Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “CORROSION PRODUCTS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 433 records · Page 24

Chemical durability of glasses

The chemical durability of silicate glasses has long been studied for many applications, in particular when glasses are subjected to environmental weathering and aqueous corrosion. Typical applications include optical instruments, glass vessels, radioactive waste confinement, and bone reparation. Glass corrosion involves ion exchange, water diffusion, network dissolution-recondensation, and secondary phase precipitation. These reactions may impact, among other things, the release of contaminants from waste glasses, and the glass mechanical, optical and catalytic properties. The glass corrosion mechanisms and alteration product formation have been well studied as a function of many environmental parameters (temperature, pH, water composition, etc.). The present chapter describes the general phenomena behind glass corrosion and details glass dissolution in aqueous conditions on one hand and glass vapor hydration on the other hand. The latter phenomenon has not received the same level of attention in the literature relative to the corrosion in aqueous solutions. Research and Development needs, in particular in complex systems such as radioactive waste geological repositories, are discussed in the conclusion of the chapter.

Abdelouas, Abdesselam↗

Influence of Sodium Silicate/Sodium Alginate Additives on Discharge Performance of Mg–Air Battery Based on AZ61 Alloy

The application of Mg–air batteries is limited due to passivation and self-corrosion of anode alloys in electrolyte. In effort of solving this problem, the present work studied the influence of sodium silicate (SS)/sodium alginate (SA) on electrochemical behaviors of AZ61 alloy in NaCl solution by circle potentiodynamic polarization and galvanostatic discharge. The corrosion morphology and discharge product were examined by scanning electron microscopy (SEM) and x-ray diffraction (XRD). Results have shown that sodium silicate/sodium alginate inhibitors have an apparent effect on the self-corrosion of AZ61 alloy without affecting its discharge performance. The discharge capacity and the anodic utilization for Mg–air battery in a 0.6 M NaCl + 0.01 M SS +0.04 M SA solution are measured to be 1397 mAhg{sup −1} and 48.2%, respectively. Electrochemical impedance spectroscopy (EIS) and SEM investigation have confirmed that the sodium silicate/sodium alginate inhibitor can obviously decrease the self-corrosion of AZ61 alloy. SEM and XRD diffraction examinations suggest that the inhibiting mechanism is due to the formation of a compact and “cracked mud” layer. AZ61 alloy can be used as the anode for Mg–air battery in a solution of 0.6 M NaCl + 0.01 M SS +0.04 M SA.

36 MATERIALS SCIENCE↗

Aging of Iron Nanoparticles in Aqueous Solution: Effects on Structure and Reactivity

Aging (or longevity) is one of the most important and potentially limiting factors in the use of nano-Fe0 to reduce groundwater contaminants. We investigated the aging of FeH2 (Toda RNIP-10DS) in water with a focus on changes in (i) the composition and structure of the particles (by XPS, XRD, TEM, and bulk Fe0 content), and (ii) the reactivity of the particles (by carbon tetrachloride reaction kinetics and electrochemical corrosion potentials). Our results show that the FeH2 becomes more reactive between 0 and ~2 days aging, and then gradually loses reactivity over the next few hundred days. These changes in reactivity correlate with evidence for rapid destruction of the original Fe(III) oxide film on FeH2 during immersion and the subsequent formation of a new passivating mixed-valence Fe(II)-Fe(III) oxide shell. The behavior of “unaged” nano-Fe0 in the laboratory may be similar to that in field-scale applications for source-zone treatment due to the short reaction times involved. Long-term aged FeH2 acquires properties that are relatively stable over weeks or even months.

