At least 415 records · Page 23

1000 to 1200 K time-dependent compressive deformation of single-crystalline and polycrystalline B2 Ni-40Al

The 1000-K and 1200-K time-dependent deformation of 100-line-oriented and non-100-line-oriented single crystals of Ni-40Al (made by a modified Bridgman technique) was examined over a large range of strain rates (from 0.1 to 10 to the -7th per sec). The results were compared with those for polycrystalline Ni-40Al made by hot pressing XD synthesized powder. The results from measurements of slow-plastic-strain-rate properties of the two materials show that single crystals offer no strength advantage over polycrystalline material. Both forms were found to deform via a dislocation climb mechanism.

Whittenberger, J. D.↗

Understanding the deformation mechanisms in Ni-based superalloys with using crystal plasticity finite element method

Nl-based superalloy is considered as a good candidate due to its excellent resistance to elevated temperature deformation for long term period application. Understanding the deformation and failure mechanisms of Ni-Based superalloys is very helpful for providing design guidelines for processing Ni-based superalloys. Experimental characterization indicates that the deformation mechanisms of Ni based superalloy is strongly microstructure dependent. Besides, damage transform from the void nucleation to the macro cracks by voids growth leading to the failure of the Ni-based superalloys are also showing strong microstructure sensitivity. Therefore, this work focuses on the prediction and comprehension of the deformation and void growth behavior in Ni based superalloy at different working conditions via crystal plasticity finite element modeling and simulation. Physically based crystal plasticity frameworks were developed for newly Ni- based superalloy Haynes 282. It was found that dislocation shearing through the precipitates were acting as the main contributor to the strength of Haynes 282 at room temperature and 815°C. Our analysis of the creeping behavior of Haynes 282 exhibited that resistance of general climb replaced by the resistance induced by the deposited climb dislocation density. In addition, in the study of void growth behavior, our simulation results demonstrated that as the main loading axis perpendicular to the grain boundary (GB), voids grow more slowly on tilt GBs in bicrystals than those in single and bicrystals with twist GBs. And tilt GBs would promote the void grow into irregular shape.

36 MATERIALS SCIENCE↗

Ground Based Program for the Physical Analysis of Macromolecular Crystal Growth

During the past year we have focused on application of in situ Atomic Force Microscopy (AFM) for studies of the growth mechanisms and kinetics of crystallization for different macromolecular systems. Mechanisms of macrostep formation and their decay, which are important in understanding of defect formation, were studied on the surfaces of thaumatin, catalase, canavalin and lysozyme crystals. Experiments revealed that step bunching on crystalline surfaces occurred either due to two- or three-dimensional nucleation on the terraces of vicinal slopes or as a result of uneven step generation by complex dislocation sources. No step bunching arising from interaction of individual steps in the course of the experiment was observed. The molecular structure of the growth steps for thaumatin and lipase crystals were deduced. It was further shown that growth step advance occurs by incorporation of single protein molecules. In singular directions growth steps move by one-dimensional nucleation on step edges followed by lateral growth. One-dimensional nuclei have different sizes, less then a single unit cell, varying for different directions of step movement. There is no roughness due to thermal fluctuations, and each protein molecule which incorporated into the step remained. Growth kinetics for catalase crystals was investigated over wide supersaturation ranges. Strong directional kinetic anisotropy in the tangential step growth rates in different directions was seen. The influence of impurities on growth kinetics and cessation of macromolecular crystals was studied. Thus, for catalase, in addition to pronounced impurity effects on the kinetics of crystallization, we were also able to directly observe adsorption of some impurities. At low supersaturation we repeatedly observed filaments which formed from impurity molecules sedimenting on the surfaces. Similar filaments were observed on the surfaces of thaumatin, canavalin and STMV crystals as well, but the frequency was low compared with catalase crystallization. Cessation of growth of xylanase and lysozyme crystals was also observed and appeared to be a consequence of the formation of dense impurity adsorption layers. Attachment: "An in situ AFM investigation of catalase crystallization", "Atomic force microscopy studies of living cells: visualization of motility, division, aggregation, transformation, and apoptosis", AFM studies on mechanisms of nucleation and growth of macromolecular crystals", and "In situ atomic force microscopy studies of surface morphology, growth kinetics, defect structure and dissolution in macromolecular crystallization".

