Adiabatic Shear Localization and Microstructure in Ultrafine Grained Aluminum Alloy at Cryogenic Temperature

Adiabatic shear localization plays an important role in the deformation and failure of ultrafine grained 6061 aluminum alloy processed by friction stir processing. To understand the effects of temperature and strain on adiabatic shear localization in the ultrafine grained 6061 aluminum alloy, it has been investigated dynamic mechanical behavior of ultrafine grained 6061 aluminum alloy under the controlled shock loading experiments. Deformation characteristics and microstructures in the shear band were performed by optical microscopy and transmission electron microscopy. The shear band in the ultrafine grained aluminum alloy is a long and straight band distinguished from the matrix. The width of the shear band decreases with increasing nominal strain. The results show that the grains in the boundary of the shear band are highly elongated along the shear direction and form the elongated cell structures (0.2 μ in width), and the core of the shear band consists of a number of recrystallized equiaxed grains 0.2-0.3 μ in diameters and the second phases distribute in both the boundary and the inner of the equiaxed new grains. The calculated temperature in the shear band is about 692 K. Rotational dynamic recrystallization mechanism is responsible for the formation of the microstructure in the shear band.

36 MATERIALS SCIENCE↗

In Situ Apparatus to Study Gas–Metal Reactions and Wettability at High Temperatures for Hot-Dip Galvanizing Applications

The understanding of gas–metal reactions and related surface wettability at high temperatures is often limited due to the lack of in situ surface characterization. Ex situ transfers at low temperature between annealing furnace, wettability device, and analytical tools induce noticeable changes of surface composition distinct from the reality of the phenomena.Therefore, a high temperature wettability device was designed in order to allow in situ sample surface characterization by x-rays photoelectron spectroscopy after gas/metal and liquid metal/solid metal surface reactions. Such airless characterization rules out any contamination and oxidation of surfaces and reveals their real composition after heat treatment and chemical reaction. The device consists of two connected reactors, respectively, dedicated to annealing treatments and wettability measurements. Heat treatments are performed in an infrared lamp furnace in a well-controlled atmosphere conditions designed to reproduce gas–metal reactions occurring during the industrial recrystallization annealing of steels. Wetting experiments are carried out in dispensed drop configuration with the precise control of the deposited droplets kinetic energies. The spreading of drops is followed by a high-speed CCD video camera at 500-2000 frames/s in order to reach information at very low contact time. First trials have started to simulate phenomena occurring during recrystallization annealing and hot-dip galvanizing on polished pure Fe and FeAl8 wt.% samples. The results demonstrate real surface chemistry of steel samples after annealing when they are put in contact with liquid zinc alloy bath during hot-dip galvanizing. The wetting results are compared to literature data and coupled with the characterization of interfacial layers by FEG-Auger. It is fair to conclude that the results show the real interest of such in situ experimental setup for interfacial chemistry studies.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Characterization of Friction-Stir-Welded Dual-Phase Brass

Friction stir welding (FSW) is an ideal process to join brass to avoid the evaporation of zinc. In the present investigation, 6-mm-thick dual-phase brass plates were joined efficiently using FSW at various tool rotational speeds. The microstructures were studied using optical microscopy, electron backscattered diffraction and transmission electron microscopy. The optical micrographs revealed the evolution of various zones across the joint line. The microstructure of the heat-affected zone was similar to that of base metal. The weld zone exhibited finer grains due to dynamic recrystallization. The recrystallization was inhomogeneous and the inhomogeneity reduced with increased tool rotational speed. The dual phase was preserved in the weld zone due to the retention of zinc. The severe plastic deformation created a lot of dislocations in the weld zone. The weld zone was strengthened after welding. The role of tool rotational speed on the joint strength is further reported.

