Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “cathode”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 397 records · Page 22

DARHT 2 kA Cathode Development

In the campaign to achieve 2 kA of electron beam current, we have made several changes to the DARHT-II injector during 2006-2007. These changes resulted in a significant increase in the beam current, achieving the 2 kA milestone. Until recently (before 2007), the maximum beam current that was produced from the 6.5-inch diameter (612M) cathode was about 1300 A when the cathode was operating at a maximum temperature of 1140 C. At this temperature level, the heat loss was dominated by radiation which is proportional to temperature to the fourth power. The maximum operating temperature was limited by the damage threshold of the potted filament and the capacity of the filament heater power supply, as well as the shortening of the cathode life time. There were also signs of overheating at other components in the cathode assembly. Thus it was clear that our approach to increase beam current could not be simply trying to run at a higher temperature and the preferred way was to operate with a cathode that has a lower work function. The dispenser cathode initially used was the type 612M made by SpectraMat. According to the manufacturer's bulletin, this cathode should be able to produce more than 10 A/cm{sup 2} of current density (corresponding to 2 kA of total beam current) at our operating conditions. Instead the measured emission (space charge limited) was 6 A/cm{sup 2}. The result was similar even after we had revised the activation and handling procedures to adhere more closely to the recommend steps (taking longer time and nonstop to do the out-gassing). Vacuum was a major concern in considering the cathode's performance. Although the vacuum gauges at the injector vessel indicated 10{sup -8} Torr, the actual vacuum condition near the cathode in the central region of the vessel, where there might be significant out-gassing from the heater region, was never determined. Poor vacuum at the surface of the cathode degraded the emission (by raising the work function value). We reexamined all the components in the cathode region and eliminated those parts that were suspected to be potential sources of contamination, e.g., feed-throughs with zinc coating. Finally, we considered a change in the cathode type, by using a different combination of impregnation and coating. Since the ETA-II accelerator at LLNL used a 12.5 cm diameter 311XW (barium oxide doped with scandium and coated with a osmium-tungsten thin film) cathode and emitted 2200A of beam current (i.e. 18 A/cm{sup 2}), it was reasonable to assume that DARHT can adopt this type of cathode to produce 2 kA (i.e., 10A/cm{sup 2}). However, it was later found that the 311XW has a higher radiation heat loss than the 612M and therefore resulted in a maximum operating temperature (as limited by filament damage) below that required to produce the high current. With the evidence provided by systematic emission tests using quarter-inch size cathodes, we confirmed that the 311XM (doped with scandium and has a osmium-ruthenium (M) coating) had the best combination of low work function and low radiation heat loss. Subsequently a 6.5-inch diameter 311XM cathode was installed in DARHT and 2 kA beam current was obtained on June 14, 2007. In testing the quarter-inch size cathode, we found that the beam current was sensitive to the partial pressure of various gases in the vacuum chamber. Furthermore, there was a hysteresis effect on the emission as a function of temperature. The phenomenon suggested that the work function of the cathode was dependent on the dynamic equilibrium between the diffusion of the impregnated material to the surface and the contamination rate from the surrounding gas. Water vapor was found to be the worst contaminant amongst the various gases that we have tested. Our data showed that the required vacuum for emitting at 10 A/cm{sup 2} is in the low 10{sup -8} Torr range.

25 ENERGY STORAGE↗

DARHT Axis II Cathode 12 (S/N 15) History as Recorded in the Historian and Shot Data Databases (DARHT Technical Note No. 501)

Long DARHT II injector cathode operating lifetimes are desirable for flash radiography of hydrodynamic tests at the dual-axis radiographic hydrotest facility (DARHT). The specification for cathode operating lifetime given to Spectra-Mat in the purchase orders for the 311X-M cathodes is ≥ 1000 hours at full operating temperature (~1120 °C). Of the five most-recent cathodes operated on DARHT II, only two have met this specification. It is desirable to have cathodes lifetimes considerably longer than the specified 1000 hours. In this report we present the thermal and vacuum history of cathode 12 (serial no. [S/N] 15), a 311X-M cathode, as recorded in the historian database and the shot data database. The hope is that by examining this history we can identify the parameter (or parameters) that are limiting the DARHT II 311X-M cathode lifetimes. This is the first in a series of 5 DARHT Tech Notes in which recent cathode thermal and vacuum histories are examined. The other tech notes in this series are DARHT Tech Notes Nos. 502 (cathode 13, S/N 19), 503 (cathode 14, S/N 20), 504 (cathode 15, S/N 21), and 505 (cathode 16, S/N 22). In DARHT Tech Note No. 506 we will compare the recorded thermal and vacuum histories of cathodes 12-16 and attempt to understand the cathode lifetime limitations based on the stored cathode data presented in DARHT Tech Notes 501-505 and other relevant information.