Malkin, Alexander J.↗

The effect of microgravity on protein crystal growth

Based on the results of microgravity crystallization experiments using the protein canavalin aboard four separate U.S. Space Shuttle missions, visual observations and diffraction data are presented that support the contention that protein crystals of improved quality can be obtained in a microgravity environment. With canavalin, no significant increase in resolution was noted, but an overall improvement in diffraction quality, as judged by statistical analyses of the data, was clear. This improvement in quality may be due primarily to the elimination of defects and dislocations rather than an overall enhancement of order. The mechanism for this improvement may be microgravity-stabilized depletion zones that develop around growing crystals that establish and maintain optimal growth conditions more rapidly following nucleation. Such zones would be destroyed by convective flow effects in earth's gravity.

Mcpherson, Alexander↗

First-principles calculations for understanding microstructures and mechanical properties of co-sputtered Al alloys

Recent experimental studies show that co-sputtering solutes with Al, together, can refine columnar grain size around few tens of nanometers and promote the formation and enhance the stability of planar defects such as stacking faults (SFs) and grain boundaries (GBs) in Al alloys. These crystal defects and fine columnar grains result in high strength, enhanced strain hardening and thermal stability of Al alloys. Using first-principles density-functional theory (DFT) calculations, we studied the role of eleven solutes in tailoring kinetics and energetics of adatoms and clusters on Al {111} surface, stable and unstable stacking fault energies, and kinetic energy barriers for the migration of defects. The calculations show that most solutes can effectively refine columnar grain size by decreasing the diffusivity of adatoms and surface clusters. These solutes do not necessarily decrease the stacking fault energy of Al alloys, but reduce the formation energy of faulted surface clusters and increase the energy barriers for the recovery of faulted surface clusters. Correspondingly, the formation of SFs is kinetically promoted during sputtering. Furthermore, solutes are segregated into the core of Shockley partial dislocations and play a pinning effect on SFs, SF arrays and twin boundaries, enhancing the thermal stability of these crystal defects. These findings provide insights into the design of high-strength Al alloys for high-temperature applications.

36 MATERIALS SCIENCE↗

Fractonic gauge theory of smectics

Motivated by striped correlated quantum matter, and the recently developed duality between elasticity of a two-dimensional (2D) crystal and a gauge theory, we derive a dual coupled U(1) vector gauge theory for a two-dimensional (2D) quantum smectic, where the disclination is mapped onto the fractonic charge, that we demonstrate can only move transversely to smectic layers. This smectic gauge theory dual also emerges from a gauge dual of a quantum crystal through a Higgs transition corresponding to a single flavor of its dipole condensation, an anisotropic quantum melting via dislocation proliferation. A condensation of the second flavor of dislocations a corresponds to another Higgs transition describing the smectic-to-nematic melting. We also utilize the electrostatic limit of this duality to formulate a melting of a 2D classical smectic in terms of a higher derivative sine–Gordon model, demonstrating its instability to a nematic at any nonzero temperature. Generalizing this classical duality to a 3D smectic, gives formulation of a 3D nematic-to-smectic transition in terms of an anisotropic Abelian-Higgs model.

36 MATERIALS SCIENCE↗

Data-driven modeling of dislocation mobility from atomistics using physics-informed machine learning

Dislocation mobility, which dictates the response of dislocations to an applied stress, is a fundamental property of crystalline materials that governs the evolution of plastic deformation. Traditional approaches for deriving mobility laws rely on phenomenological models of the underlying physics, whose free parameters are in turn fitted to a small number of intuition-driven atomic scale simulations under varying conditions of temperature and stress. This tedious and time-consuming approach becomes particularly cumbersome for materials with complex dependencies on stress, temperature, and local environment, such as body-centered cubic crystals (BCC) metals and alloys. In this paper, we present a novel, uncertainty quantification-driven active learning paradigm for learning dislocation mobility laws from automated high-throughput large-scale molecular dynamics simulations, using Graph Neural Networks (GNN) with a physics-informed architecture. We demonstrate that this Physics-informed Graph Neural Network (PI-GNN) framework captures the underlying physics more accurately compared to existing phenomenological mobility laws in BCC metals.

