Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “INTERMETALLICS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 433 records · Page 24

Solid state phase equilibria and intermetallic compounds of the Al-Cr-Ho system

The solid state phase equilibria of the Al-Cr-Ho ternary system at 500 Degree-Sign C were experimentally investigated. The phase relations at 500 Degree-Sign C are governed by 14 three-phase regions, 29 two-phase regions and 15 single-phase regions. The existences of 10 binary compounds and 2 ternary phases have been confirmed. Al{sub 11}Cr{sub 2}, Al{sub 11}Cr{sub 4} and Al{sub 17}Ho{sub 2} were not found at 500 Degree-Sign C. Crystal structures of Al{sub 9}Cr{sub 4} and Al{sub 8}Cr{sub 4}Ho were determined by the Rietveld X-ray powder data refinement. Al{sub 9}Cr{sub 4} was found to exhibit cubic structure with space group I4-bar 3m (no. 217) and lattice parameters a=0.9107(5) nm. Al{sub 8}Cr{sub 4}Ho crystallizes in ThMn{sub 12} structure type with space group I4/mmm (no. 139) and lattice parameters a=0.8909(4) nm, c=0.5120(5) nm. It is concluded that the obtained Al{sub 4}Cr phase in this work should be {mu}-Al{sub 4}Cr by comparing with XRD pattern of the hexagonal {mu}-Al{sub 4}Mn compound. - Graphical abstract: The solid state phase equilibria of the Al-Cr-Ho ternary system at 500 Degree-Sign C. Highlights: Black-Right-Pointing-Pointer Al-Cr-Ho system has been investigated. Black-Right-Pointing-Pointer Al{sub 9}Cr{sub 4} has cubic structure with space group I4-bar 3m. Black-Right-Pointing-Pointer Al{sub 8}Cr{sub 4}Ho crystallizes in ThMn{sub 12} type with space group I4/mmm. Black-Right-Pointing-Pointer Al{sub 4}Cr phase is {mu}-type at 500 Degree-Sign C.

36 MATERIALS SCIENCE↗

Characterization of intermetallic precipitates in a Nimonic alloy by ultrasonic velocity measurements

Ultrasonic velocity measurements have been carried out in Nimonic 263 specimens thermally aged at 923 and 1073 K for durations up to 75 h and correlated with the results of hardness measurements and electron microscopy studies. The ultrasonic velocities and hardness results obtained in the specimens thermally aged at both temperatures clearly indicated that ultrasonic velocity is more sensitive to the initiation of the precipitation, whereas the influence of precipitation on hardness can be observed only after the precipitates attain a minimum size to influence the movement of dislocations. Further, ultrasonic velocity measurements also revealed faster kinetics and a lesser amount of precipitation at 1073 K compared to 923 K due to higher solubility of precipitate-forming elements.

36 MATERIALS SCIENCE↗

The significance of intermetallic compounds formed during interdiffusion in aluminum and magnesium dissimilar welds

Diffusion couples between Al-AA6111 and Mg-AZ31 have been used to perform a comprehensive review of the IMC phases that develop in this system, including; their growth kinetics, texture, residual stresses, and mechanical properties. The new observations made have been compared to data in the literature with the aim of providing an in-depth understanding of the detrimental effects of interfacial reaction in aluminum–magnesium dissimilar welding. Three Al–Mg binary IMC phases were identified, γ-Al{sub 12}Mg{sub 17} and β-Al{sub 3}Mg{sub 2}, as well as ε-Al{sub 30}Mg{sub 23}, which has not been previously reported in inter-diffusion studies. The β phase had the highest growth rate and became the dominant constituent of the IMC layer at longer reaction times. The ε-phase only appeared after extended heat treatment, via transformation at the Al{sub 12}Mg{sub 17}/Al{sub 3}Mg{sub 2} interface. Intrinsic diffusion coefficients of Al and Mg, calculated in the Al{sub 3}Mg{sub 2} phase, confirmed that Al is the faster diffusing species (by an order of magnitude) during IMC growth. Indentation techniques showed that all the IMC phases had extremely low toughness (1/2 ). FIB-assisted ring core milling revealed that both the β-Al{sub 3}Mg{sub 2} and γ-Al{sub 12}Mg{sub 17} phases contained large residual stresses. Their in-situ fracture toughness was consequently found to be asymmetric with lower values parallel to the joint interface. Greater tensile residual stress was measured in the β-Al{sub 3}Mg{sub 2} phase, which, combined with a lower toughness and more rapid growth kinetics, explains why it is generally the ‘weak link’ in Al–Mg dissimilar joints.

