Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Alloy”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 433 records · Page 24

High Ductility Aluminum Alloy made from Powder by Friction Extrusion

Shear processing has been used to consolidate and extrude aluminum alloy Al-12.4TM powder into bulk nanostructured rods. Extrudates exhibited 450 MPa ultimate tensile strength, 380 MPa yield strength, and 15.7% elongation at ambient temperature. Twice the elongation was achieved compared to conventional extrusion, with similar ultimate and yield strengths, and is attributed to reduction of the Al grain size and refinement and redistribution of nanoscale second phases. Quasicrystalline approximants within the starting powder were not observed in the extrudate, indicating shear processing was effective in solutionizing some fraction of the alloying elements and re-precipitating them as second phase nanoscale intermetallics.

Extrusion, Friction, Nanostructured Materials, Alu↗

Element redistributions during early stages of oxidation in a Ni38Cr22Fe20Mn10Co10 multi-principal element alloy

Element redistributions after initial gaseous oxidation of a Ni38Cr22Fe20Mn10Co10 (at%) multi-principle element alloy at 120°C and 300°C is captured via psuedo in situ atom probe tomography. All cations contribute to the oxide in both conditions, consisting of a Cr-rich inner oxide and Fe, Mn, Co and Ni-rich outer oxide. At the lower temperature, Ni tends to be trapped at the outer/inner oxide interface, while Ni enriches at the oxide/metal interface at higher temperature in tandem with Cr metal depletion. These observations confirm oxidation of complex alloys involves the formation of metastable, multi-layered oxide films, with a distinct tendency for solute trapping.

multi-principal element alloy, oxidation mechanism↗

Computational thermodynamics-guided alloy design and phase stability in CoCrFeMnNi-based medium-and high-entropy alloys: An experimental-theoretical study

A computational thermodynamics approach has been employed to design CoCrFeMnNi-based medium- and high-entropy alloys (M/HEAs) with systematically varied compositions (Co(( 80-X )/ 2 )Cr(( 80-X )/ 2 )Fe X Mn 10 Ni 10 with x = 30, 40, and 50 at.%) and phase stability. Since the formation of sigma phase, usually brittle and undesirable, is a common concern, when this class of alloys is subjected to elevated temperatures (600–1000 °C), predicting its formation becomes essential. Thus, its formation and the phase equilibria were studied using the CALPHAD method, and two empirical methods, namely, valence electron concentration (VEC) and paired sigma-forming element (PSFE). Isothermal aging treatments at 900–1100 °C for 20 h were performed, since CALPHAD and VEC/PSFE predictions diverged. Both prediction methods were compared with experimental characterization by a combination of scanning electron microscopy and high-energy synchrotron X-ray diffraction. In conclusion, the predictions from the VEC/PSFE and CALPHAD calculations (depending on the database used) were shown to be quite accurate.

36 MATERIALS SCIENCE↗

Stability of Surface and Subsurface Hydrogen on and in Au/Ni Near-Surface Alloys

Periodic, self-consistent DFT-GGA (PW91) calculations were used to study the interaction of hydrogen atoms with the (111) surfaces of substitutional near-surface alloys (NSAs) of Au and Ni with different surface layer compositions and different arrangements of Au atoms in the surface layer. The effect of hydrogen adsorption on the surface and in the first and second subsurface layers of the NSAs was studied. Increasing the Au content in the surface layer weakens hydrogen binding on the surface, but strengthens subsurface binding, suggesting that the distribution of surface and subsurface hydrogen will be different than that on pure Ni(111). While the metal composition of the surface layer has an effect on the binding energy of hydrogen on NSA surfaces, the local composition of the binding site has a stronger effect. For example, fcc hollow sites consisting of three Ni atoms bind H nearly as strongly as on Ni(111), and fcc sites consisting of three Au atoms bind H nearly as weakly as on Au(111). Sites with one or two Au atoms show intermediate binding energies. The preference of hydrogen for three-fold Ni hollow sites alters the relative stabilities of different surface metal atom arrangements, and may provide a driving force for adsorbate-induced surface rearrangement.