36 MATERIALS SCIENCE↗

Informed unsupervised machine learning analysis of dislocation microstructure from high-resolution differential aperture X-ray structural microscopy data

This study leverages high-resolution differential-aperture X-ray structural microscopy (DAXM) to probe the local dislocation structure in deformed 304L-stainless steel at small strain, by measuring the lattice rotation and deviatoric elastic strain with a sub-micron resolution. For a single grain in a polycrystalline specimen, the measured lattice rotation field over the measured volume exhibited a multimodal distribution while the deviatoric elastic strain showed a single-mode distribution. An unsupervised Cauchy mixture machine learning model was developed to resolve the multimodal distribution of the lattice rotation. By mapping the lattice rotation data associated with each Cauchy peak in the model back onto the measured volume, we identify contiguous regions of the crystal rotated near the average values corresponding to the peaks of the overall rotation distribution. These regions represent the grain subdivision in the microstructure. Finally, the dislocation density tensor was also computed and its norm was laid over the rotation field to detect the subgrain boundaries. This step provided a validation of the Cauchy mixture model for the analysis of the lattice rotation distribution. The current study highlights the integration of advanced X-ray microscopy techniques with data-driven analysis methods to uncover detailed microstructure scales in deformed crystals.

Machine learning; Lattice rotation; High-energy X-↗

Disorder-induced suppression of charge density wave order: STM study of Pd-intercalated ErTe 3

Pd-intercalated ErTe3 is studied as a model system to explore the effect of increasing disorder on an incommensurate two-component charge density wave (CDW). The ordering vectors of the CDW components lie along the two in-plane principal axes of the nearly tetragonal crystal structure. Using scanning tunneling microscopy (STM), we show that introducing Pd intercalants (i.e., disorder) induces CDW dislocations, which appear to be associated with each CDW component separately. Increasing Pd concentration has a stronger effect on the secondary CDW order, manifested in a higher density of dislocations, and thus increases the anisotropy (nematic character) of the CDW. Suggestive evidence of Bragg glass phases at weak disorder is also discussed.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

TEM and SEM (EBIC) investigations of silicon bicrystals

The electrical and structural properties of low and medium angle tilt grain boundaries in silicon bicrystals were studied in order to obtain insight into the mechanisms determining the recombination activity. The electrical behavior of these grain boundaries was studied with the EBIC technique. Schottky barriers rather than p-n junctions were used to avoid annealing induced changes of the structure and impurity content of the as-grown crystals. Transmission electron spectroscopy reveals that the 20 deg boundary is straight, homogeneous, and free of extrinsic dislocations. It is concluded that, in the samples studied, the electrical effect of grain boundaries appears to be independent of the boundary misorientation. The dominant influence appears to be impurity segregation effects to the boundary. Cleaner bicrystals are required to study intrinsic differences in the electrical activity of the two boundaries.

Gleichmann, R.↗

Electrical, structural and chemical characterization of Si sheet material

Web Dendritic Si ribbons are deformed under a well-defined four point bending stress. Since the mechanical properties of Si are known to depend on the 0 content of the material, 0 measurements using Fourier Transform Infrared Spectroscopy were done to determine a proper control sample of non-defected single crystal Si. Four point bending revealed a unique two step bending behavior for the Web Si ribbons. An initial theory for this behavior involves the interaction of the dislocations generated by the deformation with the central twin planes of the ribbons. Measurements showed a uniformly high 0 content for the Web Si ribbons, approximately 10 to the 18th power atoms/cu.cm. The Web samples had a much broader absorption peak at 9 microns than is usually seen for well-annealed single crystal Si. This broadening is thought to be related to stress in the Web Si ribbons. Two samples containing a known amount of residual stress support this hypothesis. Also, a shoulder on the infrared absorption peak associated with interstitial 0 in Si appears in the transmission vs. wavenumber plots for some of the Web samples. This shoulder has been associated with 0-vacancy complexes or with 0 at dislocations. The O content and configuration do not seem to correlate with the growth configuration of the Web Si ribbon.

