Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Titanium”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 397 records · Page 22

Compressive behavior of titanium alloy skin-stiffener specimens selectively reinforced with boron-aluminum composite

A method of selectively reinforcing a conventional titanium airframe structure with unidirectional boron-aluminum composite attached by brazing was successfully demonstrated in compression tests of short skin-stiffener specimens. In a comparison with all-titanium specimens, improvements in structural performance recorded for the composite-reinforced specimens exceeded 25 percent on an equivalent-weight basis over the range from room temperature to 700 K (800 F) in terms of both initial buckling and maximum strengths. Performance at room temperature was not affected by prior exposure at 588 K (600 F) for 1000 hours in air or by 400 thermal cycles between 219 K and 588 K (-65 F and 600 F). The experimental results were generally predictable from existing analytical procedures. No evidence of failure was observed in the braze between the boron-aluminum composite and the titanium alloy.

Herring, H. W.↗

The role of hydrogen in hot-salt stress corrosion cracking of titanium-aluminum alloys

Additional support is presented for the previously proposed role of hydrogen as an embrittling agent in hot-salt stress corrosion cracking of titanium-aluminum alloys. The main source of hydrogen formed during the reactions of titanium alloys with hot salt was identified as water associated with the salt. Hydrogen is produced by the reaction of an intermediate (hydrogen halide) with the alloy rather than from metal-water reactions. The fracture mode of precracked tensile specimens was ductile when the specimens were tested in air, and brittle when tests were made in high-pressure hydrogen. Stressed titanium-aluminum alloys also were cracked by bombardment with hydrogen ions produced in a proton accelerator. The approximate concentrations of the hydrogen ions in the alloys were calculated.

Ondrejcin, R. S.↗

Fabrication of the titanium transition ring of the Large Space Telescope (LST)

The fabrication of the titanium transition ring is summarized. The transition ring assembly was designed for the large space telescope and consists of two large titanium rings bolted together. The cross section dimensions of the assembly are 13-inches wide by 7-inches thick. The fabrication processes are discussed, and it is concluded that the work involved fabricating the largest titanium forging ever made.

Klein, L. A.↗

Properties of Hot Pressed Titanium Alloy Powders for Cryogenic Applications.

Evaluation of strength and toughness of hot-pressed titanium alloy powders at room and at cryogenic temperatures. The purpose was to determine how the mechanical properties of solid bodies formed from powder would compare with wrought specimens of the same size and with the same chemical analysis. It was found that of five titanium powder-making processes investigated, only the Rotating Electrode Process (REP) was capable of producing ELI-grade titanium alloy powder. Blocks hot-pressed from spherical REP powders had tensile properties equivalent to or better than those obtained from wrought bar.

Friedman, G. I.↗

Time exposure studies on stress corrosion cracking of aluminum 2014-T6, 2219-T87, 2014-T651, 7075-T651, and titanium 6Al-4V

The effect of a constant applied stress in crack initiation of aluminum 2014-T6, 2219-T87, 2014-T651, 7075-T651 and titanium 6Al-4V has been investigated. Aluminum c-ring specimens (1-inch diameter) and u-band titanium samples were exposed continuously to a 3.5% NaCl solution (pH 7) and organic fluids of ethyl, methyl, and iso-propyl alcohol (reagent purity), and demineralized distilled water. Corrosive action was observed to begin during the first and second day of constant exposure as evidenced by accumulation of hydrogen bubbles on the surface of stressed aluminum samples. However, titanium stressed specimens showed no reactions to its environment. Results of this investigation seems to suggest that aluminum 2014-T6, aluminum 7075-T651 and aluminum 2014-T651 are susceptible to stress corrosion cracking in chloride solution (NaCl), while aluminum 2219-T87 seem to resist stress corrosion cracking in sodium chloride at three levels of stress (25%, 50%, and 75% Y.S.). In organic fluids of methyl, ethyl, and iso-propyl alcohol, 2014-T6 and 7075-T651 did not fail by SCC; but 2014-T651 was susceptible to SCC in methly alcohol, but resistant in ethyl alcohol, iso-propyl alcohol and demineralized distilled water.

