Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “EUTECTIC ALLOY”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 433 records · Page 24

Microstructure and Mechanical Properties of Laves Phase-strengthened Fe-Cr-Zr Alloys

Laves phase-reinforced alloys have shown some preliminary promising performance at room temperatures. This paper aims at evaluating mechanical properties of Laves phase-strengthened alloys at elevated temperatures. Three Fe-Cr-Zr alloys were designed to favor the formation of eutectic microstructures containing Laves and body-centered cubic phases with the aid of thermodynamic calculations. Microstructural characterization was carried out on the alloys in as-processed and aged states using optical microscopy, scanning electron microscopy, energy-dispersive X-ray spectroscopy, and X-ray diffraction. The effect of thermal aging and alloy composition on microstructure has been discussed based on microstructural characterization results. Mechanical properties have been evaluated by means of Vickers microhardness measurements, tensile testing at temperatures up to 973.15 K (700.15 °C), and creep testing at 873.15 K (600.15 °C) and 260 MPa. Alloys close to the eutectic composition show significantly superior strength and creep resistance compared to P92. Finally, however, their low tensile ductility may limit their applications at relatively low temperatures.

36 MATERIALS SCIENCE↗

Refinement of Promising Coating Compositions for Directionally Cast Eutectics

The successful application of high creep strength, directionally solidified gamma/gamma prime-delta (Ni-19.7Cb-6Cr-2.5Al) eutectic superalloy turbine blades requires the development of suitable coatings for airfoil, root and internal blade surfaces. In order to improve coatings for the gamma/gamma prime-delta alloy, the current investigation had the goals of (1) refining promising coating compositions for directionally solidified eutectics, (2) evaluating the effects of coating/ substrate interactions on the mechanical properties of the alloy, and (3) evaluating diffusion aluminide coatings for internal surfaces. Burner rig cyclic oxidation, furnace cyclic hot corrosion, ductility, and thermal fatigue tests indicated that NiCrAlY+Pt(63 to 127 micron Ni-18Cr-12Al-0.3Y + 6 micron Pt) and NiCrAlY(63 to 127 micron Ni-18Cr-12Al-0.3Y) coatings are capable of protecting high temperature gas path surfaces of eutectic alloy airfoils. Burner rig (Mach 0.37) testing indicated that the useful coating life of the 127 micron thick coatings exceeded 1000 hours at 1366 K (2000 deg F). Isothermal fatigue and furnance hot corrosion tests indicated that 63 micron NiCrAlY, NiCrAlY + Pt and platinum modified diffusion aluminide (Pt + Al) coating systems are capable of protecting the relatively cooler surfaces of the blade root. Finally, a gas phase coating process was evaluated for diffusion aluminizing internal surfaces and cooling holes of air-cooled gamma/gamma prime-delta turbine blades.

Strangman, T. E.↗

Non-destructive characterisation of polymers and Al-alloys by polychromatic cone-beam phase contrast tomography

X-ray computed tomography (XCT) has become a very important tool for the non-destructive characterisation of materials. Continuous improvements in the quality and performance of X-ray tubes and detectors have led to cone-beam XCT systems that can now achieve spatial resolutions down to 1 {mu}m and even below. Since not only the amplitude but also the phase of an X-ray beam is altered while passing through an object, phase contrast effects can occur even for polychromatic sources when the spatial coherence due to a small focal spot size is high enough. This can lead to significant improvements over conventional attenuation-based X-ray computed tomography. Phase contrast can increase by edge enhancement the visibility of small structures and of features which are only slightly different in attenuation. We report on the possibilities of polychromatic cone-beam phase contrast tomography for non-destructive characterisation of materials. A carbon fibre-reinforced polymer and the Al-alloys AlMg5Si7 and AlSi18 were investigated with high resolution cone-beam X-ray computed tomography with a polychromatic tube source. Under certain conditions strong phase contrast resulting in an upward and downward overshooting of the grey values across edges was observed. The phase effects are much stronger for the polymer than for the Al-alloys. The influence on the phase contrast of the parameters, including source-detector distance, focal spot size and tube acceleration voltage is presented. Maximum phase contrast was observed for a maximum distance between the source and the detector, for a low voltage and a minimum focal spot size at the X-ray source. The detectability of the different phases is improved by the edge enhancement and the resulting improvement of sharpness. Thus, a better segmentation of the carbon fibres in the fibre-reinforced polymer and of the Mg{sub 2}Si-phase in the AlMg5Si7-alloy is achieved. Primary and eutectic Si cannot be detected by attenuation-based X-ray computed tomography due to the small difference in X-ray attenuation between the Si and the Al-matrix in AlSi18. However, phase contrast effects lead to a significant detectability and the large primary Si particles become clearly visible in the tomograms of AlSi18. - Highlights: Black-Right-Pointing-Pointer Phase contrast increases with increasing distance object-detector and with decreasing U, X-ray spot. Black-Right-Pointing-Pointer The detectability of details is improved by the phase contrast. Black-Right-Pointing-Pointer For the carbon fibre-reinforced polymer the visibility of the carbon fibres is improved. Black-Right-Pointing-Pointer For AlMg5Si7 the detectability of the phases Fe-aluminides and Mg{sub 2}Si particles is improved. Black-Right-Pointing-Pointer For AlSi18 primary Si particles with a size > 50 {mu}m become detectable because of the phase contrast.

