Highlights: ► NaLa{sub 1−x}MgWO{sub 6}:xRE{sup 3+} phosphors were synthesized by solid-state reaction method. ► Compared with Y{sub 2}O{sub 3}:Eu{sup 3+}, NaLaMgWO{sub 6}:Eu{sup 3+} performed better luminescence properties. ► The results demonstrated NaLaMgWO{sub 6} as a suitable host for RE{sup 3+}-doping. -- Abstract: Single phase of NaLa{sub 1−x}MgWO{sub 6}:xRE{sup 3+} (0 < x ≤1) (RE = Eu, Sm, Tb) phosphors were prepared by solid-state reaction method. X-ray diffraction, scanning electron microscopy, the morphology energy-dispersive X-ray spectroscopy, UV–vis diffuse reflectance spectra and photoluminescence were used to characterize the samples. Under the light excitation, NaLaMgWO{sub 6}:Eu{sup 3+}, NaLaMgWO{sub 6}:Sm{sup 3+} and NaLaMgWO{sub 6}:Tb{sup 3+}, phosphors showed the characteristic emissions of Eu{sup 3+} ({sup 5}D{sub 0} → {sup 7}F{sub 4,3,2,1}), Sm{sup 3+} ({sup 4}G{sub 5/2} → {sup 6}H{sub 5/2,7/2,9/2}), and Tb{sup 3+} ({sup 5}D{sub 4} → {sup 7}F{sub 6,5,4,3}), respectively. The intensity of the red emission for Na(La{sub 0.6}Eu{sub 0.4})MgWO{sub 6} is 2.5 times higher than that of (Y{sub 0.95}Eu{sub 0.05}){sub 2}O{sub 3} under blue light irradiation. The quantum efficiencies of the entitled phosphors excited under 394 nm and 464 nm are also investigated and compared with commercial phosphors Y{sub 2}O{sub 3}:Eu{sup 3+}, Sr{sub 2}Si{sub 5}N{sub 8}:Eu{sup 2+} and Y{sub 3}A{sub 5}G{sub 12}:Ce{sup 3+}. The results demonstrated NaLaMgWO{sub 6}:RE{sup 3+} phosphors as potential candidates for white light emitting diode pumped by UV or blue chip.