Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “A. Microstructures”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 433 records · Page 24

Effects of transient thermal shock on the microstructures and corrosion properties of a reduced activation high-entropy alloy

The devices would subject transient thermal shocks (TTS) during operation under extremely harsh conditions of nuclear fusion reactors, which inevitably exert significant impact on the microstructure and performance of structural materials. Here, a reduced activation VCrFeTa 0.2 W 0.2 high-entropy alloy (HEA) was developed by vacuum arc melting. The effects of electron beam induced TTS on its microstructure, microhardness, and corrosion properties were investigated. The results indicate that the weight fraction of each phase changes after TTS, showing a significant decrease in the content of BCC1 phase and an increase in the content of BCC2 and Laves phases. The content of BCC1 phase continues to decrease slightly with increasing the power of TTS. Besides, the microhardness of the alloy increases from ~673 HV to ~714 HV after TTS treatments. In the reduced activation HEA, TTS results in a relatively low corrosion current density of ~0.472 μA/cm 2 in 3.5 wt% NaCl solution, around one-third of the current density observed in the as-cast sample. Furthermore, the VCrFeTa 0.2 W 0.2 HEA after TTS exhibits a pitting potential of ~1.165 V SCE , which is much higher than that of the as-cast sample. The refined composite multiscale entropy method is employed to analyze the influence of TTS on current fluctuation behavior during the corrosion process. The reduced activation VCrFeTa 0.2 W 0.2 HEA exhibits excellent properties in harsh environments after TTS, thereby showing advantageous property in the field of nuclear structural materials. Furthermore, TTS is an efficient and controllable strategy for the improvement of the HEAs’ microstructures and performances.

36 MATERIALS SCIENCE↗

Graded microstructure and mechanical properties of spark plasma sintered Fe-Cr alloys

Developing graded microstructure and mechanical properties is critical for accelerating the design and optimization of structural materials for a wide range of applications. Here, in this study, Fe-Cr alloys were fabricated by spark plasma sintering (SPS) technique. The microstructure, microhardness, and tensile properties of the as-fabricated and thermally annealed variants were investigated. Graded grain structures were created in the as-fabricated cylinders along both axial and radial directions. Grain size was gradually reduced from the sample periphery to the center. Microhardness measurements reveal a gradual decrease of hardness towards the periphery of the samples. The as-fabricated Fe-Cr alloys show a desired combination of tensile strength and elongation, primarily due to the formation of a high density of oxides, voids, dislocations, and grain boundaries. After in-situ thermal annealing at 600 °C under 60 MPa for 2 h using SPS, the Fe-Cr alloys underwent minimal grain growth, and the graded grain structures were retained. The hardness was more uniformly distributed in the annealed variants, and the tensile strength was reduced with an increase in the total elongation, which is attributed to the dissolution of nano-sized oxide particles and the relief of the residual stress. This study demonstrates that SPS coupled with subsequent heat treatment can tailor the graded microstructure and control the mechanical properties of Fe-Cr alloys, showing potential applications in other alloy systems.

