Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “SLIDING FRICTION”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 397 records · Page 22

Adhesion and transfer of PTFE to metals studied by auger emission spectroscopy

The adhesion and transfer of polytetrafluoroethylene (PTFE) to metals in ultrahigh vacuum has been studied using Auger emission spectroscopy. The transfer was effected both by compressive static contact and by sliding contact. The transfer observed after static contact was independent of the chemical constitution of the substrate. Electron induced desorption of the fluorine in the transferred PTFE showed that the fluorine had no chemical interaction with the metal substrate. The coefficient of friction on metals was independent of the chemical constitution of the substrate. However, sliding PTFE on soft metals such as aluminum, generated wear fragments that lodged in the PTFE and machined the substrate.

Pepper, S. V.↗

Adhesion and transfer of polytetrafluorethylene to metals studied by Auger emission spectroscopy

The adhesion and transfer of polytetrafluoroethylene (PTFE) to metals in ultrahigh vacuum were studied. The transfer was effected both by compressive static contact and by sliding contact. The transfer observed after static contact was independent of the chemical constitution of the substrate. Electron-induced desorption of the fluorine in the transferred PTFE showed that the fluorine had no chemical interaction with the metal substrate. The coefficient of friction on metals was independent of the chemical constitution of the substrate. However, sliding PTFE on soft metals, such as aluminum, generated wear fragments that lodged in the PTFE and machined the substrate.

Pepper, S. V.↗

Effect of load, area of contact, and contact stress on the wear mechanisms of a bonded solid lubricant film

A pin on disk type of friction and wear apparatus was used to study the effect of load, contact stress and rider area of contact on the friction and wear properties of polyimide bonded graphite fluoride films. Different rider area contacts were obtained by initially generating flats (with areas of 0.0035, 0.0071, 0.0145, and 0.0240 cm) on 0.476-cm radius hemispherically tipped riders. Different projected contact stresses were obtained by applying loads of 2.5- to 58.8-N to the flats. Two film wear mechanisms were observed. The first was found to be a linear function of contact stress and was independent of rider area of contact. The second was found to increase exponentially as the stress increased. The second also appeared to be a function of rider contact area. Wear equations for each mechanism were empirically derived from the experimental data. In general, friction coefficients increased with increasing rider contact area and with sliding duration. This was related to the build up of thick rider transfer films.

Fusaro, R. L.↗

Effect of load, area of contact, and contact stress on the tribological properties of polyimide bonded graphite fluoride films

A pin-on-disk type of friction and wear apparatus was used to study the effect of load, contact stress and rider area of contact on the friction and wear properties of polyimide-bonded graphite fluoride films. Different rider area contacts were obtained by initially generating flats (with areas of 0.0035, 0.0071, 0.0145, and 0.0240 cm) on 0.476-cm radius hemispherically-tipped riders. Different projected contact stresses were obtained by applying loads of 2.5-to 58.8-N to the flats. Two film wear mechanisms were observed. The first was found to be a linear function of contact stress and was independent of rider area of contact. The second was found to increase exponentially as the stress increased. The second also appeared to be a function of rider contact area. Wear equations for each mechanism were empirically derived from the experimental data. In general, friction coefficients increased with increasing rider contact area and with sliding duration. This was related to the build-up of thick rider transfer films.

Fusaro, R. L.↗

Two-Axis Track Rollers

Compact, lightweight design reduces side friction. Set of proposed two-axis track rollers enables sliding door to follow curved track in both directions without binding. Combination of cylindrical cam-follower-type roller and large ball end roller. Intended for use on sliding hatch covers on proposed Space Station Freedom, also useful on Earth to ensure ease and reliability of motion in sliding doors, windows, covers, and partitions.

Melinick, John M.↗

Lyapunov function-based control laws for revolute robot arms - Tracking control, robustness, and adaptive control

A new class of joint level control laws for all-revolute robot arms is introduced. The analysis is similar to a recently proposed energy-like Liapunov function approach, except that the closed-loop potential function is shaped in accordance with the underlying joint space topology. This approach gives way to a much simpler analysis and leads to a new class of control designs which guarantee both global asymptotic stability and local exponential stability. When Coulomb and viscous friction and parameter uncertainty are present as model perturbations, a sliding mode-like modification of the control law results in a robustness-enhancing outer loop. Adaptive control is formulated within the same framework. A linear-in-the-parameters formulation is adopted and globally asymptotically stable adaptive control laws are derived by simply replacing unknown model parameters by their estimates (i.e., certainty equivalence adaptation).

