Touchdown dynamics

Aircraft tire wear results from operating conditions that are quite different from those encountered in land vehicles. One of the most important of these is touchdown, where the tire suddenly spins up from zero to a large angular velocity. This phenomenon is studied from both the analytical and experimental points of view. The analysis is basic, using elementary properties of the tire and wheel. It results in a new dimensionless description of the process. The experimental study consists primarily of small scale laboratory data, although limited full scale tire data is also presented. The data show increasing weight loss during touchdown as the dimensionless severity increases.

Clark, Samuel K.↗

NASA wiring for space applications program test results

The objective of this test is to examine the mechanical and electrical properties of PFPI insulation. Some of the parameters considered during the test are: AC corona (400 Hz), wire fusing time, abrasion resistance, dynamic cut through, notch propagation, and weight loss (outgassing). In addition the degradation of the samples caused by the immature manufacturing status of the PFPI materials for wiring is considered.

Ide, Jim↗

The Effects of Fiber Surface Modification and Thermal Aging on Composite Toughness and Its Measurement

A detailed experimental study was conducted to establish the structure-property relationships between elevated temperature aging and fiber-matrix bonding, Mode 2 interlaminar fracture toughness, and failure modes of carbon fiber/PMR-15 composites. The fiber-matrix adhesion was varied by using carbon fibers with different surface treatments. Short beam shear tests were used to quantify the interfacial shear strength afforded by the use of the different fiber surface treatments. The results of the short beam shear tests showed that, for times up to 1000 hr, the aging process caused no changes in the bulk of the three composite materials that would degrade the shear properties of the material. Comparisons between the interlaminar shear strengths (ILSS) measured by the short beam shear tests and the GIIC test results, as measured by the ENF test, indicated that the differences in the surface treatments significantly affected the fracture properties while the effect of the aging process was probably limited to changes at the starter crack tip. The fracture properties changed due to a shift in the fracture from an interfacial failure to a failure within the matrix when the fiber was changed from AU-4 to AS-4 or AS-4G. There appears to be an effect of the fiber/matrix bonding on the thermo-oxidative stability of the composites that were tested. The low bonding afforded by the AU 1 fiber resulted in weight losses about twice those experienced by the AS 1 reinforced composites, the ones with the best TOS.

Bowles, Kenneth J.↗

Long-Term Isothermal Aging Effects on Carbon Fabric-Reinforced PMR-15 Composites: Compression Strength

A study was conducted to determine the effects of long-term isothermal thermo-oxidative aging on the compressive properties of T-650-35 fabric reinforced PMR-15 composites. The temperatures that were studied were 204, 260, 288, 316, and 343 C. Specimens of different geometries were evaluated. Cut edge-to-surface ratios of 0.03 to 0.89 were fabricated and aged. Aging times extended to a period in excess of 15,000 hours for the lower temperature runs. The unaged and aged specimens were tested in compression in accordance with ASTM D-695. Both thin and thick (plasma) specimens were tested. Three specimens were tested at each time/temperature/geometry condition. The failure modes appeared to be initiated by fiber kinking with longitudinal, interlaminar splitting. In general, it appears that the thermo-oxidative degradation of the compression strength of the composite material may occur by both thermal (time-dependent) and oxidative (weight-loss) mechanisms. Both mechanisms appear to be specimen-thickness dependent.