42 ENGINEERING↗

DARHT Axis II Cathode 16 (S/N 22) History as Recorded in the Historian and Shot Data Databases

Long DARHT II injector cathode operating lifetimes are desirable for flash radiography of hydrodynamic tests at the dual-axis radiographic hydrotest facility (DARHT). The specification for cathode operating lifetime given to Spectra-Mat in the purchase orders for the 311X-M cathodes is ≥ 1000 hours at full operating temperature (~1120 oC). Of the five most-recent cathodes operated on DARHT II, only two have met this specification. It is desirable to have cathodes lifetimes considerably longer than the specified 1000 hours. In this report we present the thermal and vacuum history of cathode 16 (serial no. [S/N] 22), a 311X-M cathode, as recorded in the historian database and the shot data database. The hope is that by examining this history we can identify the parameter (or parameters) that are limiting the DARHT II 311X-M cathode lifetimes. This is the fifth in a series of 5 DARHT Tech Notes in which recent cathode thermal and vacuum histories are examined. The other tech notes in this series are DARHT Tech Notes Nos. 501 (cathode 12, S/N 15), 502 (cathode 13, S/N 19), 503 (cathode 14, S/N 20), and 504 (cathode 15, S/N 21). In DARHT Tech Note No. 506 we will compare the recorded thermal and vacuum histories of cathodes 12-16 and attempt to understand the cathode lifetime limitations based on the stored cathode data presented in DARHT Tech Notes 501-505 and other relevant information.

43 PARTICLE ACCELERATORS↗

Effect of Ti-Al cathode composition on plasma generation and plasma transport in direct current vacuum arc

DC arc plasma from Ti, Al, and Ti{sub 1-x}Al{sub x} (x = 0.16, 0.25, 0.50, and 0.70) compound cathodes was characterized with respect to plasma chemistry and charge-state-resolved ion energy. Scanning electron microscopy, X-ray diffraction, and Energy-dispersive X-ray spectroscopy of the deposited films and the cathode surfaces were used for exploring the correlation between cathode-, plasma-, and film composition. Experimental work was performed at a base pressure of 10{sup −6} Torr, to exclude plasma-gas interaction. The plasma ion composition showed a reduction of Al of approximately 5 at. % compared to the cathode composition, while deposited films were in accordance with the cathode stoichiometry. This may be explained by presence of neutrals in the plasma/vapour phase. The average ion charge states (Ti = 2.2, Al = 1.65) were consistent with reference data for elemental cathodes, and approximately independent on the cathode composition. On the contrary, the width of the ion energy distributions (IEDs) were drastically reduced when comparing the elemental Ti and Al cathodes with Ti{sub 0.5}Al{sub 0.5}, going from ∼150 and ∼175 eV to ∼100 and ∼75 eV for Ti and Al ions, respectively. This may be explained by a reduction in electron temperature, commonly associated with the high energy tail of the IED. The average Ti and Al ion energies ranged between ∼50 and ∼61 eV, and ∼30 and ∼50 eV, respectively, for different cathode compositions. The attained energy trends were explained by the velocity rule for compound cathodes, which states that the most likely velocities of ions of different mass are equal. Hence, compared to elemental cathodes, the faster Al ions will be decelerated, and the slower Ti ions will be accelerated when originating from compound cathodes. The intensity of the macroparticle generation and thickness of the deposited films were also found to be dependent on the cathode composition. The presented results may be of importance for choice of cathodes for thin film depositions involving compound cathodes.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Highly durable platinum group metal-free catalyst fiber cathode MEAs for proton exchange membrane fuel cells

