At least 433 records · Page 24

Probing Heterogeneous Degradation of Catalyst in PEM Fuel Cells under Realistic Automotive Conditions with Multi-Modal Techniques

The heterogeneity of polymer electrolyte fuel cell catalyst degradation is studied under varied relative humidity and types of feed gas. Accelerated stress tests (ASTs) are performed on four membrane electrode assemblies (MEAs) under wet and dry conditions in an air or nitrogen environment for 30 000 square voltage cycles. The largest electrochemically active area loss is observed for MEA under wet conditions in a nitrogen gas environment AST due to constant upper potential limit of 0.95 V and significant water content. The mean Pt particle size is larger for the ASTs under wet conditions compared to dry conditions, and the Pt particle size under land is generally larger than under the channel. Observations from ASTs in both conditions and gas environments indicate that water content promotes Pt particle size growth. ASTs under wet conditions and an air environment show the largest difference in Pt particle size growth for inlet versus outlet and channel versus land, which can be attributed to larger water content at outlet and under land compared to inlet and under channel. From X-ray fluorescence experiments Pt particle size increase is a local phenomenon as Pt loading remains relatively uniform across the MEA.

25 ENERGY STORAGE↗

A Three–Dimensional Nanoscale View of Electrocatalyst Degradation in Hydrogen Fuel Cells

The loss of platinum (Pt) electrochemically active surface area (ECSA) is a critical degradation mode that often becomes a limiting factor for heavy-duty proton exchange membrane fuel cell vehicles. High surface area carbon supports have been shown to improve Pt dispersion and limit detrimental ionomer-electrocatalyst interactions due to their large interior pore volume. Here, in this work, using automated scanning transmission electron tomography, the degradation of nanoparticles located on the interior versus exterior surfaces of the carbon support is compared following a catalyst-specific accelerated stress test (AST) of 90,000 voltage cycles between 0.6 V to 0.95 V. The results reveal a notable increase in median particle size for both interior and exterior Pt catalyst particles, with a slightly higher increase in particle size distribution and loss of specific surface area for the particles located on the exterior carbon surface. The fraction of Pt nanoparticles that reside within the interior of the carbon support also increased following the AST test, accompanied by evidence of an increase in average carbon mesopore size. Here, the results shed light on the degradation mechanisms affecting electrochemical properties and the enhanced particle accessibility at lower relative humidity.

08 HYDROGEN↗

Probing Electrode Transformation under Dynamic Operation for Alkaline Water Electrolysis

Alkaline water electrolyzers (AWEs) play a pivotal role in the realm of large-scale hydrogen production. However, AWEs face significant challenges in electrode degradation particularly under dynamic operating conditions, induced by reverse current phenomenon during frequent startup/shutdown. Herein, this study aims to rationalize the degradation mechanisms of AWEs under these conditions. A three-electrode membrane electrode assembly (MEA) setup is first utilized to decouple polarization behaviors of anode and cathode in AWEs. Following a proposed accelerated stress testing protocol, the setup allows for tracking individual electrode performance transformations during frequent reverse current operation. Integrating operando cell studies with in situ and post-mortem characterizations, it is showed that continuous formation of highly active species, nickel (oxy)hydroxides, improves the anode performance for oxygen evolution reaction. On the contrary, irreversible oxidation of nickel to β-nickel hydroxide results in a severe degradation of cathode, leading to material dissolution, poor electrical conductivity and loss of catalytic activity for hydrogen evolution reaction. These results provide insights in nickel-based electrode transformation mechanisms for alkaline water electrolysis and indicate that cathode with higher redox reversibility can potentially improve durability of AWEs under dynamic conditions.

08 HYDROGEN↗

Durability of Pt-Alloy Catalyst for Heavy-Duty Polymer Electrolyte Fuel Cell Applications under Realistic Conditions

As an emerging technology, polymer electrolyte fuel cells (PEFCs) powered by clean hydrogen can be a great source of renewable power generation with flexible utilization because of high gravimetric energy density of hydrogen. To be used in real-life applications, PEFCs need to maintain their performance for long-term use under a wide range of conditions. Therefore, it's important to understand the degradation of the PEFC under protocols that are closely related to the catalyst lifetime. Alloying Pt with transitional metal improves catalyst activity. It is also crucial to understand Pt alloys degradation mechanisms to improve their durability. To study durability of Pt alloys, accelerated stress tests (ASTs) are performed on Pt-Co catalyst supported on two types of carbon. Two different AST protocols were being studied: Membrane Electrolyte Assembly (MEA) AST based on the protocol introduced by the Million Mile Fuel Cell Truck consortium in 2023 and Catalyst AST, adopted from the U.S. Department of Energy (DoE).

