Fe and FeO-like phases. Lastly, these results may offer new insights into the structure-determined ionic transport and electrochemical reactions in metal oxides, and those of other compounds sharing a ccp anion framework, reminiscent of magnetite.

25 ENERGY STORAGE↗

In Situ Measurement of Solid Electrolyte Interphase Evolution on Silicon Anodes Using Atomic Force Microscopy

In situ measurements of the growth of solid electrolyte interphase (SEI) layer on silicon and the lithiation-induced volume changes in silicon in lithium ion half-cells are reported. Thin film amorphous silicon electrodes are fabricated in a configuration that allows unambiguous separation of the total thickness change into contribution from SEI thickness and silicon volume change. Electrodes are assembled into a custom-designed electrochemical cell, which is integrated with an atomic force microscope. The electrodes are subjected to constant potential lithiation/delithiation at a sequence of potential values and the thickness measurements are made at each potential after equilibrium is reached. Experiments are carried out with two electrolytes—1.2 m lithium hexafluoro-phosphate (LiPF6) in ethylene carbonate (EC) and 1.2 m LiPF6 in propylene carbonate (PC)—to investigate the influence of electrolyte composition on SEI evolution. It is observed that SEI formation occurs predominantly during the first lithiation and the maximum SEI thickness is ≈17 and 10 nm respectively for EC and PC electrolytes. This study also presents the measured Si expansion ratio versus equilibrium potential and charge capacity versus equilibrium potential; both relationships display hysteresis, which is explained in terms of the stress–potential coupling in silicon.

36 MATERIALS SCIENCE↗

Insights into the Effect of Heat Treatment and Carbon Coating on the Electrochemical Behaviors of SiO Anodes for Li-Ion Batteries

The use of SiO as an anode material has attracted significant interest due to its high capacity and long cycling life. Many promising approaches, including structural design and carbon coating at high temperatures, effectively improve its intrinsic low electrical conductivity and poor Coulombic efficiency. However, the “heat treatment process-composition and microstructure-electrochemical properties” relationship of the SiO anode is not fundamentally understood. Here the structure and composition evolution in amorphous SiO and graphene-coated SiO is investigated using different heat-treatment conditions. X-ray absorption near-edge structure techniques are also employed to analyze the surface and bulk composition change during the initial lithiation process, supplemented by physical or chemical characterization and electrochemical testing. Here results reveal the structural transition of SiO during heat treatment, from amorphous to disproportionated hierarchical structure, where the as-formed dielectric exterior SiO 2 shell and interior SiO 2 matrix severely polarizes electrodes, hindering the lithiation process. Carbon coating on SiO effectively restricts the growth of the SiO 2 shell and facilitates charge transfer, leading to improved electrochemical performance. A schematic model is proposed to reveal the relationship between the treatments, the resultant structural evolutions, and corresponding electrochemical behaviors.

36 MATERIALS SCIENCE↗

Activated Internetwork Pathways in Partially‐Disordered Spinel Cathode Materials with Ultrahigh Rate Performance

Abstract In this study, a class of earth‐abundant, cation‐excess partially disordered spinel materials which demonstrate superior rate performance as Li‐ion cathodes compared to disordered rocksalt materials is computationally investigated. These results show that the partial disorder creates solid solution lithiation with spinel‐like features at the atomic level. A low‐voltage capacity gain is possible with lithiation past the rock salt stoichiometry. It is argued that high rate in partially disordered spinel materials comes from newly activated 16c/16d internetwork pathways which are not possible in normal spinel where only 16c intranetwork diffusion occurs. The assessment and understandings motivate the incorporation of some degree of partial spinel ordering in future disordered rocksalt electrodes to enable superior rate performance.