36 MATERIALS SCIENCE↗

GrainGNN: A dynamic graph neural network for predicting 3D grain microstructure

We propose GrainGNN, a surrogate model for the evolution of polycrystalline grain structure under rapid solidification conditions in metal additive manufacturing. High fidelity simulations of solidification microstructures are typically performed using multicomponent partial differential equations (PDEs) with moving interfaces. The inherent randomness of the PDE initial conditions (grain seeds) necessitates ensemble simulations to predict microstructure statistics, e.g., grain size, aspect ratio, and crystallographic orientation. Here, currently such ensemble simulations are prohibitively expensive and surrogates are necessary.In GrainGNN, we use a dynamic graph to represent interface motion and topological changes due to grain coarsening. We use a reduced representation of the microstructure using hand-crafted features; we combine pattern finding and altering graph algorithms with two neural networks, a classifier (for topological changes) and a regressor (for interface motion). Both networks have an encoder-decoder architecture; the encoder has a multi-layer transformer long-short-term-memory architecture; the decoder is a single layer perceptron.We evaluate GrainGNN by comparing it to high-fidelity phase field simulations for in-distribution and out-of-distribution grain configurations for solidification under laser power bed fusion conditions. GrainGNN results in 80%–90% pointwise accuracy; and nearly identical distributions of scalar quantities of interest (QoI) between phase field and GrainGNN simulations compared using Kolmogorov-Smirnov test. GrainGNN's inference speedup (PyTorch on single x86 CPU) over a high-fidelity phase field simulation (CUDA on a single NVIDIA A100 GPU) is 150×–2000× for 100-initial grain problem. Further, using GrainGNN, we model the formation of 11,600 grains in 220 seconds on a single CPU core.

36 MATERIALS SCIENCE↗

Microstructure and fracture toughness characterization of three 9Cr ODS EUROFER steels with different thermo-mechanical treatments

Ferritic martensitic ODS steels are one of the candidate structural materials for future Gen-IV nuclear fission and fusion reactors. Here, the dependence of fracture toughness on microstructure was investigated by comparing three 9Cr ODS EUROFER steels manufactured through different thermo-mechanical processing routes. Quasi-static fracture toughness testing was performed with sub-sized C(T) specimens and microstructural characterization was carried out using scanning electron microscopy, electron backscatter diffraction, and transmission electron microscopy. It was found that at lower test temperatures (-100 – 22 °C), the fracture toughness was primarily controlled by crack initiation at sub-micron particles and by production of secondary cracks during fracture. At higher temperatures (above 100 °C), fracture toughness was predominantly controlled by the matrix ductility and the grain boundary strength with a relatively ductile coarse-grained alloy demonstrating higher fracture toughness compared to high-strength fine-grained alloys. These results and discussion show that variations in thermomechanical treatments can produce significant differences in microstructure and fracture toughness behavior of ferritic martensitic ODS steels.

36 MATERIALS SCIENCE↗

In situ monitoring of microstructure evolution during thermal processing of uranium-zirconium alloys using laser-generated ultrasound

In this study, laser-generated ultrasound was used to monitor microstructure evolution during thermal processing of as-cast, polycrystalline binary uranium-zirconium metallic fuel alloys with compositions of U-20wt.%Zr (U-20Zr), U-50wt.%Zr (U-50Zr) and U-80wt.%Zr (U-80Zr). Ultrasonic waveforms were recorded during heating and cooling the samples from room temperature to >973 K and back. A phase transition temperature for all three compositions was estimated from the temperature at which an abrupt and rapid reduction in ultrasonic velocities was observed. Microstructural features on the length scale of tens of micrometers were inferred from the observation of scattering of ultrasonic waves by elastic heterogeneities above ~823 K in U-20Zr, while a hysteresis in the ultrasonic velocities of U-80Zr upon cooling was attributed to a partial retention of the high temperature phase following thermal annealing. The U-50Zr alloy exhibited a reversible viscoelastic response above 933 K, as evidenced by the observation of high frequency attenuation of the shear component of the waveforms at high temperature. Ultrasonic measurements were supplemented by in situ transmission electron microscopy (TEM). The TEM images revealed that the δ-U-Zr matrix in the three compositions underwent a spinodal decomposition above ~823 K into nanoscale regions. The ultrasonic measurements revealed larger, micron-scale structure evolution in the U-20Zr alloy at the same temperature. This large-scale structure is associated with heterogeneous regions having different Zr content. Our findings show the potential heating rate dependence of microstructural evolution in U-Zr alloys and highlight differences in the thermomechanical response and associated length scales during thermal annealing between single- and dual-phase compositions. These results demonstrate the utility of laser ultrasonics to rapidly and efficiently scan phase boundaries and monitor micrometer-scale structure evolution in metallic fuel alloys.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Uranium nitride (UN) pellets with controllable microstructure and phase – fabrication by spark plasma sintering and their thermal-mechanical and oxidation properties

