Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Ellipsometry”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 433 records · Page 24

Optical characteristics of nanocrystalline Al{sub x}Ga{sub 1−x}N thin films deposited by hollow cathode plasma-assisted atomic layer deposition

Gallium nitride (GaN), aluminum nitride (AlN), and Al{sub x}Ga{sub 1−x}N films have been deposited by hollow cathode plasma-assisted atomic layer deposition at 200 °C on c-plane sapphire and Si substrates. The dependence of film structure, absorption edge, and refractive index on postdeposition annealing were examined by x-ray diffraction, spectrophotometry, and spectroscopic ellipsometry measurements, respectively. Well-adhered, uniform, and polycrystalline wurtzite (hexagonal) GaN, AlN, and Al{sub x}Ga{sub 1−x}N films were prepared at low deposition temperature. As revealed by the x-ray diffraction analyses, crystallite sizes of the films were between 11.7 and 25.2 nm. The crystallite size of as-deposited GaN film increased from 11.7 to 12.1 and 14.4 nm when the annealing duration increased from 30 min to 2 h (800 °C). For all films, the average optical transmission was ∼85% in the visible (VIS) and near infrared spectrum. The refractive indices of AlN and Al{sub x}Ga{sub 1−x}N were lower compared to GaN thin films. The refractive index of as-deposited films decreased from 2.33 to 2.02 (λ = 550 nm) with the increased Al content x (0 ≤ x ≤ 1), while the extinction coefficients (k) were approximately zero in the VIS spectrum (>400 nm). Postdeposition annealing at 900 °C for 2 h considerably lowered the refractive index value of GaN films (2.33–1.92), indicating a significant phase change. The optical bandgap of as-deposited GaN film was found to be 3.95 eV, and it decreased to 3.90 eV for films annealed at 800 °C for 30 min and 2 h. On the other hand, this value increased to 4.1 eV for GaN films annealed at 900 °C for 2 h. This might be caused by Ga{sub 2}O{sub 3} formation and following phase change. The optical bandgap value of as-deposited Al{sub x}Ga{sub 1−x}N films decreased from 5.75 to 5.25 eV when the x values decreased from 1 to 0.68. Furthermore, postdeposition annealing did not affect the bandgap of Al-rich films.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Surface chemistry of a Cu(I) beta-diketonate precursor and the atomic layer deposition of Cu{sub 2}O on SiO{sub 2} studied by x-ray photoelectron spectroscopy

The surface chemistry of the bis(tri-n-butylphosphane) copper(I) acetylacetonate, [({sup n}Bu{sub 3}P){sub 2}Cu(acac)] and the thermal atomic layer deposition (ALD) of Cu{sub 2}O using this Cu precursor as reactant and wet oxygen as coreactant on SiO{sub 2} substrates are studied by in-situ x-ray photoelectron spectroscopy (XPS). The Cu precursor was evaporated and exposed to the substrates kept at temperatures between 22 °C and 300 °C. The measured phosphorus and carbon concentration on the substrates indicated that most of the [{sup n}Bu{sub 3}P] ligands were released either in the gas phase or during adsorption. No disproportionation was observed for the Cu precursor in the temperature range between 22 °C and 145 °C. However, disproportionation of the Cu precursor was observed at 200 °C, since C/Cu concentration ratio decreased and substantial amounts of metallic Cu were present on the substrate. The amount of metallic Cu increased, when the substrate was kept at 300 °C, indicating stronger disproportionation of the Cu precursor. Hence, the upper limit for the ALD of Cu{sub 2}O from this precursor lies in the temperature range between 145 °C and 200 °C, as the precursor must not alter its chemical and physical state after chemisorption on the substrate. Five hundred ALD cycles with the probed Cu precursor and wet O{sub 2} as coreactant were carried out on SiO{sub 2} at 145 °C. After ALD, in-situ XPS analysis confirmed the presence of Cu{sub 2}O on the substrate. Ex-situ spectroscopic ellipsometry indicated an average film thickness of 2.5 nm of Cu{sub 2}O deposited with a growth per cycle of 0.05 Å/cycle. Scanning electron microscopy and atomic force microscopy (AFM) investigations depicted a homogeneous, fine, and granular morphology of the Cu{sub 2}O ALD film on SiO{sub 2}. AFM investigations suggest that the deposited Cu{sub 2}O film is continuous on the SiO{sub 2} substrate.