Bowles, Kenneth J.↗

Synthesis of low color, atomic oxygen resistant polyimides

The purpose of this project was to develop low color, atomic oxygen resistant polyimides for potential applications on spacecraft in low earth orbit. The material is needed in order to protect satellites and spacecraft from the gases and radiation found at those altitudes. Phosphorous containing polyimides have been shown to be especially resistant to corrosion and weight loss under oxygen plasma. Unfortunately the color of these phosphorous containing polyimides is still too high for them to be good heat insulators. While they are not as effective as teflon, the current material of choice. polyimides are much less dense than teflon and would be especially valuable if they could be made with low color. The approach taken was to synthesize a monomer which would contain the elements needed for giving the final polyimide its desired properties. In particular the monomer should incorporate phosphine or phosphine oxides and have bulky side groups to block any color forming charge transfer structures. The target molecule, 3,5-di-(trifluoromethylphenyl)-bis(3-aminophenyl) phosphine oxide, (containing both a phosphine oxide group and a bulky ditrifluoromethylphenyl group) was synthesized via three reactions in overall yield of 21 percent. In addition, a model compound, bis(3-phenylamine) phenyl phosphine oxide, was synthesized two different ways in order to establish the conditions for the nitration of phosphine oxides and their reduction to the amine. Finally, a trisubstituted phosphine oxide was synthesized. In all, seven phosphorus containing organic compounds were synthesized, purified and characterized. The model compound was reacted with oxydiphthalic anhydride to form a polyamic acid with inherent viscosity of 0.34. This material was cast into a film and heated, forming a normally colored fairly strong polyimide with a Tg of 240 C. The target compound was reacted with 6-fluorodiphthalic anhydride to give a polyamic acid with inherent viscosity of 0.19 and cast to give a heavily cracked colored film with a Tg of 230 C.

MacInnes, Dave↗

Effect of KOH Concentration and Anions on the Performance of a Ni-H2 Battery Positive Plate

The capacity and voltage behavior of electrochemically impregnated sintered nickel positive plates was examined by galvanostatic charging and discharging in a flooded electrolyte cell. Three different concentrations of potassium hydroxide (KOH) (40, 31, and 26 percent) and 31 percent KOH containing dissolved nitrate, sulfate, or silicate were investigated. The end-of-charge voltage at C/10 charge and at 10 degrees C showed the following order: 40 percent KOH greater than 31 percent KOH alone and in the presence of the anions greater than 26 percent KOH. The mid discharge voltage at C/2 discharge was higher in 26 percent KOH, almost the same for 31 percent KOH with and without added contaminants, and much lower for 40 percent KOH. The plate capacity was marginally affected by cycling in all cases except for 40 percent KOH, where the capacity declined after 1,000 cycles at 80 percent depth of discharge (DOD). At the end of cycling, all the plates tested experienced a weight loss, except in the case of 31 percent KOH, as a result of active material extrusion. Cyclic voltammetry of miniature electrodes in 31 percent KOH showed that the cathodic peak potentials are less polarized in the presence and absence of silicate at -5 degrees C compared to 25 degrees C indicating a slightly higher voltage during discharge in a Ni-H2 battery. Futhermore, the features of the current-potential profile were practically unchanged in the presence of silicate.

Vaidyanathan, Hari↗

SiC Recession Due to SiO2 Scale Volatility Under Combustor Conditions

One of today's most important and challenging technological problems is the development of advanced materials and processes required to design and build a fleet of supersonic High Speed Civil Transport (HSCT) airliners, a follow-up to the Concorde SST. The innovative combustor designs required for HSCT engines will need high-temperature materials with long-term environmental stability. Higher combustor liner temperatures than today's engines and the need for lightweight materials will require the use of advanced ceramic-matrix composites (CMC's) in hot-section components. The HSCT is just one example being used to demonstrate the need for such materials. This thesis evaluates silicon carbide (SiC) as a potential base material for HSCT and other similar applications. Key issues are the environmental durability for the materials of interest. One of the leading combustor design schemes leads to an environment which will contain both oxidizing and reducing gas mixtures. The concern is that these environments may affect the stability of the silica (SiO2) scale on which SiC depends for environmental protection. A unique High Pressure Burner Rig (HPBR) was developed to simulate the combustor conditions of future gas turbine engines, and a series of tests were conducted on commercially available SiC material. These tests are intended as a feasibility study for the use of these materials in applications such as the HSCT. Linear weight loss and surface recession of the SiC is observed as a result of SiO2 volatility for both fuel-lean and fuel-rich gas mixtures. These observations are compared and agree well with thermogravimetric analysis (TGA) experiments. A strong Arrhenius-type temperature dependence exists. In addition, the secondary dependencies of pressure and gas velocity are defined. As a result, a model is developed to enable extrapolation to points outside the experimental space of the burner rig, and in particular, to potential gas turbine engine conditions.

