Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “elastomers”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 397 records · Page 22

Space Environment Effects on Silicone Seal Materials

A docking system is being developed by the NASA to support future space missions. It is expected to use redundant elastomer seals to help contain cabin air during dockings between two spacecraft. The sealing surfaces are exposed to the space environment when vehicles are not docked. In space, the seals will be exposed to temperatures between 125 to -75 C, vacuum, atomic oxygen, particle and ultraviolet radiation, and micrometeoroid and orbital debris (MMOD). Silicone rubber is the only class of space flight-qualified elastomeric seal material that functions across the expected temperature range. NASA Glenn has tested three silicone elastomers for such seal applications: two provided by Parker (S0899-50 and S0383-70) and one from Esterline (ELA-SA-401). The effects of atomic oxygen (AO), UV and electron particle radiation, and vacuum on the properties of these three elastomers were examined. Critical seal properties such as leakage, adhesion, and compression set were measured before and after simulated space exposures. The S0899-50 silicone was determined to be inadequate for extended space seal applications due to high adhesion and intolerance to UV, but both S0383-70 and ELA-SA-401 seals were adequate.

deGroh, Henry C., III↗

An Experimental Investigation of Silicone-to-Metal Bond Strength in Composite Space Docking System Seals

The National Aeronautics and Space Administration (NASA) is currently developing a new universal docking mechanism for future space exploration missions called the Low Impact Docking System (LIDS). A candidate LIDS main interface seal design is a composite assembly of silicone elastomer seals vacuum molded into grooves in an electroless nickel plated aluminum retainer. The strength of the silicone-tometal bond is a critical consideration for the new system, especially due to the presence of small areas of disbond created during the molding process. In the work presented herein, seal-to-retainer bonds of subscale seal specimens with different sizes of intentional disbond were destructively tensile tested. Nominal specimens without intentional disbonds were also tested. Tension was applied either uniformly on the entire seal circumference or locally in one short circumferential length. Bond failure due to uniform tension produced a wide scatter of observable failure modes and measured load-displacement behaviors. Although the preferable failure mode for the seal-to-retainer bond is cohesive failure of the elastomer material, the dominant observed failure mode under the uniform loading condition was found to be the less desirable adhesive failure of the bond in question. The uniform tension case results did not show a correlation between disbond size and bond strength. Localized tension was found to produce failure either as immediate tearing of the elastomer material outside the bond region or as complete peel-out of the seal in one piece. The obtained results represent a valuable benchmark for comparison in the future between adhesion loads under various separation conditions and composite seal bond strength.

Gaier, James R.↗

Force and deflection sensor with shell membrane and optical gratings and method of manufacture

A sensor for force is formed from an elastomeric cylinder having a region with apertures. The apertures have passageways formed between them, and an optical fiber is introduced into these passageways, where the optical fiber has a grating for measurement of tension positioned in the passageways between apertures. Optionally, a temperature measurement sensor is placed in or around the elastomer for temperature correction, and if required, a copper film may be deposited in the elastomer for reduced sensitivity to spot temperature variations in the elastomer near the sensors.

Park, Yong-Lae↗

Process for manufacturing shell membrane force and deflection sensor

A sensor for force is formed from an elastomeric cylinder having a region with apertures. The apertures have passageways formed between them, and an optical fiber is introduced into these passageways, where the optical fiber has a grating for measurement of tension positioned in the passageways between apertures. Optionally, a temperature measurement sensor is placed in or around the elastomer for temperature correction, and if required, a copper film may be deposited in the elastomer for reduced sensitivity to spot temperature variations in the elastomer near the sensors.

Park, Yong-Lae↗

A 3-D Computational Study of a Variable Camber Continuous Trailing Edge Flap (VCCTEF) Spanwise Segment