Yang, Julia H.↗

Lithium Insertion Mechanism in Iron‐Based Oxyfluorides with Anionic Vacancies Probed by PDF Analysis

Abstract The mechanism of lithium insertion that occurs in an iron oxyfluoride sample with a hexagonal–tungsten–bronze (HTB)‐type structure was investigated by the pair distribution function. This study reveals that upon lithiation, the HTB framework collapses to yield disordered rutile and rock salt phases followed by a conversion reaction of the fluoride phase toward lithium fluoride and nanometer‐sized metallic iron. The occurrence of anionic vacancies in the pristine framework was shown to strongly impact the electrochemical activity, that is, the reversible capacity scales with the content of anionic vacancies. Similar to FeOF‐type electrodes, upon de‐lithiation, a disordered rutile phase forms, showing that the anionic chemistry dictates the atomic arrangement of the re‐oxidized phase. Finally, it was shown that the nanoscaling and structural rearrangement induced by the conversion reaction allow the in situ formation of new electrode materials with enhanced electrochemical properties.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

3D LiMn 2 O 4 nThin Film Deposited by ALD: A Road toward High-Capacity Electrode for 3D Li-Ion Microbatteries

Miniaturized electronics suffer from a lack of energy autonomy. In that context, the fabrication of lithium-ion solid-state microbatteries with high performance is mandatory for powering the next generation of portable electronic devices. Here, the fabrication of a thin film positive electrode for 3D Li-ion microbatteries made by the atomic layer deposition (ALD) method and in situ lithiation step is demonstrated. The 3D electrodes based on spinel LiMn 2 O 4 films operate at high working potential (4.1 V vs Li/Li + ) and are capable of delivering a remarkable surface capacity (approximate to 180 mu Ah cm -2 ) at low C-rate while maintaining more than 40 mu Ah cm -2 at C/2 (time constant = 2 h). Both the thickness of the electrode material and the 3D gain of the template are carefully tuned to maximize the electrode performance. Further, advanced characterization techniques such as transmission electron and X-ray transmission microscopies are proposed as perfect tools to study the conformality of the deposited films and the interfaces between each layer: no interdiffusion or segregation are observed. This work represents a major issue towards the fabrication of 3D-lithiated electrode by ALD-without any prelithiation step by electrochemical technique-making it an attractive solution for the fabrication of 3D Li-ion solid-state microbatteries with semiconductor processing methods.

3D Li-ion micro-batteries↗

Molecular dynamics simulations of the first charge of a Li-ion—Si-anode nanobattery

Rechargeable lithium-ion batteries are the most popular devices for energy storage but still a lot of research needs to be done to improve their cycling and storage capacity. Silicon has been proposed as an anode material because of its large theoretical capacity of ~3600 mAh/g. Therefore, focus is needed on the lithiation process of silicon anodes where it is known that the anode increases its volume more than 300%, producing cracking and other damages. In this study, we performed molecular dynamics atomistic simulations to study the swelling, alloying, and amorphization of a silicon nanocrystal anode in a full nanobattery model during the first charging cycle. A dissolved salt of lithium hexafluorophosphate in ethylene carbonate was chosen as the electrolyte solution and lithium cobalt oxide as cathode. External electric fields are applied to emulate the charging, causing the migration of the Li-ions from the cathode to the anode, by drifting through the electrolyte solution, thus converting pristine Si gradually into Li 14 Si 5 when fully lithiated. When the electric field is applied to the nanobattery, the temperature never exceeds 360 K due to a temperature control imposed resembling a cooling mechanism. The volume of the anode increases with the amorphization of the silicon as the external field is applied by creating a layer of LiSi alloy between the electrolyte and the silicon nanocrystal and then, at the arrival of more Li-ions changing to an alloy, where the drift velocity of Li-ions is greater than the velocity in the initial nanocrystal structure. Charge neutrality is maintained by concerted complementary reduction-oxidation reactions at the anode and cathode, respectively. Also, the nanobattery model developed here can be used to study charge mobility, current density, conductance and resistivity, among several other properties of several candidate materials for rechargeable batteries and constitutes the initial point for further studies on the formation of the solid electrolyte interphase in the anode.