25 ENERGY STORAGE↗

Effect of Commercial Gas Diffusion Layers on Catalyst Durability of Polymer Electrolyte Fuel Cells in Varied Cathode Gas Environment

Gas diffusion layers (GDLs) play a crucial role in heat transfer and water management of cathode catalyst layers in polymer electrolyte fuel cells (PEFCs). Thermal and water gradients can accelerate electrocatalyst degradation and therefore the selection of GDLs can have a major influence on PEFC durability. Currently, the role of GDLs in electrocatalyst degradation is poorly studied. Here, we perform electrocatalyst accelerated stress test studies on membrane electrode assemblies (MEAs) prepared using three most commonly used GDLs. The effect of GDLs on electrocatalyst degradation is evaluated in both nitrogen (non-reactive) and air (reactive) gas environments at 100% relative humidity. In situ electrochemical characterization and extensive physical characterization is performed to understand the subtle differences in electrocatalyst degradation and correlated to the use of different GDLs. Overall, no difference is observed in the electrocatalyst degradation due to GDLs based on polarization curves at the end of life. But interestingly, MEA with a cracked microporous layer (MPL) in the GDL exhibited a higher electrocatalyst loading loss, which resulted in a lower and more heterogeneous increase in the average electrocatalyst nanoparticle size.

25 ENERGY STORAGE↗

Degradation Science from Nanometers to Kilometers: A Pathway to Rapid Detection for Reliable Photovoltaics

Photovoltaics reliability for terrestrial applications has more than four decades of history and experience. International standards development has prevented many early life failures and must be continued in the future. Yet, as the module product development cycle is measured in mere months, additional investment in the fundamental degradation science and rapid detection should be developed. In this article, a brief strategy is provided addressing indoor accelerated, outdoor testing, and modeling efforts required to retain high reliability in the following decade.

14 SOLAR ENERGY↗

An extensible vector toolkit and parts library for advanced engineering of plant genomes

Abstract Plant biotechnology is rife with new advances in transformation and genome engineering techniques. A common requirement for delivery and coordinated expression in plant cells, however, places the design and assembly of transformation constructs at a crucial juncture as desired reagent suites grow more complex. Modular cloning principles have simplified some aspects of vector design, yet many important components remain unavailable or poorly adapted for rapid implementation in biotechnology research. Here, we describe a universal Golden Gate cloning toolkit for vector construction. The toolkit chassis is compatible with the widely accepted Phytobrick standard for genetic parts, and supports assembly of arbitrarily complex T‐DNAs through improved capacity, positional flexibility, and extensibility in comparison to extant kits. We also provision a substantial library of newly adapted Phytobricks, including regulatory elements for monocot and dicot gene expression, and coding sequences for genes of interest such as reporters, developmental regulators, and site‐specific recombinases. Finally, we use a series of dual‐luciferase assays to measure contributions to expression from promoters, terminators, and from cross‐cassette interactions attributable to enhancer elements in certain promoters. Taken together, these publicly available cloning resources can greatly accelerate the testing and deployment of new tools for plant engineering.

42 ENGINEERING↗

Stress relaxation cracking susceptibility evaluation in 347H stainless steel welds

Abstract Stress relaxation cracking (SRC) has been reported as a dominant failure mechanism for 347H stainless steel welds at elevated service temperatures, occurring in either the heat-affected zone (HAZ) or fusion zone (FZ). In this study, SRC susceptibility of physically simulated HAZ and cross-welded E347-347H stainless steel welds was studied using a four-step accelerated SRC test with a thermomechanical physical simulator. The stress and temperature range studied represents weld-induced residual stress at 150–600 MPa and post-weld heat treatment temperatures between 800 and 1050 °C. For all temperature conditions, the cross-welded samples failed at a lower critical stress threshold than the simulated HAZ. A finite element model of a 50.8-mm-thick single-V groove weld was used to generate the residual stress maps induced by a 40-pass welding procedure, which in combination with the experimental threshold stress map predicted potential SRC failure locations. Postmortem microstructural evaluations were performed to identify contributing characteristics to SRC. It was found that HAZ samples exhibited a combination of creep void development, secondary cracks with intergranular fracture near grain boundary carbides, and eutectic phases. FZ samples showed brittle fracture with cracks propagating along straight, non-tortuous interdendritic grain boundaries.