36 MATERIALS SCIENCE↗

Processing and Mechanical Properties of NiAl-Based In-Situ Composites

In-situ composites based on the NiAl-Cr eutectic system were successfully produced by containerless processing and evaluated. The NiAl-Cr alloys had a fibrous microstructure while the NiAl-(Cr,Mo) alloys containing 1 at. percent or more molybdenum exhibited a lamellar structure. The NiAl-28Cr-6Mo eutectic displays promising high temperature strength while still maintaining a reasonable room temperature fracture toughness when compared to other NiAl-based materials. The Laves phase NiAlTa was used to strengthen NiAl and very promising creep strengths were found for the directionally solidified NiAl-NiAlTa eutectic. The eutectic composition was found to be near NiAl-15.5Ta (at. percent) and well aligned microstructures were produced at this composition. An off-eutectic composition of NiAl-14.5Ta was also processed, consisting of NiAl dendrites surrounded by aligned eutectic regions. The room temperature toughness of these two phase alloys was similar to that of polycrystalline NiAl even with the presence of the brittle Laves phase NiAlTa. Polyphase in-situ composites were generated by directional solidification of ternary eutectics. The systems investigated were the Ni-Al-Ta-X (X=Cr, Mo, or V) alloys. Ternary eutectics were found in each of these systems and both the eutectic composition and temperature were determined. Of these ternary eutectics, the one in the NiAl-Ta-Cr system was found to be the most promising. The fracture toughness of the NiAl-(Cr,Al)NiTa-Cr eutectic was intermediate between those of the NiAl-NiAlTa eutectic and the NiAl-Cr eutectic. The creep strength of this ternary eutectic was similar to or greater than that of the NiAl-Cr eutectic.

Johnson, David Ray↗

Evaluation of Pb-17Li compatibility of ODS Fe-12Cr-5Al alloys

The Dual Coolant Lead Lithium (DCLL: eutectic Pb–17Li and He) blanket concept requires improved Pb–17Li compatibility with ferritic steels in order to demonstrate acceptable performance in fusion reactors. As an initial step, static Pb-17at.%Li (Pb-17Li) capsule experiments were conducted on new oxide dispersion strengthened (ODS) FeCrAl alloys ((1) Y 2 O 3 (125Y), (2) Y 2 O 3 +ZrO 2 (125YZ), (3) Y 2 O 3 +HfO 2 (125YH), and (4) Y 2 O 3 +TiO 2 (125YT)) produced at ORNL via mechanical alloying (MA). Tests were conducted in static Pb–17Li for 1000 h at 700°C. Alloys showed promising compatibility with Pb–17Li with small mass change after testing for 125YZ, 125YH and 125YT, while the 125Y alloy experienced the highest mass loss associated with some oxide spallation and subsequent alloy dissolution. X-ray diffraction methods identified the surface reaction product as LiAlO 2 on all four alloys. A small decrease (~1 at.%) in Al content beneath the oxide scale was observed in all 4 ODS alloys, which extended through 60 μm beneath the oxide/metal interface. This indicates improvements in alloy dissolution by decreasing the amount of Al loss from the alloy. Scales formed on 125YZ, 125YH and 125YT were examined via scanning transmission electron microscopy (S/TEM) and revealed incorporation of Zr-, Hf-, and Ti-rich precipitates within the LiAlO2 product, respectively. This indicates an inward scale growth mechanism. Future work in flowing Pb–17Li is needed to further evaluate the effectiveness of this strategy in a test blanket module.

