Evaluation of present-day thermal barrier coatings for industrial/utility applications

Atmospheric burner rig tests have been conducted to evaluate the corrosion resistance of present-day thermal barrier coatings. The coatings are primarily plasma-sprayed and zirconia-based. Both duplex and graded coating systems were tested at a gas temperature of 2100 F and metal temperatures that range from 1475 F to 1650 F. The fuels ranged from clean GT No. 2 to that doped with impurity levels which simulate water-washed residual fuels. Results to date suggest that liquid sulfate condensates play an important role in the coating degradation mechanisms, whereas the role of vanadium and its salts is less clear.

Bratton, R. J.↗

Effect of thermal cycling on ZrO2-Y2O3 thermal barrier coatings

The paper studies the comparative life of plasma-sprayed ZrO2-Y2O3 thermal barrier coatings on NiCrAlY bond coats on Rene 41 in short (4 min) and long (57 min) thermal cycles at 1040 C in a 0.3-Mach flame. Attention is given to determining the effect of short- and long-duration cycles on ZrO2-Y2O3 coatings, the cause of any cycle frequency effects, and methods to improve tolerance to thermal stress. Short cycles greatly reduced the life of the ceramic coating in terms of time at temperatures as compared to longer cycles, the failed coating indicating compressive failure. The experiments and stress calculations show that repeatedly subjecting a ceramic coating to high rates of initial heating has a more destructive influence on the coating than sustained operation at temperature. The effect of such thermal compressive stresses might be minimized through coating deposition and thickness control and by turbine cycle measurement to keep starting heating rates below critical values.

Mcdonald, G.↗

Covering solid, film cooled surfaces with a duplex thermal barrier coating

Thermal barrier coating systems were applied to hardware having passageways in the walls connecting apertures in the surface to a gas supply for film cooling. An inert gas, such as argon, is discharged through the apertures during the application of the thermal barrier coating system by plasma spraying. This flow of inert gas reduces both blocking of the holes and base metal oxidation during the coating operation.

Liebert, C. H.↗

Electro-Active Polymer (EAP) Actuators for Planetary Applications

NASA is seeking to reduce the mass, size, consumed power, and cost of the instrumentation used in its future missions. An important element of many instruments and devices is the actuation mechanism and electroactive polymers (EAP) are offering an effective alternative to current actuators. In this study, two families of EAP materials were investigated, including bending ionomers and longitudinal electrostatically driven elastomers. These materials were demonstrated to effectively actuate manipulation devices and their performance is being enhanced in this on-going study. The recent observations are reported in this paper, include the operation of the bending-EAP at conditions that exceed the harsh environment on Mars, and identify the obstacles that its properties and characteristics are posing to using them as actuators. Analysis of the electrical characteristics of the ionomer EAP showed that it is a current driven material rather than voltage driven and the conductivity distribution on the surface of the material greatly influences the bending performance. An accurate equivalent circuit modeling of the ionomer EAP performance is essential for the design of effective drive electronics. The ionomer main limitations are the fact that it needs to be moist continuously and the process of electrolysis that takes place during activation. An effective coating technique using a sprayed polymer was developed extending its operation in air from a few minutes to about four months. The coating technique effectively forms the equivalent of a skin to protect the moisture content of the ionomer. In parallel to the development of the bending EAP, the development of computer control of actuated longitudinal EAP has been pursued. An EAP driven miniature robotic arm was constructed and it is controlled by a MATLAB code to drop and lift the arm and close and open EAP fingers of a 4-finger gripper. Keywords: Miniature Robotics, Electroactive Polymers, Electroactive Actuators, EAP Materials

Bar-Cohen, Y.↗

Key Durability Issues with Mullite-Based Environmental Barrier Coatings for Si-Based Ceramics

Plasma-sprayed mullite (3Al2O3.2SiO2) and mullite/yttria-stabilized-zirconia (YSZ) dual layer coatings have been developed to protect silicon -based ceramics from environmental attack. Mullite-based coating systems show excellent durability in air. However, in combustion environments, corrosive species such as molten salt or water vapor penetrate through cracks in the coating and attack the Si-based ceramics along the interface. Thus the modification of the coating system for enhanced crack-resistance is necessary for long-term durability in combustion environments. Other key durability issues include interfacial contamination and coating/substrate bonding. Interfacial contamination leads to enhanced oxidation and interfacial pore formation, while a weak coating/substrate bonding leads to rapid attack of the interface by corrosive species, both of which can cause a premature failure of the coating. Interfacial contamination can be minimized by limiting impurities in coating and substrate materials. The interface may be modified to improve the coating/substrate bond.