Terrell, J.↗

Aqueous chloride stress corrosion cracking of titanium: A comparison with environmental hydrogen embrittlement

The physical characteristics of stress corrosion cracking of titanium in an aqueous chloride environment are compared with those of embrittlement of titanium by a gaseous hydrogen environment in an effort to help contribute to the understanding of the possible role of hydrogen in the complex stress corrosion cracking process. Based on previous studies, the two forms of embrittlement are shown to be similar at low hydrogen pressures (100 N/sqm) but dissimilar at higher hydrogen pressures. In an effort to quantify this comparison, tests were conducted in an aqueous chloride solution using the same material and test techniques as had previously been employed in a gaseous hydrogen environment. The results of these tests strongly support models based on hydrogen as the embrittling species in an aqueous chloride environment. Further, it is shown that if hydrogen is the causal species, the effective hydrogen fugacity at the surface of titanium exposed to an aqueous chloride environment is equivalent to a molecular hydrogen pressure of approximately 10 N/sqm.

Nelson, H. G.↗

The effect of microstructure on the fracture toughness of titanium alloys

The high-strength titanium alloys are widely used in aircraft and aerospace structures due to their high strength to density ratios. In such applications, the fracture toughness rather than the strength is often the factor which requires larger size sections and lower useful payloads. The response of the strength and toughness of titanium alloys was analyzed generally without regard to the fracture mode or the effect of microstructure on the fracture mechanisms. Research on the fracture mechanisms in aluminum alloys and steels showed that the toughness may be improved by decreasing the sizes of inclusions and sub-micron precipitates. An investigation was conducted to study the fracture mechanisms in titanium alloys which may lead to suggestions for the improvement of the fracture toughness without a corresponding loss in strength.

Vanstone, R. H.↗

An investigation of chatter and tool wear when machining titanium

The low thermal conductivity of titanium, together with the low contact area between chip and tool and the unusually high chip velocities, gives rise to high tool tip temperatures and accelerated tool wear. Machining speeds have to be considerably reduced to avoid these high temperatures with a consequential loss of productivity. Restoring this lost productivity involves increasing other machining variables, such as feed and depth-of-cut, and can lead to another machining problem commonly known as chatter. This work is to acquaint users with these problems, to examine the variables that may be encountered when machining a material like titanium, and to advise the machine tool user on how to maximize the output from the machines and tooling available to him. Recommendations are made on ways of improving tolerances, reducing machine tool instability or chatter, and improving productivity. New tool materials, tool coatings, and coolants are reviewed and their relevance examined when machining titanium.

Sutherland, I. A.↗

Stress corrosion cracking of titanium alloys

The effect of hydrogen on the properties of metals, including titanium and its alloys, was investigated. The basic theories of stress corrosion of titanium alloys are reviewed along with the literature concerned with the effect of absorbed hydrogen on the mechanical properties of metals. Finally, the basic modes of metal fracture and their importance to this study is considered. The experimental work was designed to determine the effects of hydrogen concentration on the critical strain at which plastic instability along pure shear directions occurs. The materials used were titanium alloys Ti-8Al-lMo-lV and Ti-5Al-2.5Sn.

Statler, G. R.↗

Thin-film diffusion brazing of titanium alloys

A thin film diffusion brazing technique for joining titanium alloys by use of a Cu intermediate is described. The method has been characterized in terms of static and dynamic mechanical properties on Ti-6Al-4V alloy. These include tensile, fracture toughness, stress corrosion, shear, corrosion fatigue, mechanical fatigue and acoustic fatigue. Most of the properties of titanium joints formed by thin film diffusion brazing are equal or exceed base metal properties. The advantages of thin film diffusion brazing over solid state diffusion bonding and brazing with conventional braze alloys are discussed. The producibility advantages of this process over others provide the potential for producing high efficiency joints in structural components of titanium alloys for the minimum cost.

Mikus, E. B.↗

The oxidation of titanium films saturated with nitrogen at 300 K

In a two-chamber system designed for physical adsorption studies, a titanium film was deposited and exposed to nitrogen. Oxygen was then admitted into the system. However, the presence of oxygen could not be detected by the mass spectrometer during the first 300 seconds of oxygen admission. On the basis of the data it is assumed that the capture probability of the nitrogen-saturated titanium film for oxygen is very nearly 1. Based on this assumption, the titanium film adsorbed approximately 3 monolayers of oxygen.

Outlaw, R. A.↗

Weld-bonded titanium structures

Structurally stronger titanium articles are produced by a weld-bonding technique comprising fastening at least two plates of titanium together using spotwelding and curing an adhesive interspersed between the spot-weld nuggets. This weld-bonding may be employed to form lap joints or to stiffen titanium metal plates.

