Influencing mechanism of Al-containing Zn coating on interfacial microstructure and mechanical properties of friction stir spot welded Mg–steel joint

Highlights: • Al-containing Zn coating improved Mg–steel interfacial wettability during friction stir spot welding (FSSW). • Pre-existing Al{sub 5}Fe{sub 2} phase in coating on steel surface promoted Mg–steel metallurgical bonding. • A high tensile-shear load of 4.3 kN was obtained in FSSW AZ31–steel joint. - Abstract: 2.4 mm thick AZ31 Mg alloy sheet and 1.5 mm Q234 steel sheet with a hot-dipped Al-containing Zn coating were friction stir spot welded (FSSW) using a pinless tool. It was shown that the Al-containing Zn coating played a crucial role in joining the Mg alloy and steel during FSSW. The Zn coating observably improved the Mg–steel interfacial wettability during FSSW, and the Al{sub 5}Fe{sub 2} phase in the Zn coating on the steel substrate surface promoted the metallurgical bonding of Mg alloy and steel. It was confirmed that the Al{sub 5}Fe{sub 2} phase on the steel surface resulted from the reaction between the steel substrate and the Al in the Zn coating during hot-dipping, and was not related to the Al-containing Mg alloy substrate. The tensile-shear load of the FSSW Mg–steel joint reached 4.3 kN. The fracture of the joint occurred along the interface on the steel substrate side. The interface between the Al{sub 5}Fe{sub 2} layer and Mg alloy substrate was the weakest region of the Mg–steel joint.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Addressing the Limit of Detectability of Residual Oxide Discontinuities in Friction Stir Butt Welds of Aluminum using Phased Array Ultrasound

This activity seeks to estimate a theoretical upper bound of detectability for a layer of oxide embedded in a friction stir weld in aluminum. The oxide is theoretically modeled as an ideal planar layer of aluminum oxide, oriented normal to an interrogating ultrasound beam. Experimentally-measured grain scattering level is used to represent the practical noise floor. Echoes from naturally-occurring oxides will necessarily fall below this theoretical limit, and must be above the measurement noise to be potentially detectable.

Johnston, P. H.↗

Friction Stir Spot Welding of Advanced High Strength Steels

Experiments are continuing to evaluate the feasibility of friction stir spot welding advanced high-strength steels including, DP780, martensitic hot-stamp boron steel, and TRIP steels. Spot weld lap-shear strengths can exceed those required by industry standards such as AWS D8.1.

AHSS↗

FSW of Aluminum Tailor Welded Blanks across Machine Platforms

Development and characterization of friction stir welded aluminum tailor welded blanks was successfully carried out on three separate machine platforms. Each was a commercially available, gantry style, multi-axis machine designed specifically for friction stir welding. Weld parameters were developed to support high volume production of dissimilar thickness aluminum tailor welded blanks at speeds of 3 m/min and greater. Parameters originally developed on an ultra-high stiffness servo driven machine where first transferred to a high stiffness servo-hydraulic friction stir welding machine, and subsequently transferred to a purpose built machine designed to accommodate thin sheet aluminum welding. The inherent beam stiffness, bearing compliance, and control system for each machine were distinctly unique, which posed specific challenges in transferring welding parameters across machine platforms. This work documents the challenges imposed by successfully transferring weld parameters from machine to machine, produced from different manufacturers and with unique control systems and interfaces.

aluminum↗

A Weighting Grade-Based Optimization Method for Determining Refill Friction Stir Spot Welding Process Parameters

The welding process used in fabricating thin-walled structures by refill friction stir spot welding (RFSSW) should be characterized by a high strength of welds and high process repeatability which is demonstrated by a small dispersion of the load capacity of the joints. The present work is designed to optimize RFSSW process parameters for 7075-T6 Alclad aluminum alloy sheets used to fabricate aircraft structures. The optimization was performed by scalarization of the objective function using the weighting grades method. The study considers the effect of process parameters, i.e., tool plunge depth, duration of welding, tool rotational speed, on the tensile/shear strength of the joints, and dispersion of the load capacity. It was found that it was possible to choose the optimal welding parameters taking into account maximization of the load capacity and minimization of the dispersion of the joint strength via a best compromise between the tool rotational speed ensuring adequate plasticization of the base material and the duration of welding ensuring that a fine-grained joint microstructure is obtained.