Wen, John T.↗

The Effects of Acid Passivation, Tricresyl Phosphate Pre-Soak, and UV/Ozone Treatment on the Tribology of Perfluoropolyether-Lubricated 440C Stainless Steel Couples

The boundary-lubrication performance of perfluoropolyether (PFPE) thin films in the presence of passivated 440 C stainless steel is presented. The study utilized a standard ball-on-disc tribometer. Stainless steel surfaces were passivated with one of four techniques: 1) submersion in a chromic acid bath for 30 minutes at 46 C, 2) submersion in a chromic acid bath for 60 minutes at 56 C, 3) submersion in a tricresyl phosphate (TCP) bath for 2 days at 107 C, or 4) UV/Ozone treated for 15 minutes. After passivation, each disc had a 400 A film of PFPE (hexafluoropropene oxide) applied to it reproducibly (+/- 20%) and uniformly (+/- 15%) using a film deposition device. The lifetimes of these films were quantified by measuring the number of sliding wear cycles required to induce an increase in the friction coefficient from an initial value characteristic of the lubricated wear couple to a final, or failure value, characteristic of an unlubricated, unpassivated wear couple. The lubricated lifetime of the 440 C couple was not altered as a result of the various passivation techniques. The resulting surface chemistry of each passivation technique was examined using X-ray Photoelectron Spectroscopy (XPS). It was found that chromic acid passivation altered the Cr to Fe ratio of the surface. TCP passivation resulted in a FePO4 layer on the surface, while UV/Ozone passivation only removed the carbonaceous contamination layer. None of the passivation techniques were found to dramatically increase the oxide film thickness.

Shogrin, Bradley A.↗

Some wear studies on aircraft brake systems

An initial investigation of worn surfaces in friction pads and steel rotors used in current aircraft brakes was carried out using electron microprobe and X-ray diffraction analysis. It consists of the topographical study and the analysis of chemical element distribution. Based upon this initial examination, two approaches, microscopic and macroscopic have been conducted to interpret and formulate the wear mechanism of the aircraft brake materials. Microscopically, the wear particles were examined. The initiation and growth of surface cracks and the oxidation were emphasized in this investigation. Macroscopically, it has been found that, for the current copper based brake material sliding against 17-22 AS steel in a caliper brake, the surface temperature raised due to frictional heat is nonlinearly proportional to the load applied and slide time with speed at 1750 rpm. The wear of brake materials is then proportional to this temperature and is also a function of the melting temperature for copper.

Ho, T. L.↗

Consideration of materials for aircraft brakes

A study has been made of the frictional behavior of several aircraft brake materials using a simple high-temperature Falex-type apparatus. Tests were run at velocities of seven ft/minute; loads to 600 pounds and temperatures to 700 C. The data for these brake materials sliding against a variety of steels and other materials indicate a large reduction in friction due to surface oxidation in the temperature range 250 to 300 C. It also was found that the retention of this oxide was a function of the temperature changes. With increasing temperature the oxide was removed, while with reducing temperature it was retained. Frictional behavior was more characteristic of the steel than the brake material.

Peterson, M. B.↗

Friction and wear of iron and nickel in sodium hydroxide solutions

A loaded spherical aluminum oxider rider was made to slide, while in various solutions, on a flat iron or nickel surface reciprocate a distance of 1 cm. Time of experiments was 1 hr during which the rider passed over the center section of the track 540 times. Coeficients of friction were measured throughout the experiments. Wear was measured by scanning the track with a profilometer. Analysis of some of the wear tracks included use of the SEM (scanning electron microscope) and XPS (X-ray photoelectron spectroscopy). Investigated were the effect of various concentrations of NaOH and of water. On iron, increasing NaOH concentration above 0.01 N caused the friction and wear to decrease. This decrease is accompanied by a decrease in surface concentration of ferric oxide (Fe2O3) while more complex iron-oxygen compounds, not clearly identified, also form. At low concentrations of NaOH, such as 0.01 N, where the friction is high, the wear track is badly torn up and the surface is broken. At high concentration, such as 10 N, where the friction is low, the wear track is smooth. The general conclusion is that NaOH forms a protective, low friction film on iron which is destroyed by wear at low concentrations but remains intact at high conentrations of NaOH. Nickel behaves differently than iron in that only a little NaOH gives a low coefficient of friction and a surface which, although roughened in the wear track, remains intact. Previously announced in STAR as N83-10171

Rengstorff, G. P.↗

Computational Studies of the Interaction of H/H2 with Diamond and Silicon Surfaces

