High-Resolution PFPE-based Molding Techniques for Nanofabrication of High-Pattern Density, Sub-20 nm Features: A Fundamental Materials Approach
Explore the source record for details and available documents.
SEARCH · Engineering Papers
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Explore the source record for details and available documents.
Elastomeric matrix composites (EMC-rubbers) are considered as isotropic hyper elastic incompressible materials under static loading conditions. As a rubber material element cannot be extended to an infinite stretch ratio, a damage mechanism at large strain is considered. The phenomenon of cavitation plays an important role in the damage of EMCs and influences the toughening mechanism of rubber-modified plastics. Indeed, cavitation in elastomers is thought to be initiated from flaws, which grow primarily due to a hydrostatic tensile stress and ahead of the crack; there will not only be a high stress perpendicular to the plane of the crack but also significant stress components in the other direction. However, there exists historically much discussion on the evolution of the cavitation in elastomers under monotonic and/or static solicitation. Mainly, cavitation instability occurs when the stress levels are sufficiently high so that the void expansion rate becomes infinitely large. Many research works have been performed to understand the effects of rubber cavitation on toughening of plastics. In fact, the cavitation phenomenon is not well known in detail. The most popular idea states that the cavitation is related to the existence of the gas bubbles trapped in the material during the production stage and the growing of the cavities would then be the result of the growing gas bubbles. Further, instable failure mechanism at the end of the cavitation is not well known too.
We demonstrate facile optical manipulation of shape of birefringent colloidal microparticles made from liquid crystal elastomers. Using soft lithography and polymerization, we fabricate elastomeric microcylinders with weakly undulating director oriented on average along their long axes. These particles are infiltrated with gold nanospheres acting as heat transducers that allow for an efficient localized transfer of heat from a focused infrared laser beam to a submicrometer region within a microparticle. Photothermal control of ordering in the liquid crystal elastomer using scanned beams allows for a robust control of colloidal particles, enabling both reversible and irreversible changes of shape. Possible applications include optomechanics, microfluidics, and reconfigurable colloidal composites with shape-dependent self-assembly.
Through applying the liquid metal and elastomer as the core and shell materials, respectively, a coaxial printing method is being developed in this work for preparing a stretchable and conductive cable. When liquid metal alloy eutectic Gallium-Indium is embedded into the elastomer matrix under optimized control, the cable demonstrates well–posed extreme mechanic performance, under stretching for more than 350%. Under developed compression test, the fabricated cable also demonstrates the ability for recovering original properties due to the high flowability of the liquid metal and super elasticity of the elastomeric shell. The written cable presents high cycling reliability regarding its stretchability and conductivity, two properties which can be clearly predicted in theoretical calculation. This work can be further investigated as a strain sensor for monitoring motion status including frequency and amplitude of a curved object, with extensive applications in wearable devices, soft robots, electronic skins, and wireless communication.
The Energy Independence and Security Act (EISA) of 2007 was enacted by Congress to move the nation toward increased energy independence by increasing the production of renewable fuels to meet its transportation energy needs. The law establishes a new renewable fuel standard (RFS) that requires the nation to use 36 billion gallons annually (2.3 million barrels per day) of renewable fuel in its vehicles by 2022. Ethanol is the most widely used renewable fuel in the US, and its production has grown dramatically over the past decade. According to EISA and RFS, ethanol (produced from corn as well as cellulosic feedstocks) will make up the vast majority of the new renewable fuel requirements. However, ethanol use limited to E10 and E85 (in the case of flex fuel vehicles or FFVs) will not meet this target. Even if all of the E0 gasoline dispensers in the country were converted to E10, such sales would represent only about 15 billion gallons per year. If 15% ethanol, rather than 10% were used, the potential would be up to 22 billion gallons. The vast majority of ethanol used in the United States is blended with gasoline to create E10, that is, gasoline with up to 10% ethanol. The remaining ethanol is sold in the form of E85, a gasoline blend with as much as 85% ethanol that can only be used in FFVs. Although DOE remains committed to expanding the E85 infrastructure, that market will not be able to absorb projected volumes of ethanol in the near term. Given this reality, DOE and others have begun assessing the viability of using intermediate ethanol blends as one way to transition to higher volumes of ethanol. In October of 2010, the EPA granted a partial waiver to the Clean Air Act allowing the use of fuel