25 ENERGY STORAGE↗

Carbon/tin oxide composite electrodes for improved lithium-ion batteries

Tin and tin oxide-based electrodes are promising high-capacity anodes for lithium-ion batteries. However, poor capacity retention is the major issue with these materials due to the large volumetric expansion that occurs when lithium is alloyed with tin during lithiation and delithiation process. Here, a method to prepare a low-cost, scalable carbon and tin(II) oxide composite anode is reported. The composite material was prepared by ball milling of carbon recovered from used tire powders with 25 wt% tin(II) oxide to form lithium-ion battery anode. With the impact of energy from the ball milling, tin oxide powders were uniformly distributed inside the pores of waste-tire-derived carbon. During lithiation and delithiation, the carbon matrix can effectively absorb the volume expansion caused by tin, thereby minimizing pulverization and capacity fade of the electrodes. In conclusion, the as-synthesized anode yielded a capacity of 690 mAh g –1 after 300 cycles at a current density of 40 mA g –1 with a stable battery performance.

25 ENERGY STORAGE↗

Degradation-resistant TiO 2 @Sn anodes for high-capacity lithium-ion batteries

As the demand for higher-performance batteries has increased, so has the body of research on theoretical high-capacity anode materials. However, the research has been hindered because the high-capacity anode material properties and interactions are not well understood, largely due to the difficulty of observing cycling in situ. Using electrochemical scanning transmission electron microscopy (ec-STEM), we report the real-time observation and electrochemical analysis of pristine tin (Sn) and titanium dioxide-coated Sn (TiO 2 @Sn) electrodes during lithiation/delithiation. As expected, we observed a volume expansion of the pristine Sn electrodes during lithiation, but we further observed that the expansion was followed by Sn detachment from the current collector. Remarkably, although the TiO 2 @Sn electrodes also exhibited similar volume expansion during lithiation, they showed no evidence of Sn detachment. We found that the TiO 2 surface layer acted as an electrochemically activated artificial solid-electrolyte interphase that serves to conduct Li ions. As a physical coating, it mechanically prevented Sn detachment following volume changes during cycling, providing significant degradation resistance and 80% Coulombic efficiency for a complete lithiation/delithiation cycle. Interestingly, upon delithiation, TiO 2 @Sn electrode displayed a self-healing mechanism of small pore formation in the Sn particle followed by agglomeration into several larger pores as delithiation continued.

25 ENERGY STORAGE↗

Disintegration of Meatball Electrodes for LiNi x Mn y Co z O 2 Cathode Materials

Mechanical degradation of Li-ion batteries caused by the repetitive swelling and shrinking of electrodes upon electrochemical cycles is now well recognized. Structural disintegration of the state-of-art cathode materials of a hierarchical structure is relatively less studied. In this paper, we track the microstructural evolution of different marked regimes in LiNi x Mn y Co z O 2 (NMC) electrodes after lithiation cycles. Decohesion of primary particles constitutes the major mechanical degradation in the NMC materials, which results in the loss of connectivity of the conductive network and impedance increase. We find that the structural disintegration is largely dependent on the charging rate – slow charging causes more damage, and is relatively insensitive to the cyclic voltage window. We use finite element modeling to study the evolution of Li concentration and stresses in a NMC secondary particle and employ the cohesive zone model to simulate the interfacial fracture between primary particles. Finally, we reveal that microcracks accumulate and propagate during the cyclic lithiation and delithiation at a slow charging rate.

25 ENERGY STORAGE↗

Coal-derived graphene foam and micron-sized silicon composite anodes for lithium-ion batteries

Silicon-based materials demonstrate significant potential as lithium-ion batteries (LIBs) anode, but their expansion and degradation present engineering design challenges for commercial application. In this study, a porous three-dimensional (3D) graphene and micron-sized silicon composite anode (Si@G foam) was synthesized using humic acid (HA) derived from coal as a graphene precursor. In-situ formation of graphene structure through reducing HA was confirmed by Raman spectra. The reduced HA (rHA) shows similar electrical conductivity compared to the commercial conductive carbon. SEM images depict a 3D skeleton of coal-derived graphene, with silicon particles distributed on the 3D graphene foam's internal surface. The Si@G composite-anode displays a good reversible capacity of ~656 mAh/g at a current density of 50 mA/g, as well as a high-rate capability of ~433 mAh/g at a current density of 800 mA/g, and outstanding cycling stability –89.8% capacity retention after 300 cycles, which is significantly higher than that of other foam structures. During lithiation and de-lithiation, the graphene foam serves as a matrix of electrical conductors and a volume expansion support for silicon. This 3D graphene network will be beneficial for developing advanced silicon-based anodes for high-performance LIBs.