For this work, Fe-based platinum group metal (PGM)-free catalysts were incorporated into electrospun fiber mat or powder cathode membrane-electrode-assemblies (MEAs) with a Nafion 211 membrane and a Pt/C powder anode. Fabrication and characterization tests were performed on MEAs with: (1) a conventional powder cathode with a neat Nafion binder, (2) a fiber mat cathode with a Nafion/polyethylene oxide (PEO) binder, where PEO was extracted before MEA testing, (3) a powder cathode with a blended binder of Nafion and polyvinylidene fluoride (PVDF), and (4) a series of fiber mat cathodes with different Nafion/PVDF binder weight ratios. Cathode degradation occurred, with a loss in power output, in MEAs with a neat Nafion powder cathode or with a Nafion fiber cathode. In contrast, little or no power loss was observed for powder or fiber cathodes when the binder was a blend of Nafion and PVDF. The presence of hydrophobic PVDF drove water and electrogenerated peroxide out of the cathode, away from catalyst particles, which improved cathode durability, but PVDF also decreased the binder conductivity and slowed oxygen reduction kinetics, resulting in lower power densities. A 75:25 w:w Nafion:PVDF fiber cathode MEA was the best compromise for maximizing power and minimizing catalyst degradation. For such a cathode, with a PGM-free cathode catalyst loading of 3.0 mg cm –2 , a power density of 88 mW cm –2 at 0.5 V, 80 °C, and 200 kPa abs pressure was maintained for 80 h of continuous operation.

25 ENERGY STORAGE↗

Fundamental Investigations and Rational Design of Durable High-Performance SOFC Cathodes

The main objective of this project is to unravel the degradation mechanism of LSCF cathodes under realistic operating conditions with different types of contaminants, aiming towards the rational design of cathodes with high-performance and enhanced durability by combining a porous backbone (such as LSCF) with a thin catalyst coating. The mechanistic understanding will help us to optimize the composition and morphology of the catalyst layer and microstructure of the LSCF backbone for better performance and durability. More specifically, the technical objectives include: (1) to unravel the degradation mechanism of LSCF cathodes under realistic operating conditions with different types of contaminants using in situ and ex situ measurements performed on specially-designed cathodes; (2) to examine the microstructural and compositional evolution of LSCF cathodes as well as the cathode/electrolyte interfaces under realistic operating conditions; (3) to correlate the fuel cell performance instability and degradation with the microstructural and morphological evolution and surface chemistry change of the cathode under realistic operating conditions; (4) to explore new catalyst materials and electrode structures to enhance the stability of the LSCF cathode under realistic operating conditions; and (5) to validate the long term stability of the modified LSCF cathode in commercially available cells under realistic operating conditions. We have systematically evaluated LSCF cathodes in symmetrical cells and anode supported cells under realistic conditions with different types of contaminants such as humidity, CO 2 , and Cr. Electrochemical models for the design of test cells and understanding of mechanisms have been developed for the exploration of fundamental properties of electrode materials. It is demonstrated that the activity and stability of LSCF cathodes can be degraded by the introduction of contaminants. The microstructural and compositional evolution of LSCF cathodes as well as the cathode/electrolyte interfaces under realistic operating conditions has been studied. It is found that SrO readily segregated/enriched on the LSCF surface. More severe contamination conditions cause more SrO on surface. Novel catalyst coatings through particle depositions (PrOx) or continuous thin films (PNM) were successfully developed to improve the activity and stability of LSCF cathodes. Finally, we have demonstrated enhanced activity and stability of LSCF cathodes over longer periods of time in homemade and commercially available cells by an optimized PNM (dense film and particles) infiltration process, under clean air and realistic operating conditions (3% H 2 O, 5% CO 2 and direct Crofer contact). Both performance and durability of single cells with PNM coating has been enhanced compared with those without coating. Raman analysis of cathodes surface indicated that the intensity of SrCrO 4 was significantly decreased.

30 DIRECT ENERGY CONVERSION↗

A reduced temperature solid oxide fuel cell with three-dimensionally ordered macroporous cathode

Three-dimensionally ordered macroporous cathode was fabricated for a zirconia based micro-tubular solid oxide fuel cells (SOFCs). Three different cathodes (cathode A, no pore former; cathode B, with pore former (1.5 {micro}m in diameter); cathode C, with pore former (0.8 {micro}m in diameter)) were compared to investigate how the microstructure of it affected the cell performance at various operating temperatures. Micro-sized pores were well distributed within cathode B and C. The total porosity of cathode A is 35%, while it respectively reached 42 and 50% for cathodes B and C. At the same time, the specific surface area of them was 28.8 and 52.0% larger than that of the cathode A. As a result, the peak power density of the zirconia based cell, with cathode C, was 0.25 and 0.56 W cm{sup -2} at 550 and 600 C, while the respective value was just 0.11 and 0.30 W cm{sup -2} for the cell with cathode A. Thus, optimizing microstructure of cathode should be one of the best approaches for lowering the operating temperature for SOFCs.