36 MATERIALS SCIENCE↗

Initial growth, refractive index, and crystallinity of thermal and plasma-enhanced atomic layer deposition AlN films

The authors have studied and compared the initial growth and properties of AlN films deposited on Si(111) by thermal and plasma-enhanced atomic layer deposition (ALD) using trimethylaluminum and either ammonia or a N{sub 2}-H{sub 2} mixture as precursors. In-situ spectroscopic ellipsometry was employed to monitor the growth and measure the refractive index of the films during the deposition. The authors found that an incubation stage only occurred for thermal ALD. The linear growth for plasma-enhanced ALD (PEALD) started instantly from the beginning due to the higher nuclei density provided by the presence of plasma. The authors observed the evolution of the refractive index of AlN during the growth, which showed a rapid increase up to a thickness of about 30 nm followed by a saturation. Below this thickness, higher refractive index values were obtained for AlN films grown by PEALD, whereas above that the refractive index was slightly higher for thermal ALD films. X-ray diffraction characterization showed a wurtzite crystalline structure with a (101{sup ¯}0) preferential orientation obtained for all the layers with a slightly better crystallinity for films grown by PEALD.

36 MATERIALS SCIENCE↗

Atomic layer deposition of magnesium fluoride via bis(ethylcyclopentadienyl)magnesium and anhydrous hydrogen fluoride

A new process has been developed to deposit magnesium fluoride (MgF{sub 2}) thin films via atomic layer deposition (ALD) for use as optical coatings in the ultraviolet. MgF{sub 2} was deposited in a showerhead style ALD reactor using bis(ethylcyclopentadienyl)magnesium and anhydrous hydrogen fluoride (HF) as precursors at substrate temperatures from 100 to 250 °C. The use of HF was observed to result in improved morphology and reduced impurity content compared to other reported MgF{sub 2} ALD approaches that use metal fluoride precursors as the fluorine-containing chemistry. Characterization of these films has been performed using spectroscopic ellipsometry, atomic force microscopy, and x-ray photoelectron spectroscopy for material deposited on silicon substrates. Films at all substrate temperatures were transparent at wavelengths down to 190 nm and the low deposition temperature combined with low surface roughness makes these coatings good candidates for a variety of optical applications in the far ultraviolet.

36 MATERIALS SCIENCE↗

Spatial atomic layer deposition on flexible substrates using a modular rotating cylinder reactor

Spatial atomic layer deposition (ALD) is a new version of ALD based on the separation of reactant gases in space instead of time. In this paper, the authors present results for spatial ALD on flexible substrates using a modular rotating cylinder reactor. The design for this reactor is based on two concentric cylinders. The outer cylinder remains fixed and contains a series of slits. These slits can accept a wide range of modules that attach from the outside. The modules can easily move between the various slit positions and perform precursor dosing, purging, or pumping. The inner cylinder rotates with the flexible substrate and passes underneath the various spatially separated slits in the outer cylinder. Trimethyl aluminum and ozone were used to grow Al{sub 2}O{sub 3} ALD films at 40 °C on metallized polyethylene terephthalate (PET) substrates to characterize this spatial ALD reactor. Spectroscopic ellipsometry measurements revealed a constant Al{sub 2}O{sub 3} ALD growth rate of 1.03 Å/cycle with rotation speeds from 40 to 100 RPM with the outer cylinder configured for one Al{sub 2}O{sub 3} ALD cycle per rotation. The Al{sub 2}O{sub 3} ALD growth rate then decreased at higher rotation rates for reactant residence times < 5 ms. The Al{sub 2}O{sub 3} ALD films were also uniform to within <1% across the central portion of metallized PET substrate. Fixed deposition time experiments revealed that Al{sub 2}O{sub 3} ALD films could be deposited at 2.08 Å/s at higher rotation speeds of 175 RPM. Even faster deposition rates are possible by adding more modules for additional Al{sub 2}O{sub 3} ALD cycles for every one rotation of the inner cylinder.

