Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “MAGNETRONS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 415 records · Page 23

Electrical and optical properties of Nb-doped TiO{sub 2} films deposited by dc magnetron sputtering using slightly reduced Nb-doped TiO{sub 2-x} ceramic targets

Nb-doped anatase TiO{sub 2} films were deposited on unheated glass by dc magnetron sputtering using slightly reduced Nb-doped TiO{sub 2-x} targets (Nb concentration: 3.7 and 9.5 at. %) with various hydrogen or oxygen flow ratios. After postannealing in a vacuum (6x10{sup -4} Pa) at 500 deg. C for 1 h, both films were crystallized into the polycrystalline anatase TiO{sub 2} structure. The resistivity decreased from 1.6x10{sup -3} to 6.3x10{sup -4} {Omega} cm with increasing Nb concentration from 2.8 to 8.0 at. %, where the carrier density increased from 5.4x10{sup 20} to 2.0x10{sup 21} cm{sup -3} and the Hall mobility was almost constant at 5-7 cm{sup 2} V{sup -1} s{sup -1}. The films exhibited a high transparency of over 60%-80% in the visible region.

36 MATERIALS SCIENCE↗

Residual stress stability in fiber textured stoichiometric AlN film grown using rf magnetron sputtering

The authors report on the stability of mechanical stress with aging and thermal cycling for columnar structured stoichiometric and homogeneous aluminum nitride thin films grown using radio frequency magnetron sputtering technique. The set of deposition parameters were optimized for the best possible orientation of crystallites in the c axis of compositionally stoichiometric films. The as-grown stress in the slightly nitrogen-rich film does not change when exposed to the atmosphere following deposition, while that in the nitrogen-deficient film, it changes due to oxidation. Additionally, the magnitude of as-grown stress has been found to depend on the substrate material in addition to the deposition parameters. The stress in the film grown on a Si(001) substrate was more tensile than in the film grown on a semi-insulating (si) GaAs(001) substrate for a given set of deposition parameters. Furthermore, the stress in the film grown on Si decreased with temperature, while that on si GaAs increased, indicating the thermally induced stress component to be the major component in the residual stress. Upon subsequent cooling the stress changes in both substrates followed the same path as of heating, thus exhibiting no hysteresis with thermal cycles between room temperature and 400 deg. C.

36 MATERIALS SCIENCE↗

Highly conductive indium zinc oxide prepared by reactive magnetron cosputtering technique using indium and zinc metallic targets

Zn-doped In{sub 2}O{sub 3} film is frequently deposited from an oxide target; but the use of metallic target is increasingly expected as preparing the film with comparable properties. This work aimed to prepare a highly conductive and transparent Zn-doped In{sub 2}O{sub 3} thin film on Corning Eagle{sup 2000} glass substrate by magnetron cosputtering method using indium and zinc targets. Structural characterization was performed using x-ray diffraction and x-ray photoelectron spectroscopy. The film had an amorphous structure when the film was prepared on an unheated substrate, but had an In{sub 2}O{sub 3} polycrystalline structure when the film was deposited on 150 and 300 deg. C substrates. The electrical properties of the film were greatly affected by annealing; the Zn-doped In{sub 2}O{sub 3} film had a low resistivity of 6.1x10{sup -4} {Omega} cm and an average transmittance of 81.7% when the film was deposited without substrate heating and followed a 600 deg. C annealing.

36 MATERIALS SCIENCE↗

Reactive magnetron cosputtering of hard and conductive ternary nitride thin films: Ti-Zr-N and Ti-Ta-N

Ternary transition metal nitride thin films, with thickness up to 300 nm, were deposited by dc reactive magnetron cosputtering in Ar-N{sub 2} plasma discharges at 300 deg. C on Si substrates. Two systems were comparatively studied, Ti-Zr-N and Ti-Ta-N, as representative of isostructural and nonisostructural prototypes, with the aim of characterizing their structural, mechanical, and electrical properties. While phase-separated TiN-ZrN and TiN-TaN are the bulk equilibrium states, Ti{sub 1-x}Zr{sub x}N and Ti{sub 1-y}Ta{sub y}N solid solutions with the Na-Cl (B1-type) structure could be stabilized in a large compositional range (up to x=1 and y=0.75, respectively). Substituting Ti atoms by either Zr or Ta atoms led to significant changes in film texture, microstructure, grain size, and surface morphology, as evidenced by x-ray diffraction, x-ray reflectivity, and scanning electron and atomic force microscopies. The ternary Ti{sub 1-y}Ta{sub y}N films exhibited superior mechanical properties to Ti{sub 1-x}Zr{sub x}N films as well as binary compounds, with hardness as high as 42 GPa for y=0.69. All films were metallic, the lowest electrical resistivity {rho}{approx}65 {mu}{Omega} cm being obtained for pure ZrN, while for Ti{sub 1-y}Ta{sub y}N films a minimum was observed at y{approx}0.3. The evolution of the different film properties is discussed based on microstructrural investigations.

