Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “SLAG”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 397 records · Page 22

Cast Stone Formulation At Higher Sodium Concentrations

A low temperature waste form known as Cast Stone is being considered to provide supplemental Low Activity Waste (LAW) immobilization capacity for the Hanford site. Formulation of Cast Stone at high sodium concentrations is of interest since a significant reduction in the necessary volume of Cast Stone and subsequent disposal costs could be achieved if an acceptable waste form can be produced with a high sodium molarity salt solution combined with a high water to premix (or dry blend) ratio. The objectives of this study were to evaluate the factors involved with increasing the sodium concentration in Cast Stone, including production and performance properties and the retention and release of specific components of interest. Three factors were identified for the experimental matrix: the concentration of sodium in the simulated salt solution, the water to premix ratio, and the blast furnace slag portion of the premix. The salt solution simulants used in this study were formulated to represent the overall average waste composition. The cement, blast furnace slag, and fly ash were sourced from a supplier in the Hanford area in order to be representative. The test mixes were prepared in the laboratory and fresh properties were measured. Fresh density increased with increasing sodium molarity and with decreasing water to premix ratio, as expected given the individual densities of these components. Rheology measurements showed that all of the test mixes produced very fluid slurries. The fresh density and rheology data are of potential value in designing a future Cast Stone production facility. Standing water and density gradient testing showed that settling is not of particular concern for the high sodium compositions studied. Heat of hydration measurements may provide some insight into the reactions that occur within the test mixes, which may in turn be related to the properties and performance of the waste form. These measurements showed that increased sodium concentration in the salt solution reduced the time to peak heat flow, and reducing the amount of slag in the premix increased the time to peak heat flow. These observations may help to describe some of the cured properties of the samples, in particular the differences in compressive strength observed after 28 and 90 days of curing. Samples were cured for at least 28 days at ambient temperature in the laboratory prior to cured properties analyses. The low activity waste form for disposal at the Hanford Site is required to have a compressive strength of at least 500 psi. After 28 days of curing, several of the test mixes had mean compressive strengths that were below the 500 psi requirement. Higher sodium concentrations and higher water to premix ratios led to reduced compressive strength. Higher fly ash concentrations decreased the compressive strength after 28 days of curing. This may be explained in that the cementitious phases matured more quickly in the mixes with higher concentrations of slag, as evidenced by the data for the time to peak heat generation. All of the test mixes exhibited higher mean compressive strengths after 90 days of curing, with only one composition having a mean compressive strength of less than 500 psi. Leach indices were determined for the test mixes for contaminants of interest. The leaching performance of the mixes evaluated in this study was not particularly sensitive to the factors used in the experimental design. This may be beneficial in demonstrating that the performance of the waste form is robust with respect to changes in the mix composition. The results of this study demonstrate the potential to achieve significantly higher waste loadings in Cast Stone and other low temperature, cementitious waste forms. Additional work is needed to elucidate the hydration mechanisms occurring in Cast Stone formulated with highly concentrated salt solutions since these reactions are responsible for determining the performance of the cured waste form. The thermal analyses completed in this study provide some preliminary insight, although the limited range of the factors in the test matrix hindered the identification of individual component effects. Future work should involve broader factor ranges to identify the roles played by each of the components in the mix via thermal analyses, analytical microscopy, and characterization of phase formation.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Characterization of Oxy-combustion Impacts in Existing Coal-fired Boilers