Ast, D. G.↗

CFD Growth of 3C-SiC on 4H/6H Mesas

This article describes growth and characterization of the highest quality reproducible 3C-SiC heteroepitaxial films ever reported. By properly nucleating 3C-SiC growth on top of perfectly on-axis (0001) 4H-SiC mesa surfaces completely free of atomic scale steps and extended defects, growth of 3C-SiC mesa heterofilms completely free of extended crystal defects can be achieved. In contrast, nucleation and growth of 3C-SiC mesa heterofilms on top of 4H-SiC mesas with atomic-scale steps always results in numerous observable dislocations threading through the 3C-SiC epilayer. High-resolution X-ray diffraction and transmission electron microscopy measurements indicate non-trivial in-plane lattice mismatch between the 3C and 4H layers. This mismatch is somewhat relieved in the step-free mesa case via misfit dislocations confined to the 3C/4H interfacial region without dislocations threading into the overlying 3C-SiC layer. These results indicate that the presence or absence of steps at the 3C/4H heteroepitaxial interface critically impacts the quality, defect structure, and relaxation mechanisms of single-crystal heteroepitaxial 3C-SiC films.

Neudeck, Philip G.↗

Bridging microscale to macroscale mechanical property measurements of FeCrAl alloys by crystal plasticity modeling

FeCrAl alloys are candidates for accident tolerant fuel cladding of light water reactors. In this work, a microstructure- and temperature-dependent crystal plasticity model is employed to bridge microscale to macroscale mechanical property measurements of FeCrAl alloys. With the visco-plastic self-consistent (VPSC) polycrystal plasticity framework, a mechanism-based single crystal plasticity (MSCP) model adopts the Arrhenius type rate equation to describe the dependence of the critical resolved shear stress for dislocation slips on their temperature-dependent intrinsic frictional resistance and the microstructure-dependent irradiation hardening. The intrinsic frictional resistance associated with {110}<111> and {112}<111> slip systems were measured by in-situ micromechanical testing on unirradiated/irradiated samples at 25-500 °C. The irradiation hardening is estimated by the Bacon-Kocks-Scattergood (BKS) model with density and size of radiation-induced defects measured from microstructural characterization. Several features associated with thermo-mechanical behavior of unirradiated/irradiated polycrystalline FeCrAl alloys are captured. High density of deformation-induced dislocations and radiation-induced defects results in obvious hardening at room temperature, which is weakened at high temperature, and facilitates damage evolution during deformation. Moreover, both high temperature and radiation-induced defects, which facilitate dislocation multiplication, trigger large hardening rate. Finally, the proposed method together with application of accelerator-based ion irradiation technique is a surrogate approach to simulate neutron damage, improving the efficiency associated with evaluation of mechanical properties of FeCrAl alloys exposed to temperature, stress and radiation conditions.

36 MATERIALS SCIENCE↗

Lateral Heterostructures of Multilayer GeS and SnS van der Waals Crystals

Engineered heterostructures derive distinct properties from materials integration and interface formation. Two-dimensional crystals have been combined to form vertical stacks and lateral heterostuctures with covalent line interfaces. While thicker vertical stacks have been realized, lateral heterostructures from multilayer van der Waals crystals, which could bring the benefits of high-quality interfaces to bulk-like layered materials, have remained much less explored. In this work, we demonstrate the integration of anisotropic layered Sn and Ge monosulfides into complex heterostructures with seamless lateral interfaces and tunable vertical design using a two-step growth process. The anisotropic lattice mismatch at the lateral interfaces between GeS and SnS is relaxed via dislocations and interfacial alloying. Nanoscale optoelectronic measurements by cathodoluminescence spectroscopy show the characteristic light emission of joined high-quality van der Waals crystals. Spectroscopy across the lateral interface indicates valley-selective luminescence in the bulk SnS component that arises due to anisotropic electron transfer across the interface. The results demonstrate the ability to realize high-quality lateral heterostructures of multilayer van der Waals crystals for diverse applications, e.g., in optoelectronics or valleytronics.

36 MATERIALS SCIENCE↗

Crystallographic Orientation Dependence of Mechanical Responses of FeCrAl Micropillars

Iron-chromium-aluminum (FeCrAl) alloys are used in automobile exhaust gas purifying systems and nuclear reactors due to its superior high-temperature oxidation and excellent corrosion resistance. Single-phase FeCrAl alloys with a body centered cubic structure plastically deform through dislocation slips at room temperature. Here, we investigated the orientation dependence of mechanical responses of FeCrAl alloy through testing single-crystal and bi-crystal micropillars in a scanning electron microscopy at room temperature. Single-crystal micropillars were fabricated with specific orientations which favor the activity of single slip system or two slip systems or multiple slip systems. The strain hardening rate and flow strength increase with increasing the number of activated slip system in micropillars. Bi-crystal micropillars with respect to the continuity of slip systems across grain boundary were fabricated to study the effect of grain boundary on slip transmission. The high geometrical compatibility factor corresponds to a high flow strength and strain hardening rate. Experimental results provide insight into understanding mechanical response of FeCrAl alloy and developing the mechanisms-based constitutive laws for FeCrAl polycrystalline aggregates.

