Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “PROPYLENE”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 397 records · Page 22

Two-color two-photon excited fluorescence of indole: Determination of wavelength-dependent molecular parameters

We present a detailed study of two-color two-photon excited fluorescence in indole dissolved in propylene glycol. Femtosecond excitation pulses at effective wavelengths from 268 to 293.33 nm were used to populate the two lowest indole excited states {sup 1}L{sub a} and {sup 1}L{sub b} and polarized fluorescence was then detected. All seven molecular parameters and the two-photon polarization ratio Ω containing information on two-photon absorption dynamics, molecular lifetime τ{sub f}, and rotation correlation time τ{sub rot} have been determined from experiment and analyzed as a function of the excitation wavelength. The analysis of the experimental data has shown that {sup 1}L{sub b}–{sup 1}L{sub a} inversion occurred under the conditions of our experiment. The two-photon absorption predominantly populated the {sup 1}L{sub a} state at all excitation wavelengths but in the 287–289 nm area which contained an absorption hump of the {sup 1}L{sub b} state 0-0 origin. The components of the two-photon excitation tensor S were analyzed giving important information on the principal tensor axes and absorption symmetry. The results obtained are in a good agreement with the results reported by other groups. The lifetime τ{sub f} and the rotation correlation time τ{sub rot} showed no explicit dependence on the effective excitation wavelength. Their calculated weighted average values were found to be τ{sub f} = 3.83 ± 0.14 ns and τ{sub rot} = 0.74 ± 0.06 ns.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Controlling block copolymer phase behavior using ionic surfactant

The phase behavior of poly(ethylene oxide)-poly(propylene oxide-poly(ethylene oxide) PEO-PPO-PEO triblock copolymer [P85 (EO{sub 26}PO{sub 39}EO{sub 26})] in presence of anionic surfactant sodium dodecyl sulfate (SDS) in aqueous solution as a function of temperature has been studied using dynamic light scattering (DLS) and small-angle neutron scattering (SANS). The measurements have been carried out for fixed concentrations (1 wt%) of block copolymer and surfactants. Each of the individual components (block copolymer and surfactant) and the nanoparticle–surfactant mixed system have been examined at varying temperature. The block copolymer P85 forms spherical micelles at room temperature whereas shows sphere-to-rod like micelle transition at higher temperatures. On the other hand, SDS surfactant forms ellipsoidal micelles over a wide temperature range. Interestingly, it is found that phase behavior of mixed micellar system (P85 + SDS) as a function of temperature is drastically different from that of P85, giving the control over the temperature-dependent phase behavior of block copolymers.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Structural and electrochemical properties of PEMA with the influence of MWCNT / TiO{sub 2} filler

An attempt has been made to prepare a hybrid Nano composite polymer electrolytes (NCPES) based on Poly(ethyl methacrylate) (PEMA) doped with multiwalled carbon nanotubes (MWCNT) and Titanium oxide (TiO{sub 2}) as additives, Lithium per chlorate (LiClO{sub 4}) as ionic salt and Propylene Carbonate as plasticizer (PC) by using solvent casting technique. X-ray diffraction analysis (XRD) confirms the miscibility and amorphous nature of the prepared electrolytes. It has been found from the a.c impedance analysis that the inorganic filler reduces the bulk resistance of the electrolytes and thus ionic conductivity enhanced. A high dielectric loss value is observed for the case of doped MWCNT-PEMA in comparison with pure PEMA and doped TiO{sub 2} –PEMA membranes. Based on the study of relaxation spectra, it is found that the relaxation time decreases with increase in temperature.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Vibration-based energy harvesting with piezoelectrets having high d{sub 31} activity

Sandwiched fluoroethylene propylene films with charged, parallel-tunnel voids between the layers, which exhibit high d{sub 31} piezoelectric activity, were designed. Stripes of such piezoelectrets were exposed to mechanical stress in length direction by a seismic mass excited to vibrations. Due to the piezoelectricity of the films, a current in a terminating resistor is generated. The harvested power across the resistor amounts to about 0.2 mW for a seismic mass of 2 g and an acceleration of 1 g. In comparison with other piezoelectret or with poly(vinylidene fluoride) harvesters, the generated power referred to equal acceleration and force, is significantly larger.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

In vitro terahertz monitoring of muscle tissue dehydration under the action of hyperosmotic agents