42 ENGINEERING↗

Operando carbon corrosion measurements in fuel cells using boron-doped carbon supports

Carbonaceous materials are the most common catalyst supports in proton exchange membrane fuel cell (PEMFCs), yet their corrosion is one of the limiting factors in achieving high durability. Herein, we doped carbon supports with boron (B) to increase the corrosion-resistance of the support. Two types of B-doped carbons were synthesized and studied as platinum support materials. Further, they varied in their morphologies, surface areas, and the types of boron species. The durability of Pt/B-doped carbon catalysts was investigated using the US-DOE catalysts’ supports accelerated stress test (AST) and a mass-spectrometer connected to the fuel cell effluent stream to quantify the mass of corroded carbon support in operando. The addition of boron to the carbon increased the stability of Pt catalysts in long-term usage of PEMFC. After 4000 AST cycles, more than 50% of initial current density was preserved for the boron-containing systems, while less than 30% of it remained with Vulcan carbon (Pt/V). Also, the Pt/B-doped carbon samples demonstrated better electrochemical active surface area (ECSA) stability when compared to Pt/V. Carbon loss measurements showed that B-doped carbons have higher resistance to electrochemical corrosion than unmodified carbon. Specifically, the substitutional boron-doped carbon demonstrated an extremely high stability and low corrosion rate.

25 ENERGY STORAGE↗

Highly durable fuel cell electrocatalyst with low-loading Pt-Co nanoparticles dispersed over single-atom Pt-Co-N-Graphene nanofiber

The limited durability of Pt electrocatalysis toward cathodic oxygen reduction reaction remains challenging, yet crucial for the development of Proton Exchange Membrane Fuel Cell. Here, we present a rational design of a robust catalyst consisting of PtCo nanoparticles supported on Pt-Co-N-graphene nanofiber prepared through electrospun Cobalt-Metal-Organic-Framework. The catalyst delivers unprecedented mass activity of 2.48 A·mgPt -1 , and retains 80% of initial value after 60,000 Accelerated-Stress-Test cycles. Operando X-ray absorption spectroscopies show that the electronic configurations of Pt sites in PtCo and Co sites in Co-N4 in the hybrid catalyst are modified toward high catalytic activities. Density Functional Theory unveils that the enhanced curvature of the substrate induced by the morphology engineering lowers the reaction thermodynamic barrier on Co-N4 sites, favoring the formation of H2O and suppressing that of H2O2. This result along with the strong affinity of PtCo nanoparticles to the Pt-Co-N-graphene fiber endows the catalyst an exceptional durability.

acidic electrolyte↗

Durability of PGM catalyst MEAs of polymer electrolyte membrane fuel cells for heavy-duty vehicles

Polymer electrolyte membrane fuel cells (PEMFCs) are promising power sources for heavy-duty vehicles (HDVs) owing to cleanliness and efficiency. However, the degradation of membrane electrode assemblies (MEAs) under HDV conditions remains a huge challenge. Here, this work investigated MEA durability under HDV conditions using a US Department of Energy standard accelerated stress test for 180,000 cycles (equivalent to 1 million miles of HDV operation). Effects of catalyst Pt content on MEA durability were examined using homemade 30% Pt/C (H-Pt/C) and commercial 46% Pt/C (C-Pt/C) catalysts. Both MEAs experienced H 2 /air and H 2 /O 2 performance loss over cycles. Analysis with scanning transmission electron microscopy, X-ray diffraction, inductively coupled plasma mass spectrometry, and mercury intrusion porosimetry revealed severe degradation of Pt nanoparticles (NPs), support structures, and the catalyst layer. Two degradation stages for NPs were proposed: Ostwald ripening dominated the initial 60,000 cycles, followed by combined Ostwald ripening and particle migration. Measurements with ion chromatography, high-frequency resistance, and oxygen-diffusion resistance revealed degradation of membrane and ionomer, respectively.