Robinson, Raymond Craig↗

Thermal and Mechanical Durability of Graphite-Fiber-Reinforced PMR-15 Composites

Earlier work, which reported relationships between compression properties and elevated temperature aging times and weight losses, also pointed out the apparent influence of surface layer formation and growth on the retention of compression properties during extended aging times. Since that time, studies have been directed toward evaluating the growth of the surface layer. This layer was found to change in its composition and features as the aging temperature changed. Microcracks and small voids initiated and advanced inward at all temperatures. Visible oxidation at the surface occurred only at temperatures above 260 C. Relationships between layer thickness and aging time and temperature were evaluated and empirically formulated. Then, the compression properties were graphically related to the surface layer thickness with excellent correlation. The surface layer was observed to influence the compression strength of thin samples only.

Bowles, Kenneth J.↗

Comparison of Graphite Fabric Reinforced PMR-15 and Avimid N Composites After Long Term Isothermal Aging at Various Temperatures

Extensive effort is currently being expended to demonstrate the feasibility of using high-performance, polymer-matrix composites as engine structural materials over the expected operating lifetime of the aircraft, which can extend from 18,000 to 30,000 hr. The goal is to develop light-weight, high-strength, and high-modulus materials for use in higher temperature sections of advanced 21 st century aircraft propulsion systems. To accomplish this goal, it is necessary to pursue the development of thermal and mechanical durability models for graphite-fiber-reinforced, polymer-matrix composites. Numerous investigations have been reported regarding the thermo-oxidative stability (TOS) of the polyimide PMR-15 (1-5). A significant amount of this work has been directed at edge and geometry effects, reinforcement fiber influences, and empirical modeling of high-temperature weight loss behavior. It is yet to be determined if the information obtained from the PMR-15 composite tests is applicable to other polyimide-matrix composites. The condensation-curing polymer Avimid N is another advanced composite material often considered for structural applications at high temperatures. Avimid N has better thermo-oxidative stability than PMR-15 (6), but the latter is more easily processed. The most comprehensive study of the thermo-oxidative stability of Avimid N neat resin and composites at 371 (infinity)C is found in Salin and Seferis (7). The purposes of the work described herein were to compare the thermal aging behavior of these two matrix polymers and to determine the reasons for and the consequences of the difference in thermal durability. These results might be of some use in improving future polymer development through the incorporation of the desirable characteristics of both polyimides.

Bowles, Kenneth J.↗

Thermal and Mechanical Durability of Graphite-Fiber-Reinforced PMR-15 Composites

Earlier work, which reported relationships between compression properties and elevated temperature aging times and weight losses, also pointed out the apparent influence of surface layer formation and growth on the retention of compression properties during extended aging times. Since that time, studies have been directed toward evaluating the growth of the surface layer. This layer was found to change in its composition and features as the aging temperature changed. Microcracks and small voids initiated and advanced inward at all temperatures. Visible oxidation at the surface occurred only at temperatures above 260 deg. C. Relationships between layer thickness and aging time and temperature were evaluated and empirically formulated. Then, the compression properties were graphically related to the surface layer thickness with excellent correlation. The surface layer was observed to influence the compression strength of thin samples only.

Bowles, Kenneth J.↗

Oxidative Attack of Carbon/Carbon Substrates through Coating Pinholes

A critical issue with oxidation protected carbon/carbon composites used for spacecraft thermal protection is the formation of coating pinholes. In laboratory experiments, artificial pinholes were drilled through SiC-coatings on a carbon/carbon material and the material was oxidized at 600, 1000, and 1400 C at reduced pressures of air. The attack of the carbon/carbon was quantified by both weight loss and a novel cross-sectioning technique. A two-zone, one dimensional diffusion control model was adapted to analyze this problem. Agreement of the model with experiment was reasonable at 1000 and 1400 C; however results at lower temperatures show clear deviations from the theory suggesting that surface reaction control plays a role.