Dehydration of muscle tissue in vitro under the action of biologically compatible hyperosmotic agents is studied using a laser terahertz spectrometer in the frequency range from 0.25 to 2.5 THz. Broadband terahertz absorption and reflection spectra of the bovine skeletal muscle tissue were obtained under the action of glycerol, polyethylene glycol with the molecular weight 600 (PEG-600), and propylene glycol. The presented results are proposed for application in developing the methods of image contrast enhancement and increasing the depth of biological tissue probing with terahertz radiation. (laser biophotonics)

72 PHYSICS OF ELEMENTARY PARTICLES AND FIELDS↗

Study of diffusion of indocyanine green as a photodynamic dye into skin using backscattering spectroscopy

One of the lines of development of modern medicine is theranostics consisting in simultaneous diagnosis and laser treatment with the use of multifunctional agents such as fluorescent indocyanine green that has photodynamic and photothermal properties. Diffusion of indocyanine green dissolved in water and aqueous solutions of alcohols (glycerol, propylene glycol and ethanol) into the dermis is studied by using backscattering spectroscopy. The coefficients of the dye diffusion into the dermis are obtained for the first time by using these solvents. (laser biophotonics)

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

High-harmonic spectroscopy of molecular isomers

We demonstrate that high-order-harmonic generation (HHG) spectroscopy can be used to probe stereoisomers of randomly oriented 1,2-dichloroethylene (C{sub 2}H{sub 2}Cl{sub 2}) and 2-butene (C{sub 4}H{sub 8}). The high-harmonic spectra of these isomers are distinguishable over a range of laser intensities and wavelengths. Time-dependent numerical calculations of angle-dependent ionization yields for 1,2-dichloroethylene suggest that the harmonic spectra of molecular isomers reflect differences in their strong-field ionization. The subcycle ionization yields for the cis isomer are an order of magnitude higher than those for the trans isomer. The sensitivity in discrimination of the harmonic spectra of cis- and trans- isomers is greater than 8 and 5 for 1,2-dichloroethylene and 2-butene, respectively. We show that HHG spectroscopy cannot differentiate the harmonic spectra of the two enantiomers of the chiral molecule propylene oxide (C{sub 3}H{sub 6}O).

2-METHYLPROPENE↗

Sequential versus Simultaneous Aging of EPDM Nuclear Cable Insulation Subjected to Elevated Temperature and Gamma Radiation

Electrical cables are integral to power, control, and instrumentation systems within nuclear power plants (NPPs). Exposure of cable systems within nuclear containment to elevated temperatures and gamma radiation during decades-long operation of NPPs can lead to degradation of cable polymeric insulation. Prediction of nuclear cable insulation degradation is complicated as thermal and radiation stress are not additive. In this work, we explore the relative effects of simultaneous and sequential thermal and gamma irradiation on the aging of ethylene-propylene-diene (EPDM) elastomer insulation to better understand realistic scenarios of cable insulation degradation. Cable insulation samples of EPDM were subjected to up to 320 kGy of gamma radiation at a dose rate of 300 Gy/hr in two heating scenarios: (1) simultaneously aged samples were heated at 150°C during irradiation and (2) sequentially aged samples were heated at 150°C for designated durations followed by corresponding periods of irradiation at ambient temperature. The mass, tensile elongation at break, and carbonyl index were assessed to quantify aging of the polymers. The simultaneous aging scenario was found to the more severe of the two for EPDM insulation degradation.

ethylene-propylene-diene elastomer, EPDM, nuclear ↗

Evaluation of Copper Catalytic Effects in Cable Insulation Polymers

This paper summarizes work performed to evaluate a phenomenon that occurs in electrical cable insulation polymers subjected to accelerated aging while in contact with copper metal. This effect, commonly known as the copper catalytic effect, is a result of chemical reactions that occur when copper ions diffuse into insulation polymers. This diffusion process is observed in various types of polymeric materials exposed to elevated temperatures and happens at the interface between the insulation and metallic components (e.g., conductor, shielding, etc.) in a cable. This polymer-metal interaction has only been observed in cables constructed with copper components (i.e., no interactions observed in cables with aluminum or other metal conductor/shielding) and results in a significant catalytic effect that increases the oxidation rate (e.g., aging) of the material. Under this research, the copper catalytic effects observed in cross-linked polyethylene, cross-linked polyolefin and ethylene propylene rubber insulated cables subjected to thermal accelerated aging were evaluated. These evaluations involved applying infrared spectroscopy, microscopy, and energy dispersive X-ray spectroscopy cross-sectional depth profiling to obtain an in-depth understanding of the aging characteristics of the materials under accelerated conditions. Based on the results of these assessments, the copper catalytic effect can have a significant impact on the mechanical, thermal, chemical, and electrical properties of cable insulation polymers. Here, the results acquired from this research provided the information needed to characterize the copper catalytic effects observed in these polymers, analyze how this phenomenon affected the polymer degradation process, and compare and understand the differences in the properties of the materials.