Lee, Kang N.↗

New black paint for cryogenic infrared applications

A black paint has been developed and tested for cryogenic applications involving wavelengths beyond 10 microns. The paint has been used extensively for liquid helium cooled applications in a variety of instruments operating between 10 and 120 microns. The material is applied by brush over a spray or brush applied primer coat. A final covering is applied by either brush or spray. The composition and preparation of the paint are described, as are data about its outgassing properties. Infrared reflection and scattering data obtained by other groups which compare this material to other commercially available surface preparations are presented.

Houck, J. R.↗

Improved Metallography Of Thermal-Barrier Coatings

New technique for preparation of metallographic samples makes interpretation of images of pores and microcracks more reliable. Involves use of vacuum epoxy infiltration and interference-film coating to reduce uncertainty. Developed for inspection of plasma-sprayed ceramic thermal-barrier coatings on metals but applicable to other porous, translucent materials, including many important ceramics.

Brindley, William J.↗

Effect of aluminum phosphate additions on composition of three-component plasma-sprayed solid lubricant

Image analysis (IA) and electron microprobe X-ray analysis (EMXA) were used to characterize a plasma-sprayed, self-lubricating coating, NASA LUBE PS106, specified by weight percent as 35NiCr-35Ag-30CaF2. To minimize segregation of the powder mixture during the plasma-spraying procedure, monoaluminum phosphate was added to form agglomerate particles. Three concentrations of AlPO4 were added to the mixtures: 1.25, 2.5, and 6.25 percent by weight. Analysis showed that 1.25 wt% AlPO4 yielded a CaF2 deficiency, 2.5 wt% kept the coating closest to specification, and 6.25 wt% yielded excess CaF2 as well as more impurities and voids and a deficiency in silver. Photomicrographs and X-ray maps are presented. The methods of IA and EMXA complement each other, and the reasonable agreement in the results increases the confidence in determining the coating composition.

Jacobson, T. P.↗

Thermal barrier coating life prediction model development

This program focuses on predicting the lives of two types of strain-tolerant and oxidation-resistant thermal barrier coating (TBC) systems that are produced by commercial coating suppliers to the gas turbine industry. The plasma-sprayed TBC system is composed of a low pressure, plasma sprayed applied, oxidation resistant NiCrAlY bond coating. The other system is an air plasma sprayed yttria (8 percent) partially stabilized zirconia insulative layer.

Strangman, T. E.↗

Effect of thermal cycling on ZrO2-Y2O3 thermal barrier coatings

A study was made of the comparative life of plasma sprayed ZrO2-Y2O3 thermal barrier coatings on NiCrAlY bond coats on Rene 41 in short (4 min) and long (57 min) thermal cycles to 1040 C in a 0.3 Mach flame. Short cycles greatly reduced the life of the ceramic coating in terms of time at temperature as compared to longer cycles. Appearance of the failed coating indicated compressive failure. Failure occurred at the bond coat-ceramic coat junction. At heating rates greater than 550 kw/sq m, the calculated coating detachment stress was in the range of literature values of coating adhesive/cohesive strength. Methods are discussed for decreasing the effect of high heating rate by avoiding compressive stress.

Mcdonald, G.↗

Rugged Preheaters For Vacuum Plasma Spraying

Electric preheater units built to ensure large workpieces to be coated with metals by vacuum plasma spraying heated uniformly to requisite high temperatures by time plasma torch arrives. Units similar to electrical-resistance ribbon heaters in toasters and in some small portable electric "space" heaters. Nichrome resistance-heating ribbons wrapped around ceramic insulating spools on rings and on plates. Round workpiece placed in middle of ring preheater. Plate preheaters stacked as needed near workpiece.