36 MATERIALS SCIENCE↗

Microstructure evolution, grain morphology variation and mechanical property change of Cu-Sn intermetallic joints subjected to high-temperature aging

Highlights: • The δ-Cu{sub 41}Sn{sub 11} could be formed by reaction of 11Cu{sub 3}Sn + 9Cu → Cu{sub 41}Sn{sub 11} during aging above 350 °C. • The temperature effects on the growth rate and grain morphology of Cu{sub 41}Sn{sub 11} phase were found. • The Cu{sub 41}Sn{sub 11} joints with refined grains exhibited higher hardness and shear strength. • The Cu{sub 41}Sn{sub 11} joints exhibited a combination of transgranular and intergranular fracture during shear test. - Abstract: In this work, the aging treatment was carried out on full Cu{sub 3}Sn joints at different temperatures for various durations, the microstructure evolution, grain morphology variation and mechanical property change of joints were investigated. The temperature effects on the growth rate and grain morphology of Cu{sub 41}Sn{sub 11} phase were found: The complete transformation from Cu{sub 3}Sn phase to Cu{sub 41}Sn{sub 11} phase in joints needed 300 h at 400 °C, but 4 h at 500 °C. The Cu{sub 41}Sn{sub 11} phase formed at 400 °C consisted of columnar grains with an average width of 23.5 μm, while the Cu{sub 41}Sn{sub 11} phase formed at 500 °C consisted columnar grains with an average width of 8.5 μm. The average hardness and shear strength values of the Cu{sub 41}Sn{sub 11} joints formed at 400 °C were 432.5 HV and 62 MPa, while the joints formed at 500 °C exhibited higher hardness and shear strength (451.5 HV and 65 MPa). Besides, the Cu{sub 41}Sn{sub 11} joint was found to exhibit a combination of transgranular and intergranular fracture during shear test.

36 MATERIALS SCIENCE↗

Microstructural evolution and growth behavior of intermetallic compounds at the liquid Al/solid Fe interface by synchrotron X-ray radiography

Highlights: • A layered and tongue-like η phase was in-situ observed by synchrotron radiation X-ray radiography. • The coalescence of η phase bottom resulted in dissolution, further increasing the growth rate. • The θ phase growth behavior with different morphologies during cooling was analyzed. - Abstract: The growth of Inter-Metallic Compounds (IMCs) with dissolution was investigated on the liquid Al/solid Fe interconnection by using synchrotron radiation real-time imaging technology. At the initial stage of holding at 850 °C, a layer of the η-Fe{sub 2}Al{sub 5} phase formed at the interface, and tongue-like η grew into α-Fe. The tongue-like η phase had a stronger (001) texture than the layered phase. The coalescence of tongue-like η started at the bottom, followed by the dissolution of IMCs, which leads to a further increase in its growth rate. During solidification stage, the dotted, needle-like and flake θ-FeAl{sub 3} phases were sequentially formed.

36 MATERIALS SCIENCE↗

Formation of Fe2Al5-xZnx intermetallic crystals at the Fe-Zn interface in hot-dip galvanizing

Highlights: • Interstitial-free steels were galvanized in Zn baths containing 0.14-0.28 wt% Al. • The Fe-Al layer formed in a 0.14 wt% Al bath is composed of equiaxed Fe{sub 2}Al{sub 5-x}Zn{sub x} crystals without preferred orientations. • The layers formed in baths containing 0.18 wt% Al or more are composed of orientated domains. • Each domain contains 4-12 Fe{sub 2}Al{sub 5-x}Zn{sub x} crystal variants of specific orientations. • A layer of a single variant crystal can grow epitaxially on the α-Fe grains as the Al content reaches 0.28 wt%. - Abstract: The formation of Fe{sub 2}Al{sub 5-x}Zn{sub x} inhibition layer at the Fe-Zn interface has been characterized by scanning electron microscopy/electron backscatter diffraction and transmission electron microscopy for interstitial-free steels galvanized in Zn baths containing 0.14–0.28 wt% Al. The inhibition layer formed in the 0.14 wt% Al bath is composed of fine, equiaxed Fe{sub 2}Al{sub 5-x}Zn{sub x} crystals without preferred orientations. The inhibition layers formed in the baths containing 0.18 wt% Al or more are composed of orientated domains and each domain contains 4–12 Fe{sub 2}Al{sub 5-x}Zn{sub x} crystal variants of specific orientations. All the variants follow the same Fe{sub 2}Al{sub 5-x}Zn{sub x}/Fe orientation relationship of [110]{sub Fe2Al5-xZnx}//[1 1-bar 1]{sub Fe} and (001){sub Fe2Al5-xZnx}//(110){sub Fe}. Therefore, each domain is formed on a single α-Fe grain and the number of variants in the domain is determined by the orientation of the α-Fe grain. The fraction of the area of epitaxial growth increases with increasing Al content in bath. When the Al content reaches 0.28 wt%, a layer of a single variant (SV) crystal can grow epitaxially on the α-Fe grains having orientations distributed from <110> to <113> parallel to the normal direction of the sheet surface. The formation of a dense SV inhibition layer is the major reason for the drastic reductions in both the Al-pickup rate and the inhibition layer thickness at high Al content baths.