36 MATERIALS SCIENCE↗

Low temperature plasma enhanced atomic layer deposition of conducting zirconium nitride films using tetrakis (dimethylamido) zirconium and forming gas (5% H{sub 2} + 95% N{sub 2}) plasma

Zirconium nitride (ZrN) has the lowest bulk electrical resistivity and high thermal stability among group IV and V transition metal nitrides, which makes it a promising material for ULSI applications such as a diffusion barrier for Cu interconnects, contact metal in III-V semiconductor devices, and in high density memory structures. Plasma enhanced atomic layer deposition (PEALD) of conducting ZrN thin films using Zr[N(CH{sub 3}){sub 2}]{sub 4} and forming gas (5% H{sub 2} + 95% N{sub 2}) plasma is reported in this article. The growth per cycle (GPC) for every deposition was determined from analysis of dynamic in-situ spectroscopic ellipsometry (d-iSE) measurements. An experimental design is proposed for faster determination of ALD growth saturation curves. At substrate temperature of 150 °C, a GPC of 0.10 nm/cycle was observed for self-limiting ZrN PEALD growth. The electrical resistivity of ZrN films deposited on SiO{sub 2} substrate was found to be 559.5 ± 18.5 μΩ cm with negligible change in resistivity even after ∼1000 h exposure to air. The metallic behavior of our ZrN films was evident from the free electron dispersion component in dielectric response, the broad band of photoelectron emission across Fermi level and the positive temperature coefficient for resistivity of 0.0088/ °C.

36 MATERIALS SCIENCE↗

Comparison of B{sub 2}O{sub 3} and BN deposited by atomic layer deposition for forming ultrashallow dopant regions by solid state diffusion

In this study, the authors investigated atomic layer deposition (ALD) of B{sub 2}O{sub 3} and BN for conformal, ultrashallow B doping applications and compared the effect of dopant-containing overlayers on sheet resistance (R{sub s}) and B profiles for both types of films subjected to a drive-in thermal anneal. For the deposition of B{sub 2}O{sub 3}, tris(dimethylamido)borane and O{sub 3} were used as coreactants and for the deposition of BN, BCl{sub 3} and NH{sub 3} were used as coreactants. Due to the extreme air instability of B{sub 2}O{sub 3} films, physical analysis was performed on B{sub 2}O{sub 3} films, which were capped in-situ with ∼30 Å ALD grown Al{sub 2}O{sub 3} layers. For the BN films, in-situ ALD grown Si{sub 3}N{sub 4} capping layers (∼30 Å) were used for comparison. From spectroscopic ellipsometry, a thickness decrease was observed after 1000 °C, 30 s anneal for the B{sub 2}O{sub 3} containing stack with 60 ALD cycles of B{sub 2}O{sub 3}, whereas the BN containing stacks showed negligible thickness decrease after the annealing step, regardless of the number of BN cycles tested. The postanneal reduction in film thickness as well as decrease in R{sub s} for the B{sub 2}O{sub 3} containing stack suggests that the solid state diffusion dopant mechanism is effective, whereas for the BN containing stacks this phenomenon seems to be suppressed. Further clarification of the effectiveness of the B{sub 2}O{sub 3} containing layer compared to the film stacks with BN was evidenced in backside secondary ion mass spectrometry profiling of B atoms. Thus, B{sub 2}O{sub 3} formed by an ALD process and subsequently capped in-situ followed by a drive-in anneal offers promise as a dopant source for ultrashallow doping, whereas the same method using BN seems ineffective. An integrated approach for B{sub 2}O{sub 3} deposition and annealing on a clustered tool also demonstrated controllable R{sub s} reduction without the use of a capping layer.

36 MATERIALS SCIENCE↗

Effect of substrate composition on atomic layer deposition using self-assembled monolayers as blocking layers