36 MATERIALS SCIENCE↗

2014/2219 Tri-Point Crack Analysis

Friction stir welding (FSW) is a solid state welding process with potential advantages for aerospace and automotive industries dealing with light alloys. Self-reacting friction stir welding (SR-FSW) is one variation of the FSW process being developed at the National Aeronautics and Space Administration (NASA) for use in the fabrication of propellant tanks. Friction plug welding is used to seal the exit hole that remains in a circumferential SR-FSW. The objective of this study was to evaluate the deformation response at the tips of cracks located in the heat affected zone of friction plug welds and to study the fracture behavior of welds with defects in the form of fatigue cracks. The study used existing 2014-T6 to 2219-T87 self-reacting friction stir weld panels with 2219-T87 friction plug welds. Electro-discharge machined (EDM) notches were machined into the heat affected zone of the plug at the plug-to-base metal interface. Samples were then cycled to generate a fatigue crack emanating from the notch. After the fatigue crack reached a pre-defined length, a speckle pattern was applied and the ARAMIS system (a three dimensional imaging correlation system) was used to measure the deformations at the crack tip under a sequence of loads. Testing was conducted at ambient laboratory conditions. Fracture data from the testing was analyzed to evaluate residual strength capability of the panel as a function of flaw size. ARAMIS strain data was evaluated to examine strain and deformation patterns that develop around the crack tip and at the plug/weld interfaces. Four samples were used in this study, with three samples in a post-weld heat treated condition. Three samples contained large diameter plugs (M5) and one sample contained a small diameter plug (M3). Two samples were 4 inches in width and two samples were 8.5 inches in width. All samples failed through the precrack with residual strengths ranging from 37 ksi to 42 ksi.

Horton, Karla Renee↗

Manufacturing Challenges Associated with the Use of Metal Matrix Composites in Aerospace Structures

Metal Matrix Composites (MMCs) consist of a metal alloy reinforced with ceramic particles or fibers. These materials possess a very high strength to weight ratio, good resistance to impact and wear, and a number of other properties which make them attractive for use in aerospace and defense applications. MMCs have found use in the space shuttle orbiter's structural tubing, the Hubble Space Telescope's antenna mast, control surfaces and propulsion systems for aircraft, and tank armors. The size of MMC components is severely limited by difficulties encountered in joining these materials using fusion welding. Melting of the material results in formation of an undesirable phase (formed when molten Aluminum reacts with the reinforcement) which leaves a strength depleted region along the joint line. Friction Stir Welding (FSW) is a relatively nascent solid state joining technique developed at The Welding Institute (TWI) in 1991. The process was first used at NASA to weld the super lightweight external tank for the Space Shuttle. Today FSW is used to join structural components of the Delta IV, Atlas V, and Falcon IX rockets as well as NASA's Orion Crew Exploration Vehicle and Space Launch System. A current focus of FSW research is to extend the process to new materials, such as MMCs, which are difficult to weld using conventional fusion techniques. Since Friction Stir Welding occurs below the melting point of the workpiece material, this deleterious phase is absent in FSW-ed MMC joints. FSW of MMCs is, however, plagued by rapid wear of the welding tool, a consequence of the large discrepancy in hardness between the steel tool and the reinforcement material. This chapter summarizes the challenges encountered when joining MMCs to themselves or to other materials in structures. Specific attention is paid to the influence of process variables in Friction Stir Welding on the wear process characterizes the effect of process parameters (spindle speed, traverse rate, and length of joint) on the wear process. A phenomenological model of the wear process was constructed based on the rotating plug model of Friction Stir Welding. The effectiveness of harder tool materials (such as Tungsten Carbide, high speed steel, and tools with diamond coatings) to combat abrasive wear is also explored. In-process force, torque, and vibration signals are analyzed to assess the feasibility of in situ monitoring of tool shape changes as a result of wear (an advancement which would eliminate the need for off-line evaluation of tool condition during joining). Monitoring, controlling, and reducing tool wear in FSW of MMCs is essential to implementation of these materials in structures (such as launch vehicles) where they would be of maximum benefit. The work presented here is extendable to machining of MMCs, where wear of the tool is also a limiting factor.

Prater, Tracie↗

Linking process and structure in the friction stir scribe joining of dissimilar materials: A computational approach with experimental support

We present that friction stir welding (FSW) is a popular technique to join dissimilar materials in numerous applications. The solid state nature of the process enables joining materials with strikingly different physical properties. For welds in lap configuration, an enhancement to this technology is made by introducing a short, hard insert, referred to as a cutting-scribe, at the bottom of the tool pin. The cutting-scribe induces deformation in the bottom plate which leads to the formation of mechanical interlocks or hook like structures at the interface of two materials. A thermo-mechanical computational model employing a coupled Eulerian-Lagrangian approach is developed to quantitatively capture the morphology of these interlocks during the FSW process. Simulations using this model are validated by experimental observations. In conclusion, the identified interface morphology coupled with the predicted temperature field from this process–structure model can be used to estimate the post-weld microstructure and joint strength.