Environmental Molecular Sciences Laboratory↗

Selective butene formation in direct ethanol-to-C3+-olefin valorization over Zn-Y/Beta and single-atom alloy composite catalysts using in situ generated hydrogen

The selective production of C3+ olefins from renewable feedstocks, especially via C1 and C2 platform chemicals, is a critical challenge for obtaining economically viable low-carbon middle distillate transportation fuels (i.e., jet and diesel). Here, we report a multifunctional catalyst system composed of Zn-Y/Beta and “single-atom” alloy (SAA) Pt-Cu/Al2O3 which selectively catalyzes ethanol-to-olefins (C3+, ETO) valorization in the absence of cofed hydrogen, forming butenes as the primary olefin products. Beta zeolites containing predominately isolated Zn and Y metal sites catalyze ethanol upgrading steps (588 K, 3.1 kPa ethanol, ambient pressure) regardless of cofed hydrogen partial pressure (0-98.3 kPa H2), forming butadiene as the primary product (60% selectivity at 87% conversion). The Zn-Y/Beta catalyst possesses site-isolated Zn and Y Lewis acid sites (at ~7 wt% Y) and Brønsted acidic Y sites, the latter of which has been previously uncharacterized. A secondary bed of SAA Pt-Cu/Al2O3 selectively hydrogenates butadiene to butene isomers at a consistent reaction temperature using hydrogen generated in situ from ethanol-to-butadiene (ETB) conversion. This unique hydrogenation reactivity at near-stoichiometric hydrogen and butadiene partial pressures is not observed over monometallic Pt or Cu catalysts, highlighting these operating conditions as a critical SAA catalyst application area for conjugated diene selective hydrogenation at high reaction temperatures (>573 K) and low H2/diene ratios (e.g., 1:1). Single-bed steady state selective hydrogenation rates, associated apparent hydrogen and butadiene reaction orders, and DFT calculations of the Horiuti-Polanyi reaction mechanisms indicate that the unique butadiene selective hydrogenation reactivity over SAA Pt-Cu/Al2O3 reflects lower hydrogen scission barriers relative to monometallic Cu surfaces and limited butene binding energies relative to monometallic Pt surfaces. DFT calculations further indicate the preferential desorption of butene isomers over SAA Pt-Cu(111) and Cu(111) surfaces while Pt(111) surface favors subsequent butene hydrogenation reactions to form butane over butene desorption events. Under operating conditions without of hydrogen cofeeding, this combination of Zn-Y/Beta and SAA Pt-Cu catalysts can selectively form butenes (65% butenes, 78% C3+ selectivity at 94% conversion) and avoid butane formation using only in situ generated hydrogen, avoiding costly hydrogen cofeeding requirements that hinder many renewable energy processes.

Cordon, Michael↗

Dual Alloying Strategy to Achieve a High Thermoelectric Figure of Merit and Lattice Hardening in p-Type Nanostructured PbTe

The introduction of an alkaline earth metal telluride as a second phase in PbTe can lead to very high thermoelectric figure of merit, ZT, as a result of hierarchical structuring, e.g., in the PbTe-SrTe system. However, there are two roadblocks to this strategy: poor solubility and occurrence of incoherent nanoprecipitates in the PbTe matrix, e.g., the PbTe-BaTe system. Here we demonstrate a dual alloying approach by simultaneously alloying CaTe and BaTe in the p-type PbTe matrix to achieve ZT max ranging up to ~2.2 at high temperatures. Synergistic enhancement of the Seebeck coefficient via favorable band convergence gives rise to higher power factors up to 34 μW cm -1 K -2 and significant suppression of lattice thermal conductivity, κ L , down to ~0.6 W m -1 K -1 results from large multicenter phonon scattering. In addition, co-inclusion of Ca and Ba causes unanticipated lattice hardening in otherwise brittle PbTe, essential for practical device applications.