36 MATERIALS SCIENCE↗

Atomic dynamics in molten AlCu alloys of different compositions and at different temperatures by cold neutron scattering

The atomic motions in molten Al1-xCux (x=0.10, 0.171 and 0.25) around the eutectic composition (x=0.171) were studied by cold neutron inelastic scattering at three different temperatures (973 K, 1173 K and 1373 K). An alloy of eutectic composition containing the 63Cu isotope was also studied. Self-diffusion coefficients for the Cu ions were determined from the width of quasielastic peaks and were found to decrease slightly with increasing Cu concentration. Longitudinal current correlation functions Jl(Q,E) exhibit at all temperatures and at all compositions a shoulder at energies below 10 meV and one main maximum at higher energies. These features can be interpreted in terms of excitations of acoustic and optic nature. The shape of Jl(Q,E) is sensitive to composition, being considerably more structured for larger Cu content. This can be coupled to the existence of a prepeak in the measured zeroth moment of dynamic scattering function indicating an increased chemical ordering with increasing Cu concentration for all temperatures. Indications for an existence of a liquid–liquid phase transition are presented.

36 MATERIALS SCIENCE↗

The electrical properties of low-g processed immiscible alloys

When dispersed or mixed immiscibles are solidified on earth, a large amount of separation of the constituents takes place due to differences in densities. However, when the immiscibles are dispersed and solidified in zero-gravity, density separation does not occur, and unique composite solids can be formed with many new and promising electrical properties. By measuring the electrical resistivity and superconducting critical temperature of zero-g processed Ga-Bi samples, it has been found that the electrical properties of such materials are entirely different from the basic constituents and the ground control samples. The finest dispersions are obtained only in a low-gravity environment. Our results indicate that space-processed immiscible materials may form an entirely new class of electronic materials. The interesting electrical properties of directionally solidified Al-Cu eutectic, a two-component alloy consisting of Al and Al2Cu which was processed on Skylab (M566) are briefly reviewed. The electrical resistivity of directionally solidified eutectics with a lamellar structure are highly anisotropic and have been studied both experimentally and theoretically. The local resistivity of the space-processed samples are compared to a ground control sample and to the expected theoretical results.

Otto, G. H.↗

Effect of Ni Addition to Sn0.7Cu Solder Alloy on Thermal Behavior, Microstructure, and Mechanical Properties

The addition of Ni on lead-free solder alloys Sn0.7Cu was tested in this study. A small amount of Ni was added to the solder alloys to evaluate the thermal behavior, microstructure, and mechanical properties of the composite solders after sintering and isothermal aging for 3 days and then compared with the results of the binary Sn0.7Cu solder. The results indicated that the ultimate tensile strength and yield tensile strength changed when adding 0.25 wt.% of Ni. The tested results of the differential scanning calorimeter showed that the addition of Ni (such as 0.5 and 1 wt.%) could obviously increase the solidification temperature of Sn0.7Cu alloys in the cooling process. When the Ni content was increased to 0.25 wt.% in the ternary condition, which includes the Sn0.7Cu-xNi (x = 0, 0.1, 0.25, 0.5, and 1 wt.%) solder alloys for the indentation creep test, the minimum creep rate reached the maximum; however, the trend was reversed as the Ni content was higher than this level. In addition, the microstructure of Sn-0.7Cu-xNi solder alloys was obviously different with the eutectic Sn-0.7Cu solder, such that the Ni gradually accumulated in the (Cu, Ni){sub 6}Sn{sub 5} IMCs within the Ni-containing solder alloys. Additionally, this process refined the microstructure of the Sn-0.7Cu solder. The fracture surface of the eutectic Sn-0.7Cu solder revealed ductile fracture modes; however, there was no mixed ductile–brittle fracture mode occurred when the Ni content was in the range of 0-1 wt.%.