36 MATERIALS SCIENCE↗

Friction stirring interlocking of dissimilar materials

A method for solid state joining of dissimilar materials using a friction stir welding device wherein a pin is inserted through an aperture defined in a first material and a second material to hold the materials together and then held in place by friction stir welding a portion of the pin to a material adjacent said pin, or by friction stir welding a cap or plug that holds the pin in place to the adjacent material. The result is a connection or join wherein the central portion of the pin is not friction stir welded but the portions holding the pin in place (the ends or caps) generally are.

Whalen, Scott A.↗

Friction plug welding

Friction plug welding (FPW) usage is advantageous for friction stir welding (FSW) hole close-outs and weld repairs in 2195 Al--Cu--Li fusion or friction stir welds. Current fusion welding methods of Al--Cu--Li have produced welds containing varied defects. These areas are found by non-destructive examination both after welding and after proof testing. Current techniques for repairing typically small (<0.25) defects weaken the weldment, rely heavily on welders' skill, and are costly. Friction plug welding repairs increase strength, ductility and resistance to cracking over initial weld quality, without requiring much time or operator skill. Friction plug welding while pulling the plug is advantageous because all hardware for performing the weld can be placed on one side of the workpiece.

Takeshita, Riki↗

Microstructure and texture evolution of friction stir lap welded dissimilar multi-aluminum stack

Here this work investigates the microstructural evolution of a dissimilar multiple-aluminum alloy stack (AA7055, AA7055, AA6022) produced by friction stir lap welding (FSLW). A through-thickness analyses of grain orientation map, grain size and distribution, strain distribution, and texture evolution by electron backscattered diffraction-based characterization technique were performed. Two different welding parameters (combination of tool rotation and traverse speed) were used to study the effects of the welding parameters on these microstructural characteristics. The study shows that higher welding speed and higher rotation speed of the FSLW tool yield finer grains. FSLW resulted in shear texture formation in the weld regions due to high welding speeds. This texture development in the nugget zone is consistent with shear deformation, and (111) pole figures show ideal shear texture components. The Stir Zone (SZ) exhibits shear texture (A/A ̅ and B/B ̅ components), consistent with other shear-assisted processes. Recrystallization mechanisms observed are CDRX in SZ and DDRX in TMAZ (Thermo-Mechanically Affected Zone). Interface analysis reveals the presence of oxide layers between different aluminum sheets, affecting joint mechanical performance. The mechanical property of the lap welded joints was presented in terms of microhardness distribution across the weld cross section. Slightly higher hardness in higher speed welding setup was observed throughout the SZ and AA6022 layer, indicating greater grain refinement and uniform grain structure distribution.

36 MATERIALS SCIENCE↗

Evaluation of intermetallic compound layer at aluminum/steel interface joined by friction stir scribe technology

Heat input and high strain rate deformation during friction stir welding of aluminum and steel resulted in the diffusion-based formation of a Fe x Al y intermetallic compound (IMC) layer. Compared with conventional friction stir welding tools, a friction stir scribe tool can reduce heat input significantly limiting the IMC layer thickness (~100–750 nm). Friction stir scribe joined lap joints fractured either through the welded interface or within the base aluminum alloy on the loading side, depending on IMC layer thickness during tensile lap shear testing. In addition, a modified effective heat of formation model predicted that Al 13 Fe 4 formed first at aluminum/steel interface and, during welding process, was substituted by Al 5 Fe 2 with local silicon enrichment, which was verified via microstructural characterization.

36 MATERIALS SCIENCE↗

Reducing Intermetallic Compounds of Mg/Al Joint in Friction Stir Lap Welding

To reduce intermetallic compounds (IMCs) of Al{sub 12}Mg{sub 17} and Al{sub 3}Mg{sub 2} in Mg/Al friction stir lap welding joint, pin tip was plunged into the lower sheet at a small distance. Results showed that at a fixed welding speed of 50 mm/min, sound joints were obtained using rotating speeds from 750 to 500 rpm, and the IMCs zones were rather small. Cracks easily appeared inside IMCs inside onion ring and at lap interface. Therefore, reducing the IMC was beneficial for reducing the crack. Joint lap shear stress firstly increased and then decreased with decrease in the rotating speed. The maximum shear stress of 50.2 MPa was attained at a rotating speed of 500 rpm because of reduced IMC.