Jacobson, Nathan S.↗

Dimensionally Stable Poyimide Copolymers for Microelectronics Applications

Polyimides are finding increased applications in microelectronics due to their high thermal stability, good chemical resistance, good adhesion, low moisture absorption, good mechanical properties, and low coefficient of thermal expansion (CTE). Four series of random copolyimides were synthesized and characterized for potential application as encapsulants, stress-relief layers, and interlevel dielectrics. Several candidates exhibited good combinations of physical and mechanical properties with inherent viscosities from 1.21 to 1.42 dL/g, T(sub g)'s ranging from 251 to 277 C, 10% weight loss temperatures between 503 and 527 C, and CTEs ranging from 33 to 39 ppm/deg C. Mechanical properties at room temperature for the best candidates included tensile strengths of 17.8-21.3 ksi, moduli between 388 and 506 ksi, and elongations of 11-43%. Moisture absorption for these copolyimides ranged between 0.85 and 1.38 wt %.

Fay, Catherine C.↗

Evaluation of an Anaerobic Digestion System for Processing CELSS Crop Residues for Resource Recovery

Three bioreactors, connected in series, were used to process CELSS potato residues for recovery of resources. The first stage was an anaerobic digestor (8 L working volume; cow rumen contents inoculum; fed-batch; 8 day retention time; feed rate 25 gdw/day) that converted 33% of feed (dry weight loss) to CO2 and "volatile fatty acids" (vfa, 83:8:8 mmolar ratio acetic:propionic:butyric). High nitrate-N in the potato residue feed was absent in the anaerobic effluent, with a high portion converted to NH4(+)-N and the remainder unaccounted and probably lost to denitrification and NH4(+) volatilization. Liquid anaerobic effluent was fed to an aerobic, yeast biomass production vessel (2 L volume; Candida ingens inoculum; batch [pellicle] growth; 2 day retention time) where the VFAs and some NH4(+)-N were converted into yeast biomass. Yeast yields accounted for up to 8% of potato residue fed into the anaerobic bioreactor. The third bioreactor (0.5 L liquid working volume; commercial nitrifier inoculum; packed-bed biofilm; continuous yeast effluent feed; recirculating; constant volume; 2 day hydraulic retention time) was used to convert successfully the remaining NH4(+)-N into nitrate-N (preferred form of N for CELSS crop production) and to remove the remaining degradable soluble organic carbon. Effluents from the last two stages were used for partial replenishment of minerals for hydroponic potato production.

Strayer, R. F.↗

Effects of Bioreactor Retention Time on Aerobic Microbial Decomposition of CELSS Crop Residues

The focus of resource recovery research at the KSC-CELSS Breadboard Project has been the evaluation of microbiologically mediated biodegradation of crop residues by manipulation of bioreactor process and environmental variables. We will present results from over 3 years of studies that used laboratory- and breadboard-scale (8 and 120 L working volumes, respectively) aerobic, fed-batch, continuous stirred tank reactors (CSTR) for recovery of carbon and minerals from breadboard grown wheat and white potato residues. The paper will focus on the effects of a key process variable, bioreactor retention time, on response variables indicative of bioreactor performance. The goal is to determine the shortest retention time that is feasible for processing CELSS crop residues, thereby reducing bioreactor volume and weight requirements. Pushing the lower limits of bioreactor retention times will provide useful data for engineers who need to compare biological and physicochemical components. Bioreactor retention times were manipulated to range between 0.25 and 48 days. Results indicate that increases in retention time lead to a 4-fold increase in crop residue biodegradation, as measured by both dry weight losses and CO2 production. A similar overall trend was also observed for crop residue fiber (cellulose and hemicellulose), with a noticeable jump in cellulose degradation between the 5.3 day and 10.7 day retention times. Water-soluble organic compounds (measured as soluble TOC) were appreciably reduced by more than 4-fold at all retention times tested. Results from a study of even shorter retention times (down to 0.25 days), in progress, will also be presented.

