Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “GAS WELDING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 415 records · Page 23

Periscope For Viewing Weld Penetration

Periscope enables viewing of weld joint from inside cylindrical duct to determine when weld penetration occurs. Supplies steady stream of inert gas to shield joint. Device used to calibrate and evaluate techniques for sensing weld penetration.

Gordon, Stephen S.↗

Detecting overpenetration of electron-beam welds

Gold plate beneath weldment reveals areas of excess penetration during X-ray inspection. Technique is applicable to critical electron-beam welds, such as those in gas turbines and pressure vessels.

Macfarlane, D. I.↗

Selection And Evaluation Of An Alloy For Nozzle Application

The present work includes results on material characterization conducted under COBRA Hydrogen Cooled Nozzle Program and was funded by NASA MSFC. The nozzle requires a material that has high strength at ambient and high (up to l200 F) temperatures in air and hydrogen. Presently, a precipitation hardened steel; A-286 is used in nozzles for Space Shuttle Engines. The A-286 alloy has limited hydrogen compatibility and weldability. The present work focused on selection and characterization of JBK-75 alloy that has significantly higher capability in hydrogen and weldability in addition to other attributes. The alloy was evaluated at different temperatures and environments. Tungsten Inert Gas (TIG) and Electron Beam welding techniques were used to evaluate the weldability of material. Brazing was also conducted on the alloy and evaluated. The characterization of base JBK-75 alloy, welded and brazed alloy included tensile properties, low cycle fatigue and crack growth resistance at different temperatures in air and hydrogen environments. The results indicated that JBK-75 has excellent tensile and fatigue properties in air and hydrogen. The welded and brazed alloy also showed very good properties.

Pandey, A. B.↗

Control of Weld Residual Stress in a Thin Steel Plate through Low Transformation Temperature Welding Consumables

Low transformation temperature welding (LTTW) consumables are characterized by a low martensite start temperature and a large fraction of martensite forming in the weld. It can efficiently reduce the tensile residual stress because the volume expansion associated with the martensitic transformation compensates for the thermal contraction during cooling. In this work, a LTTW wire, designated as EH200B, was created for the arc welding of advanced high-strength steel thin plates. In comparison to conventional ER70S-3 wires, this LTTW wire generated an opposite distortion pattern. Neutron diffraction measurements along the center thickness of the welded plates showed the maximum residual stress along the longitudinal direction (LD) in the weld region, and the heat-affected zone (HAZ) immediately adjacent to the weld region was reduced from ~330 MPa to below 240 MPa by using the LTTW wire. A finite element (FE) model was developed to predict the residual stress distributions of the plates welded under these two wires. The simulation results showed reasonable agreement with the volume-average neutron diffraction data. Compressive residual stress in the weld region using the LTTW wire was predicted by the FE method. Electron backscattered diffraction and x-ray diffraction measurements confirmed ~90% martensite was present in the LTTW weld. The fatigue life of DP980 steel lap joint panels using EH200B wire nearly doubled that of ER70S-3 wire. This improvement was attributed to the high strength and low LD residual stress in the weld and HAZ immediately adjacent to the weld.

36 MATERIALS SCIENCE↗

Stainless Steel 18-10 CO2 Laser Welding And Plasma Diagnostics

The welding of materials by CO2 laser took significant considerations in industry, for the reason of the quality of the carried out weldings, and for other many advantages, but the automation of the welding operation requires a control system in real time. The operation of welding is an operation of interaction between the radiation (laser), and the matter (welded part), which is characterized by the vaporization of the matter, formation of the keyhole in material, and appearance of plasma over the material. This study relates to the relation between the welding (molten material) and the plasma which is formed on material. The light emitted by plasma during laser welding was recorded by an OMA detector (Optical Multichannel Analyzer) over a wavelength width of 450 A ring . The analysis of this light allows to determine the composition of this plasma, its dimensions, and the state of its energy according to the laser parameters. The welded material is the stainless steel 18-10, it was found that the intensity of the light emitted by plasma depends on laser power, the welding speed, the flow rate of assist gas. The relation between the plasma and the state of the bead were analyzed for on-line monitoring welding.