The authors have examined the effect of two molecules that form self-assembled monolayers (SAMs) on the subsequent growth of TaN{sub x} by atomic layer deposition (ALD) on two substrate surfaces, SiO{sub 2} and Cu. The SAMs that the authors have investigated include two vapor phase deposited, fluorinated alkyl silanes: Cl{sub 3}Si(CH{sub 2}){sub 2}(CF{sub 2}){sub 5}CF{sub 3} (FOTS) and (C{sub 2}H{sub 5}O){sub 3}Si(CH{sub 2}){sub 2}(CF{sub 2}){sub 7}CF{sub 3} (HDFTEOS). Both the SAMs themselves and the TaN{sub x} thin films, grown using Ta[N(CH{sub 3}){sub 2}]{sub 5} and NH{sub 3}, were analyzed ex situ using contact angle, spectroscopic ellipsometry, x-ray photoelectron spectroscopy (XPS), and low energy ion-scattering spectroscopy (LEISS). First, the authors find that both SAMs on SiO{sub 2} are nominally stable at T{sub s} ∼ 300 °C, the substrate temperature used for ALD, while on Cu, the authors find that HDFTEOS thermally desorbs, while FOTS is retained on the surface. The latter result reflects the difference in the head groups of these two molecules. The authors find that both SAMs strongly attenuate the ALD growth of TaN{sub x} on SiO{sub 2}, by about a factor of 10, while on Cu, the SAMs have no effect on ALD growth. Results from LEISS and XPS are decisive in determining the nature of the mechanism of growth of TaN{sub x} on all surfaces. Growth on SiO{sub 2} is 2D and approximately layer-by-layer, while on the surfaces terminated by the SAMs, it nucleates at defect sites, is islanded, and is 3D. In the latter case, our results support growth of the TaN{sub x} thin film over the SAM, with a considerable delay in formation of a continuous thin film. Growth on Cu, with or without the SAMs, is also 3D and islanded, and there is also a delay in the formation of a continuous thin film as compared to growth on SiO{sub 2}. These results highlight the power of coupling measurements from both LEISS and XPS in examinations of ultrathin films formed by ALD.

36 MATERIALS SCIENCE↗

Plasma-enhanced atomic layer deposition of titanium oxynitrides films: A comparative spectroscopic and electrical study

The process parameters' impact of the plasma-enhanced atomic layer deposition (PE-ALD) method on the oxygen to nitrogen (O/N) ratio in titanium oxynitride (TiO{sub x}N{sub y}) films was studied. Titanium(IV)isopropoxide in combination with NH{sub 3} plasma and tetrakis(dimethylamino)titanium by applying N{sub 2} plasma processes were investigated. Samples were characterized by the in situ spectroscopic ellipsometry, x-ray photoelectron spectroscopy, and electrical characterization (current–voltage: I-V and capacitance–voltage: C-V) methods. The O/N ratio in the TiO{sub x}N{sub y} films is found to be very sensitive for their electric properties such as conductivity, dielectric breakdown, and permittivity. Our results indicate that these PE-ALD film properties can be tuned, via the O/N ratio, by the selection of the process parameters and precursor/coreactant combination.

36 MATERIALS SCIENCE↗

Comparison of trimethylgallium and triethylgallium as “Ga” source materials for the growth of ultrathin GaN films on Si (100) substrates via hollow-cathode plasma-assisted atomic layer deposition

GaN films grown by hollow cathode plasma-assisted atomic layer deposition using trimethylgallium (TMG) and triethylgallium (TEG) as gallium precursors are compared. Optimized and saturated TMG/TEG pulse widths were used in order to study the effect of group-III precursors. The films were characterized by grazing incidence x-ray diffraction, atomic force microscopy, x-ray photoelectron spectroscopy, and spectroscopic ellipsometry. Refractive index follows the same trend of crystalline quality, mean grain, and crystallite sizes. GaN layers grown using TMG precursor exhibited improved structural and optical properties when compared to GaN films grown with TEG precursor.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Periodic oxidation for fabricating titanium oxynitride thin films via atomic layer deposition

This paper demonstrates thermal atomic layer deposition (ALD) combined with periodic oxidation for synthesizing titanium oxynitride (TiON) thin films. The process used a typical ALD reactor for the synthesis of titanium nitride (TiN) films wherein oxygen was supplied periodically between the ALD-TiN cycles. The great advantage of the process proposed here was that it allowed the TiN films to be oxidized efficiently. Also, a uniform depth profile of the oxygen concentration in the films could be obtained by tuning the oxidation conditions, allowing the process to produce a wide variety of TiON films. The resistivity measurement is a convenient method to confirm the reproducibility of metal film fabrication but may not be applicable for TiON films depending upon the oxidation condition because the films can easily turn into insulators when subjected to periodic oxidation. Therefore, an alternative reproducibility confirmation method was required. In this study, spectroscopic ellipsometry was applied to monitor the variation of TiON films and was able to detect changes in film structures such as conductor–insulator transitions in the TiON films.