Results of a computational study carried out to explore the effects of various elastomer configurations joining spanwise contiguous Variable Camber Continuous Trailing Edge Flap (VCCTEF) segments are reported here. This research is carried out as a proof-of-concept study that will seek to push the flight envelope in cruise with drag optimization as the objective. The cruise conditions can be well off design such as caused by environmental conditions, maneuvering, etc. To handle these off-design conditions, flap deflection is used so when the flap is deflected in a given direction, the aircraft angle of attack changes accordingly to maintain a given lift. The angle of attack is also a design parameter along with the flap deflection. In a previous 2D study,1 the effect of camber was investigated and the results revealed some insight into the relative merit of various camber settings of the VCCTEF. The present state of the art has not advanced sufficiently to do a full 3-D viscous analysis of the whole NASA Generic Transport Model (GTM) wing with VCCTEF deployed with elastomers. Therefore, this study seeks to explore the local effects of three contiguous flap segments on lift and drag of a model devised here to determine possible trades among various flap deflections to achieve desired lift and drag results. Although this approach is an approximation, it provides new insights into the "local" effects of the relative deflections of the contiguous spanwise flap systems and various elastomer segment configurations. The present study is a natural extension of the 2-D study to assess these local 3-D effects. Design cruise condition at 36,000 feet at free stream Mach number of 0.797 and a mean aerodynamic chord (MAC) based Reynolds number of 30.734x10(exp 6) is simulated for an angle of attack (AoA) range of 0 to 6 deg. In the previous 2-D study, the calculations revealed that the parabolic arc camber (1x2x3) and circular arc camber (VCCTEF222) offered the best L/D characteristics and minimum drag in cruise. In the present 3-D study, calculations show that for the same C(sub t), the 3-D circular arc camber wing segment produces the largest drag for a given lift, larger than either of the two 2-D configurations, as was also conjectured in the previous study. This study indicates a wing stall around 4.5 deg angle of attack.

Camber↗

Validation of Test Methods for Air Leak Rate Verification of Spaceflight Hardware

As deep space exploration continues to be the goal of NASAs human spaceflight program, verification of the performance of spaceflight hardware becomes increasingly critical. Suitable test methods for verifying the leak rate of sealing systems are identified in program qualification testing requirements. One acceptable method for verifying the air leak rate of gas pressure seals is the tracer gas leak detector method. In this method, a tracer gas (commonly helium) leaks past the test seal and is transported to the leak detector where the leak rate is quantified. To predict the air leak rate, a conversion factor of helium-to-air is applied depending on the magnitude of the helium flow rate. The conversion factor is based on either the molecular mass ratio or the ratio of the dynamic viscosities. The current work was aimed at validating this approach for permeation-level leak rates using a series of tests with a silicone elastomer O-ring. An established pressure decay method with constant differential pressure was used to evaluate both the air and helium leak rates of the O-ring under similar temperature and pressure conditions. The results from the pressure decay tests showed, for the elastomer O-ring, that neither the molecular flow nor the viscous flow helium-to-air conversion factors were applicable. Leak rate tests were also performed using nitrogen and argon as the test gas. Molecular mass and viscosity based helium-to-test gas conversion factors were applied, but did not correctly predict the measured leak rates of either gas. To further this study, the effect of pressure boundary conditions was investigated. Often, pressure decay leak rate tests are performed at a differential pressure of 101.3 kPa with atmospheric pressure on the downstream side of the test seal. In space applications, the differential pressure is similar, but with vacuum as the downstream pressure. The same O-ring was tested at four unique differential pressures ranging from 34.5 to 137.9 kPa. Up to six combinations of upstream and downstream pressures for each differential pressure were compared. For a given differential pressure, the various combinations of upstream and downstream dry air pressures did not significantly affect the leak rate. As expected, the leak rate of the O-ring increased with increasing differential pressure. The results suggested that the current leak test pressure conditions, used to verify spacecraft sealing systems with elastomer seals, produce accurate values even though the boundary conditions do not model the space application.

helium leak detector↗

TPSAS-NF1676L-31622-DND

Electroactive polymers, especially electromechanically active polymers, have drawn extensive attention worldwide since the piezoelectricity and ferroelectricity of poly (vinylidene fluoride) (PVDF) was discovered in 1969. In the past three decades, several new classes of electroactive polymers that demonstrate promising electromechanical properties have been developed. Electrostrictive Graft Elastomers (G-elastomer) developed at NASA Langley Research Center have been recognized as one of the promising newly developed eletroactive polymers due to their large electric field-induced strain (~4%) and high mechanical modulus (~700 MPa). The combination of large induced strain and high mechanical modulus allows the electrostrictive graft elastomer to offer very promising electromechanical properties, in terms of output mechanical energy density, and plausible as a candidate for use in high performance and low mass actuation devices in various aerospace applications. In this presentation, the molecular structures, properties, processing and mechanisms of the electromechanical performance, as well as its applications in actuation devices for advanced aerospace technologies will be comprehensively reviewed and discussed.