42 ENGINEERING↗

Low Cost, Single Layer Replacement for the Back-Sheet and Encapsulant Layers

Ethylene propylene diene monomer (EPDM) based polymers have been formulated for specific use in photovoltaic modules to produce better performance and longer term stability at a lower cost than standard materials. EPDM formulations are advantageous over ethylene vinyl-acetate (EVA) because they can use the same lamination/cure cycle as EVA, they do not need a second back-sheet protective material (e.g. PET/Tedlar), they have a lower glass transition temperature, no melting transition, more constant mechanical moduli as a function of temperature, they are less polar than EVA (provides better corrosion protection), and they have excellent damp heat (85 C/85% relative humidity) resistance against delamination. Module designs typically use EVA on the back side of cells despite the fact that transparency is not advantageous. We have developed a single encapsulant layer that will replace standard module back-sheet constructions consisting of EVA/PET/Tedlar. Because a single low-cost material layer is used, it will provide a significant materials cost savings of about $6 to $8/m{sup 2} as compared to traditional back-sheets. Electrical insulation tests were conducted using 0.85 mm thick stainless steel sheets as a model for a cell. It was found that a polymer layer thickness of about 0.33mm provided better high voltage electrical insulation than a combined film of Tedla (0.038 mm)/PET (0.051 mm)/EVA (0.55 mm). When formulated with a white pigment, reflectivity was comparable to Tedlar{trademark}. Upon accelerated exposure to light at 60C and 60% RH it was found that an EVA layer in front of these materials would decompose before significant yellowing and delamination of the back EPDM layer occurs.

14 SOLAR ENERGY↗

Polarized Fluorescence in Indole under Two-Photon Excitation by Femtosecond Laser Pulses

We have analyzed the decay of fluorescence intensity in indole dissolved in propylene glycol under two-photon excitation by linearly and circularly polarized femtosecond laser pulses in the wavelength range 475–510 nm. The dependences of fluorescence intensity I{sub 0}, anisotropy r, and parameter Ω on the excitation energy have been determined and analyzed. In particular, a nonmonotonic behavior of I{sub 0} indicating the increase of indole excited state density in the excitation energy range above 5.1 eV and the anisotropy sign reversal due to the variation of the symmetry of indole vibronic states have been observed and interpreted theoretically.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Status report for aging studies of epdm o-ring material for the h1616 shipping package

This is an interim status report for tasks carried out per Task Technical Plan SRNL-STI-2011-00506. A series of tasks/experiments are being performed at the Savannah River National Laboratory to monitor the aging performance of ethylene propylene diene monomer (EPDM) Orings used in the H1616 shipping package. The data will support the technical basis to extend the annual maintenance of the EPDM O-rings in the H1616 shipping package and to predict the life of the seals at bounding service conditions.

99 GENERAL AND MISCELLANEOUS↗

SISGR: Linking Ion Solvation and Lithium Battery Electrolyte Properties

The solvation and phase behavior of the model battery electrolyte salt lithium trifluoromethanesulfonate (LiCF 3 SO 3 ) in commonly used organic solvents; ethylene carbonate (EC), gamma-butyrolactone (GBL), and propylene carbonate (PC) was explored. Data from differential scanning calorimetry (DSC), Raman spectroscopy, and X-ray diffraction were correlated to provide insight into the solvation states present within a sample mixture. Data from DSC analyses allowed the construction of phase diagrams for each solvent system. Raman spectroscopy enabled the determination of specific solvation states present within a solvent-salt mixture, and X-ray diffraction data provided exact information concerning the structure of a solvates that could be isolated Thermal analysis of the various solvent-salt mixtures revealed the phase behavior of the model electrolytes was strongly dependent on solvent symmetry. The point groups of the solvents were (in order from high to low symmetry): C2V for EC, CS for GBL, and C1 for PC(R). The low symmetry solvents exhibited a crystallinity gap that increased as solvent symmetry decreased; no gap was observed for EC-LiTf, while a crystallinity gap was observed spanning 0.15 to 0.3 mole fraction for GBL-LiTf, and 0.1 to 0.33 mole fraction for PC(R)-LiTf mixtures. Raman analysis demonstrated the dominance of aggregated species in almost all solvent compositions. The AGG and CIP solvates represent the majority of the species in solutions for the more concentrated mixtures, and only in very dilute compositions does the SSIP solvate exist in significant amounts. Thus, the poor charge transport characteristics of CIP and AGG account for the low conductivity and transport properties of LiTf and explain why is a poor choice as a source of Li + ions in a Li-ion battery.