30 DIRECT ENERGY CONVERSION↗

Effect of scandia doping method on the emission uniformity of scandate cathode with Sc{sub 2}O{sub 3}–W matrix

Graphical abstract: Emission uniformity of the cathodes prepared by mechanical mixing (a) and spray drying method (b). - Highlights: • The emission uniformity of scandate cathodes has been quantitively obtained. • The nanoparticles on the cathode surface lead to the electric field enhancement. • The cathode prepared by spray drying method exhibits good emission uniformity. - Abstract: Scandia doped tungsten matrix dispenser cathodes were manufactured using scandia doped tungsten powder prepared by mechanical mixing, liquid–solid doping and a spray drying method. It is found the macrostructure of the cathode depended on the powder preparation method. The cathode prepared using the powder prepared by spray drying method had a homogenous and porous matrix characterized with grains with a diameter of less than 1 μm and with many nanoparticles distributing uniformly around these grains. The cathode with submicron structure and uniform distribution of scandia exhibited good emission uniformity. The emission uniformity ΔJ/J of the cathode prepared by spray drying method was 0.17, about 6 times lower than that of the cathode prepared by mechanical mixing method. The calculation results showed that the nanoparticles led to electric field enhancement. A Ba–Sc–O multilayer on the cathode surface and nanoparticles distributing mainly on W grains contributed to the emission property of the cathode.

36 MATERIALS SCIENCE↗

In-Situ FTIR Detection of Transition Metal (TM)-Ion Dissolution From Cathodes in Li-Ion Batteries

Transition metal (TM) ions, commonly Ni and Mn, play a crucial role in Li-ion battery cathodes as the reaction centers for rapid redox reactions. A major challenge with TM-based cathodes is capacity degradation, particularly at higher operating voltages. This degradation is closely linked to the dissolution of TMs from the cathode materials and their subsequent deposition on the anode. This process not only modifies the surface structure of the cathode but, more significantly, alters the SEI composition on the anode [1-2]. The dissolution of TMs cations into a liquid electrolyte from cathode materials, such as Mn-ion dissolution from Mn-rich cathode (LMR), is detrimental to the cycling performance of Li-ion batteries [3-4]. Much attention has been paid to this issue but there remains a lack of characterization techniques which can detect the TM-ion dissolution from the cathode during electrochemical measurements. In our study, we use in-situ ATR-FTIR as an effective technique to probe the TM-ion dissolution from the cathode. We have first demonstrated the detrimental effects of TM ions on the electrochemical performance of Li-ion batteries by adding a small amount of TM salt (50 mM Mn(PF6)) to the electrolyte of a Li-ion coin cell with LFP and graphite electrode. We observed a rapid capacity fade after the first delithiation cycle. To investigate TM ion dissolution, we established a baseline IR spectrum for various TM solvation states (such as Mn and Ni) by measuring concentration-dependent IR spectra. This baseline spectrum helps us detect TM ion dissolution during battery cycling. In this work, we discuss in detail the effect of TM ions on the electrochemical performance of Li-ion batteries and the detection of TM ions during battery cycling using in-situ FTIR spectroscopy. We will compare TM dissolution between coated and uncoated cathodes to examine the effect of cathode coatings to mitigate degradation due to TM dissolution and cross-over from cathode to anode. References: (1) Zhan, C.; Wu, T.; Lu, J.; Amine, K. Dissolution, migration, anddeposition of transition metal ions in Li-ion batteries exemplified byMn-based cathodes - a critical review. Energy Environ. Sci. 2018, 11,243-257. (2) Jung, R.; Linsenmann, F.; Thomas, R.; Wandt, J.; Solchenbach,S.; Maglia, F.; Stinner, C.; Tromp, M.; Gasteiger, H. A. Nickel,Manganese, and Cobalt Dissolution from Ni-Rich NMC and TheirEffects on NMC622-Graphite Cells. J. Electrochem. Soc. 2019, 166,A378-A389. (3) Zhao, L.; Chenard, E.; Capraz, O. O.; Sottos, N. R.; White, S.R. Direct Detection of Manganese Ions in Organic Electrolyte by UV-Vis Spectroscopy. J. Electrochem. Soc. 2018, 165, A345-A348 (4) Zhang, Y.; Hu, A.; Xia, D.; Hwang, S.; Sainio, S.; Nordlund, D.;Michel, F. M.; Moore, R. B.; Li, L.; Lin, F. Operando characterization and regulation of metal dissolution and redeposition dynamics nearbattery electrode surface. Nat. Nanotechnol. 2023, 18, 790.