25 ENERGY STORAGE↗

Current research in low temperature proton exchange membrane-based electrolysis and a necessary shift in focus

While hydrogen has limited use in energy markets today, significant growth is possible in grid storage and as an energy carrier in other sectors. Along with lower electricity prices, further hydrogen cost reduction can enable electrochemical water splitting, particularly as the use of intermittent, renewable power sources increases and the quantity and duration of storage requirements limit electrical storage options. With the improved viability of large-scale hydrogen production, research in low temperature electrolysis has dramatically increased. The overwhelming majority of research efforts within proton exchange membrane-based systems has focused on catalyst development, although a smaller set have developed transport layers as well. As proton exchange membrane-based electrolysis shifts into higher technology readiness levels, however, there is a growing need for work optimizing materials integration, developing component-specific and device-level accelerated stress tests, and addressing manufacturing considerations. These areas directly impact electrolyzer performance, durability, and cost, and are critical to advancing hydrogen’s value and electrochemical water splitting.

08 HYDROGEN↗

Status and challenges for the application of platinum group metal-free catalysts in proton-exchange membrane fuel cells

Platinum group metal-free (PGM-free) electrocatalysts are an important class of materials for the sustainable energy economy and significant effort has been made towards developing PGM-free catalysts to replace their costly Pt counterparts in fuel cell electric vehicles. The progress made in activity over the last decade is reviewed, along with synthesis strategies for more controlled active site formation and performance gains achieved through electrode engineering. The increased focus on durability, the growing understanding of degradation mechanisms, and the need for standard performance and accelerated stress test protocols are discussed.

25 ENERGY STORAGE↗

Carbon nanotubes decorated with Pt as a viable electrocatalyst system using electrochemical atomic layer deposition

Surface limited redox replacement (SLRR) is an electrochemical deposition method designed to deposit metal thin films, typically onto other metals, that are mere monolayers in thickness, where such low dimensions allows catalyst-support interactions to affect catalyst efficiency. Here we explore the growth of Pt, using iterative Cu-mediated SLRR cycles, directly onto carbon nanotubes (CNTs) which are potentially good candidates as electrocatalyst supports due to their electrical conductivity and chemical resistance. Here scanning electron microscope images showed that Pt grew as nanoparticles, and hydrogen underpotential deposition from cyclic voltammetry showed that the active surface area approached an asymptotic value around eight iterations. Catalytic activity, measured using the oxygen reduction reaction, reached a maximum at ten iterations. Both are shown to be influenced by the growth mode, but electrochemical modeling indicates that the trend in activity is also due to a change in activation energy, possibly due to changes in Pt electronic structure due to interactions with the CNTs. Durability cycling showed a greater than 85% retention of surface area for the first 10,000 cycles of accelerated stress testing but decayed steadily to about 50% after 30,000 cycles. This performance may be related to the phenomenon that limits surface area growth.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Degradation and Modeling of Large-Format Commercial Lithium-Ion Cells as a Function of Chemistry, Design, and Aging Conditions

Demand for large-format (>10 Ah) lithium-ion batteries has increased substantially in recent years, due to the growth of both electric vehicle and stationary energy storage markets. The economics of these applications is sensitive to the lifetime of the batteries, and end-of-life can either be due to energy or power limitations. Despite this, there is little information from cell manufacturers on the sensitivity of cell degradation to environmental conditions or battery use. This work reports accelerated aging test data from four commercial large-format lithium-ion batteries from three manufacturers, with varying design (thickness, casings, ...), chemistry (lithium-iron-phosphate (LFP) or lithium-nickel-manganese-cobalt-oxide positive electrodes (NMC), with graphite (Gr) negative electrodes), and capacity (50 to 250 Amp hours). The tested LFP|Gr cell is found to be relatively insensitive to cycling conditions like temperature or voltage window, while NMC|Gr cells have varying sensitivity. Degradation trends are further investigated by training predictive models: simple polynomial trend lines, a semi-empirical reduced-order model, and an empirical reduced-order model identified using machine-learning based on symbolic regression. Calendar and cycle life are simulated over a variety of conditions to directly compare the various batteries. Cell size and thickness are found to substantially impact sensitivity to temperature during cycle aging, while electrode chemistry impacts depth-of-discharge sensitivity. Real-world battery lifetime is evaluated by simulating residential energy storage and commercial frequency containment reserve systems in several U.S. climate regions. Predicted lifetime across cell types varies from 7 years to 20+ years, though all cells are predicted to have at least 10 year life in certain conditions.