Reaction Engineering International (REI) managed a team of experts from University of Utah, Siemens Energy, Praxair, Vattenfall AB, Sandia National Laboratories, Brigham Young University (BYU) and Corrosion Management Ltd. to perform multi-scale experiments, coupled with mechanism development, process modeling and CFD modeling, for both applied and fundamental investigations. The primary objective of this program was to acquire data and develop tools to characterize and predict impacts of CO{sub 2} flue gas recycle and burner feed design on flame characteristics (burnout, NO{sub x}, SO{sub x}, mercury and fine particle emissions, heat transfer) and operational concerns (fouling, slagging and corrosion) inherent in the retrofit of existing coal-fired boilers for oxy-coal combustion. Experimental work was conducted at Sandia National Laboratories’ Entrained Flow Reactor, the University of Utah Industrial Combustion Research Facility, and Brigham Young University. Process modeling and computational fluid dynamics (CFD) modeling was performed at REI. Successful completion of the project objectives resulted in the following key deliverables: 1) Multi-scale test data from 0.1 kW bench-scale, 100 kW and 200 kW laboratory-scale, and 1 MW semi-industrial scale combustors that describe differences in flame characteristics, fouling, slagging and corrosion for coal combustion under air-firing and oxygen-firing conditions, including sensitivity to oxy-burner design and flue gas recycle composition. 2) Validated mechanisms developed from test data that describe fouling, slagging, waterwall corrosion, heat transfer, char burnout and sooting under coal oxy-combustion conditions. The mechanisms were presented in a form suitable for inclusion in CFD models or process models. 3) Principles to guide design of pilot-scale and full-scale coal oxy-firing systems and flue gas recycle configurations, such that boiler operational impacts from oxy-combustion retrofits are minimized. 4) Assessment of oxy-combustion impacts in two full-scale coal-fired utility boiler retrofits based on computational fluid dynamics (CFD) modeling of air-fired and oxygen-fired operation. This research determined that it is technically feasible to retrofit the combustion system in an air-fired boiler for oxy-fired operation. The impacts of CO{sub 2} flue gas recycle and burner design on flame characteristics (burnout, NO{sub x}, SO{sub x}, mercury and fine particle emissions, heat transfer) and operational concerns (fouling, slagging and corrosion) were minimal, with the exception of high sulfur levels resulting from untreated flue gas recycle with medium and high-sulfur coals. This work focused on combustion in the radiant and convective sections of the boiler and did not address boiler system integration issues, plant efficiencies, impacts on downstream air pollution control devices, or CO{sub 2} capture and compression. The experimental data, oxy-firing system principles and oxy-combustion process mechanisms provided by this work can be used by electric utilities, boiler OEMs, equipment suppliers, design firms, software vendors, consultants and government agencies to assess retrofit applications of oxy-combustion technologies to existing boilers and to guide development of new designs.

20 FOSSIL-FUELED POWER PLANTS↗

Cast Stone Formulation At Higher Sodium Concentrations

A low temperature waste form known as Cast Stone is being considered to provide supplemental Low Activity Waste (LAW) immobilization capacity for the Hanford site. Formulation of Cast Stone at high sodium concentrations is of interest since a significant reduction in the necessary volume of Cast Stone and subsequent disposal costs could be achieved if an acceptable waste form can be produced with a high sodium molarity salt solution combined with a high water to premix (or dry blend) ratio. The objectives of this study were to evaluate the factors involved with increasing the sodium concentration in Cast Stone, including production and performance properties and the retention and release of specific components of interest. Three factors were identified for the experimental matrix: the concentration of sodium in the simulated salt solution, the water to premix ratio, and the blast furnace slag portion of the premix. The salt solution simulants used in this study were formulated to represent the overall average waste composition. The cement, blast furnace slag, and fly ash were sourced from a supplier in the Hanford area in order to be representative. The test mixes were prepared in the laboratory and fresh properties were measured. Fresh density increased with increasing sodium molarity and with decreasing water to premix ratio, as expected given the individual densities of these components. Rheology measurements showed that all of the test mixes produced very fluid slurries. The fresh density and rheology data are of potential value in designing a future Cast Stone production facility. Standing water and density gradient testing showed that settling is not of particular concern for the high sodium compositions studied. Heat of hydration measurements may provide some insight into the reactions that occur within the test mixes, which may in turn be related to the properties and performance of the waste form. These measurements showed that increased sodium concentration in the salt solution reduced the time to peak heat flow, and reducing the amount of slag in the premix increased the time to peak heat flow. These observations may help to describe some of the cured properties of the samples, in particular the differences in compressive strength observed after 28 and 90 days of curing. Samples were cured for at least 28 days at ambient temperature in the laboratory prior to cured properties analyses. The low activity waste form for disposal at the Hanford Site is required to have a compressive strength of at least 500 psi. After 28 days of curing, several of the test mixes had mean compressive strengths that were below the 500 psi requirement. Higher sodium concentrations and higher water to premix ratios led to reduced compressive strength. Higher fly ash concentrations decreased the compressive strength after 28 days of curing. This may be explained in that the cementitious phases matured more quickly in the mixes with higher concentrations of slag, as evidenced by the data for the time to peak heat generation. All of the test mixes exhibited higher mean compressive strengths after 90 days of curing, with only one composition having a mean compressive strength of less than 500 psi. Leachability indices were determined for the test mixes for contaminants of interest. The leaching performance of the mixes evaluated in this study was not particularly sensitive to the factors used in the experimental design. This may be beneficial in demonstrating that the performance of the waste form is robust with respect to changes in the mix composition. The results of this study demonstrate the potential to achieve significantly higher waste loadings in Cast Stone and other low temperature, cementitious waste forms. Additional work is needed to elucidate the hydration mechanisms occurring in Cast Stone formulated with highly concentrated salt solutions since these reactions are responsible for determining the performance of the cured waste form. The thermal analyses completed in this study provide some preliminary insight, although the limited range of the factors in the test matrix hindered the identification of individual component effects. Future work should involve broader factor ranges to identify the roles played by each of the components in the mix via thermal analyses, analytical microscopy, and characterization of phase formation.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Conversion of Coal Wastes and Coal Plus Other Opportunity Fuel Mixtures, Such as Coal Plus Municipal Solids, to Produce Electricity and/or Liquid Fuels