36 MATERIALS SCIENCE↗

Annealing Effects on Microstructure and Mechanical Properties of Ultrafine-Grained Al Composites Reinforced with Nano-Al{sub 2}O{sub 3} by Rotary Swaging

Microstructure evolution and variations in mechanical properties of Al-Al{sub 2}O{sub 3} nanocomposite produced by powder metallurgy were investigated and compared with commercially pure aluminum (Al-1050) after furnace annealing. Fine gas-atomized Al powder compacts were first sintered in flowing nitrogen, subsequently consolidated into wires by rotary swaging and eventually annealed at 300 and 500 °C for 24 h each. Scanning and transmission electron microscopy with energy-dispersive spectroscopy was utilized to document the microstructure evolution. Rotary swaging was proven to lead to a marked decrease in grain size. After heavy swaging to true deformation degree of φ = 6 and annealing at 500 °C, obvious recrystallization was observed at Al-1050’s existing grain boundaries and the crystals began to grow perpendicular to the flow direction. In the Al-Al{sub 2}O{sub 3} nanocomposite, fabricated from d{sub 50} = 6 μm Al powder, recrystallization partially occurred, while grains were still extremely fine. Due to the dual role of fine-grained Al{sub 2}O{sub 3} dispersion strengthening, the nanocomposite showed improved mechanical performance in terms of tensile strength, approximately twice higher than Al-1050 after annealing at 500 °C.

36 MATERIALS SCIENCE↗

Phase-Field Modeling of Nugget Zone for a AZ31-Mg-Alloy Friction Stir Weld

This work presents simulation of microstructure evolution in the nugget zone (NZ) of a AZ31-Mg-alloy friction stir weld. The process parameters (tool geometrical characteristics, rotational speed, travel speed, applied load) have been correlated with the resulting microstructural features in the NZ of the weld (grain size and population) with the aid of the MICRESS software, which provides the ability to simulate both nucleation and grain growth during dynamic recrystallization phenomena evolving in the NZ during the weld thermal cycle. The input parameters of the developed model include the tool geometry, the welding conditions as well as the recrystallization energy, the grain boundary mobility and specific material properties. NZ microstructure obtained by simulation shows good agreement with experimental measurements for both grain population and size.

36 MATERIALS SCIENCE↗

Optimization of Hot Deformation Parameters and Constitutive Analysis for As-Cast Mg-5Li-3Zn-0.3Y Alloy Using Processing Maps

Hot deformation behavior of as-cast Mg-5Li-3Zn-0.3Y (wt.%) alloy has been studied by establishing processing maps covering the range of 200-450 °C in temperature and 0.001-10 s{sup −1} in strain rate. The map corresponding to the strain of 0.7 reveals that a domain of dynamic recrystallization occurred at 340-400 °C/0.01-0.158 s{sup −1} with its peak efficiency of approximately 31%. Analysis of the flow behaviors and microstructural observations indicated that dynamic recrystallization occurred in the domain, in which fine microstructure can be achieved. The above conditions represent the optimum processing parameters, and the flow instability regimes are also recognized from the maps. The average deformation in the deformed range was 136.414 kJ/mol which is close to that for lattice self-diffusion in magnesium and far smaller than that for as-cast Mg-5.75Zn-0.73Y-0.36Zr (wt.%) alloy. It is believed that a lower activation energy for Mg-5Li-3Zn-0.3Y alloy can partly result from both the weak particle pinning effects and adding Li into the Mg-Zn-Y-Zr alloy. Results of extrusion experiments conducted at 350 °C show that the alloy can be easily extruded with good mechanical properties of the yield strength of 132 MPa, the fracture strength of 215 MPa and the elongation of 20.9%, and the grains can be well refined.

36 MATERIALS SCIENCE↗

Effect of Heat Treatment and Combination of Cold Rolling and Heat Treatment on Microstructure and Mechanical Properties of Titanium Alloy Ti6Al2V2Zr1.5Mo