Ji Su↗

TPSAS-NF1676L-31666-DND

Electroactive polymers, especially electromechanically active polymers, have drawn extensive attention worldwide since the piezoelectricity and ferroelectricity of poly (vinylidene fluoride) (PVDF) was discovered in 1969. In the past three decades, several new classes of electroactive polymers that demonstrate promising electromechanical properties have been developed. Electrostrictive Graft Elastomers (G-elastomer) developed at NASA Langley Research Center have been recognized as one of the promising newly developed eletroactive polymers due to their large electric field-induced strain (~4%) and high mechanical modulus (~700 MPa). The combination of large induced strain and high mechanical modulus allows the electrostrictive graft elastomer to offer very promising electromechanical properties, in terms of output mechanical energy density, and plausible as a candidate for use in high performance and low mass actuation devices in various aerospace applications. In this presentation, the molecular structures, properties, processing and mechanisms of the electromechanical performance, as well as its applications in actuation devices for advanced aerospace technologies will be comprehensively reviewed and discussed.

Ji Su↗

TPSAS-NF1676L-30019-DND

Electroactive polymers, especially electromechanically active polymers, have drawn extensive attention worldwide since the piezoelectricity and ferroelectricity of poly (vinylidene fluoride) (PVDF) was discovered in 1969. In the past three decades, several new classes of electroactive polymers that demonstrated promising electromechanical properties have been developed. Electrostrictive Graft Elastomers (G-elastomer) developed at NASA Langley Research Center have been recognized as one of the newly developed promising eletroactive polymers due to their large electric field-induced strain (~4%) and high mechanical modulus (~700 MPa). The combination of large induced strain and high mechanical modulus makes the electrostrictive graft elastomer offer very promising electromechanical properties, in terms of output mechanical energy density, and plausible as a candidate for use in high performance and low mass actuation devices in various aerospace applications. In this presentation, the molecular structures, properties, processing and mechanisms of the electromechanical performance, as well as its applications in actuation devices for advanced aerospace technologies will be comprehensively reviewed and discussed.

Ji Su↗

Method of protecting sulfur cathode materials for alkali metal-sulfur secondary battery

Provided is a method of producing a rechargeable alkali metal-sulfur cell, comprising: (a) providing an anode layer; (b) providing particulates comprising primary particles of a sulfur-containing material encapsulated or embraced by a thin layer of a conductive sulfonated elastomer composite, wherein the conductive sulfonated elastomer composite comprises from 0% to 50% by weight of a conductive reinforcement material dispersed in a sulfonated elastomeric matrix material, and the conductive sulfonated elastomer composite has a thickness from 1 nm to 10 μm, a fully recoverable tensile strain from 2% to 500%, a lithium ion conductivity from 10−7 S/cm to 5×10−2 S/cm, and an electrical conductivity from 10−7 S/cm to 100 S/cm; (c) forming the particulates, a resin binder, and an optional conductive additive into a cathode layer; and (d) combining the anode layer, the cathode layer, an optional porous separator, and an electrolyte to form the alkali metal-sulfur cell.

Zhamu, Aruna↗

Elastomeric Nanocomposite with Solvent‐Free, One Step, In Situ Shear Exfoliation of Graphite to Graphene

A graphene nanoflake (GNF)‐enhanced elastomeric nanocomposite (G‐EMC) is fabricated following an innovative, cost‐effective, single‐step, in situ shear exfoliation (ISE) method from low‐cost bulk material, graphite, where uniform mixing happens simultaneously within the elastomer matrix. Electron microscopy, atomic force microscopy, and photo‐induced force microscopy results show good dispersion of GNFs with exfoliation to a few layers and uniform distribution in the elastomer matrix. X‐ray photoelectron spectroscopy analysis shows less than 1% oxygen‐containing functional groups/impurity, enhanced bonding through the formation of edge sites as fracture occurs across the GNF basal plane, and pi‐pi interactions with newly exfoliated planar basal plane surfaces of the GNFs. Raman spectroscopy results confirm the formation of GNFs with only a few layers of graphene formed by the ISE process. Fabricated 10 wt.% G‐EMC nanocomposites show a 400%–500% increase in strength and fracture toughness. And 35 wt.% G‐EMCs provide an electrical conductivity of 25.64 S m −1 and a sensor gauge factor of 45. The resulting intrinsic piezo resistivity of the fabricated nanocomposite has been exploited to fabricate a multi‐functional wired and wireless sensor for detecting different body movements, speech, human vital functions, solvents, and biomolecules.