25 ENERGY STORAGE↗

New Technologies for Repairing Aging Cables in Nuclear Power Plants

The goal of this project is to demonstrate a proof-of-concept for a technique to repair aging cables that have been subjected to degradation associated with long-term thermal and radiation exposure in nuclear power plants. The physical degradation of the aging cables manifests itself primarily as cracking and increased brittleness of the polymeric electrical insulation. Therefore, the proposed cable-repair concept comprises development of techniques to impart a softening agent within the deteriorated polymer insulation jacket so as to regain the ability of the insulation to stretch without failing and possibly to heal existing cracks in the insulation. Our approach is to use commercially available ethylene-propylene rubber (EPR) as the relevant test material, demonstrate the adsorption of chemical treatments in the EPR and quantify changes in resulting physical and mechanical properties. EPR cable samples have been thermally treated in air to produce specimens corresponding to the full range of cable age-performance points from new (>350% elongation at break) to end-of-life (<50% elongation at break). The current focus is on two chemical treatments selected as candidates for restoring age-related cable elasticity loss: a rubber plasticizer and a reactive silane molecule. EPR specimens of 200, 150, 100, and 50% elongation at break have been soaked in the candidate chemical treatments and the kinetics of chemical uptake, measured by change in mass of the samples, has been determined. Mechanical properties as a function of aging and chemical treatment have been measured including ultimate tensile strength, tensile modulus at 50% strain, elongation at break, and storage modulus. Dimensional changes with treatment and changes in glass transition temperature were also investigated. These ongoing experiments are expected to provide insight into the physical-chemical nature of the effect of thermal degradation on EPR rejuvenation limits and to advance novel methods for restoring the ability of degraded EPR to be compliant and resist fracture. The results of this research reveal that absorption of chemical treatments can lower the glass transition temperature and modulus of EPR. Chemical treatments pursued thus far have proven ineffective at restoring EPR strength and elongation at break. Future work will combine the plasticizer modalities found to successfully increase the volume of the EPR, reduce EPR glass transition temperature and reduce EPR modulus with promising chemistries that will repair the damage of the polymer, potentially using the plasticizer as a host for the new chemistry.

36 MATERIALS SCIENCE↗

Aging Study Of EPDM O-Ring Material For The H1616 Shipping Package - Three Year Status

This is a 3-year status report for tasks carried out per Task Technical Plan SRNL-STI-2011-00506. A series of tasks/experiments were performed at the Savannah River National Laboratory (SRNL) to monitor the aging performance of ethylene propylene diene monomer (EPDM) O-rings used in the H1616 shipping package. The test data provide a technical basis to extend the annual maintenance of the H1616 shipping package to three years and to predict the life of the EPDM O-rings at the bounding service conditions.