The heat treatment and cold rolling combinations have been carried out on titanium alloy Ti6Al2V2Zr1.5Mo, and microstructure evolution and mechanical behavior have been studied. Solution treatment below the β-transus temperature, followed by air cooling, resulted in higher microhardness/strength as compared to the same with water quenching. A sudden drop in microhardness/strength is observed in sample solution heat-treated above β-transus temperature followed by air cooling. The former is attributed to the additional presence of fine secondary α-phase formed by dynamic aging during air cooling as compared to water-quenched samples which did not have fine secondary α-phase. Solution treatment above β-transus temperature resulted in Widmanstatten microstructure with no significant fine secondary α in air-cooled samples. Among the studied conditions of cold rolling (CR), gain in strength of the alloy from annealed condition is significant with first 15% reduction and thereafter it is marginal for 30% reduction. Initiation of cracks at the edges has been observed in 30% CR. The microstructure of cold-rolled samples confirms the fragmentation of α-plates with the presence of high dislocation density. Heat treatment of cold-rolled samples resulted in significant reduction in strength from the as-cold-rolled conditions. The marginally lower strength than the as-received (annealed) or heat-treated alloy samples is due to the recrystallization in CR samples and the formation of Widmanstatten microstructure in air-cooled samples. The alloy does not have fine secondary α or regions with large dislocation density in this condition. The microstructure in the samples heat-treated (with air cooling) below as well as above β-transus temperature (after CR) is similar to air-cooled samples (without prior CR) with heat treatment above β-transus temperature. This indicates the reduction in recrystallization temperature with cold working, which is substantiated with the reduction in strength as well.

36 MATERIALS SCIENCE↗

Hot Deformation Characteristics and Processing Map of FV520B Martensitic Precipitation-Hardened Stainless Steel

Hot deformation characteristics of FV520B martensitic precipitation-hardened stainless steel were investigated in the temperature range of 850-1150 °C and strain rate range of 0.005-0.5 s{sup −1} with true strain 0.8 by using Gleeble-3500 thermo-mechanical simulator. Critical stress and corresponding critical strain for dynamic recrystallization initiation were calculated. The constitutive equation was developed by employing Arrhenius constitutive model to represent the nonlinear relationship of true stress and deformation parameters including temperature, strain rate and strain. The correlation coefficient and average absolute relative error are 0.9979 and 2.225%, which indicates the good predictive accuracy of the established constitutive equations. Processing maps were constructed at different plastic strains levels based on dynamic material model (DMM) and established constitutive equation. Combining the processing map with microstructure, the optimum region for good workability is designated as the temperature range of 1050-1125 °C and strain rate range of 0.027-0.23 s{sup −1} with peak efficiency of 0.32. Homogeneous fine and equiaxed dynamic recrystallization (DRX) grains can be found in this optimum according to the microstructure metallographic pictures.

36 MATERIALS SCIENCE↗

Coupling Thermomechanical Processing and Alloy Design to Improve Textures in Mg-Zn-Ca Sheet Alloys

Abstract The effect of Ca and Zn additions on the microstructure and texture evolution during thermomechanical processing of Mg-Zn-Ca sheet alloys was systematically investigated and quantified. Plane strain compression testing in a Gleeble thermomechanical simulator was used to physically simulate a 10-pass rolling schedule, while allowing for careful control and monitoring of the processing parameters. Textures in the as-deformed ternary alloy samples demonstrate a weak maximum basal intensity and spreading in the transverse direction. Increasing the Zn content to 3.2 wt.% in the ternary alloys resulted in samples that exhibited weak textures in the as-deformed state. Importantly, static recrystallization (SRX) during post-deformation annealing of these alloys promoted a desirable annular texture, with the c -axis tipped from the normal direction and a lower basal texture intensity. The evolution in texture during SRX is associated with as-deformed microstructures with broad grain orientation spreads and a low degree of recrystallization.