25 ENERGY STORAGE↗

Chromium Tolerant, Highly Active and Stable Electrocatalytic Internal Surface Coating for Cathode of Commercial SOFCs (Final Report)

This project is aimed to develop a chromium (Cr) tolerant, highly active, and stable coating layer on the internal surfaces of the porous composite cathode from commercially available SOFCs. Such coating layer was developed using the additive manufacturing process of Atomic Layer Deposition (ALD) and has been applied on the cathode consisting of either an electronic conductor of LaxSr 1-x MnyO 3-δ (LSM) or mixed ionic and electronic conducting La x Sr 1-x Co y Fe 1-y O 3-δ (LSCF). PI's work has demonstrated that the internal surface of cathode from the commercial cells, can be further tailored using ALD coating to dramatically enhance the cell performance. For instance, ALD layer consisting heterostructured nano composite of nano-Pt and nano-(Mn 0.8 Co 0.2 ) 3 O 4 oxide on the internal surface of porous LSM/YSZ cathode from SOFCs, has resulted in the large reduction of the cell polarizations resistance by up to 53%, and enormous increase of power density over 370%. For the cells with LSCF/Sm 2 O 3 doped CeO 2 (SDC) cathode, the conformal layer of nano-composite consisting of superjacent CoOx and subjacent minimum amount of Pt nano-grains has resulted in the power density enhancement by 126% for the large scale industry tubular cells at 750°C, and both the performance enhancement and nanostructure of the ALD layer are stable over ~ 2000 h continuous operation performed at industry test station. In the meanwhile, those ALD coating layer developed by PI's work is also inherently Cr-tolerant, and could act as physical barrier for preventing Cr diffusion into the cathode backbone, so as to mitigate the Cr poisoning effect on the cathode. In this project, the impact of Cr on the performance of those ALD coated commercial cells has been evaluated. Based on evolution of the cell performance, the ALD coating layer chemistry and ALD coating layer thickness has been optimized to maximize the overall Cr tolerance, cell power density and cell longevity. Different ALD coating has been applied onto the internal surface of LSM/YSZ and LSCF/SDC backbone respectively. The architecture/scaffold structures on the internal surface of different cathode, designed by this project, was catalogued and analyzed using High Resolution Transmission Electron Microscopy (HRTEM), and cell power/durability performance are assured via comprehensive electrochemical performance testing in the industry operation relevant conditions. The impact of the electrochemical operation current density, the water humidity, the cell operation temperature, and cell operation duration on the Cr tolerance of ALD coated cells has been systematically investigated. There is completely different nanostructure degradation mechanisms between LSM and LSCF cells induced by Cr contamination. For the LSCF/SDC baseline cell, With the Cr source, there is no apparent Sr surface segregation phase even for the baseline cell operated for 3000 h at 750 °C. With the Cr source, there is significant amorphous (SrCr)Ox phase accumulated in the original pore region. For the commercial baseline cells, Cr contaminants on the LSM electrode severely impacted the entire cell's electrochemical performance and nanostructure degradation. Those degradations include (1). Peak power density loss of 64 % after 109 h of operation. The dramatic increase in Rp (2). They are cracking at LSM/SSZ interface, LSM grains. SSZ remains intact but with (CrMn)Ox. By contrast, ALD coating (MnCo)Ox/Pt dramatically improves the Cr resistance, as follows (1). ALD-coated cell with a power density is 280-380 % of the baseline cell, depending on the ALD layer thickness. (2). For a cell with a 20 nm thick ALD layer, there is a large performance enhancement (> 200 % power density) induced by ALD coating of Cr-tolerant Mn 0.8 Co 0.2 Ox. (3). For a cell with a 20 nm thick ALD layer, after 168 h at 750 °C power density of the ALD-coated cell is ~ 600% of that baseline cell upon operation with Cr contamination for 109 h. The ALD coating on the internal surface of cathode developed by this project integrated multi-functions. Those multi-functions include (1). Dramatically improving the cell power density for the commercial cells; (2). Dramatically improving contamination resistance of the cathode, for being an excellent protection coating layer sealing off Cr contamination. (3). Dramatically increasing the cell longevity by potentially preventing the microstructure evolution and grain coarsening of the cathode. Overall, this project will provide a simple solution to simultaneously enhance power density and increase the reliability, robustness, and endurance of commercial SOFCs, over the entire operating temperature range of 650-800 °C. For the inherently functional SOFC, the ALD coating of LSM based cathode mitigate the Cr-contamination. Power density of ALD-coated cell is ~ 600% of that baseline cell upon operation with Cr contamination. In addition to SOFCs, the novel on-demand design approach and creation of multifunctional heterogeneous architecture on the electrode surface presented in this work opens further research for their application in other types of fuel cells, batteries, and sensors for which electrochemical reactions on the surface are similarly critical.