36 MATERIALS SCIENCE↗

Structural direct-write additive manufacturing of molten metals

An alloy for structural direct-writing additive manufacturing comprising a base element selected from the group consisting of aluminum (Al), nickel (Ni) and a combination thereof, and a rare earth element selected from the group consisting of cerium (Ce), lanthanide (La) and a combination thereof, and a eutectic intermetallic present in said alloy in an amount ranging from about 0.5 wt. % to 7.5 wt. %. The invention is also directed to a method of structural direct-write additive manufacturing using the above-described alloy, as well as 3D objects produced by the method. The invention is also directed to methods of producing the above-described alloy.

Rios, Orlando↗

Cooling thermal parameters and microstructure features of directionally solidified ternary Sn–Bi–(Cu,Ag) solder alloys

Low temperature soldering technology encompasses Sn–Bi based alloys as reference materials for joints since such alloys may be molten at temperatures less than 180 °C. Despite the relatively high strength of these alloys, segregation problems and low ductility are recognized as potential disadvantages. Thus, for low-temperature applications, Bi–Sn eutectic or near-eutectic compositions with or without additions of alloying elements are considered interesting possibilities. In this context, additions of third elements such as Cu and Ag may be an alternative in order to reach sounder solder joints. The length scale of the phases and their proportions are known to be the most important factors affecting the final wear, mechanical and corrosions properties of ternary Sn–Bi–(Cu,Ag) alloys. In spite of this promising outlook, studies emphasizing interrelations of microstructure features and solidification thermal parameters regarding these multicomponent alloys are rare in the literature. In the present investigation Sn–Bi–(Cu,Ag) alloys were directionally solidified (DS) under transient heat flow conditions. A complete characterization is performed including experimental cooling thermal parameters, segregation (XRF), optical and scanning electron microscopies, X-ray diffraction (XRD) and length scale of the microstructural phases. Experimental growth laws relating dendritic spacings to solidification thermal parameters have been proposed with emphasis on the effects of Ag and Cu. The theoretical predictions of the Rappaz-Boettinger model are shown to be slightly above the experimental scatter of secondary dendritic arm spacings for both ternary Sn–Bi–Cu and Sn–Bi–Ag alloys examined. - Highlights: • Dendritic growth prevailed for the ternary Sn–Bi–Cu and Sn–Bi–Ag solder alloys. • Bi precipitates within Sn-rich dendrites were shown to be unevenly distributed. • Morphology and preferential region for the Ag{sub 3}Sn growth depend on Ag content and Ṫ{sub L}. • Rappaz-Boettinger model reasonably estimated the experimental scatter of λ{sub 2}.

36 MATERIALS SCIENCE↗

The effect of scandium addition on microstructure and mechanical properties of Al–Si–Mg alloy: A multi-refinement modifier

Effect of scandium (Sc) additions on the microstructure, mechanical properties and fracture behavior of Al–Si–Mg casting alloy (F357) were systematically investigated. It was found that Sc addition caused a multi-refining efficiency on the microstructure of as-cast F357 alloy, including refinement of grains and secondary dendrite arm spacing (SDAS), modification of eutectic Si and harmless disposal of β-Al{sub 5}FeSi phase. Subsequent T6 heat treatment had further induced the complete spheroidization of eutectic Si and precipitation of fine secondary Al{sub 3}Sc dispersoids in the Sc modified alloys. Thus the mechanical properties, especially the ductility, were significantly enhanced by the addition of Sc combined with the heat treatment. The highest ultimate tensile strength, yield strength and elongation were achieved in 0.8 wt.% Sc modified F357 alloy combined with T6 heat treatment. Furthermore, fractographic examinations indicated that the ductile fracture mechanism served as a dominate role in the modified alloys due to the formation of fine, deep and uniformly distributed dimples. - Highlights: • Detailed characterization of the multi-refining microstructure of Sc modified F357 alloy was performed. • The multi-refinement was proposed to refine grain and SDAS, modify eutectic Si and β-phase. • Sc modifier combined with T6 treatment is effective in improving tensile properties. • Modification of eutectic Si in F357 alloy with Sc is consistent with the IIT mechanism.