25 ENERGY STORAGE↗

On the dynamics of the fluoroethylene carbonate generated solid electrolyte interphase on silicon anodes during calendar life aging

Here, the widespread use of silicon (Si)-rich anodes in lithium-ion batteries (LIBs) is impeded by an unstable solid electrolyte interphase (SEI) incurring insufficient cell life. Fluoroethylene carbonate (FEC) additive in the electrolyte significantly improves cycle life. However, the gains on calendar life remain unclear; the SEI structure still undergoes detrimental alterations at rest. Thus, elucidating the SEI dynamics during calendar aging is critical to mitigating time-dependent capacity degradation. ATR-FTIR, XPS, and ToF-SIMS are used herein to investigate the SEI structure before and after calendar aging. Si cycled without FEC exhibits no notable SEI chemistry changes Pre- and Post-aging, leaving poor passivation as the main failure pathway. Conversely, the FEC-SEI starts as short oligomeric species from FEC/EC electroreduction prior to aging; after calendar aging, polymerized carbonates become consistently more prominent. Unexpectedly, the deposition of self-polymerized FEC species results from time exposure to the delithiated Si specifically as opposed to the lithiated surface. This unexpected finding is supported by another recent Si calendar-aging research, which albeit not investigating FEC, finds global failure of the SEI upon delithiation resulting in ∼247 fold more reactive surface compared to the lithiated.

Batteries↗

Synthesis of hierarchical graphene coated porous Si anode for lithium-ion batteries

The ultra-high capacity and widespread availability of Si materials have resulted in them being the focus of extensive studies to replace the graphite anode. However, the main barriers preventing the Si anodes from large-scale applications are their huge volume change and severe interface reactions in the lithiation/delithiation process, which pulverizes its structure and subsequently deteriorates its cycle life. Here, micrometer-scale porous Si coated with graphene coating (mpSi@G) has been synthesized by using SiO 2 nanoparticles and novel coal-derived humic acid as feedstocks through a magnesiothermic reduction, followed by spray drying and calcination techniques. SEM, Raman, and X-ray absorption analysis demonstrate that the hierarchical graphene shell and micrometer-sized porous Si structure effectively release the Si anode's mechanical stress upon lithiation to achieve good structural stability. Here, the synthesized mpSi@G anode delivers a high initial lithiation capacity of 2974.9 mAh g –1 at 0.1 A g –1 with an initial coulombic efficiency of 70.2 %. Furthermore, the conductive hierarchical graphene network, along with the tight contacts of porous-Si and the graphene shell, contribute to a high capacity of 1109.5 mAh g –1 at a high current density of 5.0 A g –1 , showing excellent rate capability.

25 ENERGY STORAGE↗

Tracking the evolution of processes occurring in silicon anodes in lithium ion batteries by 3D visualization of relaxation times

An unconventional electroanalytical method has been used for tracking processes in silicon anodes in lithium ion batteries: a 3D visualization of relaxation times. Impedance data of the electrodes were collected at different potentials and different cycles during cyclic voltammetry, and were treated by means of the Distribution of Relaxation Times (DRT) method. A 3D visualization of the results allowed to identify the formation of a solid electrolyte interphase on the anode, composed of two layers with different relaxation times. Such findings are not possible by conventional analysis of impedance data by modeling with equivalent circuits, nor by simple DRT alone. Additionally, it was possible to observe that the characteristic relaxation time of the lithiation of the Si anode becomes smaller upon cycling, indicating that the material experiences structural transformations that allow it to lithiate faster. The result is relevant to motivate the use of micron-sized particles in the anode.