that contains up to 15% ethanol for the model year 2007 and newer light-duty motor vehicles. This waiver represents the first of a number of actions that are needed to move toward the commercialization of E15 gasoline blends. On January 2011, this waiver was expanded to include model year 2001 light-duty vehicles, but specifically prohibited use in motorcycles and off-road vehicles and equipment. UST stakeholders generally consider fueling infrastructure materials designed for use with E0 to be adequate for use with E10, and there are no known instances of major leaks or failures directly attributable to ethanol use. It is conceivable that many compatibility issues, including accelerated corrosion, do arise and are corrected onsite and, therefore do not lead to a release. However, there is some concern that higher ethanol concentrations, such as E15 or E20, may be incompatible with current materials used in standard gasoline fueling hardware. In the summer of 2008, DOE recognized the need to assess the impact of intermediate blends of ethanol on the fueling infrastructure, specifically located at the fueling station. This includes the dispenser and hanging hardware, the underground storage tank, and associated piping. The DOE program has been co-led and funded by the Office of the Biomass Program and Vehicle Technologies Program with technical expertise from the Oak Ridge National Laboratory (ORNL) and the National Renewable Energy Laboratory (NREL). The infrastructure material compatibility work has been supported through strong collaborations and testing at Underwriters Laboratories (UL). ORNL performed a compatibility study investigating the compatibility of fuel infrastructure materials to gasoline containing intermediate levels of ethanol. These results can be found in the ORNL report entitled Intermediate Ethanol Blends Infrastructure Materials Compatibility Study: Elastomers, Metals and Sealants (hereafter referred to as the ORNL intermediate blends material compatibility study). These materials included elastomers, plastics, metals and sealants typically found in fuel dispenser infrastructure. The test fuels evaluated in the ORNL study were SAE standard test fuel formulations used to assess material-fuel compatibility within a relatively short timeframe. Initially, these material studies included test fuels of Fuel C, CE10a, CE17a, and CE25a. The CE17a test fuel was selected to represent E15 since surveys have shown that the actual ethanol upper limit can be as high as 17%. Later, CE50a and CE85a test fuels were added to the investigation and these results are being compiled for a follow-on report to be published in 2012. Fuel C was used as the baseline reference and is a 50:50 blend of isooctane and toluene. This particular composition was used to represent premium-grade gasoline and was also used as the base fuel for the ethanol blends, where it is denoted by 'C' in the fuel name. The level of ethanol is represented by the number following the letter E. Therefore a 10% blend of ethanol in Fuel C is written as CE10a, where 'a' represents an aggressive formulation of the ethanol that contains water, NaCl, acetic and sulfuric acids per the SAE J1681 protocol.
As part of the Enhance Surveillance mission, it is the goal to provide suitable lifetime assessment of stockpile materials. This report is an accumulation of historical publication on the DC745U material and their findings. It is the intention that the B61 LEP program uses this collection of data to further develop their understanding and potential areas of study. DC745U is a commercially available silicone elastomer consisting of dimethyl, methyl-phenyl, and methyl-vinyl siloxane repeat units. Originally, this material was manufactured by Dow Corning as Silastic® DC745U at their manufacturing facility in Kendallville, IN. Recently, Dow Corning shifted this material to the Xiameter® brand product line. Currently, DC745U is available through Xiameter® or Dow Corning's distributor R. D. Abbott Company. DC745U is cured using 0.5 wt% vinyl-specific peroxide curing agent known as Luperox 101 or Varox DBPH-50. This silicone elastomer is used in numerous parts, including two major components (outer pressure pads and aft cap support) in the W80 and as pressure pads on the B61. DC745U is a proprietary formulation, thus Dow Corning provides limited information on its composition and properties. Based on past experience with Dow Corning, DC745U is at risk of formulation changes without notification to the costumer. A formulation change for DC745U may have a significant impact because the network structure is a key variable in determining material properties. The purpose of this report is to provide an overview of historical DC745U studies and identify gaps that need to be addressed in future work. Some of the previous studies include the following: 1. Spectroscopic characterization of raw gum stock. 2. Spectroscopic, thermal, and mechanical studies on cured DC745U. 3. Nuclear Magnetic Resonance (NMR) and solvent swelling studies on DC745U with different crosslink densities. 4. NMR, solvent swelling, thermal, and mechanical studies on thermally aged DC745U. 5. NMR, solvent swelling, thermal, and mechanical studies on radiolytically aged DC745U. Each area is reviewed and further work is suggested to improve our understanding of DC745U for systems engineering, surveillance, aging assessments, and lifetime assessment.