36 MATERIALS SCIENCE↗

Directional solidification of eutectic composites in space environment

The Ni-Ni3Ta eutectic and a nickel-base alloy containing 30 wt pct Ta were solidified unidirectionally in an electron beam floating zone melting apparatus. It was found that the volume fraction of the Ni3Ta phase in the Ni-Ni3Ta eutectic mixture was increased from 7.6 to 36 volume pct in agreement with the theory as predicted. Tensile properties of the randomly solidified and unidirectionally solidified Ni-Ni3Ta eutectic were determined as function of solidification rate and temperature. It was found that the ultimate tensile strength decreased as both the test temperature and solidification rate increased. An elongation of 40 pct was obtained for a nickelbase alloy containing 30 wt at room temperature. This unusually large elongation was attributed to the superplastic behavior of the alloy. The critical currents versus the external fields at 2.5, 3.0, 3.5 and 4.2 deg for the unidirectionally solidified Pb-Sn eutectic were measured. The values of critical fields at zero critical currents were obtained by extrapolation.

Yue, A. S.↗

Thermodynamic characteristics of praseodymium in the gallium–aluminum eutectic melt

The Ga–Al eutectic melt saturated with praseodymium was studied in the temperature range 572–1076 K by electromotive force (emf) method relative to the reference electrode (In{sub L} + PrIn{sub 3}, where L is the liquid phase) in a LiCl–KCl–CsCl eutectic electrolyte. The partial molar thermodynamic functions (enthalpy, entropy, and Gibbs energy) of praseo dymium in a Ga–Al eutectic melt were calculated. According to the emf measurements of the two-phase Pr–Ga–Al{sub L} + intermetallic compound alloys equilibrated with the Ga–Al eutectic melt saturated with praseodymium, there are intermetallic compounds PrGa{sub 6}, PrGa{sub 4}, and Pr{sub 0.22}Ga{sub 0.78}(PrGa{sub 2}) in the temperature ranges 572–741, 741–883, and 883–1076 K, respectively.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

A New Recycled Al–Si–Mg Alloy for Sustainable Structural Die Casting Applications

The use of secondary aluminum for structural components in the automotive industry is limited by the high Fe contents in recycled alloys which often result in the formation of brittle β-Al 5 FeSi phase which reduces the ductility of aluminum castings. In this study, a new secondary Al-Si-Mg alloy with high Fe content (about 0.44 wt.%) was developed for die casting applications. Based on thermodynamic modeling, manganese was added to obtain a designed Fe-to-Mn ratio of 2 which successfully suppressed the formation of β-Al 5 FeSi phase, by forming α-Al 15 (Fe,Mn) 3 Si 2 phase with rounded or hexagonal morphology. Additionally, a fine needle-like π-Al 8 FeMg 3 Si 2 phase was also formed within the eutectic regions. The new recycled alloy showed comparable mechanical properties in as-cast and heat treated (T5 and T6) conditions to three major primary die cast alloys (≤ 0.2 wt.% Fe) with similar composition. Ductility up to 7.4% from tensile elongation was achieved in as-cast recycled alloy due to the modification and refinement of α-Al 15 (Fe,Mn) 3 Si 2 by Mn and Sr additions. Tensile elongation was further improved to 9.1% after T6 treatment as a result of dissolution of π-Al 8 FeMg 3 Si 2 phase, defragmentation of α-Al 15 (Fe,Mn) 3 Si 2 and the spheroidization of Si phase. This new alloy provides a promising path for increasing usage of recycled aluminum with high Fe content in structural die castings for automotive and other applications.

36 MATERIALS SCIENCE↗

Effect of Friction Stir Processing on Microstructure and Tensile Properties of an Investment Cast Al-7Si-0.6Mg Alloy

Friction stir processing (FSP) is emerging as a promising tool for microstructural modification. The present study assesses the effects of FSP on the microstructure and mechanical properties of an investment cast Al-7Si-Mg alloy. FSP eliminates porosity and significantly refines eutectic Si particles. The extent of particle refinement varied with changes in processing conditions. High tool rotation rate and low to intermediate tool traverse speed generated a higher volume fraction of finer particles. Tensile ductility changed significantly as a result of FSP, whereas UTS improved only marginally. Yield strength was similar in both cast and FSPed samples under various heat treated conditions, with the highest value obtained after a T6 heat treatment. Further, FSP caused significant grain refinement in the stir zone, subsequently transforming into very coarse grains as abnormal grain growth (AGG) occurred during solution treatment at high temperature.