36 MATERIALS SCIENCE↗

Progress in developing laser based post irradiation examination infrastructure

To be able to understand the performance of reactor fuels and materials, irradiated materials must be characterized effectively and efficiently in high rad environments. This characterization work is performed remotely and in environments generally hostile to instrumentation. Laser based characterization techniques provide the ability to operate remotely and robustly in a hot-cell environment. Laser based instrumentation also can provide high spatial resolution suitable for scanning and imaging large areas. The INL is currently developing three laser based Post Irradiation Examination (PIE) stations for the Hot Fuel Examination Facility (HFEF) at the INL. These laser based systems will characterize irradiated materials and fuels. The characterization systems are the following: -) laser shock, -) laser based ultrasonic C-scan system and -) gas assay, sample and recharge system (GASR, up-grade to an existing system). The laser shock technique will characterize material properties and failure loads/mechanisms in various materials such as Light Water Reactor (LWR) fuel, plate fuel, and next generation fuel forms in high radiation areas. The laser shock-technique induces large amplitude shock waves to mechanically characterize interfaces such as the fuel-clad bond. As part of the laser shock system, a laser-based ultrasonic C-scan system will be used to detect and characterize de bonding caused by the application of the laser shock as well as performing classical non-destructive evaluation testing and imaging functions such as microstructure characterization, flaw detection and dimensional metrology. A spectroscopy capability can be added later as the salient components to perform Light Induced Breakdown Spectroscopy will be in place. Additional fiber ports in the feed-through will also enable future spectroscopic techniques to be efficiently installed and operated. The purpose of the GASR is to measure the pressure/volume of the plenum of an irradiated fuel element/capsule and obtain fission gas samples for analysis. The study of pressure and volume in the plenum of an irradiated fuel element/capsule and the analysis of fission gases released is important to understanding the performance of reactor fuels and materials. The main function of the laser in this application is to puncture the fuel rod or plate to allow the fission gas to escape and if necessary to weld the hole close. This system may also be used to measure the pressure/volume of other components (such as control blades) and obtain gas samples from these components for analysis. The GASR upgrade will match the functionality of the current system and provide these important functions on fuels made from current and future engineered materials. The GASR station will also have the inherent capability to perform cutting welding and joining functions within a hot-cell. The extra fiber ports built into the hot cell feed-through will also enable the efficient installation of future laser processing work benches. (authors)

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Modular In-Chamber Electron Beam Welding – Process Planning: Welding, Cladding, Inspection, and Manufacturing

Electron beam welding (EBW) is commonly employed by industry today to join relatively thin section components. Industrial sectors which utilize the technology include; automotive, aircraft, aerospace, defense, medical, oil & gas, etc. The ability to produce single pass, thick section (up to 6 inches, 150mm) welds has also been available for more than 40 years; however, the technology has not been deployed for civil nuclear manufacturing and fabrication such as reactor pressure vessels, steam generators, or pressurizers. Instead, thick section joining is performed much in the same manner it has been for decades using submerged arc or gas tungsten arc welding processes. Recent research performed under U.S. Department of Energy (DOE) project DE-NE0008629 has demonstrated that the overall welding time to produce one major reactor pressure vessel (RPV) girth weld can be reduced from weeks to less than 90 minutes, while maintaining exceptional quality and inspection characteristics. The subject project (DE-NE0008846) investigates a modular in-chamber (MIC) EBW approach which allows various RPV sections to be joined within a “modular” chamber. The MIC-EBW approach utilizes individual modules that can be stacked and de-stacked to various heights to enable production girth welds to be performed at a given elevation. This report describes the various processing methodology necessary to complete major girth weldments for the NuScale Power small modular reactor including welding development, manufacturing, production sequence, inspection, and cladding.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Manufacturing High-Quality Carbon Nanotubes at Lower Cost