Using gas-gun driven plate impact experiments, we have measured the U S - u p Hugoniot of the silicone elastomer DC745U cooled to -60 °C. In summary, the initial density changes from p 0 (23°C) = 1.312 ± 0.010 g/cm 3 to p 0 (-60°C) = 1.447 ± 0.011 g/cm 3 . The linear U S - u p Hugoniot changes from U S = 1.62 + 1.74u p km/s at +23°C, to U S = 2.03 ± 0.06 + (2.03 ± 0.06) u p km/s at -60°C. DC745U, therefore is much stiffer at -60°C than at +23°C, probably due to the crystallization that occurs at ~ -50°C. Caveats/deficiencies: 1) This report does not provide an adequate pedigree of the DC745U used. 2) References to unpublished room temperature shock compression data on the elastomer are inadequate. 3) The report has not been fact checked by a DC745 subject matter expert.
Hydrosilylation cured silicone elastomers are subject to reaction inefficiency, leading to incomplete and non-uniform crosslink networks, restricting the potential of mechanical reinforcement. This work investigates pre-synthesized, functional PDMS architectures as additives to improve ultimate mechanical performance relative to conventional single-step curing. Three custom, functional structures were prepared: a partially crosslinked PDMS scaffold (Structure A), a bottle-brush PDMS (Structure B), and a star-shaped PDMS derived from an MQ resin (Structure C). Rheological characterization was used to identify the ultimate design space and proper stoichiometric ratio for Structure A, and confirm successful formation of all structures for suitable incorporation into a base silicone formulation at 30wt%. Mechanical tests indicated that all three structures increased in ultimate tensile strength relative to their single-step counterparts, with Structure A providing additional improvements to toughness (432 vs. 258 kJ/m3) and ultimate elongation (158 vs. 115%). Furthermore, Structure B remained very soft in the unfilled state, while Structure C provided hardness (23 vs. 18 Shore A) and stiffness (780 vs. 420 kPa Young’s modulus) increases. In silica filled systems, Structure A retained increased strength but reduced elongation, while Structure B indicated strong reinforcement in terms of strength, toughness, and stiffness. Thermal analysis on the cure profiles of these materials suggested that pre-formation of network architectures enable a more complete reaction than a single-step process (15.9 vs. 15.1 J/g). Ultimately, these results indicate that tailoring PDMS architecture before the final cure can improve ultimate mechanical properties via improved network development in silicone elastomers. Furthermore, this work offers a promising strategy for designing higher-performance, more tunable silicone formulations.
The Nez Perce Tribe, through funding provided by the Bonneville Power Administration, has implemented a small scale chinook salmon supplementation program on Johnson Creek, a tributary in the South Fork of the Salmon River, Idaho. The Johnson Creek Artificial Propagation Enhancement project was established to enhance the number of threatened Snake River spring/summer chinook salmon (Oncorhynchus tshawytscha) returning to Johnson Creek to spawn through artificial propagation. This was the sixth season of adult chinook broodstock collection in Johnson Creek following collections in 1998, 2000, 2001, 2002, and 2003. Weir installation was completed on June 21, 2004 with the first chinook captured on June 22, 2004 and the last fish captured on September 6, 2004. The weir was removed on September 18, 2004. A total of 338 adult chinook, including jacks, were captured during the season. Of these, 211 were of natural origin, 111 were hatchery origin Johnson Creek supplementation fish, and 16 were adipose fin clipped fish from other hatchery operations and therefore strays into Johnson Creek. Over the course of the run, 57 natural origin Johnson Creek adult chinook were retained for broodstock, transported to the South Fork Salmon River adult holding and spawning facility and held until spawned. The remaining natural origin Johnson Creek fish along with all the Johnson Creek supplementation fish were released upstream of the weir to spawn naturally. Twenty-seven Johnson Creek females were artificially spawned with 25 Johnson Creek males. Four females were diagnosed with high bacterial kidney disease levels resulting in their eggs being culled. The 27 females produced 116,598 green eggs, 16,531 green eggs were culled, with an average eye-up rate of 90.6% resulting in 90,647 eyed eggs. Juvenile fish were reared indoors at the McCall Fish Hatchery until November 2005 and then transferred to the outdoor rearing facilities during the Visual Implant Elastomer tagging operation. These fish continued rearing in the outdoor collection basin until release in March 2006. All of these fish were marked with Coded Wire Tags and Visual Implant Elastomer tags. In addition 12,056 of the smolts released were also tagged with Passive Integrated Transponder tags. Hand counts provided by marking crews were used to amend the number of juvenile salmon released from the original egg count. A total of 90,450 smolts were released directly into Johnson Creek on March 13 through 15, 2006.