For the foreseeable future, the Nation’s energy demand will continue to come largely from indigenous fossil energy resources and hydrocarbon fuels. Specifically waste coal plus other opportunity fuels need to be utilized as a feedstock to eliminate a waste stream and optimized to maximize energy yield and cleanly minimize pollutant emissions. Modular equipment is needed for installation in coal preparation locations, military installations, and research park facilities. Thermal decomposition of coal, biomass, and mixed solid waste (MSW) have been shown to reduce a waste stream while providing liquid and gaseous fuel products with low pollutant emissions. However, thermal decomposition processes have several challenges associated with preprocessing biomass and MSW, feeding and conveying material into the reactor, and post processing of syngas to remove undesirable products while upgrading to increase yield of high value products. Increasing total energy output from power plants by utilizing biomass and mixed wastes ultimately lowers energy costs, harmful environmental impacts of emissions, and has significant impacts on the energy security and sustainability of the U.S. economy. Entrained flow gasifiers (EFGs) produce very little CH4 and a wide range of H2/CO ratios (0.5–2.0) but are limited in their ability to effectively feed large biomass or MSW particles into the reactor. A solution to the feeding problems is to use pyrolysis torrefaction (PT) for conversion of waste materials to create a feedstock similar to coal and capable of grinding down and mixing with the coal feed. Mainstream experimentally explored reaction pathways for the conversion of coal waste plus municipal solids (CWPMS) and demonstrated a bench-scale reactor used for torrefaction of the municipal solid waste (MSW) to create a coal-like feed for blending with the coal waste. The material was processed in a pilot-scale EFG to determine product yield and emissions with CWPMS fuels, as well as the ash content and slagging properties of these feedstocks. The PT-EFG system was experimentally validated, where emissions and yield data were used to develop a high-fidelity process model and economic analysis. The following was accomplished in the Phase I: Determined optimal torrefaction process conditions for MSW and biomass through TGA; maximized heating value of fuel while maximizing final mass of torrefied product Demonstrated torrefaction of MSW and biomass feedstocks at 334°C, pulverized to uniform 74 µm particle size, and processed into coal-like feedstocks Demonstrated 8 lb/h pilot-scale EFG using MSW and biomass blends with waste coal; demonstrated 100% biomass in EFG Determined major effects of MSW torrefaction and co-gasifying high-ash coal waste-MSW blends have on pilot-scale EFG Demonstrated blending low-ash, low-sulfur torrefied biomass with high-ash waste bituminous and anthracite refuse coals generates a higher quality syngas compared to syngas from high-ash waste coals Demonstrated a high carbon conversion (> 99.5%) and syngas with 29.47% H2 content, and 0% CH4 content; greater water–gas shift occurs in EFG than predicted by equilibrium ASPEN Plus model Blended lower-ash, high-alkali biomass MSW to lower slag viscosities of the high-ash coal refuse sufficiently for better slag flow compared to feeding the high-ash coal Used low-sulfur biomass to greatly reduce the EFG syngas H2S concentrations and produce non-leachable slag and quench water with very little organic and trace metal contamination Developed a process model and TEA showing the modular PT EFG is cost competitive to existing power plants with the advantage of using low- or negative-value feedstocks such as waste coal stockpiles and non-landfilled MSW; providing a large incentive to implement an economical PT-EFG process