36 MATERIALS SCIENCE↗

High-Performance Low-Cobalt Cathode Materials for Li-ion Batteries

The layer-structured Li[Ni x Co y Mn 1-x-y ]O 2 (NCM) cathode materials have been the best choice for increasing electric vehicle driving distance per charge. The high Ni layered oxide represents successfully commercialized NCM cathodes (such as NCM622 and NCA) in lithium-ion batteries (LIBs) for EV applications due to their high energy density and acceptable cycling stability. However, the price of cobalt, the key element within LIBs for stability, has nearly tripled over the past few years due to increased demand from the cell phone industry. As mentioned in the DOE Funding Opportunity Announcement, the current materials shortage will also cause speculation for a future global shortage. Therefore, to meet the requirement and sustainability of the next-generation long-range and low-cost EVs, developing cathode materials with low-Co content to achieve higher energy density and lower cost is both essential and urgent. The overarching objective of this work is to develop stabilized NCM cathode materials with low Co content (namely LiNi x Co y Mn 1-x-y O 2 , y ≤ 0.04) to meet DOE’s goal of reducing Co loading below 50 mg Wh -1 while maintaining energy density greater than 600 Wh kg -1 based on cathode material. Via various dopings and coatings scalable methods, we explored and enhanced the cycling performance of low-cobalt cathodes. The final obtained NCM cathodes paired with graphite anode aim to deliver batteries with a high initial specific energy density of over 240 Wh kg -1 and a low capacity fading rate of less than 20% in 1000 cycles under a C/3 discharge rate. To accomplish this goal, a multidisciplinary team with several co-investigators has been formed from three organizations: The Pennsylvania State University (PSU), Oak Ridge National Laboratory (ORNL), and Pacific Northwest National Laboratory (PNNL). The PI and co-investigators are Dr. Donghai Wang (PI) from PSU with expertise in the synthesis of nanostructured materials and manipulation of interfacial properties of electrochemically active materials, Dr. Jagjit Nanda, with substantial knowledge of and expertise in state-of-the-art cathodes from ORNL, Dr. Chao-Yang Wang with significant experience in advanced cell design and fabrication and cell diagnostics from PSU, and Dr. Chongmin Wang with world-wide known expertise of advance atomic scale characterization of electrode materials from PNNL. Furthermore, this project will leverage and synergistically work with the current DOE-funded programs on battery materials at PSU and ORNL and electrode materials characterization at PNNL. During this funded period, we have accomplished milestones stated as follows: • Scale up production of LiFePO 4 (LFP) coated NCM811 with a production of 300g/batch. Fifteen (≥2 Ah) pouch cells with LFP-coated NCM811 cathode are delivered. Self-evaluated pouch cells in PSU show superior over 80% capacity retention performance even after 1500 cycles at C/3 rate. • Various cations (Al, Ti, Zr, and Mo) substitute cobalt in low-cobalt partially and Co-free cathodes. Their effects on crystal structure and electrochemical behavior are explored. • Phosphate compounds as coating materials represent promising surface protection precursors for low-cobalt cathode materials. Therefore, several metal phosphates were selected for improving the NMC cycling performance and are regarded as effective approaches for a scalable and practical surface protection method. • Production of NCM92, where Nickel content is 92% among transition metals, is scaled up from synthesis to coating and heat treatment procedures. Fifteen 2.7Ah pouch cells with Ti-doped NCM92 cathodes and industrial graphite anode are delivered to Idaho National Lab for testing.