42 ENGINEERING↗

REMOVAL OF IODIDE FROM GROUNDWATER USING SILVER CHLORIDE WHITE PAPER

Releases from the F and H Area Seepage Basins on the Savannah River Site (SRS) have caused groundwater plumes that contain a variety of contaminants. These plumes are releasing contaminants into Fourmile Branch, which is a small tributary of the Savannah River. The metallic contaminant releases to the branch are being controlled by base injection. The base injection targets cationic contaminants and was not intended to reduce the concentration of I-129 in groundwater. SRS and the regulatory agencies believe it is appropriate to investigate remedial alternatives that could reduce the I-129. The Savannah River Site Area Closures Projects (ACP) and the Savannah River National Laboratory (SRNL) are developing an innovative in situ treatment for I-129 using silver chloride (AgCl). The proposed AgCl amendment has a very small particle size and is designed to be injected into the contaminated aquifer to capture I-129. The solubility of AgI is several orders of magnitude lower than the solubility of AgCl. Thus, when I-129 comes in contact with AgCl it forms silver iodide (AgI), which is very stable and essentially insoluble in water. SRNL has been performing bench-scale column tests on the effectiveness of silver chloride to capture iodine in an aqueous solution. These initial tests evaluate silver chloride in four different particle sizes; 4-5 millimeters (standard reagent silver chloride), approximately 1 millimeters (sieved reagent silver chloride), approximately 2 micrometers (ultra fine grind without a grinding agent), and <1 micrometer (ultra fine grind with a grinding agent). The first two experiments with macro-sized particles were proof of principle tests. In these the AgCl was mechanically mixed into a portion of the soil filling the columns. The last two were to test the effectiveness of injecting particles suspended in an aqueous solution--the ability to inject the particles, their retention in the column and their effectiveness at removing dissolved iodide from solution. The amendments for these two columns were obtained from a private company specializing in ultra-fine grinding of materials. They were ground in propylene glycol because when ground in water silver metal electroplated onto the steel grinding equipment. Table 1 shows the list of columns and the amendment characteristics. The results of these column experiments demonstrate that solid silver chloride is highly effective at removing dissolved iodine from water and should be an effective amendment for removing I-129 from groundwater. Based on known groundwater chemistry and the reaction of AgCl with I- to produce AgI, the only interference will be natural dissolved stable iodine (I-127). Millings et al. (2002) reported a maximum I-127 concentration of 2.2 ug/L in groundwater from well P-27D, a background water table well near F-Area. The concentration of dissolved iodide used in these experiments is approximately 4500 times this natural concentration. Therefore, a AgCl amendment in the subsurface at the same concentration used in these experiments, might effectively remove I-129 for up to 4500 times the number of pore volumes of groundwater as observed here. This assumes homogeneous distribution of the amendment and no occlusion by other minerals in the subsurface. The only reliable way to evaluate these effects is by trial in the field. The column studies also suggest that the amendment is readily injectable into sediments, but will not be highly mobile. The fact that the effluent from Column 4 shows no iodide breakthrough after nearly 11 pore volumes indicates that some of the injected AgCl was trapped in the column. A mass balance on iodide reacted so far suggests that a minimum of 0.056 grams of silver chloride was trapped in the column to react with the iodide. This is 5.6% of the mass injected. Assume the 1-foot column represents the first foot of sediment in the subsurface into which the amendment is injected. If 5.6% of the AgCl particles are trapped in each subsequent foot of sediment through which the injectate moves, at 100 feet the concentration of particles will be 3% of the injection concentration. This is the maximum possible concentration indicated by these column studies, because far more AgCl may have been trapped in the column. Continued data collection will tell how much more. Dissolved silver concentrations from the silver chloride amendment will be low. Effluent from Column 1 was analyzed for dissolved silver and the concentrations were below the detection limit of 0.2 mg/L.

36 MATERIALS SCIENCE↗

DOE Award No. DE-FC36-03GO13108 NOVEL NON-PRECIOUS METAL CATALYSTS FOR PEMFC: CATALYST SELECTION THROUGH MOLECULAR MODELING AND DURABILITY STUDIES Final Report (September 2003 – October 2008)

The objective of this project is to develop novel non-precious metal electrocatalysts for oxygen reduction reaction (ORR), and demonstrate the potential of the catalysts to perform at least as good as conventional Pt catalysts currently in use in polymer electrolyte membrane fuel cell (PEMFC) with a cost at least 50 % less than a target of 0.2 g (Pt loading)/peak kW and with durability > 2,000 h operation with less than 10 % power degradation. A novel nitrogen-modified carbon-based catalyst was obtained by modifying carbon black with nitrogen-containing organic precursor in the absence of transition metal precursor. The catalyst shows the onset potential of approximately 0.76 V (NHE) for ORR and the amount of H2O2 of approximately 3% at 0.5 V (NHE). Furthermore, a carbon composite catalyst was achieved through the high-temperature pyrolysis of the precursors of transition metal (Co and Fe) and nitrogen supported on the nitrogen-modified carbon-based catalyst, followed by chemical post-treatment. This catalyst showed an onset potential for ORR as high as 0.87 V (NHE), and generated less than 1 % of H2O2. The PEM fuel cell exhibited a current density of 2.3 A cm-2 at 0.2 V for a catalyst loading of 6.0 mg cm-2. No significant performance degradation was observed for 480 h continuous operation. The characterization studies indicated that the metal-nitrogen chelate complexes decompose at the temperatures above 800 oC. During the pyrolysis, the transition metals facilitate the incorporation of pyridinic and graphitic nitrogen groups into the carbon matrix, and the carbon surface modified with nitrogen is active for ORR. In order to elucidate the role of transition metal precursor played in the formation of active sites in the non-precious metal catalysts, a novel ruthenium-based chelate (RuNx) catalyst was synthesized by using RuCl3 and propylene diammine as the Ru and N precursors, respectively, followed by high-temperature pyrolysis. This catalyst exhibited comparable catalytic activity and selectivity for ORR as the Pt catalyst. A theoretical analysis is made of the four-electron reduction reaction of oxygen to water over the mixed anion and cation (202) surface of pentlandite structure Co9Se8, one of several selenide phases. Reversible potentials for forming adsorbed reaction intermediates in acid are predicted using adsorption energies calculated with the Vienna ab initio simulation program (VASP) and the known bulk solution values together in a linear Gibbs energy relationship. The effect of hydrophobic and structural properties of a single/dual-layer cathode gas diffusion layer on mass transport in PEM fuel cells was studied using an analytical expression. The simulations indicated that liquid water transport at the cathode is controlled by the fraction of hydrophilic surface and the average pore diameter in the cathode gas diffusion layer. The optimized hydrophobicity and pore geometry in a dual-layer cathode GDL leads to an effective water management, and enhances the oxygen diffusion kinetics.