36 MATERIALS SCIENCE↗

Investigation of microstructure, surface morphology, and hardness properties of PtIr films by magnetron sputtering

Pt{sub 1-x}Ir{sub x} films with x varying from 22.76 to 63.25 at. % are deposited on (100) Si wafer substrates at 400 deg. C by magnetron sputtering deposition. The effects of the Ir concentration on the microstructure, morphology, and hardness of PtIr films are investigated by field emission scanning electron microscopy, x-ray diffraction, atomic force microscopy, and nanoindentation system. The columnar structures are observed by field emission scanning electron microscopy. X-ray diffraction analysis reveals that PtIr films have preferred orientation along Pt(111) when the Ir concentration is below 50.84 at. %. When the Ir content is more than 50.84 at. %, the PtIr film shifts to another preferred orientation, Ir(111). The surface morphology is analyzed by atomic force microscopy. The roughness of the PtIr films decreases with increasing Ir content. The hardness of all the PtIr films is below 20 GPa. The maximum hardness of the PtIr films is about 14.9 GPa when the Ir concentration is 57.9 at. %.

36 MATERIALS SCIENCE↗

Formation of pyrite (FeS{sub 2}) thin films by thermal sulfurization of dc magnetron sputtered iron

Iron films deposited by direct current magnetron sputtering onto glass substrates were converted into FeS{sub 2} films by thermal sulfurization. Experiments were carried out to optimize the sulfurization process, and the formation of FeS{sub 2} thin films was investigated under different annealing temperatures and times. High quality FeS{sub 2} films were fabricated using this process, and single phase pyrite films were obtained after sulfurization in a sulfur and nitrogen atmosphere at 450 deg. C for 1 h. Film crystallinity and phase identification were determined by using x-ray diffraction. The cubic phase pyrite films prepared were p-type, and scanning electron microscopy studies exhibited a homogeneous surface of pyrite. The authors have found that the best Ohmic contact for their pyrite thin films, using inexpensive metals, was Ni. The following were chosen for the study: Al, Mo, Fe, and Ni, and the one that led to the lowest resistance, 333 {Omega}, was Ni.

36 MATERIALS SCIENCE↗

Comprehensive study of the p-type conductivity formation in radio frequency magnetron sputtered arsenic-doped ZnO film

Arsenic doped ZnO and ZnMgO films were deposited on SiO{sub 2} using radio frequency magnetron sputtering and ZnO-Zn{sub 3}As{sub 2} and ZnO-Zn{sub 3}As{sub 2}-MgO targets, respectively. It was found that thermal activation is required to activate the formation of p-type conductivity. Hall measurements showed that p-type films with a hole concentration of {approx}10{sup 17} cm{sup -3} and mobility of {approx}8 cm{sup 2} V{sup -1} s{sup -1} were obtained at substrate temperatures of 400-500 deg. C The shallow acceptor formation mechanism was investigated using x-ray photoelectron spectroscopy, positron annihilation, low temperature photoluminescence, and nuclear reaction analysis. The authors suggest that the thermal annealing activates the formation of the As{sub Zn}-2V{sub Zn} shallow acceptor complex and removes the compensating hydrogen center.