36 MATERIALS SCIENCE↗

Process-Structure-Property Modeling for Severe Plastic Deformation Processes Using Orientation Imaging Microscopy and Data-Driven Techniques

Machining is a severe plastic deformation process, wherein the workpiece material is subjected to high deformation rates and temperatures. During metal machining, the dynamic recrystallization mechanism causes grain refinement into the sub-micron range. In this study, we investigate the microstructure evolution of oxygen-free high conductivity copper (OFHC Cu) subject to a machining process where the cutting speed and rake angle are controlled to manipulate the process strain, strain rate, and temperatures. Microstructures of the deformed chips are quantified using orientation imaging microscopy and novel statistical descriptors that capture the morphology and local lattice misorientations generated during the several mechanistic stages of the dynamic recrystallization process. Mechanical properties of the resulting chips are quantified using spherical nanoindentation protocols. A multiple output Gaussian process regression model is used to simultaneously model the structure-property evolution, which differs from more common approaches that establish such relationships sequentially. This modeling strategy is particularly attractive since it can flexibly provide both structure and property uncertainty estimates. In addition, the statistical modeling framework allows for the inclusion of multi-fidelity data. The statistical metrics utilized serve as efficient microstructure descriptors, which retain the physics of the observed structures without having to introduce ad hoc microstructure feature definitions.

36 MATERIALS SCIENCE↗

Microstructure and hardness evolution induced by annealing of ion irradiated LiTaO 3

We report the evolution of the microstructure and mechanical properties of low-energy heavy-ion-irradiated LiTaO 3 crystals annealed at various temperatures was investigated by transmission electron microscopy (TEM) observations and nanoindentation tests to extend the applications of irradiated LiTaO 3 crystals. Before annealing, randomly distributed voids formed in an approximately 200 nm thick region at the end of the ion irradiation range, which was attributed to preferential absorption of interstitials by the amorphous-crystalline interface. After annealing, a new directional diffusion path of defects was identified, resulting in a void string. Furthermore, void string diffusion to the free surface was also found during the annealing temperature increase process, which offers a potential application in designing custom sized-thickness exfoliation at the nanoscale. Meanwhile, two competing processes were identified during the annealing process: epitaxial recrystallization from the amorphous-crystalline interface and grain nucleation process in the amorphous region, which formed phases different from the matrix crystal structure, resulting in an interaction between them. Furthermore, the hardness of irradiated samples was also found to be affected by the annealing process; in particular, a hardness decrease induced by the interstitial Fe ions in the recrystallized region was also confirmed, which can improve the processability of samples for further application.

36 MATERIALS SCIENCE↗

A novel reduction synthesis of the graphene/Mn{sub 3}O{sub 4} nanocomposite for supercapacitors

Graphene/Mn{sub 3}O{sub 4} nanocomposite is successfully synthesized from graphene oxide (GO)/MnO{sub 2} precursor using dilute hydrazine hydrate assisted hydrothermal reaction (DAH method). X-ray photoelectron spectroscopy (XPS) and Raman characterizations confirm the decrease of oxygen-containing functional groups of GO. The results indicate that GO have been reduced to graphene to a large degree to increase the electronic conductive channels. The morphology and the phase transformation of MnO{sub 2} can be ascribed to the “dissolution-recrystallization” mechanism. Such nanocomposite, as electrode material for supercapacitor, exhibits a high specific capacitance of 326.9 F g{sup −1}, almost 4 times that of GO/MnO{sub 2} precursor (81.3 F g{sup −1}). The good cycle stability of 94.6% capacitance retention after 1000 cycles, can be explained by the firm interfacial cohesion between graphene and Mn{sub 3}O{sub 4} nanoparticle. This soft chemical DAH process could be readily extended to the preparation of other classes of hybrids. - Graphical abstract: The phase transition can be explained by the “dissolution-recrystallization” model. The GO/MnO{sub 2} precursor is reduced into graphene/Mn{sub 3}O{sub 4} by the DAH process, and the electrochemical property is dramatically enhanced. - Highlights: • Graphene/Mn{sub 3}O{sub 4} nanocomposite is firstly synthesized successfully from GO/MnO{sub 2} precursor. • The phase transformation from MnO{sub 2} to Mn{sub 3}O{sub 4} has occurred. • The specific capacitance of the graphene/Mn{sub 3}O{sub 4} (326.9 F/g) is 4 times that of GO/MnO{sub 2} precursor.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Texture evolution in Fe-3% Si steel treated under unconventional annealing conditions