36 MATERIALS SCIENCE↗

One-Component, Vinyl-Functional Fluorosilicone Pastes for Direct Ink Write Additive Manufacturing

In this study, one-component (“all-in-one”) fluorosilicone pastes specifically designed for application in direct ink write (DIW) additive manufacturing (AM) have been developed. They consist of vinyl-functional, methyltrifluoropropyl-containing (MeTfpS) terpolysiloxane base polymer(s), hydrosilyl-functional cross-linker(s), UV-sensitive hydrosilylation catalyst, thixotropic additive, and trimethylsilylated fumed silica filler, with other additives that are optional. Their base polymers were completely amorphous and linear, with molecular weights (M n ) ranging from approximately 7000 to 50,000 and specifically targeted for the viscosity range ideal for DIW. These polymers were prepared by anionic ring-opening polymerizations (A-ROP) of appropriate mixtures of cyclic siloxanes initiated by oligomeric, difunctional tetramethylammonium silanolate in the presence of a difunctional tetramethyldivinyldisiloxane end-blocker and molecular weight regulator. Two series of these terpolymers were prepared: one containing 5 mol % MeTfpS repeat units but varying degrees of polymerization (DP) from 80 to 600 and the other containing 5, 10, and 15 mol % MeTfpS at a constant DP of 600. All polymers contained mostly random distributions of MeTfpS repeat units. The pastes were prepared by speed-mixing, ready for use in DIW, they exhibited ideal thixotropy, long-term (over a year) rheological stability, and can be quickly (within seconds) and permanently cured by room-temperature, UV-activated hydrosilylation in air. The resulting elastomers showed base polymer molecular weight- and composition-dependent stress-induced crystallization (SIC) at higher molecular weights and lower trifluoropropyl contents and tunable Shore A hardness (30A–40A) typical for soft polysiloxane rubbers. Preliminary DIW tests indicated excellent printability with high precision of printed shapes and clearly present these one-component pastes as prime candidates for simple and practical printing of silicone elastomer objects.

36 MATERIALS SCIENCE↗

Tailored Silicone Network Architecture for Ultimate Mechanical Reinforcement

Hydrosilylation cured silicone elastomers are subject to reaction inefficiency, leading to incomplete and non-uniform crosslink networks, restricting the potential of mechanical reinforcement. This work investigates pre-synthesized, functional PDMS architectures as additives to improve ultimate mechanical performance relative to conventional single-step curing. Three custom, functional structures were prepared: a partially crosslinked PDMS scaffold (Structure A), a bottle-brush PDMS (Structure B), and a star-shaped PDMS derived from an MQ resin (Structure C). Rheological characterization was used to identify the ultimate design space and proper stoichiometric ratio for Structure A, and confirm successful formation of all structures for suitable incorporation into a base silicone formulation at 30wt%. Mechanical tests indicated that all three structures increased in ultimate tensile strength relative to their single-step counterparts, with Structure A providing additional improvements to toughness (432 vs. 258 kJ/m3) and ultimate elongation (158 vs. 115%). Furthermore, Structure B remained very soft in the unfilled state, while Structure C provided hardness (23 vs. 18 Shore A) and stiffness (780 vs. 420 kPa Young’s modulus) increases. In silica filled systems, Structure A retained increased strength but reduced elongation, while Structure B indicated strong reinforcement in terms of strength, toughness, and stiffness. Thermal analysis on the cure profiles of these materials suggested that pre-formation of network architectures enable a more complete reaction than a single-step process (15.9 vs. 15.1 J/g). Ultimately, these results indicate that tailoring PDMS architecture before the final cure can improve ultimate mechanical properties via improved network development in silicone elastomers. Furthermore, this work offers a promising strategy for designing higher-performance, more tunable silicone formulations.