36 MATERIALS SCIENCE↗

Pressure-Induced Disordered Substitution Alloy in Sb[subscript 2]Te[subscript 3]

A new type of disordered substitution alloy of Sb and Te at above 15.1 GPa was discovered by performing in situ high-pressure angle-dispersive X-ray diffraction experiments on antimony telluride (Sb{sub 2}Te{sub 3}), a topological insulator and thermoelectric material, at room temperature. In this disordered substitution alloy, Sb{sub 2}Te{sub 3} crystallizes into a monoclinic structure with the space group C2/m, which is different from the corresponding high-pressure phase of the similar isostructural compound Bi{sub 2}Te{sub 3}. Above 19.8 GPa, Sb{sub 2}Te{sub 3} adopts a body-centered-cubic structure with the disordered atomic array in the crystal lattice. The in situ high-pressure experiments down to about 13 K show that Sb{sub 2}Te{sub 3} undergoes the same phase-transition sequence with increasing pressure at low temperature, with almost the same phase-transition pressures.

36 MATERIALS SCIENCE↗

All-Scale Hierarchically Structured p-Type PbSe Alloys with High Thermoelectric Performance Enabled by Improved Band Degeneracy

We show an example of hierarchically designing electronic bands of PbSe toward excellent thermoelectric performance. We find that alloying 15 mol % PbTe into PbSe causes a negligible change in the light and heavy valence band energy offsets (ΔE V ) of PbSe around room temperature; however, with rising temperature it makes ΔE V decrease at a significantly higher rate than in PbSe. In other words, the temperature-induced valence band convergence of PbSe is accelerated by alloying with PbTe. On this basis, applying 3 mol % Cd substitution on the Pb sites of PbSe 0.85 Te 0.15 decreases ΔE V and enhances the Seebeck coefficient at all temperatures. Here, excess Cd precipitates out as CdSe 1-y Te y , whose valence band aligns with that of the p-type Na-doped PbSe 0.85 Te 0.15 matrix. This enables facile charge transport across the matrix/precipitate interfaces and retains the high carrier mobilities. Meanwhile, compared to PbSe the lattice thermal conductivity of PbSe 0.85 Te 0.15 is significantly decreased to its amorphous limit of 0.5 W m -1 K -1 . Consequently, a highest peak ZT of 1.7 at 900 K and a record high average ZT of ~1 (400-900 K) for a PbSe-based system are achieved in the composition Pb 0.95 Na 0.02 Cd 0.03 Se 0.85 Te 0.15 , which are ~70% and ~50% higher than those of Pb 0.98 Na 0.02 Se control sample, respectively.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Correlation of the energy product with evolution of the nanostructure in Y,Dy,Nd-(Fe,Co)-B magnetic alloy

The devitrification behavior of nanocrystalline MRE{sub 2}(Fe,Co){sub 14}B+ZrC (MRE = Nd+Y+Dy) was studied using differential scanning calorimetry (DSC), synchrotron high temperature x-ray diffraction, and analytical transmission electron microscopy (TEM) techniques. Alloy ribbons were melt spun at 25 m/s to obtain an amorphous structure. Optimum hard magnetic properties (B{sub r} = 7.2 kG, H{sub c} = 12.7 kOe and (BH){sub max} = 10.8 MG Oe) were obtained in ribbons annealed at 750 C for 15 min. A reduced annealing temperature of 638 C and holding time from 0 to 11 min were chosen based on DSC analysis. Large changes in both microstructure and hard magnetic properties were found in a narrow window of annealing time, 4.5-6 min, resulting in a dramatic increase in energy product, remanence and coercivity: 0.96 MG Oe, 5.2 kG, 2.7 kOe to 5.7 MG Oe, 7.2 kG, 8.5 kOe for (BH){sub max}, B{sub r} and H{sub c}, respectively. Energy dispersive x-ray spectroscopy and energy filtered TEM analyses indicate that Zr- and C-rich particles ({approx} 5 nm) and thin grain boundary layers (1-2 nm thick) are formed surrounding 2-14-1 hard phase grains when the annealing time is over 6 min. Further annealing resulted in a more distinct hard phase surrounded by a nonmagnetic grain boundary phase {approx} 1 nm in thickness. The thin grain boundary layer phase starts to disappear with annealing time over 11 min. The partitioning behavior of various elements at different annealing conditions appears to be associated with significant changes in magnetic properties, leading to an improved optimum microstructure.

