Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “phase transformations”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 397 records · Page 22

Titanium α-ω phase transformation pathway and a predicted metastable structure

A titanium is a highly utilized metal for structural lightweighting and its phases, transformation pathways (transition states), and structures have scientific and industrial importance. Using a proper solid-state nudged elastic band method employing two climbing images combined with density functional theory DFT + U methods for accurate energetics, we detail the pressure-induced α (ductile) to ω (brittle) transformation at the coexistence pressure. We also find two transition states along the minimal-enthalpy path and discover a metastable body-centered orthorhombic structure, with stable phonons, a lower density than the end-point phases, and decreasing stability with increasing pressure.

72 PHYSICS OF ELEMENTARY PARTICLES AND FIELDS↗

Magnetic field-induced phase transformation in NiMnCoIn magnetic shape memory alloys - a new actuation mechanism with large work output.

Magnetic shape memory alloys (MSMAs) have recently been developed into a new class of functional materials that are capable of magnetic-field-induced actuation, mechanical sensing, magnetic refrigeration, and energy harvesting. In the present work, the magnetic field-induced martensitic phase transformation (FIPT) in Ni{sub 45}Mn{sub 36.5}Co{sub 5}In{sub 13.5} MSMA single crystals is characterized as a new actuation mechanism with potential to result in ultra-high actuation work outputs. The effects of the applied magnetic field on the transformation temperatures, magnetization, and superelastic response are investigated. The magnetic work output of NiMnCoIn alloys is determined to be more than 1 MJ m{sup -3} per Tesla, which is one order of magnitude higher than that of the most well-known MSMAs, i.e., NiMnGa alloys. In addition, the work output of NiMnCoIn alloys is orientation independent, potentially surpassing the need for single crystals, and not limited by a saturation magnetic field, as opposed to NiMnGa MSMAs. Experimental and theoretical transformation strains and magnetostress levels are determined as a function of crystal orientation. It is found that [111]-oriented crystals can demonstrate a magnetostress level of 140 MPa T{sup -1} with 1.2% axial strain under compression. These field-induced stress and strain levels are significantly higher than those from existing piezoelectric and magnetostrictive actuators. A thermodynamical framework is introduced to comprehend the magnetic energy contributions during FIPT. The present work reveals that the magnetic FIPT mechanism is promising for magnetic actuation applications and provides new opportunities for applications requiring high actuation work-outputs with relatively large actuation frequencies. One potential issue is the requirement for relatively high critical magnetic fields and field intervals (1.5-3 T) for the onset of FIPT and for reversible FIPT, respectively.

36 MATERIALS SCIENCE↗

Dual phase transformation and resultant magnetic properties in Fe{sub 3}Pt thin films

Fifty-nm-thick Fe{sub 75}Pt{sub 25} thin films have been made on glass substrates by rf magnetron sputtering at room temperature, and subsequently annealed at 300 -700 deg. C (T{sub a}) for 1 h. The as-deposited Fe{sub 3}Pt film exhibits high magnetization of 1530 emu/cm{sup 3} and a disordered bcc structure, confirmed by high-resolution synchrotron radiation x-ray diffractometry. First-phase transformation from the bcc to disorder fcc structure occurs for samples annealed at 300 deg. C. With increasing of T{sub a} up to 375 deg. C, the film displays a nearly disordered fcc phase with low magnetization of 1083 emu/cm{sup 3}. The fcc phase changes to ordered L1{sub 2} structure for samples with T{sub a} {>=} 400 deg. C. The highly ordered L1{sub 2} phase with magnetization of 1270 emu/cm{sup 3} and coercivity of 66 Oe was obtained in Fe{sub 3}Pt film at 700 deg. C-annealing.

36 MATERIALS SCIENCE↗

Intergranular precipitation-enhanced wetting and phase transformation in an Al0.4CoCrFeNi high-entropy alloy exposed to lead-bismuth eutectic

We report after exposure to oxygen-poor (10 -13 –10 -14 wt%) liquid lead-bismuth eutectic (LBE) at 500 °C for 500 h, LBE penetrates more than one order of magnitude deeper in an FCC Al 0.4 CoCrFeNi high-entropy alloy (HEA) decorated with a network of BCC (Ni, Al)-rich intergranular (IG) precipitates than in a single-phase, FCC Al 0.3 CoCrFeNi HEA without the IG precipitate network. This deterioration of corrosion resistance is attributed to the energetic nature of the BCC/FCC interphase boundaries (IBs) and resultant IB wetting. The LBE ingress film selectively leaches nickel located at those low-indexed crystalline planes, resulting in phase transformation from FCC to BCC structure.