Vaughan, R. W.↗

Detection of tightly closed flaws by nondestructive testing (NDT) methods in steel and titanium

X-radiographic, liquid penetrant, ultrasonic, eddy current and magnetic particle testing techniques were optimized and applied to the evaluation of 4340 steel (180 KSI-UTS) and 6Al-4V titanium (STA) alloy specimens. Sixty steel specimens containing a total of 176 fatigue cracks and 60 titanium specimens containing a total of 135 fatigue cracks were evaluated. The cracks ranged in length from .043 cm (0.017 inch) to 1.02 cm (.400 inch) and in depth from .005 cm (.002 inch) to .239 cm (.094 inch) for steel specimens. Lengths ranged from .048 cm (0.019 inch) to 1.03 cm (.407 inch) and depths from 0.010 cm (.004 inch) to .261 cm (0.103 inch) for titanium specimens. Specimen thicknesses were nominally .152 cm (0.060 inch) and 0.635 cm (0.250 inch) and surface finishes were nominally 125 rms. Specimens were evaluated in the "as machined" surface condition, after etch surface and after proof loading in a randomized inspection sequence.

Rummel, W. D.↗

Effects of service environments on aluminum-brazed titanium (ABTi)

Aluminum brazed titanium (ABTi) structures were evaluated during prolonged exposure to extreme environments: elevated temperature exposure to airline service fluids, hydraulic fluid, and seawater, followed by laboratory corrosion tests. Solid-face and perforated face honeycomb sandwich panel specimens, stressed panel assemblies, and faying surface brazed joints were tested. The corrosion resistance of ABTi is satisfactory for commercial airline service. Unprotected ABTi proved inherently resistant to attack by all of the extreme service aircraft environments except: seawater at 700 K (800 F) and above, dripping phosphate ester hydraulic fluid at 505 K (450 F), and a marine environment at ambient temperature. The natural oxides and deposits present on titanium surfaces in airline service provide protection against hot salt corrosion pitting. Coatings are required to protect titanium dripping phosphate ester fluid at elevated temperatures and to protect exposed acoustic honeycomb parts against corrosion in a marine environment.

Cotton, W. L.↗

Graphite/epoxy pressure vessels lined with ultra-thin titanium

Filament-wound, titanium-lined, fiber/epoxy pressure vessels were made using a very high-strength graphite fiber (3570-MPa typical fiber strength). The 0.254-mm-thick titanium liner was used to improve burst performance. The pressure vessels achieved an average burst performance of 241 kPa.cu m/kg, and the fatigue life of titanium liners with good welds (cycled to 50% of the average expected burst pressure) was in excess of 2000 cycles.

Hamstad, M. A.↗

Experimentally reproduced textures and mineral chemistries of high-titanium mare basalts

Many of the textures, morphologies, and mineral chemistries of the high-titanium mare basalts have been experimentally duplicated using single-stage cooling histories. Lunar high-titanium mare basalts are modeled in a 1 m thick gravitationally differentiating flow based on cooling rates, thermal models, and modal olivine contents. The low-pressure equilibrium phase relations of a synthetic high-titanium basalt composition were investigated as a function of oxygen fugacity, and petrographic criteria are developed for the recognition of phenocrysts which were present in the liquid at the time of eruption.

Usselman, T. M.↗

Fretting wear of iron, nickel, and titanium under varied environmental conditions

Fretting wear experiments were conducted on high purity iron, nickel and titanium in air under conditions of varied humidity and temperature, and in nitrogen. For iron and titanium, maximum fretting occurred at 10 and 30 percent relative humidity respectively. Nickel showed a minimum in fretting wear at about 10 percent relative humidity. With increasing temperature, all three metals initially showed reduced fretting wear, with increasing wear observed as temperatures increased beyond 200-300 C. For titanium, dramatically reduced fretting wear was observed at temperatures above 500 C, relatable to a change in oxidation kinetics. All three metals showed much less fretting wear in N2 with the presence of moisture in N2 having a proportionally stronger effect than in air.

Bill, R. C.↗

Titanium-alloy, metallic-fluid heat pipes for space service

Reactivities of titanium limit its long-term terrestrial use for unprotected heat-pipe envelopes to about 870 K (1100 F). But this external thermochemical limitation disappears when considerations shift to space applications. In such hard-vacuum utilization much higher operating temperatures are possible. Primary restrictions in space environment result from vaporization, thermal creep, and internal compatibilities. Unfortunately, a respected head-pipe reference indicates that titanium is compatible only with cesium from the alkali-metal working-fluid family. This problem and others are subjects of the present paper which advocates titanium-alloy, metallic-fluid heat pipes for long-lived, weight-effective space service between 500 and 1300 K (440 and 1880 F).

Morris, J. F.↗