36 MATERIALS SCIENCE↗

Stretchable and Self‐Healable Semiconductive Composites Based on Hydrogen Bonding Cross‐linked Elastomeric Matrix

Abstract Semiconductors with both high stretchability and self‐healing capability are highly desirable for various wearable devices. Much progress has been achieved in designing highly stretchable semiconductive polymers or composites. The demonstration of self‐healable semiconductive composite is still rare. Here, an extremely soft, highly stretchable, and self‐healable hydrogen bonding cross‐linked elastomer, amide functionalized‐polyisobutylene (PIB‐amide) is developed, to enable a self‐healable semiconductive composite through compounding with a high‐performance conjugated diketopyrrolopyrrole (DPP‐T) polymer. The composite, consisting of 20% DPP‐T and 80% PIB‐amide, shows record high crack‐onset strain (COS ≈1500%), extremely low elastic modulus (E≈1.6 MPa), and unique ability to spontaneously self‐heal atroom temperature within 5 min. Unlike previous works, these unique composite materials also show strain‐independent charge mobility. An in‐depth morphological study based on multi‐model techniques indicate that all composites show blending ratio‐ and stretching‐independent fibril‐like aggregation due to the strong hydrogen bond in elastomer to enable the unique stable charge mobility. This study provides a new direction to develop highly healable and electronically stable semiconductive composite and will enable new applications of stretchable electronics.

Chemistry↗

Toluene Uptake and Outgassing by a 3D-Printed Silicone and the Impact on Mechanical Performance

Silicone elastomers have advantageous physical properties and are widely used in various applications. Additive manufacturing (AM) of silicones provides additional utility by enabling tunable mechanical and functional properties. However, the performance of these elastomers deteriorates over time with exposure to environmental stressors. Organic solvents and volatile organic compounds (VOCs) are stressors that can cause dimensional changes to silicones with exposure and impact the overall function. Yet, the effects of such exposure on mechanical performance, including load response (LR), are not well understood. Here, in this study, we investigated the impact of a nonpolar solvent, toluene, on AM silicone material properties and compressive load. We observed that AM silicones rapidly absorbed toluene and swelled, leading to an increase in relative LR. Toluene concentration and compression did not affect uptake or swelling rates. In contrast, outgassing rates were slower for compressed coupons compared to uncompressed specimens, attributed to geometric constraints and polymer network changes impacting toluene diffusion outward. Compression also pinned the AM silicones at an enlarged state, significantly reducing relative LR after outgassing. Depending on toluene concentrations and compression, AM silicones can remain robust against toluene exposure and recover their initial printing geometry and mechanical performance after toluene outgassing and polymer relaxation.

Materials science↗

Degradation in Photovoltaic Encapsulant Transmittance: Results of the Second PVQAT TG5 Artificial Weathering Study

The optical degradation of encapsulants from ultraviolet (UV) radiation has historically resulted in a significant loss in performance throughout the life of a photovoltaic (PV) module. International Electrotechnical Commission (IEC) test methods have recently been developed to screen for PV encapsulants prone to loss in optical performance. The present study was performed to benchmark polymeric packaging materials relative to IEC 62788-1-4 (covering the measurement of optical transmittance) and IEC 62788-1-7 (on the durability of transmittance), provide feedback toward improvement of the methods, and develop insight regarding optical degradation. Contemporary materials were examined, including poly(ethylene-co-vinyl acetate) (EVA), thermoplastic polyolefin (TPO), polyolefin elastomer (POE), and polyvinyl butyral (PVB) encapsulants; a poly(ethene-co-tetrafluoroethene)/poly(ethylene terephthalate) (ETFE/PET) transparent backsheet; and a polystyrene (PS) working reference material. The use of silica-, specialty-, and rolled-glass was also compared in laminated coupons. Specimen size was separately examined from 2.5 to 12.5 cm. Weathering was performed with a xenon source, using IEC TS 62788-7-2 methods A2, A3, A4, and A5 (chamber temperature of 55 degrees C, 65 degrees C, 75 degrees C, or 85 degrees C), respectively. Characterizations were made using a UV-visible-near-infrared (UV-VIS-NIR) spectrophotometer (transmittance and reflectance, with and without an integrating sphere), a UV-VIS fluorescence spectrophotometer, a camera, and an optical microscope. Performance was analyzed, including solar weighted transmittance, yellowness index, UV cut-off wavelength, and haze (scattering). Separate Arrhenius analyses were performed to assess retention of transmittance and changes in yellowness index. The activation energy for both characteristics was found to range from 15-80 kJ mol-1, with an average of 48 kJ mol-1, similar to the average of 45 kJ mol-1 identified in the previous international PV Quality Assurance Task Force (PVQAT) Task Group 5 (TG5) study of more traditional encapsulants. The separate degradation modes of discoloration and scattering were distinguished in the encapsulants using a comprehensive spectral characterization. Based on these results, the IEC 62788-1-7 pass/fail criteria of 5% change in transmittance was confirmed to identify a known bad encapsulant.