36 MATERIALS SCIENCE↗

Phase transformations and thermal expansion coefficients of unirradiated U-X wt.% Zr (X = 6, 10, 20, 30) measured via neutron diffraction

This work characterizes the crystallographic evolution of unirradiated U-X wt.% Zr (X = 6, 10, 20, 30) while cooling from equilibration, single phase γ-U-Zr, at 900 °C to ambient temperature using time-of-flight neutron diffraction. The β-U phase was unobserved during cooling at 1 °C/min in all alloys. All alloys followed the phase transformation pathway of γ-U-Zr→γ-U-Zr+α-U→α-U +δ-UZr2 with an observed miscibility gap in γ-U-Zr. The α-U and δ-UZr2 transformation took place simultaneously in the U-30 wt.% Zr sample. These findings strengthen the need to re-approach the U-Zr phase diagram in entirety. Bulk volumetric CTEs agree well with published data, strengthening the quantification of lattice-specific CTEs reported in this study. A compositionally dependent discontinuity in thermal expansion, increasing in magnitude with decreasing U content, occurs during the γ-U-Zr→α-U+δ-UZr2 transformation. The γ-U-Zr lattice parameter was measured to have a compositional dependency.

36 MATERIALS SCIENCE↗

Thermomechanical Analysis of A-TIG and MP-TIG Welding of 2.25Cr-1Mo Steel Considering Phase Transformation

In the present study, a finite element-based 3D mesh model is used to simulate the effect of welding processes on the temperature distribution, residual stress and distortion in 11-mm-thick 2.25Cr-1Mo steel weld joints. Tungsten inert gas (TIG) and activated-TIG (A-TIG) welding processes were employed for the fabrication of weld joints. Austenite-to-bainite phase transformation is taken into account in the numerical analysis. The heat input fitting tool has been used to calibrate the heat source by matching the simulated weld bead with that of the actual weld bead. Peak temperature was higher at the weld center for A-TIG weld joint, and the weld joint exhibited a sharp temperature gradient at the weld interface. There was good agreement between the predicted and measured thermal cycles. A-TIG and multipass-TIG (MP-TIG) weld joints exhibited similar longitudinal residual stresses in heat affected zone with a difference of 50 MPa. Moreover, A-TIG weld joint fabricated by double-side welding technique employing two passes exhibited reduced distortion than MP-TIG weld joints. A higher magnitude of distortion was in MP-TIG weld joint which was attributed to more weld metal volume caused by more number of weld passes required to fill the V-groove. There was good agreement between the predicted and measured residual stress and distortion values.

36 MATERIALS SCIENCE↗

ε- and β-LiVOPO 4 : Phase Transformation and Electrochemistry

In this paper, ε- and β-LiVOPO 4 were synthesized from the same precursor at different temperatures in an air atmosphere. ε-LiVOPO 4 is obtained at 400 and 700 °C. The 700 °C sample has better purity and crystallinity, but the 400 °C sample has a little better electrochemical performance due to its smaller particle size and the conducting carbon residue in the sample. β-LiVOPO 4 is formed between the above two temperatures, which gives slightly lower capacity than that of the ε-LiVOPO 4 sample, indicating higher kinetics of the lithium reaction for the ε phase than those of the β one. The phase transformation from ε to β then back reversibly to ε was also observed by ex situ X-ray diffraction. Finally, this thermal study verifies that ε-LiVOPO 4 is the more stable phase for LiVOPO 4 ; however, reaction kinetics control the phases formed at lower temperatures.