Strayer, R. F.↗

Long Term Degradation of Polyimide Composites

The durability of polymer matrix composites exposed to harsh environments is a major concern. Surface degradation and damage are observed in polyimide composites used in air at 125-300 C. It is believed that diffusion of oxygen into the material and oxidative chemical reactions are responsible. Previous work has characterized and modeled diffusion behavior, and thermogravimetric analyses (TGAS) have been carried out in nitrogen, air, and oxygen to provide quantitative information on thermal and oxidative reactions. However, the model developed using these data did not successfully extrapolate TGA data down to conditions seen in service. A test program that focuses on lower temperatures and makes use of isothermal tests was undertaken to achieve a better understanding of the degradation reactions under use conditions. A new, low-cost technique was developed to collect chemical degradation data for isothermal tests lasting over 200 hours in the temperature range 125-300 C. Results indicate complex behavior not captured by the previous model, including the presence of weight-adding reactions. Weight gain reactions dominated in the 125-225 C temperature range, while weight loss reactions dominated beyond 225 C. The data obtained from isothermal tests and earlier TGAs is used to develop an advanced model of the material behavior.

Patekar, Kaustubh A.↗

Granular Superconductors and Gravity

As a Bose condensate, superconductors provide novel conditions for revisiting previously proposed couplings between electromagnetism and gravity. Strong variations in Cooper pair density, large conductivity and low magnetic permeability define superconductive and degenerate condensates without the traditional density limits imposed by the Fermi energy (approx. 10(exp -6) g cu cm). Recent experiments have reported anomalous weight loss for a test mass suspended above a rotating Type II, YBCO superconductor, with a relatively high percentage change (0.05-2.1%) independent of the test mass' chemical composition and diamagnetic properties. A variation of 5 parts per 104 was reported above a stationary (non-rotating) superconductor. In experiments using a sensitive gravimeter, bulk YBCO superconductors were stably levitated in a DC magnetic field and exposed without levitation to low-field strength AC magnetic fields. Changes in observed gravity signals were measured to be less than 2 parts in 108 of the normal gravitational acceleration. Given the high sensitivity of the test, future work will examine variants on the basic magnetic behavior of granular superconductors, with particular focus on quantifying their proposed importance to gravity.

Noever, David↗

Static Test for a Gravitational Force Coupled to Type 2 YBCO Superconductors

As a Bose condensate, superconductors provide novel conditions for revisiting previously proposed couplings between electromagnetism and gravity. Strong variations in Cooper pair density, large conductivity and low magnetic permeability define superconductive and degenerate condensates without the traditional density limits imposed by the Fermi energy (approx. 10(exp -6) g cc. Recent experiments have reported anomalous weight loss for a test mass suspended above a rotating type II, YBCO superconductor, with the percentage change (0.05 - 2.1 %) independent of the test mass' chemical composition and diamagnetic properties. A variation of 5 parts per 10' was reported above a stationary (non-rotating) superconductor. In experiments using a sensitive gravimeter, bulk YBCO superconductors were stably levitated in a DC magnetic field. Changes in acceleration were measured to be less than 2 parts in 108 of the normal gravitational acceleration. This result puts new limits on the strength and range of the proposed coupling between static superconductors and gravity.

Li, Ning↗

Long-Term Cyclic Oxidation Behavior of Uncoated and Coated Re-108 and In-939 at 980 and 870 C

Very long-term cyclic oxidation behavior of Re-108 and ln-939 with and without a protective coating was evaluated at 980 and 870 C, respectively. Re-108 and ln-939 without a protective coating began to show rapid weight loss at 3000 h due to scale spallation, indicating the need for an oxidation protective coating for longer than thousands of hours of oxidative life. NiAl-base coatings of a vapor phase aluminide (VPA), a pack aluminide (CODEP), and a slurry paint aluminide (SERMALOY J) were applied on Re-108 and ln-939. VPA and CODEP on Re-108 and all three coatings on ln-939 showed excellent cyclic oxidation resistance out to 10000 hr. Coated alloys were annealed in an inert atmosphere to determine the loss of Al from the coating into the alloy substrate through diffusion. The Al loss from the coating through diffusion was twice as great as the Al loss through oxidation after 10000 h of cyclic exposure. Oxidation life of VPA-coated Re-108 was estimated by calculating the amount of Al initially available for protective oxidation and the amount of Al lost through oxidation and diffusion.

Lee, K. N.↗