36 MATERIALS SCIENCE↗

Compatibility of Zircaloy-4 in eutectic PbSn and PbBiSn liquid metals

Here, a novel nuclear fuel concept has been proposed, consisting of UO₂ particles suspended in a liquid metal alloy. To evaluate its feasibility, the compatibility of Zircaloy-4 cladding with candidate eutectic PbSn and PbBiSn alloys—as well as with pure Pb, Bi, and Sn—was investigated through 1000-hour exposures at 400 °C and 600 °C. Severe degradation of the Zircaloy-4 specimens was observed in eutectic PbSn at 600 °C, whereas oxidation and oxygen diffusion were evident after exposure at 400 °C. At 600 °C, the formation of Zr₃Fe precipitates at the oxide–alloy interface was identified in specimens exposed to Pb and PbBiSn. Thermodynamic analysis suggested that the observed intermetallic formation resulted from the destabilization of Laves phases due to oxygen ingress at elevated temperatures.

Bismuth↗

Mechanical properties of Haynes Alloy 188 after exposure to LiF-22CaF2, air, and vacuum at 1093 K for periods up to 10,000 hours

As part of a program to provide reassurance that the cobalt-base superalloy Haynes Alloy 188 can adequately contain a LiF-CaF2 eutectic thermal energy storage salt, 4900- and 10,000-hr exposures of Haynes Alloy 188 to LiF-22CaF2, its vapor, vacuum, and air at 1093 K have been undertaken. Following such exposures, the microstructure has been characterized and the 77 to 1200 K tensile properties measured. In addition, 1050 K vacuum creep-rupture testing of as-received and molten salt- and vacuum-exposed samples has been undertaken. Although slight degradation of the mechanical properties of Haynes Alloy 188 due to prior exposure was observed, basically none of the losses could be ascribed to a particular environment. Hence, observed decreases in properties are due to thermal aging effects, not corrosive attack. In view of these findings, Haynes Alloy 188 is still deemed to be suitable for containment of the eutectic LiF-CaF2 thermal energy storage media.

Whittenberger, J. D.↗

A Novel Low-Activation VCrFeTa x W x (x = 0.1, 0.2, 0.3, 0.4, and 1) High-Entropy Alloys with Excellent Heat-Softening Resistance

The microstructure, Vickers hardness, and compressive properties of novel low-activation VCrFeTa x W x (x = 0.1, 0.2, 0.3, 0.4, and 1) high-entropy alloys (HEAs) were studied. The alloys were fabricated by vacuum-arc melting and the characteristics of these alloys were explored. The microstructures of all the alloys exhibited a typical morphology of dendritic and eutectic structures. The VCrFeTa 0.1 W 0.1 and VCrFeTa 0.2 W 0.2 alloys are essentially single phase, consisting of a disordered body-centered-cubic (BCC) phase, whereas the VCrFeTa 0.2 W 0.2 alloy contains fine, nanoscale precipitates distributed in the BCC matrix. The lattice parameters and compositions of the identified phases were investigated. The alloys have Vickers hardness values ranging from 546 HV0.2 to 1135 HV0.2 with the x ranging from 0.1 to 1, respectively. The VCrFeTa 0.1 W 0.1 and VCrFeTa 0.2 W 0.2 alloys exhibit compressive yield strengths of 1341 MPa and 1742 MPa, with compressive plastic strains of 42.2% and 35.7%, respectively. VCrFeTa 0.1 W 0.1 and VCrFeTa 0.2 W 0.2 alloys have excellent hardness after annealing for 25 h at 600–1000 °C, and presented compressive yield strength exceeding 1000 MPa with excellent heat-softening resistance at 600–800 °C. By applying the HEA criteria, Ta and W additions into the VCrFeTaW are proposed as a family of candidate materials for fusion reactors and high-temperature structural applications.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