25 ENERGY STORAGE↗

TEM study of the martensitic phases in the ductile DyCu and YCu intermetallic compounds [The martensitic phase transformation in ductile DyCu and YCu intermetallic compounds]

DyCu and YCu are representatives of the family of CsCl-type B2 rare earth intermetallic compounds that exhibit high room temperature ductility. Structure, orientation relationship, and morphology of the martensites in the equiatomic compounds DyCu and YCu are examined using transmission electron microscopy (TEM). TEM studies show that the martensite structures in DyCu and YCu alloys are virtually identical. The martensite is of orthorhombic CrB-type B33 structure with lattice parameters a = 0.38 nm, b = 1.22 nm, and c = 0.40 nm. (021¯) twins were observed in the B33 DyCu and YCu martensites. The orientation relationship of B33 and B2 phases is (111¯)[112]B33 || (110)[001]B2. The simulated electron diffraction patterns of the B33 phase are consistent with those of experimental observations. TEM investigations also reveal that a dominant orthorhombic FeB-type B27 martensite with lattice parameters a = 0.71 nm, b = 0.45 nm, and c = 0.54 nm exists in YCu alloy. (11¯ 1) twins were observed in the B27 YCu martensite. As a result, the formation mechanism of B2 to B33 and B2 to B27 phase transformation is discussed.

36 MATERIALS SCIENCE↗

Mesocrystalline Ordering and Phase Transformation of Iron Oxide Biominerals in the Ultrahard Teeth of Cryptochiton stelleri

Biological organisms naturally synthesize complex, hierarchical, multifunctional materials through mineralization processes at ambient conditions and under physiological pH. One such example is the ultrahard and wear-resistant radular teeth found in mollusks, which are used to scape against the rock to feed on algae. Herein, the biologically controlled structural development of the hard, outer magnetite-containing shell of the chitin teeth is revealed. Specifically, the formation of a series of mesocrystalline iron oxide phases, templated by chitin-binding proteins, is identified. The initial domains, consisting of ferrihydrite mesocrystals with a spherulite-like morphology, undergo a solid-state phase transformation to form magnetite while maintaining mesocrystallinity, likely via a shear-induced solid-state reaction, without any noticeable architectural changes. Subsequent growth via Ostwald ripening leads to nearly single-crystalline rod-like elements. In addition, an interpenetrating organic matrix is identified that, at early stages of tooth development, potentially contains iron-binding proteins that guide the self-assembly of the mesocrystalline mineral and influence the preferred orientation of the later-formed magnetite nanorods, which ultimately determines the mechanical behavior of the mature chiton teeth.

36 MATERIALS SCIENCE↗

The study of aluminum loss and consequent phase transformation in heat-treated acid-leached kaolin

This study investigates the effect of Al leaching during Fe removal from kaolin to mullite. Heat-treated kaolin was obtained by heating natural kaolin at 400, 500, 600, 700, 800 and 900 deg. C. The heat-treated kaolin was then leached at 100 deg. C with 4 M, 3 M, 2 M, 1 M, 0.2 M solution of H{sub 2}SO{sub 4} and 0.2 M solution of oxalic acid. The dried samples were sintered to 1300 deg. C for 4 h at a heating rate of 10 deg. C min{sup -1}. X-ray diffractometry and differential thermal analysis were used to study the phase transformation of kaolin to mullite. It was found that 700 deg. C is the optimum preheat-treatment temperature to leach out Fe and also Al for both types of the acids used. The majority of the 4 M sulfuric acid-treated kaolins formed the cristobalite phase when sintered. On the other hand, 1 M, 0.2 M sulfuric acid and 0.2 M oxalic acid leached heat-treated kaolin formed mullite and quartz phase after sintering. - Research Highlights: {yields} Preheat-treatment of kaolin improves the leachability of unwanted iron. {yields} The optimum preheat-treatment temperature is 700 deg. C. {yields} Sintered 4 M sulfuric acid-treated kaolin majorly formed the cristobalite phase. {yields} Sintered 0.2 M oxalic acid-treated kaolin formed lesser amorphous silicate phase.

36 MATERIALS SCIENCE↗

Revealing the Structural Evolution and Phase Transformation of O3-Type NaNi 1/3 Fe 1/3 Mn 1/3 O 2 Cathode Material on Sintering and Cycling Processes

O-type layered oxide cathode materials can be easily synthesized for a full sodium stoichiometry with high specific capacity, but they all suffer from a capacity fade on cycling. The sintering process control and optimization are critical to ensure a high quality and consistency of the prepared cathode materials with stable structure. Herein, in situ high-energy X-ray diffraction (HEXRD) was first employed to investigate the phase evolution of the oxides during the sintering process of O3-type NaNi 1/3 Fe 1/3 Mn 1/3 O 2 . The in situ HEXRD and both operando Bragg coherent diffraction (BCXD) and coherent multicrystal diffraction (CMCD) were utilized to investigate the phase transformation of the cathode materials during the sodiation/desodiation process. A composite structure comprised of O-type and P-type oxides was formed after the initial electrochemical activation of the cathode material, resulting in good structural and electrochemical stability. This finding implies that strain engineering can be a new design philosophy for the development of next generation high-performance sodium ion cathodes.