36 MATERIALS SCIENCE↗

Synthesis and characteristic of FeNi{sub 3} intermetallic compound obtained by electrical explosion of wire

In this work, the FeNi{sub 3} permalloy nanopowder was synthesized by wire explosion in deionized water. X-ray diffraction was used to identify and characterize the prepared nanopowder exhibiting a FeNi{sub 3} phase. The morphology and size of the prepared powders were observed by field emission-scanning electron microscopy and transmission electron microscopy. The compositions of the wire before exploding and the nanopowder were determined with electron probe microanalysis. The results indicate that the FeNi{sub 3} permalloy nanopowder was synthesized with an average particle size {approx}50 nm. The magnetic properties of the nanopowder indicate a symmetric hysteresis loop of ferromagnetic behavior with coercivity of 199.3 Oe and saturation magnetization of 56.7 emu/g.

36 MATERIALS SCIENCE↗

Role of spin-orbit coupling on crystal-field splitting and phase-stability of rare-earth based layered intermetallic

Layered and incommensurate heterostructures have attracted much attention for the occurrence of superconductivity and charge density waves with the possibility of intercalating foreign atoms. However, lanthanide-based heterostructures where (Eu x Sm 1-x )S and TaS 2 are alternatively stacked have been scarcely investigated. In this work, we performed phase stability, bonding behavior and electronic-structure analysis of (Eu x Sm 1-x )TaS 3 using first-principles density-functional theory methods. Our phase stability analysis suggests 50 at.% solubility of Eu in (Eu x Sm 1-x )TaS 3 compared to Eu solubility in all proportions in cubic SmS. The instability of Eu beyond 50 at.% in (Eu x Sm 1-x )TaS 3 was attributed to higher density of Eu-4f states at the Fermi-level. Based on band position calculated from spin-orbit coupling effect, we constructed a qualitative schematic of possible crystal-field analysis. The local change in bond-length and bond-angle around Eu-S in (Eu x Sm 1-x )TaS 3 correlate well with our crystal-field analysis. We believe that quantum mechanical insights provided in this work will be useful to understand other complex heterostructures.

36 MATERIALS SCIENCE↗

Mechanistic Insights into Acetate Selectivity on Intermetallic CuPd(110) in CO Reduction

Experimental studies demonstrate that CuPd(110) uniquely favors acetate formation during CO reduction (CORR), contrasting with the preference for ethylene on Cu surfaces. To elucidate this selectivity, we employed explicit solvation density functional theory (DFT) calculations to investigate the reaction mechanism from both thermodynamic and kinetic angles. Here, our findings reveal that on CuPd(110), the acetate-pathway intermediate H 2 CCO is thermodynamically favored at experimental conditions, while CHCHO─a precursor to ethylene─is preferred on Cu(111). Beyond thermodynamics, we find that H 2 CCO is kinetically accessible under the experimental conditions on CuPd(110), aiding acetate formation. Electron density difference analyses further corroborate distinct protonation preferences supporting this mechanism. We propose a thermodynamic screening parameter based on the Gibbs free energy, G H 2 CCO < G CHCHO , as a guide for designing Cu-based catalysts with enhanced acetate selectivity. These results offer critical mechanistic insights into the CORR product distribution and a rational framework for future catalyst design.