36 MATERIALS SCIENCE↗

Atomic layer deposition of cerium oxide for potential use in diesel soot combustion

The particulate soot emission from diesel motors has a severe impact on the environment and people's health. The use of catalytic convertors is one of the ways to minimize the emission and decrease the hazard level. In this paper, the activity of cerium oxide for catalytic combustion of diesel soot was studied. Thin films of cerium dioxide were synthesized by atomic layer deposition using tetrakis(2,2,6,6-tetramethyl-3,5-heptanedionato)cerium [Ce(thd){sub 4}] and ozone as precursors. The characteristics of the films were studied as a function of deposition conditions within the reaction temperature range of 180–350 °C. Thickness, crystallinity, elemental composition, and morphology of the CeO{sub 2} films deposited on Si (100) were characterized by ellipsometry, x-ray diffraction, x-ray photoelectron spectroscopy, atomic force microscopy, and field emission scanning electron microscopy, respectively. The growth rate of CeO{sub 2} was observed to be 0.30 Å/cycle at temperatures up to 250 °C with a slight increase to 0.37 Å/cycle at 300 °C. The effect of CeO{sub 2} films grown on stainless steel foil supports on soot combustion was measured with annealing tests. Based on the analysis of these, in catalytic applications, CeO{sub 2} has been shown to be effective in lowering the soot combustion temperature from 600 °C for the uncoated substrates to 370 °C for the CeO{sub 2} coated ones. It was found that the higher deposition temperatures had a positive effect on the catalyst performance.

36 MATERIALS SCIENCE↗

Silicon nitride and silicon etching by CH{sub 3}F/O{sub 2} and CH{sub 3}F/CO{sub 2} plasma beams

Silicon nitride (SiN, where Si:N ≠ 1:1) films low pressure-chemical vapor deposited on Si substrates, Si films on Ge on Si substrates, and p-Si samples were exposed to plasma beams emanating from CH{sub 3}F/O{sub 2} or CH{sub 3}F/CO{sub 2} inductively coupled plasmas. Conditions within the plasma beam source were maintained at power of 300 W (1.9 W/cm{sup 3}), pressure of 10 mTorr, and total gas flow rate of 10 sccm. X-ray photoelectron spectroscopy was used to determine the thicknesses of Si/Ge in addition to hydrofluorocarbon polymer films formed at low %O{sub 2} or %CO{sub 2} addition on p-Si and SiN. Polymer film thickness decreased sharply as a function of increasing %O{sub 2} or %CO{sub 2} addition and dropped to monolayer thickness above the transition point (∼48% O{sub 2} or ∼75% CO{sub 2}) at which the polymer etchants (O and F) number densities in the plasma increased abruptly. The C(1s) spectra for the polymer films deposited on p-Si substrates appeared similar to those on SiN. Spectroscopic ellipsometry was used to measure the thickness of SiN films etched using the CH{sub 3}F/O{sub 2} and CH{sub 3}F/CO{sub 2} plasma beams. SiN etching rates peaked near 50% O{sub 2} addition and 73% CO{sub 2} addition. Faster etching rates were measured in CH{sub 3}F/CO{sub 2} than CH{sub 3}F/O{sub 2} plasmas above 70% O{sub 2} or CO{sub 2} addition. The etching of Si stopped after a loss of ∼3 nm, regardless of beam exposure time and %O{sub 2} or %CO{sub 2} addition, apparently due to plasma assisted oxidation of Si. An additional GeO{sub x}F{sub y} peak was observed at 32.5 eV in the Ge(3d) region, suggesting deep penetration of F into Si, under the conditions investigated.

36 MATERIALS SCIENCE↗

Structure and optical band gaps of (Ba,Sr)SnO{sub 3} films grown by molecular beam epitaxy

Epitaxial growth of (Ba{sub x}Sr{sub 1−x})SnO{sub 3} films with 0 ≤ x ≤ 1 using molecular beam epitaxy is reported. It is shown that SrSnO{sub 3} films can be grown coherently strained on closely lattice and symmetry matched PrScO{sub 3} substrates. The evolution of the optical band gap as a function of composition is determined by spectroscopic ellipsometry. The direct band gap monotonously decreases with x from to 4.46 eV (x = 0) to 3.36 eV (x = 1). A large Burnstein-Moss shift is observed with La-doping of BaSnO{sub 3} films. The shift corresponds approximately to the increase in Fermi level and is consistent with the low conduction band mass.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Thermal atomic layer etching of crystalline aluminum nitride using sequential, self-limiting hydrogen fluoride and Sn(acac){sub 2} reactions and enhancement by H{sub 2} and Ar plasmas