durability↗

Fuel Properties of Oxymethylene Ethers with Terminating Groups from Methyl to Butyl

Oxymethylene ethers (OMEs) have been studied as possible additives or replacements for diesel fuels. Typically, studies have considered only methyl-terminated OMEs. Recent structure-property relationship models suggest that extended-alkyl OMEs may provide improvements to many of the properties of methyl-terminated OMEs that make them less suitable as diesel fuel blendstocks. In this work, we describe the synthesis and characterization of 16 different OMEs with methyl, ethyl, propyl, butyl, isopropyl, and isobutyl terminating alkyl groups with varying oxymethylene chain length. Indicated Cetane Number, Lower Heating Value, Flash Point, Density, Viscosity, Vapor Pressure, and Oxidative Stability are tested via ASTM standard methods. Additionally, Water Solubility, Boiling Point, seal material compatibility, and sooting propensity (via the Yield Sooting Index) are measured for these fuels. For diesel compatibility, all tested OMEs except smaller methyl and ethyl OMEs, and the branched isopropyl OME, meet cetane number requirements. Further, extending the alkyl end group increases the heating value, but all OMEs, due to their oxygen content, have heating values less than diesel; despite this, all OMEs show significant reductions in soot production per unit heating value. Only the heaviest OMEs meet diesel viscosity requirements, and most are higher density than diesel. OMEs with larger alkyl groups show the highest stability under accelerated auto-oxidation conditions. Increases in alkyl group length cause order of magnitude reduction in water solubility, from hundreds of g/L for methyl terminated OMEs to hundreds of mg/L for butyl terminated OMEs. Limited seal material testing indicates that PEEK polymers are unaffected by OMEs; while extended alkyl groups may improve compatibility with FKM (Viton), other common elastomers (NBR, silicone) remain incompatible with all tested OMEs. Overall, it is found that methyl-terminated OMEs exhibit the most potential for soot reduction, but OMEs with larger propyl and butyl terminating alkyl groups show improved compatibility with existing diesel systems.

09 BIOMASS FUELS↗

Diels–Alder Augmented Epoxies with Plasmonic Nanoparticle Fillers for Efficient Photothermal Depolymerization

Thermally reversible epoxies through the Diels–Alder (DA) reaction have been used for applications such as recycling, self-healing, and 3D printing. Depolymerization by bulk heating, however, would be a slow and inefficient process due to its low thermal conductivity. In this paper, photothermal conversion using refractory plasmonic titanium nitride (TiN) nanoparticles was employed for efficient and rapid depolymerization of reversible epoxies. TiN nanoparticles have superior thermal stability, broader light absorption, and higher light-to-heat conversion efficiency. They are also less expensive than more common plasmonic gold nanoparticles. Photothermal behavior of TiN nanoparticle-filled reversible epoxies was investigated as a function of concentration of TiN nanoparticles and as a function of the intensity of a light source. TiN nanoparticles could induce sufficient heat for depolymerization with a trace content, 0.01% by weight, under a broad-spectrum white light of intensity 1760 mW/cm 2 instead of a strong light source such as a laser. The reversible epoxies were prepared by a reaction between furan precursors and a bismaleimide compound. Crosslinking density was controlled by altering the architecture of furan precursors and the feed ratio between the furan precursor and the bismaleimide compound. These changes in chemical structure and degree of crosslinking permit the control of the thermomechanical properties of the reversible epoxy from soft elastomers to hard elastomers. Here, the reversible epoxies display a flow region at around 110 °C. Depolymerization through the retro-DA was confirmed by Fourier transform infrared spectroscopy as a function of duration at a high temperature. Light-induced removability and recyclability were demonstrated by adhesion tests using the reversible epoxy/nanoparticle composites.

36 MATERIALS SCIENCE↗