Environmental Molecular Sciences Laboratory↗

Aging of Iron Nanoparticles in Water: Effects on Structure and Reactivity

We studied the aging of Fe0-core/oxide-shell nanoparticles in water with a focus on changes in (i) the composition and structure of the particles (by XRD, TEM, XPS, and bulk Fe0 content), and (ii) the reactivity of the particles (by carbon tetrachloride reaction kinetics, electrochemical corrosion potentials, and H2 production rates). The results show that nano-Fe0 become more reactive between 0 and ~2 days exposure to water, and then gradually it loses reactivity over the next few hundred days. The behavior of unaged nano-Fe0 in our laboratory experiments may be similar to that in field-scale applications for source-zone treatment due to the short reaction times involved. However, nano-Fe0 that has been aged in water for >3 days acquires properties that are relatively stable over weeks or even months.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

AFIP-6 Breach Assessment Report

Analysis of the AFIP-6 experiment is summarized in this report in order to determine the cause of gaseous fission product release observed during irradiation. During the irradiation, a series of small fission product releases were observed. In order to limit the potential for primary coolant contamination, the operating cycle was terminated and the AFIP-6 experiment was removed for examination. Both in-canal and post-irradiation examination revealed the presence of an unusually thick oxide layer and discrete surface blisters on the fuel plates. These blisters were the likely cause of fission product release. Subsequent detailed thermal hydraulic analysis of the experiment indicated that the combination of the high operating power and test vehicle configuration led to high nominal operating temperatures for the fuel plates. This elevated temperature led to accelerated surface corrosion and eventually spallation of the fuel plate cladding. The thermal insulating nature of this corrosion layer led to significantly elevated fuel meat temperatures that induced blistering. Analysis was performed to validate a corrosion rate model and criteria for onset of spallation type surface corrosion were determined. The corrosion rate model will be used to estimate the oxide thickness anticipated for experiments in the future. The margin to the spallation threshold will then be used to project the experiment performance.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Multi–length scale characterization of point defects in thermally oxidized, proton irradiated iron oxides

A key for the success of safe nuclear power generation system is to consider structural materials that are economical, meet mechanical property needs, possess good corrosion resistance, and are radiation tolerant. Nevertheless, fundamental insights that elucidate the details of radiation damage on materials corrosion performance are lacking. This includes the behavior of surface oxides which often regulate corrosion. For example, it is unclear how non-equilibrium point defects, oxide structure, mass transport in oxides, and subsequent oxidation behavior are altered by the radiation. Here, in this work, some of the effects of proton irradiation on the attributes of point defects, iron oxide microstructures, and the physical nature of the oxidation product were correlated with corrosion behavior. Iron oxides, fabricated by thermal oxidation in air at 400°C and 800°C for 1 h, were subjected to 200 keV, 0.03 dpa (displacements per atom) of proton irradiation, and subjected to corrosion reactivity assessment using AC and DC electrochemical methods. Experimental methods that target materials information at different length scales, such as positron annihilation spectroscopy (atomistic), transmission electron microscopy (mesoscopic), and electrochemical methods (macroscopic), were coupled to shed light on the impact of radiation-induced defect modifications and structural changes in oxides on corrosion reactivity which ultimately affects durability in harsh environments.

36 MATERIALS SCIENCE↗

Glass ceramic development for the combined fission products streams

After immobilization, nuclear waste is stored for minimally hundreds of years. In waste-forms {beta}, {gamma}-radiation are main causes for damage. The objectives is to test radiation stability of PNNL synthesized glass-ceramics. Monitoring was done looking for changes in the microstructure or phase composition. These are designed for immobilization of: lanthanides, alkaline metals, alkaline arths, transition metals, high molybdenum content - 6.94%, and multi-phase glass-ceramic. The conclusion on aqueous stability is the PNNL glass ceramics - glass phase erodes but crystalline phases don't and it's more resistant to corrosion than vitrified waste. Leachability tests in accordance with standards will be performed and the results will be compared to XRD.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Pre-Demonstration Development of Controlled-Release Corrosion Inhibitors and Healing Agents as Alternatives to Hexavalent Chromium