The influence of temperature and radiation on Viton{reg_sign} GLT and GLT-S fluoroelastomer O-rings is an ongoing research focus at the Savannah River National Laboratory. The O-rings are credited for leaktight containment in the Model 9975 shipping package used for transportation of plutonium-bearing materials. At the Savannah River Site, the Model 9975 packages are being used for interim storage. Primary research efforts have focused on surveillance of O-rings from actual packages, leak testing of seals at bounding aging conditions and the effect of aging temperature on compression stress relaxation behavior, with the goal of service life prediction for long-term storage conditions. Recently, an additional effort to evaluate the effect of aging temperature on the oxidation of the materials has begun. Degradation in the mechanical properties of elastomers is directly related to the oxidation of the polymer. Sensitive measurements of the oxidation rate can be performed in a more timely manner than waiting for a measurable change in mechanical properties, especially at service temperatures. Measuring the oxidation rate therefore provides a means to validate the assumption that the degradation mechanisms(s) do not change from the elevated temperatures used for accelerated aging and the lower service temperatures. Monitoring the amount of oxygen uptake by the material over time at various temperatures can provide increased confidence in lifetime predictions. Preliminary oxygen consumption analysis of a Viton GLT-based fluoroelastomer compound (Parker V0835-75) using an Oxzilla II differential oxygen analyzer in the temperature range of 40-120 C was performed. Early data suggests oxygen consumption rates may level off within the first 100,000 hours (10-12 years) at 40 C and that sharp changes in the degradation mechanism (stress-relaxation) are not expected over the temperature range examined. This is consistent with the known long-term heat aging resistance of fluoroelastomers relative to hydrocarbon-based elastomers, and in absence of antioxidants that may be consumed over time. Additional experimental effort will be undertaken in the short term range within the first 100 hours of thermal aging to capture further details of the oxygen consumption rate.
Light activated polymers, which are capable of mechanically responding to light, promise to offer exciting, innovative, and unique material capabilities. Such materials include: photo-radical mediated cleavage and reformation of the polymer backbone in cross-linked elastomers that results in local stress relaxation; photo-switching cross-links in shape memory polymers; and photo-isomerization of azobenzene groups contained in liquid crystal elastomers. In this paper, using our recent material model that couples multiphysical processes involved in light-activated polymers, we demonstrate that a variety of patterns can be created on light activated polymer thin films when coupling mechanical deformation with light irradiation. Here, the polymer thin film is first stretched uniaxially or biaxially. Light is then irradiated on the surface of the thin film. After light irradiation, removal external load partially recovers the initial stretching of the polymer thin film and induces patterns. The variation of the geometry of the patterns can be controlled by a variety of parameters such as initial stretching, light intensity, etc. Photo-patterning with light activated polymer therefore offers a novel way to create surface patterns.