Dense uranium mononitride (UN) pellets with controlled microstructures and tailored grain size from large-grained to a few microns are synthesized by spark plasma sintering (SPS) combined with high energy ball milling. The impacts of the sintering conditions on fuel microstructure, grain size, physical density, and phase behavior are systematically investigated, and the thermal-mechanical properties and oxidation behavior of the SPS densified UN pellets are characterized. Higher sintering temperatures and longer ball milling durations and thus finer starting UN powders promote sintering and densification, and dense UN pellets above 95% theoretical density can be achieved by SPS at 1873 K for 10 min. UN phase purity is maintained in the SPS-densified pellets sintered at a lower temperature and short duration. A phase heterogeneity with secondary UO 2 or uranium sesquinitride (U 2 N 3 ) occurs for the UN pellets sintered at higher temperatures using finer UN powders. The hardness and fracture toughness of the SPS-densified UN pellets increase with smaller grain sizes and higher densities to 7.9 GPa and 3.5 MPa m 1/2 , respectively. Furthermore, both small (1–2 μm) and large grain-sized (30–50 µm) UN pellets exhibit good thermal conductivity. Dynamic oxidation testing by a thermogravimetric analyzer in air shows that the onset temperature for oxidation varies with microstructure and phase heterogeneity of the SPS densified UN pellets. Particularly, the smaller-grained (micron-sized) UN pellets containing uranium oxides and U 2 N 3 display lower weight gain and significantly-reduced oxidation kinetics, and full oxidation completes at a temperature above 1173 K when tested with a ramp rate of 10 K/min.

36 MATERIALS SCIENCE↗

The effects of Ti content and quenching on phase transformations, microstructures, and mechanical properties in uranium-titanium alloys

In this work, the effect of Ti content on phase transformations, microstructures, and mechanical properties of U-Ti alloys are described for alloys containing 0.3 wt.% to 2.0 wt.%Ti. Rapid cooling is required to overcome diffusional decomposition of γ-phase and facilitate diffusionless transformation to supersaturated variants of α-phase. Critical cooling rate increases with increasing Ti content, opposite to the trend observed in U-Mo and U-Nb alloys. This difference occurs because the martensite transformation temperatures in these relatively dilute U-Ti alloys are above the knee of the C-curve for diffusional decomposition, unlike those in the more concentrated U-Mo and U-Nb alloys. In these U-Ti alloys critical cooling rate depends on the amount of undercooling required to reach M s , which increases with increasing Ti content, and the time for diffusional decomposition to occur just above M s , which decreases with increasing Ti content. The net result is that higher cooling rates are required as Ti content increases. Full quenching results in diffusionless transformation of γ-phase to supersaturated variants of α-phase. Very dilute alloys transform via a γ → β → α m sequence of massive transformations. Martensitic γ → α' a transformation begins at ~0.4%Ti, and 100% α' a microstructures are obtained from ~0.65% to ~1.4% Ti. A transition to banded α'b martensite occurs at ~1.5%Ti. Evidence suggests that the α' a to α' b transition may occur when the cubic γ-phase first transforms to tetragonal γ°, which in turn transforms to orthorhombic α' b via the sequence γ → γ° → α' b . Fully quenched alloys exhibit moderate strengths and ductilities, and their supersaturation with Ti makes them amenable to subsequent age hardening. Subcritical quenching typically results in two-phase microstructures with lower ductilities and near-zero Ti-supersaturation, eliminating the possibility of subsequent age hardening.