36 MATERIALS SCIENCE↗

On the microstructure characterization of the AA2098-T351 alloy welded by FSW

Highlights: • The microstructural characterization of the AA2098-T351 Al-Cu-Li alloy welded by FSW was carried out. • There was strong correlation between the results of the various techniques. • DSC was an effective technique for characterization of GP zones complementing the microstructural characterization by TEM. - Abstract: The complex structure of the AA2098-T351 alloy welded by friction stir welding (FSW) was investigated by transmission electron microscopy (TEM), differential scanning calorimetry (DSC) and microhardness measurements. Thermal modelling process of the FSW process was carried out by soldering thermocouples at distances of 6, 9 and 12 mm from the weld centerline, and thermocouple measurements were used as input data into the model. Finite element software COMSOL v5.2 was used for data analysis. The prevailing phases in the base metal (BM) are T1 (Al{sub 2}CuLi) θ′ (Al{sub 2}Cu), δ′/β′(Al{sub 3}(Li,Zr)) and Ω (Al{sub 2}Cu). In the heat affected zone (HAZ), either in the retreating or advancing sides, θ′ phase was not identified. In the thermomechanical affected zone (TMAZ), T1, δ′/β′, GP zones phase were detected in the retreating side, whereas T1 and Guinier-Preston (GP) zones were not observed in the advancing side. This result supports the asymmetric behavior observed in the microhardness profile of the weld. In the stir zone (SZ), GP zones, T1, δ′/β′ (Al{sub 3}(Li,Zr)) and Ω were identified.

36 MATERIALS SCIENCE↗

Friction Stir Lap Welding 0.8-mm-Thick 2024 Aluminum Alloy with the Assistance of Stationary Shoulder

In this work, 0.8-mm-thick 2024 aluminum alloy was friction stir lap welded with the assistance of a stationary shoulder system. The joint surface formation, microstructure and mechanical properties of the welded joints were studied. The results showed that sound joints without defect could be obtained at a wide parameter range because stationary shoulder increased the material flow during welding. The stationary shoulder decreased the joint roughness from 125.5 to 58.9 µm. A thickness reduction of 4% was achieved at a welding speed of 200 mm/min. The joint fabricated by the stationary shoulder system had superior lap shear properties compared to the joint fabricated using the conventional tool. A high failure load of 7440 N was achieved at welding speed of 200 mm/min. The joint presented tensile fracture mode and the fracture morphology showed typical ductile fracture.

36 MATERIALS SCIENCE↗

Growth kinetics of Al–Fe intermetallic compounds during annealing treatment of friction stir lap welds

In this study, we explored the growth kinetics of the Al–Fe intermetallic (IM) layer at the joint interface of the St-12/Al-5083 friction stir lap welds during post-weld annealing treatment at 350, 400 and 450 °C for 30 to 180 min. Optical microscope (OM), field emission gun scanning electron microscope (FEG-SEM) and transmission electron microscope (TEM) were employed to investigate the structure of the weld zone. The thickness and composition of the IM layers were evaluated using image analysis system and electron back-scatter diffraction (EBSD), respectively. Moreover, kernel average misorientation (KAM) analysis was performed to evaluate the level of stored energy in the as-welded state. The results showed that the growth kinetics of the IM layer was not governed by a parabolic diffusion law. Presence of the IM compounds as well as high stored energy near the joint interface of the as-welded sample was recognized to be the origin of the observed deviation from the parabolic diffusion law. - Highlights: • This work provided a new insight into growth kinetics of Al–Fe IM thickness. • The growth kinetics of IM layer was not governed by a parabolic diffusion law. • IM near the joint interface was the origin of deviation from the parabolic law. • High stored energy at joint interface was origin of deviation from parabolic law.

36 MATERIALS SCIENCE↗

Numerical Simulation and Experimental Validation of Joint Performance in Aluminum-Steel Lap Welds Formed by Friction Stir Dovetailing

Friction stir dovetailing (FSD) is a new dissimilar material joining process that simultaneously forms a mechanical interlock and metallurgical bond at the dissimilar material interface. This work presents development of a modeling and simulation approach to predict mechanical performance of FSD thick section aluminum to steel joints. A finite element analysis (FEA) was carried out in order to predict the load-carrying capacity and failure location for aluminum thicknesses between 12.7 mm and 50.8 mm with different numbers of dovetails. The numerical results and corresponding experimental investigation are in agreement and suggest that the developed methods can be used effectively for design and analysis of FSD joints using standard FEA tools.

Friction stir dovetailing, Friction stir welding, ↗

Welding Development: Marshall Space Flight Center

This paper presents the basic understanding of the friction stir welding process. It covers process description, pin tool operation and materials, metal flow theory, mechanical properties, and materials welded using the process. It also discusses the thermal stir welding process and the differences between thermal stir and friction stir welding. MSFC weld tools used for development are also presented.

Ding, Jeff↗