The interaction of hydrogen atoms and molecules with diamond and silicon surfaces is important in several important applications. Two areas that we are interested are: 1) tribology (molecular level friction) and 2) the role of H atoms in silicon chemical vapor deposition (CVD). In the tribology area, H atoms can be used to tie off dangling bonds, which otherwise form bonds between adjacent surfaces, and lead to resistance to sliding the surfaces by each other. Processes which are important in understanding molecular level friction include barriers to addition of H/H2 to the surface and barriers to migration of H atoms on the surface. In the silicon CVD area, we have studied the process of H2 elimination from the 100 surface of silicon. Cluster models for the dime surfaces of diamond are presented. The unrelaxed 100 surface has carbene like surface carbon atoms; however, for the relaxed surface these dimerize to give rows of surface dimers and there is a significant amount of p bonding between the radical orbitals of the dimer. The 110 surface has zig-zag rows of carbon atoms with a dangling bond on each carbon atom. These dangling bonds are hybridized away from each other and thus interact less strongly than for the 100 surface. Finally, the 111 surface has surface C atoms arranged in a triangular pattern and the surface dangling bonds are well separated from each other (second nearest neighbor distance) leading to almost no interaction between adjacent dangling bonds. These qualitative features may be quantified by computing the overlap of adjacent dangling bonds in a GVB(pp) calculation. The overlaps are 0.462, 0.292, and 0.016 for the diamond 100, 110, and 111 surfaces, respectively.

Walch, Stephen P.↗

Friction and wear of iron and nickel in sodium hydroxide solutions

A loaded spherical aluminum oxider rider was made to slide, while in various solutions, on a flat iron or nickel surface reciprocate a distance of 1 cm. Time of experiments was 1 hr during which the rider passed over the rider passed over the center section of the track 540 times. Coefficients of friction were measured throughout the experiments. Wear was measured by scanning the track with a profilometer. Analysis of some of the wear tracks included use of the SEM (scanning electron microscrope) and XPS (X-ray photoelectron spectroscopy). Investigated were the effect of various concentractions of NaOH and of water. On iron, increasing NaOH concentration above 0.01 N caused the friction and wear to decrease. This decrease is accompanied by a decrease in surface concentration of ferric oxide (Fe2O3) while more complex iron-oxygen compounds, not clearly identified, also form. At low concentrations of NaOH, such as 0.01 N, where the friction is high, the wear track is badely torn up and the surface is broken. At high concentration, such as 10 N, where the friction is low, the wear track is smooth. The general conclusion is that NaOH forms a protective, low friction film on iron which is destroyed by wear at low concentrations but remains intact at high concentrations of NaOH. Nickel behaves differently than iron in that only a little NaOH gives a low coefficient of friction and a surface which, although roughened in the wear track, remains intact.

Rengstorff, G. W. P.↗

Anisotropic friction, deformation, and fracture of single-crystal silicon carbide at room temperature

Anisotropic friction, deformation, and fracture studies were conducted with /0001/, /10(-1)0/, and /11(-2)0/ silicon carbide surfaces in sliding contact with diamond. The experiments were conducted with loads of 0.1, 0.2, and 0.3 N at a sliding velocity of 3 mm/min in mineral oil or in dry argon at room temperature. The 1010 direction on the basal /0001/ plane exhibits the lowest coefficient of friction and the greatest resistance to abrasion for silicon carbide. Anisotropic friction and deformation of the /0001/, /10(-1)0/, and /11(-2)0/ silicon carbide surfaces are primarily controlled by the slip system /10(-1)0/ 11(-2)0. The anisotropic fracture during sliding on the basal plane is due to surface cracking along /10(-1)0/ and subsurface cracking along /0001/. The fracture during sliding on the /11(-2)0/ or /10(-1)0/ surfaces is due to surface cracking along /0001/ and /11(-2)0/ or /10(-1)-1 and to subsurface cracking along /10(-1)0/.

Miyoshi, K.↗

Halogen-Containing Gases as Boundary Lubricants for Corrosion-Resistant Alloys at 1200 F

The extreme temperatures anticipated for lubricated parts in advanced flight powerplants dictate the consideration of unconventional methods of lubrication such as solid lubricants and the reactive gases described in the present research. These halogen-containing "reactive" gases such as dichlorodifluoromethane, CF2Cl2, are among the most stable of organic molecules. The high "flash" temperatures generated at the contacting asperities as a result of frictional heat are sufficient to cause local decomposition of the halogen-containing gases. The active atoms thus released (e.g., chlorine) then react with the metal to be lubricated to form halides capable of effective lubrication. The presence of small amounts of a sulfur-containing gas (e.g., 1 percent sulfur hexafluoride, SF6) was found to catalyze the formation of metal halides. Friction and wear studies were made with a hemisphere (3/16-in. rad.) rider sliding in a circumferential path on the flat surface of a rotating disk (2 1/2-in. diam.). The specimens of corrosion-resistant 2 alloys were run in an atmosphere of the various gases with a load of 1200 grams, a sliding velocity of 120 feet per minute, and temperature from 75 to 1200 F. An effective lubricant for ferritic materials (M-1 tool steel) was CF2Cl2, but significant corrosion occurred above 600 F. Corrosion evaluation in CF2Cl2 suggested a number of nickel- and cobalt-base alloys for additional lubrication study. Several combinations of gases and these metals were found to lubricate to 1200 F without excessive corrosion. The gases were CF2Cl2 Plus 1 percent SF6, monobromotrifluoromethane CF3Br plus 1 percent SF6, dibromodifluoromethane CF2Br2, iodotrifluoromethane, CF3I, and I2. Careful selection of metals and gas are necessary for successful lubrication over specific temperature ranges. Optimum combinations give friction coefficients as low as 0.05 without