36 MATERIALS SCIENCE↗

Microstructural and compositional evolutions in $γ$-LiAlO 2 pellets during ion irradiation at an elevated temperature

This study reports on the microstructural, phasic and compositional evolutions of γ-LiAlO 2 during ion irradiation. Polycrystalline γ-LiAlO 2 pellets were irradiated sequentially with He + and D 2 + ions to the same combined fluences of up to 3 × 10 17 (He + +D + )/cm 2 at 773 K. The irradiated pellets were characterized using scanning transmission electron microscopy and atom probe tomography. Surface amorphization likely due to radiolysis and planar defects as a possible precursor for formation of precipitates are created at 5 × 10 16 (He + +D + )/cm 2 , followed by the formation of nano-sized precipitates and fractures at higher doses. Spinel-like precipitates of non-stoichiometric LiAl 5 O 8 and gas-filled cavities are observed to grow with increasing dose. Faceted precipitates and rounded cavities appear at 2 × 10 17 (He + +D + )/cm 2 . With further increasing ion fluence to 3 × 10 17 (He + +D + )/cm 2 , amorphization of the precipitates takes place and micron-sized fractures appear. Surface exfoliation could occur at an extremely high ion fluence. There are compositional changes in the γ-LiAlO 2 pellets during the microstructural evolution. In the precipitate and amorphized regions, Li concentrations decrease to ~7 and 3.7 at.% from 25 at.% in γ-LiAlO 2 , respectively. This study reveals a full-cycle microstructural evolution with corresponding compositional changes in γ-LiAlO 2 pellets during ion irradiation at 773 K. In conclusion, the data could help model, assess, and predict the material performance during neutron irradiation in reactors.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Gas tungsten arc welding and post weld heat treatment effects on microstructure and mechanical property of castable nanostructured alloy steel

Here, this paper details the first study of castable nanostructured alloy (CNA) steel gas tungsten arc weldability and the post-weld heat treatment (PWHT) effects. Effects of welding heat input, thermal cycles, and PWHT on microstructures, microhardness distributions, room temperature tensile properties, and fracture characteristics are discussed. Results show that CNA steel exhibits excellent weldability (i.e., no indication of welding defects and reasonable tensile properties). The welded joint exhibited heterogeneous microstructures with δ-ferrite as well as large microhardness variation and fluctuation. The welded joint yield and ultimate tensile strengths were similar to those of the base metal, but the elongations decreased by 30 %. However, with normalization and tempering PWHT, the δ-ferrite was eliminated, microstructure was modified, hardness was unified, and joint ductility was restored. The study indicated that the CNA reduced-activation ferritic-martensitic steel owns excellent weldability, and PWHT is needed for the industrial application of welded structures.

36 MATERIALS SCIENCE↗

Microstructural and material property changes in severely deformed Eurofer-97

Severe plastic deformation changes the microstructure and properties of steels, which may be favourable for their use in structural components of nuclear reactors. In this study, high-pressure torsion (HPT) was used to refine the grain structure of Eurofer-97, a ferritic/martensitic steel. Electron microscopy and X-ray diffraction were used to characterise the microstructural changes. Following HPT at room temperature to a maximum shear strain of 230, the average grain size reduced by a factor of ~30, with a marked increase in high-angle grain boundaries. Dislocation density also increased by more than one order of magnitude. The thermal stability of the deformed material was investigated via in-situ annealing during synchrotron X-ray diffraction. This revealed substantial recovery between 450 K – 800 K. Irradiation with 20 MeV Fe-ions to ~0.1 dpa caused a 20% reduction in dislocation density compared to the as-deformed material. However, HPT deformation prior to irradiation only had a minor effect in mitigating the irradiation-induced reductions in thermal diffusivity and surface acoustic wave velocity of the material. Microstructural and material property changes are dominated by deformation compared to irradiation. In light of this, the benefits of using HPT to improve the irradiation resistance of Eurofer-97 are limited. These results provide a multi-faceted view of the changes in ferritic/martensitic steels due to severe plastic deformation, and how these changes can be used to alter material properties.