A modified electric-arc welding process has been developed for manufacturing high-quality batches of carbon nanotubes at relatively low cost. Unlike in some other processes for making carbon nanotubes, metal catalysts are not used and, consequently, it is not necessary to perform extensive cleaning and purification. Also, unlike some other processes, this process is carried out at atmospheric pressure under a hood instead of in a closed, pressurized chamber; as a result, the present process can be implemented more easily. Although the present welding-based process includes an electric arc, it differs from a prior electric-arc nanotube-production process. The welding equipment used in this process includes an AC/DC welding power source with an integral helium-gas delivery system and circulating water for cooling an assembly that holds one of the welding electrodes (in this case, the anode). The cathode is a hollow carbon (optionally, graphite) rod having an outside diameter of 2 in. (approximately equal to 5.1 cm) and an inside diameter of 5/8 in. (approximately equal to 1.6 cm). The cathode is partly immersed in a water bath, such that it protrudes about 2 in. (about 5.1 cm) above the surface of the water. The bottom end of the cathode is held underwater by a clamp, to which is connected the grounding cable of the welding power source. The anode is a carbon rod 1/8 in. (approximately equal to 0.3 cm) in diameter. The assembly that holds the anode includes a thumbknob- driven mechanism for controlling the height of the anode. A small hood is placed over the anode to direct a flow of helium downward from the anode to the cathode during the welding process. A bell-shaped exhaust hood collects the helium and other gases from the process. During the process, as the anode is consumed, the height of the anode is adjusted to maintain an anode-to-cathode gap of 1 mm. The arc-welding process is continued until the upper end of the anode has been lowered to a specified height above the surface of the water bath. The process causes carbon nanotubes to form in the lowest 2.5 cm of the anode. It also causes a deposit reminiscent of a sandcastle to form on the cathode. The nanotube-containing material is harvested. The cathode and anode can then be cleaned (or the anode is replaced, if necessary) and the process repeated to produce more nanotubes. Tests have shown that the process results in approximately equal to 50-percent yield of carbon nanotubes (mostly of the single-wall type) of various sizes. Whereas the unit cost of purified single-wall carbon nanotubes produced by other process is about $1,000/g in the year 2000, it has been estimated that for the present process, the corresponding cost would be about $10/g.

Benavides, Jeanette M.↗

Compact monitoring and control console for pressurized gas bottles

Compact monitoring and control console dispenses gas over a range of pressures from conventional compressed-gas cylinders. It incorporates in a single assembly the necessary equipment for a portable pressurization system that can be used in welding and other operations requiring a controlled gas supply.

Freeman, B.↗

Hydrogen accelerated fatigue crack growth of friction stir welded X52 steel pipe

Friction stir welded steel pipelines were tested in high pressure hydrogen gas to examine the effects of hydrogen accelerated fatigue crack growth. Fatigue crack growth rate (da/dN) vs. stress-intensity factor range (ΔK) relationships were measured for an X52 friction stir welded pipe tested in 21 MPa hydrogen gas at a frequency of 1 Hz and R = 0.5. Tests were performed on three regions: base metal (BM), center of friction stir weld (FSW), and 15 mm off-center of the weld. For all three material regions, tests in hydrogen exhibited accelerated fatigue crack growth rates that exceeded an order of magnitude compared to companion tests in air. Among tests in hydrogen, fatigue crack growth rates were modestly higher in the FSW than the BM and 15 mm off-center tests. Select regions of the fracture surfaces associated with specified ΔK levels were examined which revealed intergranular fracture in the BM and 15 mm off-center specimens but an absence of intergranular features in the FSW specimens. In conclusion, the X52 friction stir weld and base metal tested in hydrogen exhibited fatigue crack growth rate relationships that are comparable to those for conventional arc welded steel pipeline of similar strength found in the literature.

08 HYDROGEN↗

Friction Stir Welding Development at NASA, Marshall Space Flight Center

Friction stir welding (FSW) is a solid state process that pan be used to join materials without melting. The process was invented by The Welding Institute (TWI), Cambridge, England. Friction stir welding exhibits several advantages over fusion welding in that it produces welds with fewer defects and higher joint efficiency and is capable of joining alloys that are generally considered non-weldable with a fusion weld process. In 1994, NASA-Marshall began collaborating with TWI to transform FSW from a laboratory curiosity to a viable metal joining process suitable for manufacturing hardware. While teamed with TWI, NASA-Marshall began its own FSW research and development effort to investigate possible aerospace applications for the FSW process. The work involved nearly all aspects of FSW development, including process modeling, scale-up issues, applications to advanced materials and development of tooling to use FSW on components of the Space Shuttle with particular emphasis on aluminum tanks. The friction stir welding process involves spinning a pin-tool at an appropriate speed, plunging it into the base metal pieces to be joined, and then translating it along the joint of the work pieces. In aluminum alloys the rotating speed typically ranges from 200 to 400 revolutions per minute and the translation speed is approximately two to five inches per minute. The pin-tool is inserted at a small lead angle from the axis normal to the work piece and requires significant loading along the axis of the tool. An anvil or reaction structure is required behind the welded material to react the load along the axis of the pin tool. The process requires no external heat input, filler material, protective shielding gas or inert atmosphere typical of fusion weld processes. The FSW solid-state weld process has resulted in aluminum welds with significantly higher strengths, higher joint efficiencies and fewer defects than fusion welds used to join similar alloys.