Thermal atomic layer etching (ALE) of crystalline aluminum nitride (AlN) films was demonstrated using sequential, self-limiting reactions with hydrogen fluoride (HF) and tin(II) acetylacetonate [Sn(acac){sub 2}] as the reactants. Film thicknesses were monitored versus number of ALE reaction cycles at 275 °C using in situ spectroscopic ellipsometry (SE). A low etch rate of ∼0.07 Å/cycle was measured during etching of the first 40 Å of the film. This small etch rate corresponded with the AlO{sub x}N{sub y} layer on the AlN film. The etch rate then increased to ∼0.36 Å/cycle for the pure AlN films. In situ SE experiments established the HF and Sn(acac){sub 2} exposures that were necessary for self-limiting surface reactions. In the proposed reaction mechanism for thermal AlN ALE, HF fluorinates the AlN film and produces an AlF{sub 3} layer on the surface. The metal precursor, Sn(acac){sub 2}, then accepts fluorine from the AlF{sub 3} layer and transfers an acac ligand to the AlF{sub 3} layer in a ligand-exchange reaction. The possible volatile etch products are SnF(acac) and either Al(acac){sub 3} or AlF(acac){sub 2}. Adding a H{sub 2} plasma exposure after each Sn(acac){sub 2} exposure dramatically increased the AlN etch rate from 0.36 to 1.96 Å/cycle. This enhanced etch rate is believed to result from the ability of the H{sub 2} plasma to remove acac surface species that may limit the AlN etch rate. The active agent from the H{sub 2} plasma is either hydrogen radicals or radiation. Adding an Ar plasma exposure after each Sn(acac){sub 2} exposure increased the AlN etch rate from 0.36 to 0.66 Å/cycle. This enhanced etch rate is attributed to either ions or radiation from the Ar plasma that may also lead to the desorption of acac surface species.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Measurement of the infrared optical constants for spectral modeling: n and k values for (NH4)2SO4 via single-angle reflectance and ellipsometric methods

The optical constants n and k can be used to model infrared spectra, including refraction, absorption, reflectance, and emissivity, but obtaining reliable values for solid materials (pure or otherwise) presents a challenge: In the past, the best results for n and k have been obtained from bulk, homogeneous materials, free of defects. That is, materials where the Fresnel equations are operant since there is no light scattering. Since it is often not possible to obtain a pure macroscopic (crystalline) material, it may be possible to press the material into a (uniform, void-free) disk. We have recently been able to do this with ammonium sulfate powder and then measured the n & k values via two independent methods: 1) Ellipsometry - which measures the changes in amplitude and phase of light reflected from the material of interest as a function of wavelength and angle of incidence, and 2) Single angle specular reflectance with an FT spectrometer using a specular reflectance device within an FT instrument which measures the change in amplitude of light reflected from the material of interest as a function of wavelength and angle of incidence over a wide wavelength range. The quality of the derived n & k values was tested by generating the reflectance spectra of the pellet and comparing to the calculated to measured reflectance spectra of the pure material which has been previously published. The comparison to literature values showed good accuracy and good agreement, indicating promise to measure other materials by such methods.

ammonium sulfate↗

Comparison of methods to derive infrared optical constants for organic materials for optical modeling

Reflectance spectroscopy, especially at infrared wavelengths, is often used for contact, standoff, and remote sensing of solid materials. The reflectance spectra of solids, however, are complex, relying on many factors, even for the same material. Such phenomena can be modeled if the optical constants as a function of wavelength or wavenumber, n(?) and k(?), are known. Methods to measure the optical constants of solids, however, are challenging, particularly for powdered materials. For powdered materials, a pressed pellet of the neat material is often used when a crystalline specimen is not available. In this work, three techniques, including ellipsometry, single-angle reflectance and KBr transmission spectroscopy, are applied to an organic material, acetaminophen, for comparison, and the effects on the modeled spectra are shown.

ellipsometry, infrared (IR) spectroscopy, FTIR, hy↗

Dispersion of the refractive index in high-k dielectrics

A brief review of the optical properties of oxide materials that are used at present as dielectrics in modern microelectronics is presented. Using spectral ellipsometry, dispersion dependencies for different materials are measured. A brief comparative analysis of different dielectric coatings is carried out. The results of our research will be useful in further studies of the properties of dielectrics, as well as in technologies that are employed in the development of new semiconductor instruments and devices.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