25 ENERGY STORAGE↗

Formation of lithium fluoride/metal nanocomposites for energy storage through solid state reduction of metal fluorides

In order to utilize high energy metal fluoride electrode materials as direct replacement electrode materials for lithium ion batteries in the future, a methodology to prelithiate the cathode or anode must be developed. Herein, we introduce the use of a solid state Li(3)N route to achieve the lithiation and mechanoreduction of metal fluoride based nanocomposites. The resulting prelithiation was found to be effective with the formation of xLiF:Me structures of very fine nanodimensions analogous to what is found by electrochemical lithiation. Physical and electrochemical properties of these nanocomposites for the bismuth and iron lithium fluoride systems are reported. (C) 2011 Elsevier B.V. All rights reserved.

Amatucci, GG↗

Avoiding Fracture in a Conversion Battery Material through Reaction with Larger Ions

Conversion and alloying electrode materials offer high specific capacity for emerging sodium- and potassium-ion batteries, but the larger volume changes compared to reaction with lithium are thought to limit cyclability. The reaction mechanisms of many materials with Na + and K + are unknown, however, and this knowledge is key for engineering mechanically resilient materials. Here, in situ transmission electron microscopy is used to uncover the nanoscale transformations during the reaction of FeS 2 electrode materials with Li + , Na + , and K + . Surprisingly, despite larger volume changes during the conversion reaction with Na + and K + , the FeS 2 crystals only fracture during lithiation. Modeling of reaction-induced deformation shows that the shape of the two-phase reaction front influences stress evolution, and unique behavior during lithiation causes stress concentrations and fracture. The larger volume changes in Na- and K-ion battery materials may therefore be managed through understanding and control of reaction mechanisms, ultimately leading to better alkali-ion batteries.

25 ENERGY STORAGE↗

Reinvestigation on the state-of-the-art nonaqueous carbonate electrolytes for 5 V Li-ion battery applications

The charging voltage limits of mixed carbonate solvents for Li-ion batteries have been systematically investigated from 4.9 to 5.3 V in half cells using Cr-doped spinel cathode material LiNi0.45Cr0.05Mn1.5O4. We found that the stability of conventional carbonate electrolytes is strongly related to the stability and properties of the cathode materials at both lithiated and de-lithiated states. It is the first time to report that the conventional electrolytes based on mixtures of ethylene carbonate (EC) and linear carbonate (dimethyl carbonate - DMC, ethyl methyl carbonate - EMC, and diethyl carbonate - DEC) have shown very similar long-term cycling performance when cycled up to 5.2 V on LiNi0.45Cr0.05Mn1.5O4. The discharge capacity increases with the charge cutoff voltage and reaches the highest discharge capacity at 5.2 V. The capacity retention is about 87% after 500 cycles at 1C rate for all three carbonate mixtures when cycled between 3.0 V and 5.2V. The first-cycle efficiency has a maximum value at 5.1 V, with an average from 83% to 85% at C/10 rate. When cycled to 5.3 V, EC-DMC still shows good cycling performance but EC-EMC and EC-DEC show faster capacity fading. EC-DMC and EC-EMC have much better rate capability than EC-DEC. In addition, the first-cycle irreversible capacity loss increases with the cutoff voltage and the 'inactive' conductive carbon has also been found to be partly associated with the low first-cycle Coulombic efficiency at high voltages due to electrolyte decomposition and probably the PF6- anion irreversible intercalation.

25 ENERGY STORAGE↗

Understanding the crack formation of graphite particles in cycled commercial lithium-ion batteries by focused ion beam - scanning electron microscopy

Here in this paper, the structure degradation of commercial Lithium-ion battery (LIB) graphite anodes with different cycling numbers and charge rates was investigated by focused ion beam (FIB) and scanning electron microscopy (SEM). The cross-section image of graphite anode by FIB milling shows that cracks, resulted in the volume expansion of graphite electrode during long-term cycling, were formed in parallel with the current collector. The crack occurs in the bulk of graphite particles near the lithium insertion surface, which might derive from the stress induced during lithiation and de-lithiation cycles. Subsequently, crack takes place along grain boundaries of the polycrystalline graphite, but only in the direction parallel with the current collector. Furthermore, fast charge graphite electrodes are more prone to form cracks since the tensile strength of graphite is more likely to be surpassed at higher charge rates. Therefore, for LIBs long-term or high charge rate applications, the tensile strength of graphite anode should be taken into account.

25 ENERGY STORAGE↗