This Limited Scope Study was directed to achieve the following objectives: (1) Scale-up of materials that can meet MIL-PRF-23377 (solvent-based primer). (2) Provide evidence of resistance to aircraft alkaline cleaners and de-icing fluids. (3) Provide formulation for initial ecological and toxicity screening. (4) Submit an interim report that will provide the basis for a future ESTCP (the Dept. of Defense's (DoD's) Environmental Security Technology Certification Program) demonstration effort.The encapsulation procedure for two corrosion inhibitors was scaled up from lab scale to 2.0 kilograms. This scale will accommodate high volume production of coatings with encapsulated corrosion inhibitors for large surface areas during a follow-on ESTCP demonstration effort. Test results provided evidence of resistance to alkaline cleaners and aircraft de-icing fluids and compliance with MIL-PRF-23377. All the MIL-PRF-23377 requirements were met with the exception of the adhesion requirement, in top coated panels, and the flexibility requirement. Work on solving these two problems will be done prior to validation and demonstration of the technology. An initial ecological and toxicity screening identified several factors that were not critical to the acceptance of the encapsulated corrosion inhibitor. This new technology will lead to environmentally friendly alternatives to hexavalent chromium that will enable DoD to protect its assets. Field demonstration, licensing, qualification, and commercialization will allow its real world utilization. Abstract for Appendix A. Toxicology Report: Corrosion controls a significant problem for military equipment. Many surface treatment materials currently in use on items of military or aerospace materiel contain chromium (VI) as a component, a source of significant human health and environmental hazard. The formulation under evaluation contains no chromium. Most of the proposed components are low to moderate toxicity and are not a significant concern. Two of the formulation components are associated with some cancer hazard - 2-mercaptobenzothiazole and formaldehyde, but both find widespread use in industry and additional investigation is not required for this project.

Calle, Luz Marina↗

Pre-demonstration Development of Controlled-Release Corrosion Inhibitors and Healing Agents as Alternatives to Hexavalent Chromium

This Limited Scope Study was directed to achieve the following objectives:(1) Scale-up of materials that can meet MIL-PRF-23377 (solvent-based primer).(2) Provide evidence of resistance to aircraft alkaline cleaners and deicing fluids.(3) Provide formulation for initial ecological and toxicity screening.(4) Submit an interim report that will provide the basis for a future ESTCP demonstration effort.The encapsulation procedure for two corrosion inhibitors was scaled up from lab scale to 2.0 kg. This scale will accommodate high volume production of coatings with encapsulated corrosion inhibitors for large surface areas during a follow on ESTCP demonstration effort.Test results provided evidence of resistance to alkaline cleaners and aircraft deicing fluids and compliance with MIL-PRF-23377. All the MIL-PRF-23377 requirements were met with the exception of the adhesion requirement, in top coated panels, and the flexibility requirement. Work on solving these two problems will be done prior to validation and demonstration of the technology. An initial ecological and toxicity screening identified several factors that were not critical to the acceptance of the encapsulated corrosion inhibitor. This new technology will lead to environmentally friendly alternatives to hexavalent chromium that will enable DoD to protect its assets. Field demonstration, licensing, qualification, and commercialization will allow its real world utilization.

Calle, L. M.↗

Pre-Demonstration Development of Controlled-Release Corrosion Inhibitors and Healing Agents as Alternatives to Hexavalent Chromium

This Limited Scope Study was directed to achieve the following objectives: (1) Scale-up of materials that can meet MIL-PRF-23377 (solvent-based primer). (2) Provide evidence of resistance to aircraft alkaline cleaners and deicing fluids. (3) Provide formulation for initial ecological and toxicity screening. (4) Submit an interim report that will provide the basis for a future ESTCP demonstration effort. The encapsulation procedure for two corrosion inhibitors was scaled up from lab scale to 2.0 kg. This scale will accommodate high volume production of coatings with encapsulated corrosion inhibitors for large surface areas during a follow on ESTCP demonstration effort. Test results provided evidence of resistance to alkaline cleaners and aircraft deicing fluids and compliance with MIL-PRF-23377. All the MIL-PRF-23377 requirements were met with the exception of the adhesion requirement, in top coated panels, and the flexibility requirement. Work on solving these two problems will be done prior to validation and demonstration of the technology. An initial ecological and toxicity screening identified several factors that were not critical to the acceptance of the encapsulated corrosion inhibitor. This new technology will lead to environmentally friendly alternatives to hexavalent chromium that will enable DoD to protect its assets. Field demonstration, licensing, qualification, and commercialization will allow its real world utilization.