36 MATERIALS SCIENCE↗

Effect of loading path on grain misorientation and geometrically necessary dislocation density in polycrystalline aluminum under reciprocating shear

Solid phase processing (SPP) is a promising alloy fabrication technique to produce fine and homogeneous grain structures for high-performance alloys. However, there is very limited modeling capability to understand and predict the grain refinement during SPP. In this work, the crystal plasticity theory was used to study elastic-plastic deformation in polycrystalline aluminums under large shear deformation. Two approaches, kernel averaged misorientation (KAM) and grain reference orientation deviation (GROD), were used to assess the grain misorientations. The geometrically necessary dislocation (GND) density was computed with the plastic strain rate. The deformation simulations were carried out under two loading conditions to investigate the effect of loading paths on the evolutions of grain misorientation and GND density. The results show that the regions with high misorientation and GND density first appear near grain boundaries. These regions then extend toward interior grains. The loading path affects dislocation system activation and dislocation recovery, hence dislocation evolution and misorientation. In conclusion, both two- and three-dimensional simulations showed that the spatial and temporal evolutions of GROD, KAM, and GND density in are closely correlated, which indicates they all can be used as criteria of grain refinement or recrystallization.

36 MATERIALS SCIENCE↗

Nucleation and Crystallization of Globular Proteins: What we Know and What is Missing

Recently. much progress has been made in understanding the nucleation and crystallization of globular proteins, including the formation of compositional and structural crystal defects, Insight into the interactions of (screened) protein macro-ions in solution, obtained from light scattering, small angle X-ray scattering and osmotic pressure studies. can guide the search for crystallization conditions. These studies show that the nucleation of globular proteins is governed by the same principles as that of small molecules. However, failure to account for direct and indirect (hydrodynamic) protein interactions in the solutions results in unrealistic aggregation scenarios. Microscopic studies of numerous proteins reveal that crystals grow by the attachment of growth units through the same layer-spreading mechanisms as inorganic crystals. Investigations of the growth kinetics of hen-egg-white lysozyme (HEWL) reveal non-steady behavior under steady external conditions. Long-term variations in growth rates are due to changes in step-originating dislocation groups. Fluctuations on a shorter timescale reflect the non-linear dynamics of layer growth that results from the interplay between interfacial kinetics and bulk transport. Systematic gel electrophoretic analyses suggest that most HEWL crystallization studies have been performed with material containing other proteins at percent levels. Yet, sub-percent levels of protein impurities impede growth step propagation and play a role in the formation of structural/compositional inhomogeneities. In crystal growth from highly purified HEWL solutions, however, such inhomogeneities are much weaker and form only in response to unusually large changes in growth conditions. Equally important for connecting growth conditions to crystal perfection and diffraction resolution are recent advances in structural characterization through high-resolution Bragg reflection profiling and X-ray topography.

Rosenberger, F.↗

Fracture of single crystals of the nickel-base superalloy PWA 1480E in helium at 22 C

The fracture behavior and deformation of He-charged (at 22 C) single crystals of PWA 1480E Ni-base superalloy were investigated using SEM and TEM techniques to observe the behavior of tensile fractures in notched single crystals with seven different crystal growth orientations: 100-line, 110-line, 111-line, 013-line, 112-line, 123-line, and 223-line. To identify the cleavage plane orientation, a stereoscopic technique, combined with the use of planar gamma-prime morphologies, was applied. It was found that gamma-prime particles were orderly and closely aligned with edges along the 100-line, 010-line, and 001-line-oriented directions of the gamma matrix. Different crystal growth orientations were found not to affect the morphology of gamma-prime particles. The accumulation of dislocations around gamma/gamma-prime interfaces formed strong barriers to subsequent dislocation movement and was the primary strengthening mechanism at room temperature.