25 ENERGY STORAGE↗

Enabling Extreme Fast-Charging: Challenges at the Cathode and Mitigation Strategies

We report charging lithium-ion batteries (LiBs) in 10 to 15 min via extreme fast-charging (XFC) is important for the widespread adoption of electric vehicles (EVs). Lately, the battery research community has focused on identifying XFC bottlenecks and determining novel design solutions. Like other LiB components, cathodes can present XFC bottlenecks, especially when considering long-term battery life. Therefore, it is necessary to develop a comprehensive understanding of how XFC conditions degrade LiB cathodes. The present article reviews relevant cathode-focused studies and summarizes the current understanding regarding cathode performance and aging issues under XFC conditions. Dominant aging modes and mechanisms are identified at different length-scales with electrochemical correlations for LiNi x Mn y Co z O 2 (NMC)-based cathodes. A range of electrochemical techniques and models provide key insights into cathode performance and life issues. A suite of multimodal and multiscale microscopy and X-ray techniques is surveyed to quantify chemical, structural, and crystallographic NMC-cathode degradation. Cathode cycle-life is scaled to equivalent EV miles to illustrate how cathode degradation translates to real-world scenarios and quantifies cathode-related bottlenecks that hinder XFC adoption. Finally, the article discusses several cathode cycle-life aging mitigation strategies with example case studies and identifies remaining challenges.

25 ENERGY STORAGE↗

Modeling and validation of single-chamber microbial fuel cell cathode biofilm growth and response to oxidant gas composition

This work describes experiments and computational simulations to analyze single-chamber, air-cathode microbial fuel cell (MFC) performance and cathodic limitations in terms of current generation, power output, mass transport, biomass competition, and biofilm growth. Steady-state and transient cathode models were developed and experimentally validated. Two cathode gas mixtures were used to explore oxygen transport in the cathode: the MFCs exposed to a helium-oxygen mixture (heliox) produced higher current and power output than the group of MFCs exposed to air or a nitrogen-oxygen mixture (nitrox), indicating a dependence on gas-phase transport in the cathode. Multi-substance transport, biological reactions, and electrochemical reactions in a multi-layer and multi-biomass cathode biofilm were also simulated in a transient model. The transient model described biofilm growth over 15 days while providing insight into mass transport and cathodic dissolved species concentration profiles during biofilm growth. Lastly, simulation results predict that the dissolved oxygen content and diffusion in the cathode are key parameters affecting the power output of the air-cathode MFC system, with greater oxygen content in the cathode resulting in increased power output and fully-matured biomass.

59 BASIC BIOLOGICAL SCIENCES↗

Joule heat generation in thermionic cathodes of high-pressure arc discharges

The nonlinear surface heating model of plasma-cathode interaction in high-pressure arcs is extended to take into account the Joule effect inside the cathode body. Calculation results are given for different modes of current transfer to tungsten cathodes of different configurations in argon plasmas of atmospheric or higher pressures. Special attention is paid to analysis of energy balances of the cathode and the near-cathode plasma layer. In all the cases, the variation of potential inside the cathode is much smaller than the near-cathode voltage drop. However, this variation can be comparable to the volt equivalent of the energy flux from the plasma to the cathode and then the Joule effect is essential. Such is the case of the diffuse and mixed modes on rod cathodes at high currents, where the Joule heating causes a dramatic change of thermal and electrical regimes of the cathode. The Joule heating has virtually no effect over characteristics of spots on rod and infinite planar cathodes.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Charge state, angular distribution, and kinetic energy of ions from multicomponent-cathodes in vacuum arc devices

We present research results on vacuum arc plasma produced with multicomponent cathode made of several different elements. The ion mass-to-charge-state spectra of the plasmas were studied by time-of-flight spectrometry. The angular distributions of different ion species were measured, and the kinetic energy of their directed (streaming) motion was determined. It is shown that the fractional composition of ions of different cathode components in the plasma flow from the cathode spot closely matches the fractional content of these components in the composite cathode. The charge states of ions of the various cathode components are determined by the average electron temperature in the cathode spot plasma. The angular distribution of lower mass ions in the plasma from a multicomponent cathode is less isotropic and broader than for the plasma from a single-component cathode of the same light element. The directed kinetic energies of the ions of the different components for plasma from a multicomponent cathode are lower for lighter elements and greater for heavier elements compared to the ion directed energy for plasmas from single-component cathodes made of the same materials. The physical processes responsible for these changes in the ion charge states in multicomponent-cathode vacuum arc plasma are discussed.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Effect of N{sub 2} and Ar gas on DC arc plasma generation and film composition from Ti-Al compound cathodes