08 HYDROGEN↗

DOE Award No. DE-FC36-03GO13108 NOVEL NON-PRECIOUS METAL CATALYSTS FOR PEMFC: CATALYST SELECTION THROUGH MOLECULAR MODELING AND DURABILITY STUDIES Final Report (September 2003 – October 2008)

The objective of this project is to develop novel non-precious metal electrocatalysts for oxygen reduction reaction (ORR), and demonstrate the potential of the catalysts to perform at least as good as conventional Pt catalysts currently in use in polymer electrolyte membrane fuel cell (PEMFC) with a cost at least 50 % less than a target of 0.2 g (Pt loading)/peak kW and with durability > 2,000 h operation with less than 10 % power degradation. A novel nitrogen-modified carbon-based catalyst was obtained by modifying carbon black with nitrogen-containing organic precursor in the absence of transition metal precursor. The catalyst shows the onset potential of approximately 0.76 V (NHE) for ORR and the amount of H2O2 of approximately 3% at 0.5 V (NHE). Furthermore, a carbon composite catalyst was achieved through the high-temperature pyrolysis of the precursors of transition metal (Co and Fe) and nitrogen supported on the nitrogen-modified carbon-based catalyst, followed by chemical post-treatment. This catalyst showed an onset potential for ORR as high as 0.87 V (NHE), and generated less than 1 % of H2O2. The PEM fuel cell exhibited a current density of 2.3 A cm-2 at 0.2 V for a catalyst loading of 6.0 mg cm-2. No significant performance degradation was observed for 480 h continuous operation. The characterization studies indicated that the metal-nitrogen chelate complexes decompose at the temperatures above 800 oC. During the pyrolysis, the transition metals facilitate the incorporation of pyridinic and graphitic nitrogen groups into the carbon matrix, and the carbon surface modified with nitrogen is active for ORR. In order to elucidate the role of transition metal precursor played in the formation of active sites in the non-precious metal catalysts, a novel ruthenium-based chelate (RuNx) catalyst was synthesized by using RuCl3 and propylene diammine as the Ru and N precursors, respectively, followed by high-temperature pyrolysis. This catalyst exhibited comparable catalytic activity and selectivity for ORR as the Pt catalyst. A theoretical analysis is made of the four-electron reduction reaction of oxygen to water over the mixed anion and cation (202) surface of pentlandite structure Co9Se8, one of several selenide phases. Reversible potentials for forming adsorbed reaction intermediates in acid are predicted using adsorption energies calculated with the Vienna ab initio simulation program (VASP) and the known bulk solution values together in a linear Gibbs energy relationship. The effect of hydrophobic and structural properties of a single/dual-layer cathode gas diffusion layer on mass transport in PEM fuel cells was studied using an analytical expression. The simulations indicated that liquid water transport at the cathode is controlled by the fraction of hydrophilic surface and the average pore diameter in the cathode gas diffusion layer. The optimized hydrophobicity and pore geometry in a dual-layer cathode GDL leads to an effective water management, and enhances the oxygen diffusion kinetics.

08 HYDROGEN↗