30 DIRECT ENERGY CONVERSION↗

Time Dependence of Methane Generation Rates from Saltstone

This report documents the tests performed to address the requirements listed in the Technical Request, which resulted in a Task Technical & Quality Assurance Plan (TTQAP) and a Run Plan to obtain the required information. The research expands previous scoping work to better understand methane generation in the Saltstone Disposal Facility (SDF). That scoping work demonstrated that methane is produced when sulfide-containing material is added to methylmercury (MeHg), which is found in the SDF Tank 50 feed waste. When Tank 50 waste is combined with grout premix solids dry feed ingredients of cement, slag cement, and fly ash, sulfides are released from the slag cement component of the premix. The prior testing results showed that while the concentration of total mercury was not affected in the pH 14 waste, the MeHg likely reacted with the sulfide contained in the slag. The scoping tests were performed in sealed reactors and thus, methane generation was not measured continuously; rather, it was measured after one hour and after 24 hours. After 24 hours, a large percentage of the MeHg was converted to methane, but after 1 hour only a small percentage of methane was released. It is noteworthy that the methane generation rate (MGR) was greater at the one-hour measurement. The data compiled from the scoping work needed to be expanded to better understand the generation of methane released from grout mixed with Tank 50 waste. This expanded study developed a more extensive knowledge of how and when methane is generated to inform the Documented Safety Analysis (DSA) of the SDF. As such, employing 8 sealed reactors, the methane generation time periods were extended to 2, 4, 6, 18, 30, 48, 72, and 96 hours (4 days). Results are documented herein to determine the capacity for MeHg, contained within Tank 50 salt solution (T50SS) simulant, to produce methane when mixed with saltstone dry feed ingredients, i.e., individual components (cement, slag, and fly ash) or a combination of those components.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Characterization of Saltstone Grout Line Samples

During a prestart recirculation operation in the Saltstone Processing Facility (SPF), operations staff noticed hardened scaling falling into the hopper. As a result, SPF operators and Saltstone Engineering decided to postpone operation and conduct a process room hopper cleanout. During the cleanout effort personnel noted greater than normal buildup of damp solid material in the transfer line. A borescope investigation was conducted and confirmed buildup was present throughout the transfer line to the downstream valves. Savannah River National Laboratory personnel were asked to characterize the scale material and samples collected from the saltstone grout line and provide recommendations and/or further guidance as to whether additional corrosion testing is needed for useful equipment operating life information. Based on the samples characterized results, the plug material contained only the 60:40 slag:fly ash saltstone. Portland cement in the original 10:45:45 Portland cement:slag:fly ash mix may result in a less abrasive slurry compared to the 60:40 slag:fly ash mix because the slag is > 95 % crushed angular, sharp edged glass. Saltstone grout erosion and corrosion testing of A36 carbon steel is needed to determine if the 60:40 mix is more abrasive and corrosive for A36 carbon steel than the 10:45:45 mix.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Plume diagnostics of SRM static firings for pressure perturbation studies