Acetate↗

Multiscale Morphology of Nanoporous Copper Made from Intermetallic Phases

Many application-relevant properties of nanoporous metals critically depend on their multiscale architecture. For example, the intrinsically high step-edge density of curved surfaces at the nanoscale provides highly reactive sites for catalysis, whereas the macroscale pore and grain morphology determines the macroscopic properties, such as mass transport, electrical conductivity, or mechanical properties. Here, in this work, we systematically study the effects of alloy composition and dealloying conditions on the multiscale morphology of nanoporous copper (np-Cu) made from various commercial Zn–Cu precursor alloys. Using a combination of X-ray diffraction, electron backscatter diffraction, and focused ion beam cross-sectional analysis, our results reveal that the macroscopic grain structure of the starting alloy surprisingly survives the dealloying process, despite a change in crystal structure from body-centered cubic (Zn–Cu starting alloy) to face-centered cubic (Cu). The nanoscale structure can be controlled by the acid used for dealloying with HCl leading to a larger and more faceted ligament morphology compared to that of H 3 PO 4 . Finally, anhydrous ethanol dehydrogenation was used as a probe reaction to test the effect of the nanoscale ligament morphology on the apparent activation energy of the reaction.

36 MATERIALS SCIENCE↗

Synthesis, structure, and bonding in K12Au21Sn4. A polar intermetallic compound with dense Au20 and open AuSn4 layers

The new phase K{sub 12}Au{sub 21}Sn{sub 4} has been synthesized by direct reaction of the elements at elevated temperatures. Single crystal X-ray diffraction established its orthorhombic structure, space group Pmmn (No. 59), a = 12.162(2); b = 18.058(4); c = 8.657(2) {angstrom}, V = 1901.3(7) {angstrom}{sup 3}, and Z = 2. The structure consists of infinite puckered sheets of vertex-sharing gold tetrahedra (Au{sub 20}) that are tied together by thin layers of alternating four-bonded-Sn and -Au atoms (AuSn{sub 4}). Remarkably, the dense but electron-poorer blocks of Au tetrahedra coexist with more open and saturated Au-Sn layers, which are fragments of a zinc blende type structure that maximize tetrahedral heteroatomic bonding outside of the network of gold tetrahedra. LMTO band structure calculations reveal metallic properties and a pseudogap at 256 valence electrons per formula unit, only three electrons fewer than in the title compound and at a point at which strong Au-Sn bonding is optimized. Additionally, the tight coordination of the Au framework atoms by K plays an important bonding role: each Au tetrahedra has 10 K neighbors and each K atom has 8-12 Au contacts. The appreciably different role of the p element Sn in this structure from that in the triel members in K{sub 3}Au{sub 5}In and Rb{sub 2}Au{sub 3}Tl appears to arise from its higher electron count which leads to better p-bonding (valence electron concentrations = 1.32 versus 1.22).

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Magnetic ordering in the rare earth intermetallic compound Tb2Ti3Ge4: Magnetization and neutron diffraction studies

Magnetization and neutron diffraction studies on a polycrystalline Tb2Ti3Ge4 sample (orthorhombic Sm5Ge4-type structure, space group Pnma, No. 62) have been carried out. This compound is found to order antiferromagnetically at ~18 K (TN). The magnetization versus field isotherms obtained at 2, 3, 5, and 10 K indicate a field-induced antiferromagnetic to ferromagnetic transition in fields of the order of 0.5 T. The saturation magnetization value at 2.5 K (M extrapolated to 1/H 0) is only ~5.6uB/Tb3+, suggesting the possible presence of crystal field effects with or without a persisting antiferromagnetic component. Neutron powder diffraction data at 10 K confirm the existence of a magnetic long range order. Modeling of the magnetic scattering reveals a complex and incommensurate antiferromagnetic spin structure below TN.

72 PHYSICS OF ELEMENTARY PARTICLES AND FIELDS↗

Mechanical Properties of Iron Alumininides Intermetallic Alloy with Molybdenum Addition

In this work, FeAl-based alloys with and without molybdenum addition were fabricated by sintering of mechanically alloyed powders in order to investigate the effect of molybdenum on iron aluminide mechanical properties. Bulk samples were prepared by mechanical alloying for 4 hours, pressing at 360 MPa and sintering at 1000 deg. C for 2 hours. The specimens were tested in compression at room temperature using Instron machine. The phase identification and microstructure of the consolidated material was examined by x-ray diffraction and scanning electron microscope correspondingly. Results show that 2.5 wt%Mo addition significantly increased the ultimate stress and ultimate strain in compressive mode due to solid solution hardening. However, the addition of Mo more than 2.5 wt% was accompanied by a reduction in both properties caused by the presence of Mo-rich precipitate particles.

36 MATERIALS SCIENCE↗