ion-irradiation↗

Influence of high-strain-rate compression and subsequent heat treatment on (TiNbZr) 89 (AlTa) 11 refractory high-entropy alloys: Dynamic-mechanical behavior and microstructural changes

This study explored the dynamic-mechanical behavior of a novel low-density (TiNbZr) 89 (AlTa) 11 refractory high-entropy alloy (RHEA) across strain rates ranging from 1.0×10 3 to 3.5×10 3 s –1 . A significant increase in the yield and ultimate compressive strengths with rising strain rates up to 3.0×10 3 s –1 was observed and attributed to enhanced dislocation activities and stress-induced microstructural transformations. The formation of the B2 phase and Zr 5 Al 3 precipitates was found to be crucial in bolstering the alloy strength at high strain rates. Beyond strain rates of 3.0×10 3 s –1 , a decrease in strength occurred due to thermal softening and strain localization. Microstructural analyses at 3.5×10 3 s –1 revealed grain refinement, the development of micro shear bands, and dislocation tangles, which were indicative of dynamic recrystallization. Besides, the findings also revealed that the post-dynamic compression heat treatment further enhanced the hardness and microstructural stability of the alloy. These results highlight the potential of the (TiNbZr) 89 (AlTa) 11 RHEA for applications requiring materials with high strength-to-weight ratios, particularly in dynamically loaded environments. It is expected that the results of this study will further advance our fundamental understanding of the behavior of RHEAs under extreme conditions, thereby opening new avenues for material innovation.

36 MATERIALS SCIENCE↗

Microstructure effects on fatigue crack growth in additively manufactured Ti–6Al–4V

In this article we investigate the relationship between the different microstructural features in additively-manufactured (AM) Direct Metal Laser Deposited Ti–6Al–4V alloys and the observed fatigue and fracture behaviors, using high resolution Digital Image Correlation experiments and microstructural imaging. Fatigue cracks in the AM specimens were observed to periodically propagate parallel to the α' laths and deflect at prior β grain boundaries. Corresponding plastic strain distributions show needle-like regions of high strain that correlated to the α' laths, suggesting significant influence of the microstructure on the plastic zone. In many cases, the fatigue cracks also propagated towards voids from unsintered powder or gas entrapment in the vicinity. In several experiments, premature failure of the AM specimens occurred under monotonic fracture or cyclic fatigue loading, which we attribute to the presence of void clusters located near the crack-tip. These fatigue and fracture characteristics were similar for AM specimens of different build-orientations.

36 MATERIALS SCIENCE↗

Evolution of microstructure and strength of a high entropy alloy undergoing the strain-induced martensitic transformation

In a recent work, we have reported outstanding strength and work hardening exhibited by a metastable high entropy alloy (HEA), Fe 42 Mn 28 Co 10 Cr 15 Si 5 (in at. %), undergoing the strain-induced martensitic transformation from metastable gamma austenite (γ) to stable epsilon martensite (ε). However, the alloy exhibited poor ductility, which was attributed to the presence of the brittle sigma (σ) phase in its microstructure. The present work reports the evolution of microstructure, strength, and ductility of a similar HEA, Fe 38.5 Mn 20 Co 20 Cr 15 Si 5 Cu 1.5 (in at. %), designed to suppress the formation of σ phase. A cast and then rolled plate of the alloy was processed into four conditions by annealing for 10 and 30 min at 1100 °C and by friction stir processing (FSP) at tool rotation rates of 150 and 400 revolutions per minute (RPM) to facilitate detailed examinations of variable initial grain structures. Neutron diffraction and electron microscopy were employed to characterize the microstructure and texture evolution. The initial materials had variable grain size but nearly 100% γ structure. Diffusionless strain induced γ→ε phase transformation took place under compression with higher rate initially and slower rate at the later stages of deformation, independent on the initial grain size. The transformation facilitated part of plastic strain accommodation and rapid strain hardening owing to a transformation-induced dynamic Hall-Petch-type barrier effect, increase in dislocation density, and texture. Here, the peak strength of nearly 2 GPa was achieved under compression using the structure created by double pass FSP (150 RPM followed by 150 RPM). Remarkably, the tensile elongation exhibited by the alloy was nearly 20% with fracture surfaces featuring a combination of ductile dimples and cleavage.