Buckley, Donald H.↗

Low wear partially fluorinated polyimides

Tribological studies were conducted on five different polyimide solid bodies formulated from the diamine 2,2-bis 4-(4-aminophenoxy)phenyl hexafluoropropane (4-BDAF) and the dianhydrides pyromellitic acid (PMDS) and benzophenonetetracarboxylic acid (BTDA). The following polyimides were evaluated 4-BDAF/PMDA, 4-BDAF/BTDA, 4-BDAF/80 mole percent PMDA, 20 mole percent BTDA, 4-BDAF/60 mole percent BTDA. Friction coefficients, polyimide wear rates, polyimide surface morphology and transfer films were evaluated at sliding speeds of 0.31 to 11.6 m/s and at temperatures of 25 C to 300 C. The results indicate that the tribological properties are highly dependent on the composition of the polyimide and on the experimental conditions. Two polyimides were found which produced very low wear rates but very high friction coefficients (greater than 0.85) under ambient conditions. They offer considerable potential for high traction types of application such as brakes.

Fusaro, R. L.↗

Low-wear partially fluorinated polyimides

Tribological studies were conducted on five different polyimide solid bodies formulated from the diamine 2,2-bis 4-(4-aminophenoxy)pgenyl hexafluoropropane (4-BDAF) and the dianhydrides pyromellitic acid (PMDS) and benzophenonetetracarboxylic acid (BTDA). The following polyimides were evaluated 4-BDAF/PMDA, 4-BDAF/BTDA, 4-BDAF/80 mole percent PMDA, 20 mole percent BTDA, 4-BDAF/60 mole percent BTDA. Friction coefficients, polyimide wear rates, polyimide surface morphology and transfer films were evaluated at sliding speeds of 0.31 to 11.6 m/s and at temperatures of 25 C to 300 C. The results indicate that the tribological properties are highly dependent on the composition of the polyimide and on the experimental conditions. Two polyimides were found which produced very low wear rates but very high friction coefficients (greater than 0.85) under ambient conditions. They offer considerable potential for high traction types of application such as brakes.

Fusaro, R. L.↗

Theoretical model of impact damage in structural ceramics

This paper presents a mechanistically consistent model of impact damage based on elastic failures due to tensile and shear overloading. An elastic axisymmetric finite element model is used to determine the dynamic stresses generated by a single particle impact. Local failures in a finite element are assumed to occur when the primary/secondary principal stresses or the maximum shear stress reach critical tensile or shear stresses, respectively. The succession of failed elements thus models macrocrack growth. Sliding motions of cracks, which closed during unloading, are resisted by friction and the unrecovered deformation represents the 'plastic deformation' reported in the literature. The predicted ring cracks on the contact surface, as well as the cone cracks, median cracks, radial cracks, lateral cracks, and damage-induced porous zones in the interior of hot-pressed silicon nitride plates, matched those observed experimentally. The finite element model also predicted the uplifting of the free surface surrounding the impact site.

Liaw, B. M.↗

Performance and Durability of High Temperature Foil Air Bearing for Oil-Free Turbomachinery

The performance and durability of advanced, high temperature foil air bearings are evaluated under a wide range (10-50 kPa) of loads at temperatures from 25 to 650 C. The bearings are made from uncoated nickel based superalloy foils. The foil surface experiences sliding contact with the shaft during initial start/stop operation. To reduce friction and wear, the solid lubricant coating, PS304, is applied to the shaft by plasma spraying. PS304, is a NiCr based Cr2O3 coating with silver and barium fluoride/calcium fluoride solid lubricant additions. The results show that the bearings provide lives well in excess of 30,000 cycles under all of the conditions tested. Several bearings exhibited lives in excess of 100,000 cycles. Wear is a linear function of the bearing load. The excellent performance measured in this study suggests that these bearings and the PS304 coating are well suited for advanced high temperature, oil-free turbomachinery applications.

DellaCorte, C.↗