25 ENERGY STORAGE↗

Anomalous Size-Induced Crystalline to Amorphous Uphill Phase Transformation of Hydroxyapatite Nanoparticles

The objective of the present paper was to produce nanoscale hydroxyapatite at room temperature under 10 nm through a simple method that requires no specialized equipment, surfactants, or additives. The Ca(C2H3O2)2-K3PO4-H2O synthesis system explored in previous literature was employed and the nanoscale powder product completely characterized through x-ray diffraction, transmission electron microscopy, BET nitrogen surface area adsorption, helium pycnometry, TGA and Karl Fisher titration. In accordance with other materials, it was found that hydroxyapatite under 5 nm produced by this chemistry undergoes an uphill phase transformation when left in dry storage over 5 months. Although it is possible to produce hydroxyapatite (and other materials) in this size range, it is imperative that care is taken through storage alterations to prevent any undesirable changes in structure or surface chemistry

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

In situ high-energy synchrotron radiation study of boehmite formation, growth, and phase transformation to alumina in sub- and supercritical water.

Boehmite (AlOOH) nanoparticles have been synthesized in subcritical (300 bar, 350 C) and supercritical (300 bar, 400 C) water. The formation and growth of AlOOH nanoparticles were studied in situ by small- and wide-angle X-ray scattering (SAXS and WAXS) using 80 keV synchrotron radiation. The SAXS/WAXS data were measured simultaneously with a time resolution greater than 10 s and revealed the initial nucleation of amorphous particles takes place within 10 s with subsequent crystallization after 30 s. No diffraction signals were observed from Al(OH){sub 3} within the time resolution of the experiment, which shows that the dehydration step of the reaction is fast and the hydrolysis step rate-determining. The sizes of the crystalline particles were determined as a function of time. The overall size evolution patterns are similar in sub- and supercritical water, but the growth is faster and the final particle size larger under supercritical conditions. After approximately 5 min, the rate of particle growth decreases in both sub- and supercritical water. Heating of the boehmite nanoparticle suspension allowed an in situ X-ray investigation of the phase transformation of boehmite to aluminium oxide. Under the wet conditions used in this work, the transition starts at 530 C and gives a two-phase product of hydrated and non-hydrated aluminium oxide.

38 RADIATION CHEMISTRY, RADIOCHEMISTRY, AND NUCLEA↗

Effects of Heating and Quenching Processing Parameters on Phase Transformation of 55CrMo Steel

Microstructure and mechanical properties after induction hardening have a significant effect on the wear resistance performance and lifetime of 55CrMo steel ball screw. In the paper, the dilatometric curves were recorded at the different heating rate by a Gleeble-1500D thermo-mechanical simulator to determine the effect of heating rate on the austenitizing temperature of 55CrMo steel. Heat treatment of some specimens was performed by the Gleeble-1500D thermal simulator at the different heating temperature, holding time and cooling rate to investigate the effect of induction hardening parameters on the phase transformation, microstructure and microhardness of 55CrMo steel. Microstructure of specimen was analyzed using an optical microscope and a scanning electron microscope. Volume fraction of retained austenite was measured using an x-ray diffractometer. The mechanical properties were evaluated by a microhardness tester. The results show that the austenitizing temperature of 55CrMo steel increases with the increasing heating rate. Increasing the heating temperature, holding time and cooling rate of specimen is helpful in obtaining a uniform cryptocrystalline martensite. Volume fraction of retained austenite is less as the heating temperature is in the range of 900-950 °C. In the induction hardening of 55CrMo steel, the heating temperature should be in the range of 900-1000 °C.