36 MATERIALS SCIENCE↗

Effects of rejuvenation modes on the microstructures and mechanical properties of metallic glasses

This study systematically investigates the effects of three rejuvenation modes, namely biaxial loading, thermal pressure loading, and cryogenic thermal cycling, on the microstructures and mechanical properties of Cu 64 Zr 36 metallic glasses (MGs) using molecular dynamics (MD) simulations. The simulation results demonstrate that biaxial tension application during loading results in a rejuvenated glassy state with high strength. Specifically, we find that the yield stress, Young's modulus, and shear modulus of the rejuvenated glass obtained by biaxial tensile loading decreased by 2.8%, 2.1%, and 2.7%, respectively, compared to an as-cast MG reference. We also find that MGs achieve the greatest degree of rejuvenation, at the expense of strength, with the use of thermal pressure loading. Interestingly, the application of cryogenic thermal cycling results in a rejuvenated state with a lower strength drop compared to thermal pressure loading. Furthermore, analysis of the potential energy and medium-range-order (MRO) size indicates that the microstructures of MGs achieves a high-energy ordered glass state after thermal pressure loading, but a high-energy disordered glass state after biaxial tensile loading and cryogenic thermal cycling. Furthermore, these findings provide meaningful insights into the effect of rejuvenation modes on the microstructures and mechanical properties of MGs, as well as useful guidelines for designing MGs with high strength and superior plasticity for prospective applications in industry.

36 MATERIALS SCIENCE↗

Process and feedstock driven microstructure for laser powder bed fusion of 316L stainless steel

Here in the pursuit of improving additively manufactured (AM) component quality and reliability, fine-tuning critical process parameters such as laser power and scan speed is a great first step toward limiting defect formation and optimizing the microstructure. However, the synergistic effects between these process parameters, layer thickness, and feedstock attributes (e.g. powder size distribution) on part characteristics such as microstructure, density, hardness, and surface roughness are not as well-studied. In this work, we investigate 316L stainless steel density cubes built via laser powder bed fusion (L-PBF), emphasizing the significant microstructural changes that occur due to altering the volumetric energy density (VED) via laser power, scan speed, and layer thickness changes, coupled with different starting powder size distributions. This study demonstrates that there is not one ideal process set and powder size distribution for each machine. Instead, there are several combinations or feedstock/process parameter ‘recipes’ to achieve similar goals. This study also establishes that for equivalent VEDs, changing powder size can significantly alter part density, GND density, and hardness. Through proper parameter and feedstock control, part attributes such as density, grain size, texture, dislocation density, hardness, and surface roughness can be customized, thereby creating multiple high-performance regions in the AM process space.

316L stainless steel↗

Microstructural evolution and phase stability in Nb-containing interstitial Fe-Mn-Co-Cr-C high-entropy alloys: An in-situ synchrotron X-ray diffraction study during laser melting

The influence of Nb on phase stability and microstructural evolution in an interstitial Fe-Mn-Co-Cr-C high-entropy alloy was investigated using in-situ synchrotron X-ray diffraction (SXRD) during laser melting. Scheil-Gulliver simulations predict the formation of σ and γ-f.c.c. phases in all three alloys, along with NbC in Nb-containing compositions. SXRD confirmed the presence of most predicted phases, but the σ phase was absent. Nb promotes crystallite refinement and increases dislocation density, though excessive additions reduce refinement efficiency due to solubility limits and secondary phase formation. Furthermore, Nb addition also enhances ε-h.c.p. phase formation by reducing stacking fault energy through NbC-induced carbon depletion. Analysis of intensity peak evolution reveals that Nb alters preferred grain orientations, reducing {111} γ intensity while enhancing {220} γ , leading to a more isotropic grain distribution. Overall, Nb plays a key role in phase selection, microstructure refinement, and preferred orientation evolution, allowing the tailored microstructure of high-entropy alloys via rapid solidification.