36 MATERIALS SCIENCE↗

DC reactive magnetron sputtering, annealing, and characterization of CuAlO{sub 2} thin films

CuAlO{sub x} thin films were prepared at three substrate temperatures (T{sub S}=60, 300, and 600 deg. C) and two oxygen partial pressures (P{sub O{sub 2}}=0.5 and 2 mTorr) via dc reactive magnetron sputtering from Cu-Al 50-50 at. % alloy targets and subsequent annealing. As-deposited films with P{sub O{sub 2}}=0.5 mTorr were oxygen deficient; although the delafossite structure formed upon annealing, electrical properties were poor. Films deposited with P{sub O{sub 2}}=2 mTorr transformed into the delafossite structure and exhibited p-type conductivity after annealing under N{sub 2} at temperatures T{sub A}{>=}750 deg. C. Conductivity generally increased with increasing T{sub S} and decreasing T{sub A}. A special case of P{sub O{sub 2}}=2 mTorr and low T{sub S} (60 deg. C) resulted in a partially crystalline oxide phase that transformed into the delafossite structure at T{sub A}=700 deg. C and yielded the highest conductivity of 1.8 S cm{sup -1}. In general, a T{sub A} near the phase formation boundary led to an increase in conductivity. Low-temperature hydrothermal annealing was also investigated and shown to produce mixed phase films exhibiting the delafossite structure along with CuO, AlOOH, and Al{sub 2}O{sub 3}.

36 MATERIALS SCIENCE↗

Spectroscopic ellipsometry and x-ray photoelectron spectroscopy of La{sub 2}O{sub 3} thin films deposited by reactive magnetron sputtering

Lanthanum oxide (La{sub 2}O{sub 3}) films were grown by the reactive dc magnetron sputtering and studied their structural, chemical and optical parameters. La{sub 2}O{sub 3} films were deposited onto Si substrates by sputtering La-metal in a reactive gas (Ar+O{sub 2}) mixture at a substrate temperature of 200 deg. C Reflection high-energy electron diffraction measurements confirm the amorphous state of La{sub 2}O{sub 3} films. Chemical analysis of the top-surface layers evaluated with x-ray photoelectron spectroscopy indicates the presence of a layer modified by hydroxylation due to interaction with atmosphere. Optical parameters of a-La{sub 2}O{sub 3} were determined with spectroscopic ellipsometry (SE). There is no optical absorption over spectral range {lambda}=250-1100 nm. Dispersion of refractive index of a-La{sub 2}O{sub 3} was defined by fitting of SE parameters over {lambda}=250-1100 nm.

36 MATERIALS SCIENCE↗

Highly textured growth of AlN films on sapphire by magnetron sputtering for high temperature surface acoustic wave applications

Piezoelectric aluminum nitride films were deposited onto 3 in. [0001] sapphire substrates by reactive magnetron sputtering to explore the possibility of making highly (002)-textured AlN films to be used in surface acoustic wave (SAW) devices for high temperature applications. The synthesized films, typically 1 {mu}m thick, exhibited a columnar microstructure and a high c-axis texture. The relationship between the microstructures and process conditions was examined by x-ray diffraction (XRD), transmission electron microscopy, and atomic force microscopy analyses. The authors found that highly (002)-textured AlN films with a full width at half maximum of the rocking curve of less than 0.3 deg. can be achieved under high nitrogen concentration and moderate growth temperature, i.e., 250 deg. C. The phi-scan XRD reveals the high in-plane texture of deposited AlN films. The SAW devices, based on the optimized AlN films on sapphire substrate, were characterized before and after an air annealing process at 800 deg. C for 90 min. The frequency response, recorded after the annealing process, confirmed that the thin films were still strong in a high temperature environment and that they had retained their piezoelectric properties.

36 MATERIALS SCIENCE↗

Microstructure and residual stress of magnetron sputtered nanocrystalline palladium and palladium gold films on polymer substrates

The authors report the structural properties and residual stresses of 500-nm-thick nanocrystalline Pd and PdAu films on compliant substrates prepared by magnetron sputtering as a function of the pressure of the Ar-sputtering gas. Films were analyzed by x-ray diffraction, cross-sectional transmission electron microscopy, and x-ray photoelectron spectroscopy. At low pressures the metal films exhibit strong compressive stresses, which rapidly change to highly tensile with increasing pressure, and then gradually decrease. Along with this effect a change in microstructure is observed from a dense equiaxed structure at low pressures to distinctive columns with reduced atomic density at the column walls at higher pressures. The preparation of nearly stress-free dense nanocrystalline films is demonstrated.