Alternatives to Hexavalent Chromium↗

Pre-Demonstration Development of Controlled-Release Corrosion Inhibitors and Healing Agents as Alternatives to Hexavalent Chromium

This Limited Scope Study was directed to achieve the following objectives: (1) Scale-up of materials that can meet MIL-PRF-23377 (solvent-based primer). (2) Provide evidence of resistance to aircraft alkaline cleaners and deicing fluids. (3) Provide formulation for initial ecological and toxicity screening. (4) Submit an interim report that will provide the basis for a future ESTCP demonstration effort. The encapsulation procedure for two corrosion inhibitors was scaled up from lab scale to 2.0 kg. This scale will accommodate high volume production of coatings with encapsulated corrosion inhibitors for large surface areas during a follow on ESTCP demonstration effort. Test results provided evidence of resistance to alkaline cleaners and aircraft deicing fluids and compliance with MIL-PRF-23377. All the MIL-PRF-23377 requirements were met with the exception of the adhesion requirement, in top coated panels, and the flexibility requirement. Work on solving these two problems will be done prior to validation and demonstration of the technology. An initial ecological and toxicity screening identified several factors that were not critical to the acceptance of the encapsulated corrosion inhibitor. This new technology will lead to environmentally friendly alternatives to hexavalent chromium that will enable DoD to protect its assets. Field demonstration, licensing, qualification, and commercialization will allow its real world utilization.

Alternatives to Hexavalent Chromium, Controlled Re↗

Spent nuclear fuel recycling with plasma reduction and etching

A method of extracting uranium from spent nuclear fuel (SNF) particles is disclosed. Spent nuclear fuel (SNF) (containing oxides of uranium, oxides of fission products (FP) and oxides of transuranic (TRU) elements (including plutonium)) are subjected to a hydrogen plasma and a fluorine plasma. The hydrogen plasma reduces the uranium and plutonium oxides from their oxide state. The fluorine plasma etches the SNF metals to form UF 6 and PuF 4 . During subjection of the SNF particles to the fluorine plasma, the temperature is maintained in the range of 1200-2000 deg K to: a) allow any PuF 6 (gas) that is formed to decompose back to PuF 4 (solid), and b) to maintain stability of the UF 6 . Uranium (in the form of gaseous UF 6 ) is easily extracted and separated from the plutonium (in the form of solid PuF 4 ). The use of plasmas instead of high temperature reactors or flames mitigates the high temperature corrosive atmosphere and the production of PuF 6 (as a final product). Use of plasmas provide faster reaction rates, greater control over the individual electron and ion temperatures, and allow the use of CF 4 or NF 3 as the fluorine sources instead of F 2 or HF.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Some Expected Characteristics of Lunar Dust: A Geological View Applied to Engineering

Compared to the Earth the geologic nature of the lunar regolith is quite distinct. Even though similar minerals exist on the Earth and Moon, they may have very different properties due to the absence of chemical modification in the lunar environment. The engineering properties of the lunar regolith reflect aspects of the parent rock and the consequences of hypervelocity meteor bombardment. On scales relevant to machinery and chemical processing for In-Situ Resource Utilization, ISRU (such as water production), the lunar regolith compositional range is much more restricted than terrestrial material. This fact impacts predictions of properties required by design engineers for constructing equipment for lunar use. In this paper two examples will be covered. 1) Abrasion is related to hardness and hardness is a commonly measured property for both minerals and engineering materials. Although different hardness scales are routinely employed for minerals and engineering materials, a significant amount of literature is available relating the two. As one example, we will discuss how to relate hardness to abrasion for the design of lunar equipment. We also indicate how abundant the various mineral phases are and typical size distributions for lunar regolith which will impact abrasive nature. 2) Mineral characteristics that may seem trivial to the non-geologist or material scientist may have significant bearing on ISRU processing technologies. As a second example we discuss the impact of traces of F-, Cl-, and OH-, H2O, CO2, and sulfur species which can radically alter melting points and the corrosive nature of reaction products thereby significantly changing bulk chemistry and associated processing technologies. For many engineering uses, a simulant s fidelity to bulk lunar regolith chemistry may be insufficient. Therefore, simulant users need to engage in continuing dialogue with simulant developers and geoscientists.