During the shuttle launches, the solid rocket motors (SRM) occasionally experience pressure perturbations (8-13 psi) between 65 and 75 seconds into the motor burn time. The magnitudes of these perturbations are very small in comparison with the operating motor chamber pressure, which is over 600 psi during this time frame. These SRM pressure perturbations are believed to be caused primarily by the expulsion of slag (aluminum oxide). Two SRM static tests, TEM-11 and FSM-4, were instrumented extensive]y for the study of the phenomenon associated with pressure perturbations. The test instrumentation used included nonintrusive optical and infrared diagnostics of the plume, such as high-speed photography, radiometers, and thermal image cameras. Results from all these nonintrusive observations strongly support the scenario that the pressure perturbation event in the shuttle SRM is caused primarily by the expulsion of molten slag. The slag was also expelled preferentially near the bottom of the nozzle due to slag accumulation at the bottom of the aft end of the horizontally oriented motor.

Sambamurthi, J. K.↗

Plume Diagnostics of the RSRM Static Firings for the Pressure Perturbation Studies

During the STS-54 launch (RSRM-29), the right hand solid rocket motor experienced a 13.9 psi chamber pressure perturbation at 67 seconds into the motor operation. This pressure augmentation equated to a thrust change of 51 klb. Concerns were raised regarding the adverse effects of this thrust imbalance on the shuttle system and the overall thrust into the external tank structural elements. Pressure perturbations have been observed in solid rocket motors due to expulsion of igniter or insulation materials; the motor thrust during such events drop abruptly before rising. However, the RSRM motors do not exhibit such behavior during the large chamber pressure perturbation events. Several scenarios were investigated to explain these pressure perturbations in the RSRM motors based on a fault tree developed after STS-54. Of these, the expulsion of the slag accumulated in the submerged nozzle region appeared to be the most plausible scenario to explain the observations. Slag is a natural combustion product of aluminized solid rocket motors. The RSRM propellant contains 16% by weight of aluminum. Any ejection of this slag mass during nozzle vectoring or other side loads on the motor will result in the chamber pressure perturbation. Two RSRM static firings were instrumented extensively to further understand the slag expulsion phenomenon in the RSRM and the associated pressure perturbations.

Mathias, Edward C.↗

Self-degradable Slag/Class F Fly Ash-Blend Cements

Self-degradable slag/Class F fly ash blend pozzolana cements were formulated, assuming that they might serve well as alternative temporary fracture sealers in Enhanced Geothermal System (EGS) wells operating at temperatures of {ge} 200 C. Two candidate formulas were screened based upon material criteria including an initial setting time {ge} 60 min at 85 C, compressive strength {ge} 2000 psi for a 200 C autoclaved specimen, and the extent of self-degradation of cement heated at {ge} 200 C for it was contacted with water. The first screened dry mix formula consisted of 76.5 wt% slag-19.0 wt% Class F fly ash-3.8 wt% sodium silicate as alkali activator, and 0.7 wt% carboxymethyl cellulose (CMC) as the self-degradation promoting additive, and second formula comprised of 57.3 wt% slag, 38.2 wt% Class F fly ash, 3.8 wt% sodium silicate, and 0.7 wt% CMC. After mixing with water and autoclaving it at 200 C, the aluminum-substituted 1.1 nm tobermorite crystal phase was identified as hydrothermal reaction product responsible for the development of a compressive strength of 5983 psi. The 200 C-autoclaved cement made with the latter formula had the combined phases of tobermorite as its major reaction product and amorphous geopolymer as its minor one providing a compressive strength of 5271 psi. Sodium hydroxide derived from the hydrolysis of sodium silicate activator not only initiated the pozzolanic reaction of slag and fly ash, but also played an important role in generating in-situ exothermic heat that significantly contributed to promoting self-degradation of cementitious sealers. The source of this exothermic heat was the interactions between sodium hydroxide, and gaseous CO{sub 2} and CH{sub 3}COOH by-products generated from thermal decomposition of CMC at {ge} 200 C in an aqueous medium. Thus, the magnitude of this self-degradation depended on the exothermic temperature evolved in the sealer; a higher temperature led to a sever disintegration of sealer. The exothermic temperature was controlled by the extent of thermal decomposition of CMC, demonstrating that CMC decomposed at higher temperature emitted more gaseous reactants. Hence, such large emission enhanced the evolution of in-situ exothermic heat. In contrast, the excessive formation of geopolymer phase due to more incorporation of Class F fly ash into this cementitious system affected its ability to self-degrade, reflecting that there was no self-degradation. The geopolymer was formed by hydrothermal reactions between sodium hydroxide from sodium silicate and mullite in Class F fly ash. Thus, the major reason why geopolymer-based cementitiuos sealers did not degrade after heated sealers came in contact with water was their lack of free sodium hydroxide.