McGill, Preston↗

Effect of Ni content on the microstructure and mechanical properties of weld metal with both-side submerged arc welding technique

Highlights: • This manuscript primarily studied the effects of Ni content on the K65 weld metals; • Increase Ni content could significantly improve the strength and low temperature impact toughness of the weld metal. • The beneficial effect of Ni is attributed to its positive effect on phase transformation. • GBF keeps K-S or N-W relations only with one austenite and the variants belong to the same bain group are two reasons. • The M/A islands are considered to be another reason for the reduced toughness. - Abstract: The effects of nickel (Ni) content on the mechanical properties and microstructure evolution in the weld metals of commercial K65 oil and gas pipeline steel were studied. Increase Ni content could significantly improve the strength and low temperature impact toughness (−40 °C and −60 °C) of the weld metal. The above influences of Ni were attributed to the formation of predominant acicular ferrite (AF), at the expense of grain boundary ferrite (GBF), ferrite side plates (FSP) and martensite/austenite (M/A) constituent in weld metal. EBSD results indicated that GBF keeps K-S or N-W relations only with the prior austensite grain that belongs to one side of the grain boundary and the variants belong to the same bain group which always forms low angle boundary. Moreover, the retained austenite as one part of M/A constituent was mainly found in the weld metal with lower Ni content. It indicated that the transformation process could be promoted more completely by the increase of Ni content. The mechanism of the toughness improvement brought by Ni increasing was ascribed to the relatively uniform transformation to final microstructure, which reduces the appearance of GBF and M/A constituents.

36 MATERIALS SCIENCE↗

PDC IC Weld Failure Evaluation and Resolution

During final preparations for start of the PDCF Inner Can (IC) qualification effort, welding was performed on an automated weld system known as the PICN. During the initial weld, using a pedigree canister and plug, a weld defect was observed. The defect resulted in a hole in the sidewall of the canister, and it was observed that the plug sidewall had not been consumed. This was a new type of failure not seen during development and production of legacy Bagless Transfer Cans (FB-Line/Hanford). Therefore, a team was assembled to determine the root cause and to determine if the process could be improved. After several brain storming sessions (MS and T, R and D Engineering, PDC Project), an evaluation matrix was established to direct this effort. The matrix identified numerous activities that could be taken and then prioritized those activities. This effort was limited by both time and resources (the number of canisters and plugs available for testing was limited). A discovery process was initiated to evaluate the Vendor's IC fabrication process relative to legacy processes. There were no significant findings, however, some information regarding forging/anneal processes could not be obtained. Evaluations were conducted to compare mechanical properties of the PDC canisters relative to the legacy canisters. Some differences were identified, but mechanical properties were determined to be consistent with legacy materials. A number of process changes were also evaluated. A heat treatment procedure was established that could reduce the magnetic characteristics to levels similar to the legacy materials. An in-situ arc annealing process was developed that resulted in improved weld characteristics for test articles. Also several tack welds configurations were addressed, it was found that increasing the number of tack welds (and changing the sequence) resulted in decreased can to plug gaps and a more stable weld for test articles. Incorporating all of the process improvements for the actual can welding process, however, did not result in an improved weld geometry. Several possibilities for the lack of positive response exist, some of which are that (1) an insufficient number of test articles were welded under prototypic conditions, (2) the process was not optimized so that significant improvements were observable over the "noise", and (3) the in-situ arc anneal closed the gap down too much so the can was unable to exhaust pressure ahead of the weld. Several operational and mechanical improvements were identified. The weld clamps were changed to a design consistent with those used in the legacy operations. A helium puff operation was eliminated; it is believed that this operation was the cause of the original weld defect. Also, timing of plug mast movement was found to correspond with weld irregularities. The timing of the movement was changed to occur during weld head travel between tacks. In the end a three sequential tack weld process followed by a pulse weld at the same current and travel speed as was used for the legacy processes was suggested for use during the IC qualification effort. Relative to legacy welds, the PDC IC weld demonstrates greater fluctuation in the region of the weld located between tack welds. However, canister weld response (canister to canister) is consistent and with the aid of the optical mapping system (for targeting the cut position) is considered adequate. DR measurements and METs show the PDC IC welds to have sufficient ligament length to ensure adequate canister pressure/impact capacity and to ensure adequate stub function. The PDC welding process has not been optimized as a result of this effort. Differences remain between the legacy BTC welds and the PDC IC weld, but these differences are not sufficient to prevent resumption of the current PDC IC qualification effort. During the PDC IC qualification effort, a total of 17 cans will be welded and a variety of tests/inspections will be performed. The extensive data collected during that qualification effort should be of a sufficient population to determine if additional weld process optimization is necessary prior to production release.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Friction surfaced Stellite6 coatings