The present work investigates texture evolution stages in grain-oriented steel heat-treated using unconventional conditions. The Fe-3%Si steel taken after final cold rolling reduction from an industrial line was subjected to a laboratory isothermal annealing at different temperatures. The annealing temperatures were varied in a range of 850-1150 deg. C. During the annealing each specimen was heated at 10 deg. C/s and kept at the stated temperature for 5 min. Development of microstructure and texture in the annealed specimens were followed by the DC measurements of magnetic properties. The grain oriented steel, taken from the same industrial line after final box annealing was also analyzed and compared with the laboratory annealed specimens. It was shown that there is an optimal temperature region that, with combination of a fast heating rate, led to the best conditions of a drastically reduced development time of the {l_brace}110{r_brace} < 001 > crystallographic texture in the cold rolled grain-oriented steel. Materials heat treated below the optimum temperature region account for a primary recrystallization, while applying heat above this region leads to a secondary recrystallization without abnormal grain growth. Moreover, in the optimum temperature range, there was a particular temperature leading to the most optimal microstructure and texture. The magnetic properties, measured after the optimal heat treatment, were close to that measured on specimens taken after the final box annealing. The electron back scattered diffraction measurement technique revealed that sharpness of the {l_brace}110{r_brace} < 001 > crystallographic texture, developed at the optimum temperature is comparable to the steel taken after the industrial final box annealing. This fact is evidence that there is a temperature where the abnormal grain growth proceeds optimally.

36 MATERIALS SCIENCE↗

Formation mechanism of linear friction welded Ti-6Al-4V alloy joint based on microstructure observation

The microstructure of the linear friction welded Ti-6Al-4V titanium alloy joint was investigated by optical microscope, scanning electronic microscope and transmission electron microscope. Results show that the dynamic recovery and recrystallization resulting from the intensive plastic deformation and fast heating and cooling processes during linear friction welding account for the superfine {alpha} + {beta} grains in the weld center. Fine {alpha} grains distribute in the {beta} matrix or at the boundaries of {beta} grains. A mass of dislocations networks and metastructures present within the {alpha} and {beta} grains. - Research Highlights: {yields} TEM is employed in the analysis. {yields} The dynamic recovery is the main mechanism in thermal deformation of TC4. {yields} Superfine grains in the weld result from dynamic recovery and dynamic recrystallizaion, but the recrystallization is inadequate.

36 MATERIALS SCIENCE↗

Microstructural and textural evolution of AZ61 magnesium alloy sheet during bidirectional cyclic bending

In this work, the microstructural and textural evolution in the sheets of AZ61 magnesium alloy was studied by means of bidirectional cyclic bending for 8 passes at 623 K. The bended samples were examined by optical microscopy and electron backscatter diffraction analysis. The results showed that a gradient structure with fine grains about 3 μm in the regions near two surfaces and, in contrast, coarse grains in the middle of the sheet were formed. The evident grain refinement was attributed to twin-assisted dynamic recrystallization and continuous dynamic recrystallization induced by kink bands. The texture intensity was clearly reduced, resulting in a negative gradient distribution, with the texture intensity decreases from the center of the sheet to two surfaces. The weakened texture greatly facilitated the reduction of the yield strength. A higher fracture elongation and a slightly improved ultimate tensile strength were achieved concurrently. - Highlights: • The AZ61 Mg alloy is deformed at 623 K by bidirectional cyclic bending. • A symmetric gradient distribution of fine grains along the thickness is formed. • The basal texture in the regions near two surfaces is weakened significantly.

36 MATERIALS SCIENCE↗

Micromechanisms of grain refinement during extrusion of Mg–0.3 at.% Al at low homologous temperature