15 GEOTHERMAL ENERGY↗

Formation Mechanism of Oxide-Sulfide Complex Inclusions in High-Sulfur-Containing Steel Melts

The [S] content in resulfurized steel is controlled in the range of 200 to 800 ppm to ensure good machinability and workability. It is well known that “MgAl{sub 2}O{sub 4}(spinel)+CaS” complex inclusions are formed in molten steel during the ladle refining process, and these cause nozzle clogging during continuous casting. Thus, in the present study, the “Refractory-Slag-Metal-Inclusions (ReSMI)” multiphase reaction model was employed in conjunction with experiments to investigate the influence of slag composition and [S] content in the steel on the formation of oxide-sulfide complex inclusions. The critical [S] and [Al] contents necessary for the precipitation of CaS in the CaO-Al{sub 2}O{sub 3}-MgO-SiO{sub 2} (CAMS) oxide inclusions were predicted from the composition of the liquid inclusions, as observed by scanning electron microscopy–electron dispersive spectrometry (SEM-EDS) and calculated using the ReSMI multiphase reaction model. The critical [S] content increases with increasing content of SiO{sub 2} in the slag at a given [Al] content. Formation mechanisms for spinel+CaS and spinel+MnS complex inclusions were also proposed.

36 MATERIALS SCIENCE↗

Dynamic Model of Basic Oxygen Steelmaking Process Based on Multizone Reaction Kinetics: Modeling of Decarburization

In a previous study by the authors (Rout et al. in Metall Mater Trans B 49:537–557, 2018), a dynamic model for the BOF, employing the concept of multizone kinetics was developed. In the current study, the kinetics of decarburization reaction is investigated. The jet impact and slag–metal emulsion zones were identified to be primary zones for carbon oxidation. The dynamic parameters in the rate equation of decarburization such as residence time of metal drops in the emulsion, interfacial area evolution, initial size, and the effects of surface-active oxides have been included in the kinetic rate equation of the metal droplet. A modified mass-transfer coefficient based on the ideal Langmuir adsorption equilibrium has been proposed to take into account the surface blockage effects of SiO{sub 2} and P{sub 2}O{sub 5} in slag on the decarburization kinetics of a metal droplet in the emulsion. Further, a size distribution function has been included in the rate equation to evaluate the effect of droplet size on reaction kinetics. The mathematical simulation indicates that decarburization of the droplet in the emulsion is a strong function of the initial size and residence time. A modified droplet generation rate proposed previously by the authors has been used to estimate the total decarburization rate by slag–metal emulsion. The model’s prediction shows that about 76 pct of total carbon is removed by reactions in the emulsion, and the remaining is removed by reactions at the jet impact zone. The predicted bath carbon by the model has been found to be in good agreement with the industrially measured data.

36 MATERIALS SCIENCE↗

Experimental Investigation of Gas/Slag/Matte/Spinel Equilibria in the Cu-Fe-O-S-Si System at 1473 K (1200 °C) and P(SO{sub 2}) = 0.25 atm

New experimental data were obtained on the gas/slag/matte/spinel equilibria in the Cu-Fe-O-S-Si system at 1473 K (1200 °C) and P(SO{sub 2}) = 0.25 atm covering Cu concentrations in matte between 42 and 78 wt pct Cu. Accurate measurements were obtained using high-temperature equilibration and the rapid quenching technique, followed by electron-probe X-ray microanalysis of equilibrium phase compositions. The use of spinel substrates made to support the samples ensures equilibrium with this primary phase solid, eliminates crucible contamination, and facilitates direct gas–condensed phase equilibrium and high quenching rates. Particular attention was given to the confirmation of the achievement of equilibrium. The results quantify the relationship between Cu in matte and oxygen partial pressure, sulfur in matte, oxygen in matte, Fe/SiO{sub 2} at slag liquidus, sulfur in slag, and dissolved copper in slag.