36 MATERIALS SCIENCE↗

Combinatorial Synthesis and High-Throughput Characterization of Microstructure and Phase Transformation in Ni–Ti–Cu–V Quaternary Thin-Film Library

Ni–Ti–based shape memory alloys (SMAs) have found widespread use in the last 70 years, but improving their functional stability remains a key quest for more robust and advanced applications. Named for their ability to retain their processed shape as a result of a reversible martensitic transformation, SMAs are highly sensitive to compositional variations. Alloying with ternary and quaternary elements to fine-tune the lattice parameters and the thermal hysteresis of an SMA, therefore, becomes a challenge in materials exploration. Combinatorial materials science allows streamlining of the synthesis process and data management from multiple characterization techniques. In this study, a composition spread of Ni–Ti–Cu–V thin-film library was synthesized by magnetron co-sputtering on a thermally oxidized Si wafer. Composition-dependent phase transformation temperature and microstructure were investigated and determined using high-throughput wavelength dispersive spectroscopy, synchrotron X-ray diffraction, and temperature-dependent resistance measurements. Of the 177 compositions in the materials library, 32 were observed to have shape memory effect, of which five had zero or near-zero thermal hysteresis. These compositions provide flexibility in the operating temperature regimes that they can be used in. A phase map for the quaternary system and correlations of functional properties are discussed with respect to the local microstructure and composition of the thin-film library.

42 ENGINEERING↗

Controlled synthesis of crystalline calcium carbonate aggregates with unusual morphologies involving the phase transformation from amorphous calcium carbonate

Peanut-shaped CaCO{sub 3} aggregates, featured of two dandelion-like heads built up from rod-like subunits, have been synthesized via a facile precipitation reaction between Na{sub 2}CO{sub 3} and CaCl{sub 2} at ambient temperature in the presence of magnesium ions and ethanol solvent. The as-prepared products were characterized by X-ray diffraction (XRD), scanning electron microscopy (SEM) and inductively coupled plasma atomic emission spectrometry (ICP-AES). The results show that a high magnesium concentration and ethanol solvent are necessary for the formation of the unusual peanut-like aggregates. In addition, a multistep phase transformation process from amorphous calcium carbonate (ACC) to a mixture of ACC and calcite and ultimately to calcite and aragonite was observed in the formation process of the unusual structures. A possible mechanism for the formation of the unusual peanut-shape aggregates has been proposed and discussed.

36 MATERIALS SCIENCE↗

Self-assembly of tin wires via phase transformation of heteroepitaxial germanium-tin on germanium substrate

This work demonstrates and describes for the first time an unusual strain-relaxation mechanism by the formation and self-assembly of well-ordered tin wires during the thermal annealing of epitaxial Ge{sub 0.83}Sn{sub 0.17}-on-Ge(001) substrate. Fully strained germanium-tin alloys (Ge{sub 0.83}Sn{sub 0.17}) were epitaxially grown on Ge(001) substrate by molecular beam epitaxy. The morphological and compositional evolution of Ge{sub 0.83}Sn{sub 0.17} during thermal annealing is studied by atomic force microscopy, X-ray diffraction, transmission electron microscopy. Under certain annealing conditions, the Ge{sub 0.83}Sn{sub 0.17} layer decomposes into two stable phases, and well-defined Sn wires that are preferentially oriented along two orthogonal 〈100〉 azimuths are formed. The formation of the Sn wires is related to the annealing temperature and the Ge{sub 0.83}Sn{sub 0.17} thickness, and can be explained by the nucleation of a grain with Sn islands on the outer front, followed by grain boundary migration. The Sn wire formation process is found to be thermally activated, and an activation enthalpy (E{sub c}) of 0.41 eV is extracted. This thermally activated phase transformation, i.e., 2D epitaxial layer to 3D wires, occurs via a mechanism akin to “cellular precipitation.” This synthesis route of Sn wires opens new possibilities for creation of nanoscale patterns at high-throughput without the need for lithography.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Perovskite phase transformation in 0.65Pb(Mg{sub 1/3}Nb{sub 2/3})O{sub 3}-0.35PbTiO{sub 3} nanoparticles derived by sol-gel

Fabrication of 0.65Pb(Mg{sub 1/3}Nb{sub 2/3})O{sub 3}-0.35PbTiO{sub 3} (PMN-PT) nanoparticles with an average size of about 40 nm and their phase transformation behavior from pyrochlore to perovskite phase is investigated. A novel sol-gel method was used for the synthesis of air-stable and precipitate-free diol-based sol of PMN-PT which was dried and partially calcined at 450 deg. C for 1 h to decompose organics and bring down the free energy barrier for perovskite crystallization and then finally annealed in the temperature range 600 to 700 deg. C. Annealed at around 700 deg. C for 1 h, PMN-PT gel powder exhibited nanocrystalline morphology with perovskite phase as confirmed by the transmission electron microscopy and X-ray diffraction techniques.

36 MATERIALS SCIENCE↗