36 MATERIALS SCIENCE↗

Resonance hairpin and Langmuir probe-assisted laser photodetachment measurements of the negative ion density in a pulsed dc magnetron discharge

The time-resolved negative oxygen ion density n{sub -} close to the center line in a reactive pulsed dc magnetron discharge (10 kHz and 50% duty cycle) has been determined for the first time using a combination of laser photodetachment and resonance hairpin probing. The discharge was operated at a power of 50 W in 70% argon and 30% oxygen gas mixtures at 1.3 Pa pressure. The results show that the O{sup -} density remains pretty constant during the driven phase of the discharge at values typically below 5x10{sup 14} m{sup -3}; however, in the off-time, the O{sup -} density grows reaching values several times those in the on-time. This leads to the negative ion fraction (or degree of electronegativity) {alpha}=n{sub -}/n{sub e} being higher in the off phase (maximum value {alpha}{approx}1) than in the on phase ({alpha}=0.05-0.3). The authors also see higher values of {alpha} at positions close to the magnetic null than in the more magnetized region of the plasma. This fractional increase in negative ion density during the off-phase is attributed to the enhanced dissociative electron attachment of highly excited oxygen molecules in the cooling plasma. The results show that close to the magnetic null the photodetached electron density decays quickly after the laser pulse, followed by a slow decay over a few microseconds governed by the negative ion temperature. However, in the magnetized regions of the plasma, this decay is more gradual. This is attributed to the different cross-field transport rates for electrons in these two regions. The resonance hairpin probe measurements of the photoelectron densities are compared directly to photoelectron currents obtained using a conventional Langmuir probe. There is good agreement in the general trends, particularly in the off-time.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Compositional study of vacuum annealed Al doped ZnO thin films obtained by RF magnetron sputtering

Aluminum doped zinc oxide (AZO) thin films were obtained by RF magnetron sputtering. The effects of deposition parameters such as power, gas flow conditions, and substrate heating have been studied. Deposited and annealed films were characterized for composition as well as microstructure using x ray photoelectron spectroscopy and x ray diffraction. Films produced were polycrystalline in nature. Surface imaging and roughness studies were carried out using SEM and AFM, respectively. Columnar grain growth was predominantly observed. Optical and electrical properties were evaluated for transparent conducting oxide applications. Processing conditions were optimized to obtain highly transparent AZO films with a low resistivity value of 6.67 x 10{sup -4}{Omega} cm.

36 MATERIALS SCIENCE↗

Properties of double-layered Ga-doped Al-zinc-oxide/titanium-doped indium-tin-oxide thin films prepared by dc magnetron sputtering applied for Si-based thin film solar cells

In this article, Ga-doped Al-zinc-oxide (GAZO)/titanium-doped indium-tin-oxide (ITIO) bi-layer films were deposited onto glass substrates by direct current (dc) magnetron sputtering. The bottom ITIO film, with a thickness of 200 nm, was sputtered onto the glass substrate. The ITIO film was post-annealed at 350 deg. C for 10-120 min as a seed layer. The effect of post-annealing conditions on the morphologies, electrical, and optical properties of ITIO films was investigated. A GAZO layer with a thickness of 1200 nm was continuously sputtered onto the ITIO bottom layer. The results show that the properties of the GAZO/ITIO films were strongly dependent on the post-annealed conditions. The spectral haze (T{sub diffuse}/T{sub total}) of the GAZO/ITIO bi-layer films increases upon increasing the post-annealing time. The haze and resistivity of the GAZO/ITIO bi-layer films were improved with the post-annealed process. After optimizing the deposition and annealing parameters, the GAZO/ITIO bi-layer film has an average transmittance of 83.20% at the 400-800 nm wavelengths, a maximum haze of 16%, and the lowest resistivity of 1.04 x 10{sup -3}{Omega} cm. Finally, the GAZO/ITIO bi-layer films, as a front electrode for silicon-based thin film solar cells, obtained a maximum efficiency of 7.10%. These encouraging experimental results have potential applications in GAZO/ITIO bi-layer film deposition by in-line sputtering without the wet-etching process and enable the production of highly efficient, low-cost thin film solar cells.

36 MATERIALS SCIENCE↗

Populations of metastable and resonant argon atoms in radio frequency magnetron plasmas used for deposition of indium-zinc-oxide films