Solid state Stellite6 coatings were deposited on steel substrate by friction surfacing and compared with Stellite6 cast rod and coatings deposited by gas tungsten arc and plasma transferred arc welding processes. Friction surfaced coatings exhibited finer and uniformly distributed carbides and were characterized by the absence of solidification structure and compositional homogeneity compared to cast rod, gas tungsten arc and plasma transferred coatings. Friction surfaced coating showed relatively higher hardness. X-ray diffraction of samples showed only face centered cubic Co peaks while cold worked coating showed hexagonally close packed Co also. - Highlights: Black-Right-Pointing-Pointer Stellite6 used as coating material for friction surfacing. Black-Right-Pointing-Pointer Friction surfaced (FS) coatings compared with casting, GTA and PTA processes. Black-Right-Pointing-Pointer Finer and uniformly distributed carbides in friction surfaced coatings. Black-Right-Pointing-Pointer Absence of melting results compositional homogeneity in FS Stellite6 coatings.

36 MATERIALS SCIENCE↗

Creep Rupture Testing of Alloy 617 and A508/533 Base Metals and Weldments

The NGNP, which is an advanced HTGR concept with emphasis on both electricity and hydrogen production, involves helium as the coolant and a closed-cycle gas turbine for power generation with a core outlet/gas turbine inlet temperature of 750-1000°C. Alloy 617 is a prime candidate for VHTR structural components such as reactor internals, piping, and heat exchangers in view of its resistance to oxidation and elevated temperature strength. However, lack of adequate data on the performance of the alloy in welded condition prompted to initiate a creep test program at Argonne National Laboratory. In addition, Testing has been initiated to evaluate the creep rupture properties of the pressure vessel steel A508/533 in air and in helium environments. The program, which began in December 2009, was certified for quality assurance NQA-1 requirements during January and February 2010. Specimens were designed and fabricated during March and the tests were initiated in April 2010. During the past year, several creep tests were conducted in air on Alloy 617 base metal and weldment specimens at temperatures of 750, 850, and 950°C. Idaho National Laboratory, using gas tungsten arc welding method with Alloy 617 weld wire, fabricated the weldment specimens. Eight tests were conducted on Alloy 617 base metal specimens and nine were on Alloy 617 weldments. The creep rupture times for the base alloy and weldment tests were up to ~3900 and ~4500 h, respectively. The results showed that the creep rupture lives of weld specimens are much longer than those for the base alloy, when tested under identical test conditions. The test results also showed that the creep strain at fracture is in the range of 7-18% for weldment samples and were much lower than those for the base alloy, under similar test conditions. In general, the weldment specimens showed more of a flat or constant creep rate region than the base metal specimens. The base alloy and the weldment exhibited tertiary creep after 50-60% of the rupture life, irrespective of test temperature in the range of 750-950°C. The results showed that the stress dependence of the creep rate followed a power law for both base alloy and weldments. The data also showed that the stress exponent for creep is the same and one can infer that the same mechanism is operative in both base metal and weldments in the temperature range of the current study. SEM fractography analysis indicated that both base metal and weldment showed combined fracture modes consisting of dimple rupture and intergranular cracking. Intergranular cracking was more evident in the weldment specimens, which is consistent with the observation of lower creep ductility in the weldment than in the base metal.

08 HYDROGEN↗

Toroidal ring prevents gas ignition at vent stack outlet

Torodial ring welded to the vent stack outlet prevents static discharges which ignite combustible gases in a venting system. The ring inhibits the flow of current by removing the cause of turbulence characteristics of a sharply defined vent exit.

Spring, T. R.↗

Experimental Study of High-Velocity Projectile Impact Welding

The purpose of this study is to investigate the effect of various parameters on the welding process with high-velocity projectiles. For carrying out Impact Spot Welding tests, a single stage compressed gas gun impact test facility was used to launch flat- and conical-nosed projectiles within the velocity range from 100 to 150 m/s and performed. Different types of materials such as steel, copper, brass, and aluminum alloy were used. In the present experimental study, the steel plate with a thickness of 4 mm was considered as a back layer and the other plates made of copper, brass, and aluminum alloy were considered as front layers. Different gaps of 0.1, 0.2, and 0.5 mm were considered between the layers. The shape of the welded interface was studied by Scanning Electron Microscopy (SEM). The depth of penetration in the specimen and the kinetic energy of the projectiles were calculated. The experimental results showed that a complete bonding has occurred in the collision zone, especially in the central areas.

36 MATERIALS SCIENCE↗