36 MATERIALS SCIENCE↗

Stress transfer during different deformation stages in a nano-precipitate-strengthened Ni-Ti shape memory alloy

Understanding the role of fine coherent precipitates in the micromechanical behavior of precipitate-strengthened shape memory alloys (SMAs), which still remains a mystery heretofore, is of crucial importance to the design of advanced SMAs with optimal functional and mechanical properties. Here, we investigate the lattice strain evolution of, and the stress partition between the nanoscale Ni{sub 4}Ti{sub 3} precipitates and the matrix in a precipitate-strengthened Ni-Ti SMA during different deformation stages by in-situ synchrotron high-energy X-ray diffraction technique. We found that, during R-phase reorientation and stress-induced martensitic transformation, which both involve the shear deformation process, the lattice strain of the nanoscale precipitates drastically increases by a magnitude of 0.5%, which corresponds to an abrupt increase of ∼520 MPa in internal stress. This indicates that stress repartition occurs and most of the stress is transferred to the precipitates during the shear deformation of the matrix. It is further revealed that the nanoscale precipitates which only have a low volume fraction bear a considerable amount of applied stress during all deformation stages investigated, implying that the nanoscale precipitates play an important role in the deformation behavior of the precipitate-strengthened Ni-Ti SMAs.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Identifying the dominant interstitial complex in dilute GaAsN alloys

Significant composition-dependent incorporation of N into non-substitutional sites is often reported for dilute GaAsN alloys. To distinguish (N-N){sub As}, (N-As){sub As}, and (As{sub Ga}-N{sub As}) complexes, we compare Rutherford backscattering spectrometry and nuclear reaction analysis (NRA) spectra with Monte Carlo-Molecular Dynamics simulations along the [100], [110], and [111] directions. For the Monte Carlo simulation, we assume that (N-N){sub As} is aligned along the [111] direction, while (N-As){sub As} is aligned along the [010] direction. The measured channeling NRA spectra exhibit the highest (lowest) yield in the [111] ([100]) directions. Similar trends are observed for simulations of (N-As){sub As}, suggesting that (N-As){sub As} is the dominant interstitial complex in dilute GaAsN.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Magnetism and electronic structure of CoFeCrX (X = Si, Ge) Heusler alloys

The structural, electronic, and magnetic properties of CoFeCrX (X = Si, Ge) Heusler alloys have been investigated. Experimentally, the alloys were synthesized in the cubic L2{sub 1} structure with small disorder. The cubic phase of CoFeCrSi was found to be highly stable against heat treatment, but CoFeCrGe disintegrated into other new compounds when the temperature reached 402 °C (675 K). Although the first-principle calculation predicted the possibility of tetragonal phase in CoFeCrGe, the tetragonal phase could not be stabilized experimentally. Both CoFeCrSi and CoFeCrGe compounds showed ferrimagnetic spin order at room temperature and have Curie temperatures (T{sub C}) significantly above room temperature. The measured T{sub C} for CoFeCrSi is 790 K but that of CoFeCrGe could not be measured due to its dissociation into new compounds at 675 K. The saturation magnetizations of CoFeCrSi and CoFeCrGe are 2.82 μ{sub B}/f.u. and 2.78 μ{sub B}/f.u., respectively, which are close to the theoretically predicted value of 3 μ{sub B}/f.u. for their half-metallic phases. The calculated band gaps for CoFeCrSi and CoFeCrGe are, respectively, 1 eV and 0.5 eV. These materials have potential for spintronic device applications, as they exhibit half-metallic electronic structures with large band gaps, and Curie temperatures significantly above room temperature.

36 MATERIALS SCIENCE↗

Shape Memory Alloys and their Applications in Power Generation and Refrigeration

The shape memory effect is closely related to the reversible martensitic phase transformation, which is diffusionless and involves shear deformation. The recoverable transformation between the two phases with different crystalline symmetry results in reversible changes in physical properties such as electrical conductivity, magnetization, and elasticity. Accompanying the transformation is a change of entropy. Fascinating applications are developed based on these changes. In this paper, the history, fundamentals and technical challenges of both thermoelastic and ferromagnetic shape memory alloys are briefly reviewed; applications related to energy conversion such as power generation and refrigeration as well as recent developments will be discussed.

energy generation↗