battery lifetime↗

Visualization, understanding, and mitigation of process-induced-membrane irregularities in gas diffusion electrode-based polymer electrolyte membrane fuel cells

Polymer electrolyte membrane fuel cells (PEMFC) show substantial promise for their application in electric vehicles. For large-scale manufacturing of PEMFCs, roll-to-roll coated gas-diffusion-electrodes (GDE) offer certain advantages over other production pathways. Procedures including hot pressing and coating an ionomer overlayer may be necessary for this manufacturing pathway to enable a suitable catalyst layer/membrane interface. The same procedures may potentially introduce membrane irregularities, especially when thin membranes are used. Limited understanding exists regarding if and to what extent such irregularities impact PEMFC performance and lifetime, and therefore be considered defects. In this study, NREL's customized fuel cell hardware that enables quasi in-situ infrared (IR) thermography studies was utilized to visualize spatial hydrogen crossover and identify membrane irregularities that originated from the GDE-based MEA fabrication process. The structure of these membrane irregularities was investigated by scanning electron microscopy (SEM) and its impact on initial H2/air performance was determined. Accelerated stress testing (AST) revealed that these irregularities develop into failure point locations. These results were validated across many MEAs with identified process-induced membrane irregularities. By selecting specific gas diffusion media properties and by fine tuning the MEA hot pressing parameters, the formation of such membrane irregularities was mitigated.

08 HYDROGEN↗

Nanochannel electrodes facilitating interfacial transport for PEM water electrolysis

Proton-exchange membrane water electrolyzers (PEMWEs) are a promising technology for green hydrogen production; however, interfacial transport behaviors are poorly understood, hindering device performance and longevity. Here, we first utilized finite-gap electrolyzer to demonstrate the possibility of proton transfer through water in PEMWEs. The measured high-frequency resistances (HFRs) exhibit a linear trend with increasing gap distance, where extrapolation shows a lower value compared with HFRs in regular zero-gap electrolyzers, indicating that ohmic resistance could be further reduced. We introduce nanochannels to facilitate mass transport, as evidenced by both liquid-fed and vapor-fed electrolysis. Nanochannel electrodes achieve a voltage reduction of 190 mV at 9 A·cm –2 compared with the Ir-PTEs without nanochannels. Furthermore, nanochannel electrodes show negligible degradation through 100,000 accelerated-stress tests and over 2,000 h of operation at 1.8 A·cm –2 with a decay rate of 11.66 μV·h –1 . These results provide new insights into localized transport dynamics for PEMWEs and highlight the significance of interfacial engineering for electrochemical devices.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Estimate long-term impact on battery degradation by considering electric vehicle real-world end-use factors

Many estimates of battery capacity degradation are based on accelerated lab tests that involve charge-discharge cycles or rely on data or electrochemical modeling. These methods are reasonable for technology benchmarking but rarely consider real-world end-use factors. To address this issue, this study develops the Battery Run-down under Electric Vehicle Operation (BREVO) model. It links the driver's travel pattern to physics-based battery degradation and powertrain energy consumption models. The model simulates the impacts of charging behavior, charging rate, driving patterns, and multiple energy management modules on battery capacity degradation. It finds that, over a 10-year timespan, firstly, for a random driver situated in the New England area, daily direct-current fast charging (60 kW) could lead to up to 22% less battery capacity when compared to daily Level-1 charging (1.8 kW). Second, the battery thermal management system can delay battery degradation by approximately 0.5% in the New England area. Third, warmer ambient temperatures enhance BEV battery usage. The model indicates that the battery capacity in the Los Angeles area is 6% higher than that in the New England area. The BREVO model provides crucial information for consumers and BEV manufacturers on range anxiety, BEV battery design, and decision support of battery warranty.

25 ENERGY STORAGE↗