36 MATERIALS SCIENCE↗

Rate of MgO Pickup in Alumina Inclusions in Aluminum-Killed Steel

This work aims to clarify the rate and mechanism of MgO pickup by alumina inclusions and the effect of oxide impurities in MgO crucibles on this transformation. Two MgO crucibles from different batches from the same supplier were used in laboratory experiments with Al-killed steel. A kinetic model was developed, based on mass-transfer control in the liquid steel. Rate constants were fitted using inclusion analysis. The rate of magnesium transfer from the two types of crucibles was found to differ by a factor of 20; faster magnesium transfer was associated with formation of a slag layer on the inner surface of the crucible wall (rather than a solid spinel product layer). The kinetic model was also used to simulate industrial scale ladle refining (1) to illustrate the effects of total oxygen concentration and (2) to evaluate the contribution of steel-refractory reaction (in addition to steel-slag reaction) on the rate of MgO pickup in alumina inclusion. The rate of MgO pickup was higher with a lower inclusion concentration. For ladle desulfurization, the extent of MgO pickup in inclusions is directly linked to the extent of desulfurization; both reactions are controlled by the oxygen potential at the steel-slag interface.

36 MATERIALS SCIENCE↗

Evolution of Oxide Inclusions in Si-Mn-Killed Steel During Protective Atmosphere Electroslag Remelting

The current study was motivated to reveal the evolution of MnO-SiO{sub 2}-Al{sub 2}O{sub 3} inclusions during protective atmosphere electroslag remelting (P-ESR), and the effect of slag composition on the inclusion evolution. The oxide inclusions in the consumable steel electrode were ternary (7.1-26.4 mass pct) MnO-(53.3-82.8 mass pct) SiO{sub 2}-(8.3-23.1 mass pct) Al{sub 2}O{sub 3} without exception, which were fully removed during the P-ESR in two ways: a portion of these inclusions were dissociated in its individual chemical species into liquid steel, whereas the others were removed by absorbing them into molten slag before liquid metal droplets collected in liquid metal pool during P-ESR. The oxide inclusions both in liquid metal pool and in remelted ingots are mostly MgAl{sub 2}O{sub 4} (containing about 3 mass pct MgO) and Al{sub 2}O{sub 3} inclusions, irrespective of the SiO{sub 2} contents (1.9 to 9.0 mass pct) in the slag. These inclusions readily formed in the liquid metal pool as a result of the reaction between alloying elements and the dissolved oxygen in liquid steel that dissociated from MnO-SiO{sub 2}-Al{sub 2}O{sub 3} inclusions.

36 MATERIALS SCIENCE↗

A Review of Methodology Development for Controlling Loss of Alloying Elements During the Electroslag Remelting Process

Electroslag remelting (ESR) is an advanced secondary refining technology for the production of clean, fully dense, and homogeneous castings of steels and alloys by removal of undesirable elements and nonmetallic inclusions. However, because of some potential reactions between reactive elements, i.e., Al and Ti, in liquid metal and oxygen as well as weak oxides, such as FeO and SiO{sub 2}, in slag during the ESR process, it is impossible to hold those oxidative elements within specification or to maintain them uniformly from the bottom to top of the resultant ingot. According to a literature survey, recent fundamental research on the oxidation behaviors of Al and Ti in nickel-based alloy by ESR-type slag is scarce. Therefore, summarizing previous knowledge on the controlling loss reactive elements during ESR of Fe- and Ni-based alloys in view of thermodynamics and kinetics is in order to increase the basic understanding of the reaction mechanism between those elements and oxygen and weak oxides in the slag, which can guide the development of a new remelting technique that retards the oxidation of Al and Ti in Inconel 718 alloys during the ESR process. The presence of impurity elements, such as oxygen and sulfur, can also deteriorate the mechanical properties of metal products. Therefore, the inter-related literature about desulfurization during the ESR process is also reviewed in this article.