Coarse grained Mg–0.3 at.% Al (0.33 in wt.%) alloy was processed by direct extrusion with a reduction ratio of 25:1 at a temperature of ∼ 433 K. The extrusion remainder was removed from the die and analysed in three distinct zones: the cast billet, the conical zone of extrusion die, and the as-extruded rod. The zones were characterized by electron backscatter diffraction (EBSD) and light microscopy techniques to identify the processes responsible for grain refinement. Complex networks of (10–12) twins in practically all grains produced a noticeable microstructural fragmentation even before the material reached the conical zone of the die. Deformation twinning extended up to the entrance zone of the conical die where it was followed by a continuous dynamic recrystallization (CDRX) that gradually changed low angle boundaries to high angle boundaries. It is apparent that geometrically necessary dislocations play a crucial role in the formation of new grain boundaries. CDRX results in a bimodal structure with grain diameters ∼ 3 and ∼ 30 μm. As a material flows through the conical zone, the ratio of large to small grains is progressively decreased by CDRX in favour of fine grains. The as-extruded microstructure (a rod 8 mm in diameter), with an average grain diameter of ∼ 2.1 μm, shows a strong texture where the vast majority of grains (99.99%) have the c-axis oriented at least 30° from the extrusion direction. - Highlights: • Coarse grained Mg–0.3 at.% Al alloy was extruded at temperature of ∼ 433 K. • Processes responsible for grain refinement were analysed in extrusion remainder. • In the first stage, complex (10–12) twinning produced a noticeable fragmentation. • Deformation twinning was followed by continuous dynamic recrystallization. • 99.99% of grains in extruded rod have c-axis oriented > 30° from extrusion direction.

36 MATERIALS SCIENCE↗

Microstructure characterization and mechanical behaviors of a hot forged high Nb containing PM-TiAl alloy

In this work, the effects of deformation on the microstructure and mechanical behaviors of TiAl alloy were investigated. Deformed microstructure observation was characterized by scanning electron microscopy, electron back scattered diffraction technique, transmission electron microscopy and DEFORM-3D software. Results indicated that the core area of the TiAl pancake was characterized by completely dynamically recrystallized microstructures, however some residual lamellar colonies can be observed near the edge area, which are primarily caused by a temperature drop and inhomogenous plastic flow. The main softening mechanism is dynamic recrystallization of γ grains. The as-forged alloy exhibited excellent mechanical properties at both room temperature and high temperature. Tensile test results showed that the ultimate tensile strength of the alloy increased from 832 MPa at room temperature to 853 MPa at 700 °C, while the elongation increased from 2.7% to 17.8%. Even at the temperature of 850 °C, the ultimate tensile strength maintained 404 MPa, and the elongation increased to 75%. The as-forged alloy also exhibited remarkable low-temperature superplasticity at 850 °C, with an elongation of 120%. - Highlights: • The core area of the TiAl pancake was characterized by DRX microstructure. • The elongation at RT is higher than that of other high Nb-containing TiAl alloys. • The forged alloy exhibited low-temperature superplasticity at 850 °C.

36 MATERIALS SCIENCE↗

Microstructural characteristics of adiabatic shear localization in a metastable beta titanium alloy deformed at high strain rate and elevated temperatures

The microstructural evolution and grain refinement within adiabatic shear bands in the Ti6554 alloy deformed at high strain rates and elevated temperatures have been characterized using transmission electron microscopy. No stress drops were observed in the corresponding stress–strain curve, indicating that the initiation of adiabatic shear bands does not lead to the loss of load capacity for the Ti6554 alloy. The outer region of the shear bands mainly consists of cell structures bounded by dislocation clusters. Equiaxed subgrains in the core area of the shear band can be evolved from the subdivision of cell structures or reconstruction and transverse segmentation of dislocation clusters. It is proposed that dislocation activity dominates the grain refinement process. The rotational recrystallization mechanism may operate as the kinetic requirements for it are fulfilled. The coexistence of different substructures across the shear bands implies that the microstructural evolution inside the shear bands is not homogeneous and different grain refinement mechanisms may operate simultaneously to refine the structure. - Graphical abstract: Display Omitted - Highlights: • The microstructure within the adiabatic shear band was characterized by TEM. • No stress drops were observed in the corresponding stress–strain curve. • Dislocation activity dominated the grain refinement process. • The kinetic requirements for rotational recrystallization mechanism were fulfilled. • Different grain refinement mechanisms operated simultaneously to refine the structure.

36 MATERIALS SCIENCE↗