This work reports optical absorption spectroscopy measurements of the number density of Ar atoms in resonant ({sup 3}P{sub 1}, {sup 1}P{sub 1}) and metastable ({sup 3}P{sub 2}, {sup 3}P{sub 0}) states in rf magnetron sputtering plasmas used for the deposition of ZnO-based thin films. While the density of Ar {sup 3}P{sub 2} and {sup 3}P{sub 0} was fairly independent of pressure in the range of experimental conditions investigated, the density of Ar {sup 3}P{sub 1} and {sup 1}P{sub 1} first sharply increased with pressure and then reached a plateau at values close to those of the {sup 3}P{sub 2} and {sup 3}P{sub 0} levels at pressures above about 50 mTorr. At such pressures, ultraviolet radiation from resonant states becomes trapped such that these levels behave as metastable states. For a self-bias voltage of -115 V and pressures in the 5-100 mTorr range, similar number densities of Ar resonant and metastable atoms were obtained for Zn, ZnO, and In{sub 2}O{sub 3} targets, suggesting that, over the range of experimental conditions investigated, collisions between these excited species and sputtered Zn, In, and O atoms played only a minor role on the discharge kinetics. The metastable-to-ground state number density ratios were also fitted to the predictions of a global model using the average electron temperature, T{sub e}, as the only adjustable parameter. For all targets examined, the values of T{sub e} deduced from this method were in excellent agreement with those obtained from Langmuir probe measurements.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Tribological behavior of Ti-Al-Si-C-N hard coatings deposited by hybrid arc-enhanced magnetron sputtering

Ti-Al-Si-C-N hard coatings are deposited on high speed steel by hybrid arc-enhanced magnetron sputtering, and the hardness, adhesion, and tribological behavior are studied. On account of the nanocomposite structure, the coatings possess hardness of more than 30 GPa. Failure of the coating during the scratch test is due to the buckling and wedge spallation failure mechanism. Compared to Ti-Al-Si-N, the presence of C in the Ti-Al-Si-C-N coatings leads to reduced friction coefficient and wear rate, indicating effective lubrication rendered by amorphous C. According to the wear tracks examined by scanning electron microscopy, the wear mechanism can be explained by plowing abrasion.

36 MATERIALS SCIENCE↗

Visible light-induced photocatalytic properties of WO{sub 3} films deposited by dc reactive magnetron sputtering

The authors examined the photocatalytic activity of WO{sub 3} films (thickness 500-600 nm) deposited on a fused quartz substrate heated at 350-800 deg. C by dc reactive magnetron sputtering using a W metal target under the O{sub 2} gas pressure from 1.0 to 5.0 Pa. Films deposited at 800 deg. C under 5.0 Pa have excellent crystallinity of triclinic, P1(1) structure and a large surface area, as confirmed by x-ray diffraction, scanning electron microscopy, and atomic force microscopy. Exposure of acetaldehyde (CH{sub 3}CHO) adsorbed onto the film surface to ultraviolet, visible, or standard fluorescence light induces oxidative photocatalytic decomposition indicated by a decrease in CH{sub 3}CHO concentration and generation of CO{sub 2} gas. For all three types of irradiation, concentration ratio of decreased CH{sub 3}CHO to increased CO{sub 2} is about 1:1, suggesting the possible presence of intermediates. The sputter-deposited WO{sub 3} film can be a good candidate as a visible light-responsive photocatalyst.

36 MATERIALS SCIENCE↗

Magnetron-sputter deposition of Fe{sub 3}S{sub 4} thin films and their conversion into pyrite (FeS{sub 2}) by thermal sulfurization for photovoltaic applications

The authors report on the fabrication of FeS{sub 2} (pyrite) thin films by sulfurizing Fe{sub 3}S{sub 4} that were deposited by direct current magnetron sputtering at room temperature. Under the selected sputtering conditions, Fe{sub 3}S{sub 4} nanocrystal films are obtained and the nanocrystals tend to locally cluster and closely pack into ricelike nanoparticles with an increase in film thickness. Meanwhile, the film tends to crack when the film thickness is increased over {approx}1.3 {mu}m. The film cracking can be effectively suppressed by an introduction of a 3-nm Cu intermediate layer prior to Fe{sub 3}S{sub 4} deposition. However, an introduction of a 3-nm Al intermediate layer tends to enhance the film cracking. By post-growth thermal sulfurization of the Fe{sub 3}S{sub 4} thin films in a tube-furnace, FeS{sub 2} with high phase purity, as determined by using x ray diffraction, is obtained. Optical absorption spectroscopy was employed to characterize the resultant FeS{sub 2} thin films, which revealed two absorption edges at 0.9 and 1.2 eV, respectively. These two absorption edges are assigned to the direct bandgap (0.9 eV) and the indirect allowed transitions (1.2 eV) of FeS{sub 2}, respectively.

36 MATERIALS SCIENCE↗