DC arc plasma from Ti, Al, and Ti{sub 1−x}Al{sub x} (x = 0.16, 0.25, 0.50, and 0.70) compound cathodes has been characterized with respect to plasma chemistry (charged particles) and charge-state-resolved ion energy for Ar and N{sub 2} pressures in the range 10{sup −6} to 3 × 10{sup −2} Torr. Scanning electron microscopy was used for exploring the correlation between the cathode and film composition, which in turn was correlated with the plasma properties. In an Ar atmosphere, the plasma ion composition showed a reduction of Al of approximately 5 at. % compared to the cathode composition, while deposited films were in accordance with the cathode stoichiometry. Introducing N{sub 2} above ∼5 × 10{sup −3} Torr, lead to a reduced Al content in the plasma as well as in the film, and hence a 1:1 correlation between the cathode and film composition cannot be expected in a reactive environment. This may be explained by an influence of the reactive gas on the arc mode and type of erosion of Ti and Al rich contaminations, as well as on the plasma transport. Throughout the investigated pressure range, a higher deposition rate was obtained from cathodes with higher Al content. The origin of generated gas ions was investigated through the velocity rule, stating that the most likely ion velocities of all cathode elements from a compound cathode are equal. The results suggest that the major part of the gas ions in Ar is generated from electron impact ionization, while gas ions in a N{sub 2} atmosphere primarily originate from a nitrogen contaminated layer on the cathode surface. The presented results provide a contribution to the understanding processes of plasma generation from compound cathodes. It also allows for a more reasonable approach to the selection of composite cathode and experimental conditions for thin film depositions.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Investigation of the flickering of La{sub 2}O{sub 3} and ThO{sub 2} doped tungsten cathodes

Short-arc lamps are equipped with tungsten electrodes due to their ability to withstand a high thermal load during operation. Nominal currents of more than one hundred amperes lead to a cathode tip temperature near the melting point of tungsten. To reduce the electrode temperature and, thereby, to increase the maintenance of such lamps, ThO{sub 2} or tentatively La{sub 2}O{sub 3} are added to the electrode material. They generate a reduced work function by establishing a monolayer of emitter atoms on the tungsten surface. Emitter enrichments on the lateral surface of doped cathodes are formed. They are traced back to transport mechanisms of emitter oxides in the interior of the electrode and on the electrode surface in dependence of the electrode temperature and to the redeposition of vaporized and ionized emitter atoms onto the cathode tip by the electric field in front. The investigation is undertaken by means of glow discharge mass spectrometry, scanning electron microscope images, energy dispersive x-ray spectroscopy, and through measurements of the optical surface emissivity. The effect of emitter enrichments on the stability of the arc attachment is presented by means of temporally resolved electrode temperature measurements and by measurements of the luminous flux from the cathode-near plasma. They show that the emitter enrichments on the lateral surface of the cathode are attractive for the arc attachment if the emitter at the cathode tip is depleted. In this case, it moves along the lateral surface from the cathode tip to sections of the cathode with a reduced work function. It induces a temporary variation of the cathode tip temperature and of the light intensity from the cathode-near plasma, a so-called flickering. In particular, in case of lanthanated cathodes, strong flickering is observed.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effect of thermionic cathode heating current self-magnetic field on gaseous plasma generator characteristics

The performance capabilities of the PINK, a plasma generator with a thermionic cathode mounted in the cavity of a hollow cathode, depending for its operation on a non-self-sustained low-pressure gas discharge have been investigated. It has been shown that when a single-filament tungsten cathode 2 mm in diameter is used and the peak filament current is equal to or higher than 100 A, the self-magnetic field of the filament current significantly affects the discharge current and voltage waveforms. This effect is due to changes in the time and space distributions of the emission current density from the hot cathode. When the electron mean free path is close to the characteristic dimensions of the thermionic cathode, the synthesized plasma density distribution is nonuniform and the cathode is etched nonuniformly. The cathode lifetime in this case is 8–12 h. Using a cathode consisting of several parallel-connected tungsten filaments ∼0.8 mm in diameter moderates the effect of the self-magnetic field of the filament current and nearly doubles the cathode lifetime. The use of this type of cathode together with a discharge igniting electrode reduces the minimum operating pressure in the plasma generator to about one third of that required for the generator operation with a single-filament cathode (to 0.04 Pa)

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