Woodford, William H.↗

A sputtered zirconia primer for improved thermal shock resistance of plasma-sprayed ceramic turbine seals

It is shown that the application of sputtered Y2O3-stabilized ZrO2 (YSZ) primer in plasma-sprayed YSZ ceramic-coated turbine blades results in an improvement, by a factor of 5-6, in the thermal shock life of specimens with a sprayed, porous, Ni-Cr-Al-Y intermediate layer. Species with and without the primer were found to be able to survive 1000 cycles when the intermediate layer was used, but reduced laminar cracking was observed in the specimen with the primer. It is suggested that the sputtered YZS primer-induced properties are due to (1) more effective wetting and adherence of the plasma-sprayed YZS particles to the primer, and (2) the primer's retardation of impinging, molten plasma sprayed particles solidification rates, which result in a less detrimental residual stress distribution.

Bill, R. C.↗

Thermal barrier coating life prediction model development

The objective of this program is to develop an integrated life prediction model accounting for all potential life-limiting Thermal Barrier Coating (TBC) degradation and failure modes including spallation resulting from cyclic thermal stress, oxidative degradation, hot corrosion, erosion, and foreign object damage (FOD). The mechanisms and relative importance of the various degradation and failure modes will be determined, and the methodology to predict predominant mode failure life in turbine airfoil application will be developed and verified. An empirically based correlative model relating coating life to parametrically expressed driving forces such as temperature and stress will be employed. The two-layer TBC system being investigated, designated PWA264, currently is in commercial aircraft revenue service. It consists of an inner low pressure chamber plasma-sprayed NiCoCrAlY metallic bond coat underlayer (4 to 6 mils) and an outer air plasma-sprayed 7 w/o Y2O3-ZrO2 (8 to 12 mils) ceramic top layer.

Demasi, J.↗

Degradation mechanisms of ceramic thermal barrier coatings in corrosive environments

Chemical as well as thermal-mechanical interactions between the ceramics and gas turbine combustion gases/condensates are found to play critical roles in the degradation of porous plasma-sprayed ceramic thermal barrier coatings. The detailed degradation mechanisms of several state-of-the-art ceramic thermal barrier coatings, including several zirconia compositions and a calcium silicate, in corrosive environments are examined in this paper. Approaches to extend coating lifetime are also described.

Lau, S. K.↗

Thermal barrier coating system

An oxide thermal barrier coating comprises ZrO3-Yb2O3 that is plasma sprayed onto a previously applied bond coating. The zirconia is partially stabilized with about 124 w/o ytterbia to insure cubic, monoclinic, and terragonal phases.

Stecura, S.↗

Oxidation behavior of a thermal barrier coating

Thermal barrier coatings, consisting of a plasma sprayed calcium silicate ceramic layer and a CoCrAlY or NiCrAlY bond coat, were applied on B-1900 coupons and cycled hourly in air in a rapid-response furnace to maximum temperatures of 1030, 1100, or 1160 C. Eight specimens were tested for each of the six conditions of bond-coat composition and temperature. Specimens were removed from test at the onset of failure, which was taken to be the formation of a fine surface crack visible at 10X magnification. Specimens were weighed periodically, and plots of weight gain vs time indicate that weight is gained at a parabolic rate after an initial period where weight was gained at a much greater rate. The high initial oxidation rate is thought to arise from the initially high surface area in the porous bond coat. Specimen life (time to first crack) was found to be a strong function of temperature. However, while test lives varied greatly with time, the weight gain at the time of specimen failure was quite insensitive to temperature. This indicates that there is a critical weight gain at which the coating fails when subjected to this test.

Miller, R. A.↗

Quality control of the tribological coating PS212

PS212 is a self-lubricating, composite coating that is applied by the plasma spray process. It is a functional lubricating coating from 25 C (or lower) to 900 C. The coating is prepared from a blend of three different powders with very dissimilar properties. Therefore, the final chemical composition and lubricating effectiveness of the coatings are very sensitive to the process variables used in their preparation. Defined here are the relevant variables. The process and analytical procedures that will result in satisfactory tribological coatings are discussed.

Sliney, Harold E.↗