36 MATERIALS SCIENCE↗

Numerical Simulation and Experimental Investigation of Nitrogen Transfer Mechanism from Gas to Liquid Steel During Pressurized Electroslag Remelting Process

Since the gas–slag–metal three-phase transfer mechanism of nitrogen is not suitable to account for the nitrogen pickup during pressurized electroslag remelting process, the laboratory experiments have been carried out to study the transfer mechanism of nitrogen using different nitrogen partial pressures and electrode immersion depths. Then, two possible transfer mechanisms of nitrogen have been proposed, and a 2D transient numerical model has been developed to investigate the behavior of nitrogen based on the new proposed mechanisms. The simulated results are compared with the experiment to validate the feasibility of new proposed mechanism. The results show that the nitrogen content in ingot increases with the increasing nitrogen partial pressure and decreasing electrode immersion depth. At the current experimental condition, the electrode immersion depth seems to play a more important role in the nitrogen pickup than the nitrogen partial pressure. Due to the limits of thermodynamic and kinetic conditions, the nitrogen pickup is negligible via the transfer from gas to liquid metal through molten slag whether nitrogen chemically or physically dissolves into slag. The mechanism that nitrogen directly reacts with the partially exposed liquid metal film under the electrode tip due to the fluctuation of gas/slag interface could reasonably account for the experimental results. Furthermore, based on the mechanism, the predicted variation tendency of nitrogen content in ingot is in agreement with the experiment.

36 MATERIALS SCIENCE↗

Interaction between BaCO{sub 3} and OPC/BFS composite cements at 20 {sup o}C and 60 {sup o}C

A BaCO{sub 3} slurry, containing radioactive {sup 14}C, is produced during the reprocessing of spent nuclear fuel. This slurry is encapsulated in a Portland-blastfurnace slag composite cement. The effect of BaCO{sub 3} on the hydration of OPC and Portland-blastfurnace slag cements has been studied in this work. Samples containing a simulant BaCO{sub 3} slurry were cured for up to 720 days at 20 and 60 {sup o}C and analysed by XRD, SEM(EDX) and ICC. BaCO{sub 3} reacted with OPC to precipitate BaSO{sub 4} from a reaction between soluble sulfate and BaCO{sub 3}. Calcium monocarboaluminate subsequently formed from the carbonate released. The monocarboaluminate precipitated as crystals in voids formed during hydration. At 60 {sup o}C in OPC, it was not identified by XRD, suggesting the phase is unstable in this system around this temperature. In the Portland-blastfurnace slag cements containing BaCO{sub 3}, less monocarboaluminate and BaSO{sub 4} were formed, but the hydration of BFS was promoted and monocarboaluminate was stable up to 60 {sup o}C.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

X-ray microtomography shows pore structure and tortuosity in alkali-activated binders

Durability of alkali-activated binders is of vital importance in their commercial application, and depends strongly on microstructure and pore network characteristics. X-ray microtomography ({mu}CT) offers, for the first time, direct insight into microstructural and pore structure characteristics in three dimensions. Here, {mu}CT is performed on a set of sodium metasilicate-activated fly ash/slag blends, using a synchrotron beamline instrument. Segmentation of the samples into pore and solid regions is then conducted, and pore tortuosity is calculated by a random walker method. Segmented porosity and diffusion tortuosity are correlated, and vary as a function of slag content (slag addition reduces porosity and increases tortuosity), and sample age (extended curing gives lower porosity and higher tortuosity). This is particularly notable for samples with {>=} 50% slag content, where a space-filling calcium (alumino)silicate hydrate gel provides porosity reductions which are not observed for the sodium aluminosilicate ('geopolymer') gels which do not chemically bind water of hydration.

36 MATERIALS SCIENCE↗