AREVA Federal Services LLC, under contract to the Los Alamos National Laboratory's Offsite Source Recovery Project, is developing a new Type B(U)-96 package for the transport of unwanted or abandoned high activity gamma and neutron radioactive sealed sources (sources). The sources were used primarily in medical or industrial devices, and are of domestic (USA) or foreign origin. To promote public safety and mitigate the possibility of loss or misuse, the Offsite Source Recovery Project is recovering and managing sources worldwide. The package, denoted the LANL-B, is designed to accommodate the sources within an internal gamma shield. The sources are located either in the IAEA's Long Term Storage Shield (LTSS), or within intact medical or industrial irradiation devices. As the sources are already shielded separately, the package does not include any shielding of its own. A particular challenge in the design of the LANL-B has been weight. Since the LTSS shield weighs approximately 5,000 lb [2,270 kg], and the total package gross weight must be limited to 10,000 lb [4,540 kg], the net weight of the package was limited to 5,000 lb, for an efficiency of 50% (i.e., the payload weight is 50% of the gross weight of the package). This required implementation of a light-weight bell-jar concept, in which the containment takes the form of a vertical bell which is bolted to a base. A single impact limiter is used on the bottom, to protect the elastomer seals and bolted joint. A top-end impact is mitigated by the deformation of a tori spherically-shaped head. Impacts in various orientations on the bottom end are mitigated by a cylindrical, polyurethane foam-filled impact limiter. Internally, energy is absorbed using honeycomb blocks at each end, which fill the torispherical head volumes. As many of the sources are considered to be in normal form, the LANL-B package offers leak-tight containment using an elastomer seal at the joint between the bell and the base, as well as on the single vent port. Leak testing prior to transport may be either using helium mass spectrometry or the pressure-rise concept.
Organic getters are used to reduce the amount of reactive hydrogen in applications such as nuclear plants and transuranic waste. Here, the present study examines the performance of getter loaded silicone elastomers in reducing reactive hydrogen gas from the gas phase and their capability of being 3D printed using direct ink writing techniques. The samples are placed in closed vessels and exposed to hydrogen atmosphere at pressures of 580 torr and 750 mtorr and at a temperature of 25 °C. The hydrogen consumption is measured as a function of time and normalized to getter concentration in the polymer. The performance of the getter-loaded silicone elastomer containing 1,4-bis[phenylethynyl]benzene (DEB) as the organic getter and Pd/C catalyst (ratio of 3:1 DEB to catalyst) decreases with increasing the resin's curing temperature. Chemical analysis suggests that DEB reacts with the silicone resin at high temperatures. In addition, it is demonstrated that the increased surface area of 3D printed composites results in improved getter performance.
Abstract Semiconductors with both high stretchability and self‐healing capability are highly desirable for various wearable devices. Much progress has been achieved in designing highly stretchable semiconductive polymers or composites. The demonstration of self‐healable semiconductive composite is still rare. Here, an extremely soft, highly stretchable, and self‐healable hydrogen bonding cross‐linked elastomer, amide functionalized‐polyisobutylene (PIB‐amide) is developed, to enable a self‐healable semiconductive composite through compounding with a high‐performance conjugated diketopyrrolopyrrole (DPP‐T) polymer. The composite, consisting of 20% DPP‐T and 80% PIB‐amide, shows record high crack‐onset strain (COS ≈1500%), extremely low elastic modulus (E≈1.6 MPa), and unique ability to spontaneously self‐heal atroom temperature within 5 min. Unlike previous works, these unique composite materials also show strain‐independent charge mobility. An in‐depth morphological study based on multi‐model techniques indicate that all composites show blending ratio‐ and stretching‐independent fibril‐like aggregation due to the strong hydrogen bond in elastomer to enable the unique stable charge mobility. This study provides a new direction to develop highly healable and electronically stable semiconductive composite and will enable new applications of stretchable electronics.
Silicone elastomers have advantageous physical properties and are widely used in various applications. Additive manufacturing (AM) of silicones provides additional utility by enabling tunable mechanical and functional properties. However, the performance of these elastomers deteriorates over time with exposure to environmental stressors. Organic solvents and volatile organic compounds (VOCs) are stressors that can cause dimensional changes to silicones with exposure and impact the overall function. Yet, the effects of such exposure on mechanical performance, including load response (LR), are not well understood. Here, in this study, we investigated the impact of a nonpolar solvent, toluene, on AM silicone material properties and compressive load. We observed that AM silicones rapidly absorbed toluene and swelled, leading to an increase in relative LR. Toluene concentration and compression did not affect uptake or swelling rates. In contrast, outgassing rates were slower for compressed coupons compared to uncompressed specimens, attributed to geometric constraints and polymer network changes impacting toluene diffusion outward. Compression also pinned the AM silicones at an enlarged state, significantly reducing relative LR after outgassing. Depending on toluene concentrations and compression, AM silicones can remain robust against toluene exposure and recover their initial printing geometry and mechanical performance after toluene outgassing and polymer relaxation.