Interstitial high entropy alloys↗

Laser-interference pulse number dependence of surface chemistry and sub-surface microstructure of AA2024-T3 alloy

The laser-based treatment of a metal surface is an intrinsically non-chemical technique that can alter both the topology and chemistry of surfaces. A laser-based treatment for coating and joining applications can offer alternative surface preparations to the chemically-based surface preparation techniques, which are subject to severe environmental protection and hazardous-waste management considerations. In this study, the surface chemistry and sub-surface microstructural changes are investigated for a novel surface processing method using laser interferometry produced by two beams of a pulsed Nd:YAG laser. The two-beam laser-interference allowed the structuring of the surface at length scales much less than that of the laser beam spot. Surface chemistry changes in the oxide layer of AA 2024-T3 aluminum alloy rolled sheet due to laser processing were investigated using x-ray photoelectron spectroscopy (XPS). Near surface microstructural changes have been investigated with scanning electron microscopy and energy dispersive x-ray spectroscopy (SEM/EDS), and scanning transmission electron microscopy (STEM) as a function of number of interfering laser shots. SEM microstructure pictures of the top surface shows the minimization of surface defects, as all of the sharp features from a rolled sheet surface were smoothed by laser-structuring. STEM images indicate that the laser-interference processing reduced the formation of CuMn-rich precipitates over a 500–800 nm depth from the top surface. XPS data indicated that the Al oxide layer is modified compared to that of the baseline specimen and that the oxide thickness increases with the number of shots per spot. Finally, the additional thicker oxide on Al alloys is expected to increase the corrosion resistance of the coated Al 2024.

36 MATERIALS SCIENCE↗

Effect of CMAS viscosity on the infiltration depth in thermal barrier coatings of different microstructures

Calcium magnesium aluminum silicate (CMAS) is one of the leading concerns for the gas turbine industry. The effects of CMAS viscosity and the coating microstructure on CMAS infiltration depth were explored by conducting a time dependent interaction study. Three CMAS compositions were used from literature, and their viscosities predicted through FactSage viscosity module were drastically different. The interaction was carried out on three different TBCs synthesized using the solution precursor plasma spray process (SPPS): two of the TBCs were made of yttrium aluminum garnet (YAG) having different microstructures that promote different modes of CMAS infiltration, and one TBC was made of gadolinium zirconate (GZO). All samples had stress relieving vertical cracks and different intensities of horizontally banded porosity, (inter pass boundaries IPBs). A concentration of 100 mg/cm 2 of CMAS was applied on the TBCs which were then subjected to a 5-minute interaction at 1300 °C. Samples were analyzed using scanning electron microscopy (SEM), electron dispersive X-ray spectroscopy (EDXS), and transmission electron microscopy (TEM). Low viscosity CMAS readily penetrated the TBCs while more viscous CMAS showed less penetration. The depth of CMAS infiltration depended on the coating microstructure. In the YAG with IPBs, the CMAS spread horizontally in the IPBs before infiltrating deeper, resulting in reduced infiltration depth compared to other samples in spite of having wider vertical cracks. TEM and EDXS analysis were performed to investigate the phases present in the CMAS-TBC interaction region in YAG. Two regions were chosen, the top TBC surface in direct contact with the sea of CMAS, and the region at the CMAS penetration ended within the coating. Finally, the results showed that no secondary phases like apatite were observed in YAG, thus it can be concluded that the arrest of CMAS happened solely because of CMAS viscosity and the short infiltration time.