Street, Kenneth W.↗

Some Expected Characteristics of Lunar Dust: A Geological View Applied to Engineering

Compared to the Earth the geologic nature of the lunar regolith is quite distinct. Even though similar minerals exist on the Earth and Moon, they may have very different properties due to the absence of chemical modification in the lunar environment. The engineering properties of the lunar regolith reflect aspects of the parent rock and the consequences of hypervelocity meteor bombardment. On scales relevant to machinery and chemical processing for In-Situ Resource Utilization, ISRU (such as water production), the lunar regolith compositional range is much more restricted than terrestrial material. This fact impacts predictions of properties required by design engineers for constructing equipment for lunar use. In this paper two examples will be covered. 1) Abrasion is related to hardness and hardness is a commonly measured property for both minerals and engineering materials. Although different hardness scales are routinely employed for minerals and engineering materials, a significant amount of literature is available relating the two. As one example, we will discuss how to relate hardness to abrasion for the design of lunar equipment. We also indicate how abundant the various mineral phases are and typical size distributions for lunar regolith which will impact abrasive nature. 2) Mineral characteristics that may seem trivial to the non-geologist or material scientist may have significant bearing on ISRU processing technologies. As a second example we discuss the impact of traces of fluoride, chloride, and hydroxide, water, carbon dioxide, and sulfur species which can radically alter melting points and the corrosive nature of reaction products thereby significantly changing bulk chemistry and associated processing technologies. For many engineering uses, a simulant's fidelity to bulk lunar regolith chemistry may be insufficient. Therefore, simulant users need to engage in continuing dialogue with simulant developers and geoscientists.

Street, Kenneth W.↗

Device-scale CFD study for mass transfer coefficient and effective mass transfer area in packed column

Carbon dioxide (CO 2 ) is a significant contributor of greenhouse gases emissions responsible for global warming. The fossil-fueled power plant is one of the major sources of CO 2 emission worldwide and needs to be mitigated. Post-combustion carbon capture by chemical absorption can be a promising technology to reduce CO 2 emission from power plants. The absorption is carried out via countercurrent flow in the packed columns. Although monoethanolamine (MEA) is a popular solvent, it has also limitations such as high volatility of solvent, corrosivity that leads to product degradation and damage to apparatuses, low CO 2 loading capacity, etc. Therefore, alternate solvents are being explored as prospective materials for carbon capture. A water-lean solvent, CO 2 binding organic liquids (CO2BOL), is currently being developed as a prospective material in carbon capture at the Pacific Northwest National Laboratory. Since the development of the material is at the primitive stage, it needs extensive investigation before industrial deployments. Hydrodynamics and mass transfer phenomena in the packed column using CO 2 BOL is unknown. Computational fluid dynamics (CFD) can be a useful tool to understand these phenomena in the packed column. Before employing the extensive CFD investigations, one needs to carefully validate CFD predictions for accurate flow predictions. This report demonstrates the validation of multiphase flow simulations against the experimental results for both structured and random packed columns. The reactive multiphase flow simulations using volume of fluid method were conducted at a wide range of liquid loads and contacts angles. The effective area is one of the critical factors dictating interphase mass transfer due to chemical reactions. Accordingly, CFD-predicted effective areas were compared with the experimental results of Tsai et al. [1] for Mellapak 250.Y structured packing. Both results matched well at different liquid loads in the presence of fast chemical kinetics using caustic solvents. Further, reactive multiphase flow simulations were also conducted in pall ring random packing to compute effective areas in the presence of fast chemical reactions. The CFD-predicted effective area compared well with correlation developed by Song et al. [2]. With successful validations, the current simulation framework can be further used for prediction of hydrodynamics and mass transfer phenomena using CO 2 BOL solvents in the packed column. Subsequently, it would be helpful in design optimization of a packed column. In addition to validation of the CFD model, this report also explains the mechanism for enhanced liquid side mass transfer for a structured packed column as compared to the wetted wall column.