The optical degradation of encapsulants from ultraviolet (UV) radiation has historically resulted in a significant loss in performance throughout the life of a photovoltaic (PV) module. International Electrotechnical Commission (IEC) test methods have recently been developed to screen for PV encapsulants prone to loss in optical performance. The present study was performed to benchmark polymeric packaging materials relative to IEC 62788-1-4 (covering the measurement of optical transmittance) and IEC 62788-1-7 (on the durability of transmittance), provide feedback toward improvement of the methods, and develop insight regarding optical degradation. Contemporary materials were examined, including poly(ethylene-co-vinyl acetate) (EVA), thermoplastic polyolefin (TPO), polyolefin elastomer (POE), and polyvinyl butyral (PVB) encapsulants; a poly(ethene-co-tetrafluoroethene)/poly(ethylene terephthalate) (ETFE/PET) transparent backsheet; and a polystyrene (PS) working reference material. The use of silica-, specialty-, and rolled-glass was also compared in laminated coupons. Specimen size was separately examined from 2.5 to 12.5 cm. Weathering was performed with a xenon source, using IEC TS 62788-7-2 methods A2, A3, A4, and A5 (chamber temperature of 55 degrees C, 65 degrees C, 75 degrees C, or 85 degrees C), respectively. Characterizations were made using a UV-visible-near-infrared (UV-VIS-NIR) spectrophotometer (transmittance and reflectance, with and without an integrating sphere), a UV-VIS fluorescence spectrophotometer, a camera, and an optical microscope. Performance was analyzed, including solar weighted transmittance, yellowness index, UV cut-off wavelength, and haze (scattering). Separate Arrhenius analyses were performed to assess retention of transmittance and changes in yellowness index. The activation energy for both characteristics was found to range from 15-80 kJ mol-1, with an average of 48 kJ mol-1, similar to the average of 45 kJ mol-1 identified in the previous international PV Quality Assurance Task Force (PVQAT) Task Group 5 (TG5) study of more traditional encapsulants. The separate degradation modes of discoloration and scattering were distinguished in the encapsulants using a comprehensive spectral characterization. Based on these results, the IEC 62788-1-7 pass/fail criteria of 5% change in transmittance was confirmed to identify a known bad encapsulant.
Oxymethylene ethers (OMEs) have been studied as possible additives or replacements for diesel fuels. Typically, studies have considered only methyl-terminated OMEs. Recent structure-property relationship models suggest that extended-alkyl OMEs may provide improvements to many of the properties of methyl-terminated OMEs that make them less suitable as diesel fuel blendstocks. In this work, we describe the synthesis and characterization of 16 different OMEs with methyl, ethyl, propyl, butyl, isopropyl, and isobutyl terminating alkyl groups with varying oxymethylene chain length. Indicated Cetane Number, Lower Heating Value, Flash Point, Density, Viscosity, Vapor Pressure, and Oxidative Stability are tested via ASTM standard methods. Additionally, Water Solubility, Boiling Point, seal material compatibility, and sooting propensity (via the Yield Sooting Index) are measured for these fuels. For diesel compatibility, all tested OMEs except smaller methyl and ethyl OMEs, and the branched isopropyl OME, meet cetane number requirements. Further, extending the alkyl end group increases the heating value, but all OMEs, due to their oxygen content, have heating values less than diesel; despite this, all OMEs show significant reductions in soot production per unit heating value. Only the heaviest OMEs meet diesel viscosity requirements, and most are higher density than diesel. OMEs with larger alkyl groups show the highest stability under accelerated auto-oxidation conditions. Increases in alkyl group length cause order of magnitude reduction in water solubility, from hundreds of g/L for methyl terminated OMEs to hundreds of mg/L for butyl terminated OMEs. Limited seal material testing indicates that PEEK polymers are unaffected by OMEs; while extended alkyl groups may improve compatibility with FKM (Viton), other common elastomers (NBR, silicone) remain incompatible with all tested OMEs. Overall, it is found that methyl-terminated OMEs exhibit the most potential for soot reduction, but OMEs with larger propyl and butyl terminating alkyl groups show improved compatibility with existing diesel systems.