20 FOSSIL-FUELED POWER PLANTS↗

Dust Emission at 8 and 24 μ m as Diagnostics of H ii Region Radiative Transfer

We use the Spitzer Surveying the Agents of Galaxy Evolution (SAGE) survey of the Magellanic Clouds to evaluate the relationship between the 8 μ m polycyclic aromatic hydrocarbon (PAH) emission, 24 μ m hot dust emission, and H ii region radiative transfer. We confirm that in the higher-metallicity Large Magellanic Cloud, PAH destruction is sensitive to optically thin conditions in the nebular Lyman continuum: objects identified as optically thin candidates based on nebular ionization structure show six times lower median 8 μ m surface brightness (0.18 mJy arcsec{sup −2}) than their optically thick counterparts (1.2 mJy arcsec{sup −2}). The 24 μ m surface brightness also shows a factor of three offset between the two classes of objects (0.13 versus 0.44 mJy arcsec{sup −2}, respectively), which is driven by the association between the very small dust grains and higher density gas found at higher nebular optical depths. In contrast, PAH and dust formation in the low-metallicity Small Magellanic Cloud is strongly inhibited such that we find no variation in either 8 μ m or 24 μ m emission between our optically thick and thin samples. This is attributable to extremely low PAH and dust production together with high, corrosive UV photon fluxes in this low-metallicity environment. The dust mass surface densities and gas-to-dust ratios determined from dust maps using Herschel HERITAGE survey data support this interpretation.

79 ASTRONOMY AND ASTROPHYSICS↗

Potential structural material problems in a hydrogen energy system

Potential structural material problems that may be encountered in the three components of a hydrogen energy system - production, transmission/storage, and utilization - were identified. Hydrogen embrittlement, corrosion, oxidation, and erosion may occur during the production of hydrogen. Hydrogen embrittlement is of major concern during both transmission and utilization of hydrogen. Specific materials research and development programs necessary to support a hydrogen energy system are described.

Gray, H. R.↗

Performance of Structural Alloys in Bio-oil Production, Upgrading, and Storage Systems

Selection of corrosion-resistant, cost-effective structural materials for the process and containment vessels required for the production, upgrading, and storage of biomass-derived oils has been the subject of study in our laboratory for many years. The wide variety of biomass resources and the many liquefaction techniques and processing conditions result in products with a broad range of properties and compositions. Here, this paper will address the materials issues in three distinct areas. In production, materials are exposed to temperatures that range from 350 to 550 °C depending upon the process. Generally, austenitic stainless steels have performed reasonably well, although thicker oxide scales and intergranular attack have sometimes been observed. For storage and transport of the bio-oil products, temperatures experienced by the containment materials are not expected to exceed 50 °C. Our studies have shown that most raw bio-oils contain significant concentrations of organic acids, and low-molecular-weight organic acids were quite corrosive to carbon and low alloy steels. For some applications, subsequent processing is required, which includes hydrotreating or co-processing with a petroleum-derived liquid. These processes utilize a catalyst that requires periodic retreatment with a sulfidizing gas, and the exposure to this gas at elevated temperatures can cause appreciable corrosion to the more common austenitic stainless steels. The materials considered most cost-effective and sufficiently corrosion-resistant for each of these environments were identified.

36 MATERIALS SCIENCE↗