Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “MAGNETRON SPUTTERING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 397 records · Page 22

Observation of a periodic runaway in the reactive Ar/O{sub 2} high power impulse magnetron sputtering discharge

This paper reports the observation of a periodic runaway of plasma to a higher density for the reactive discharge of the target material (Ti) with moderate sputter yield. Variable emission of secondary electrons, for the alternating transition of the target from metal mode to oxide mode, is understood to be the main reason for the runaway occurring periodically. Increasing the pulsing frequency can bring the target back to a metal (or suboxide) mode, and eliminate the periodic transition of the target. Therefore, a pulsing frequency interval is defined for the reactive Ar/O{sub 2} discharge in order to sustain the plasma in a runaway-free mode without exceeding the maximum power that the magnetron can tolerate.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Process-structure-property correlations in pulsed dc reactive magnetron sputtered vanadium oxide thin films

Cathode hysteresis in the reactive pulsed dc sputtering of a vanadium metal target was investigated to correlate the structural and electrical properties of the resultant vanadium oxide thin films within the framework of Berg's model [Berg et al., J. Vac. Sci. Technol. A 5, 202 (1987)]. The process hysteresis during reactive pulsed dc sputtering of a vanadium metal target was monitored by measuring the cathode (target) current under different total gas flow rates and oxygen-to-argon ratios for a power density of {approx}6.6.W/cm{sup 2}. Approximately 20%-25% hysteretic change in the cathode current was noticed between the metallic and oxidized states of the V-metal target. The extent of the hysteresis varied with changes in the mass flow of oxygen as predicted by Berg's model. The corresponding microstructure of the films changed from columnar to equiaxed grain structure with increased oxygen flow rates. Micro-Raman spectroscopy indicates subtle changes in the film structure as a function of processing conditions. The resistivity, temperature coefficient of resistance, and charge transport mechanism, obeying the Meyer-Neldel relation [Meyer and Neldel, Z. Tech. Phys. (Leipzig) 12, 588 (1937)], were correlated with the cathode current hysteric behavior.

36 MATERIALS SCIENCE↗

An in situ x-ray photoelectron spectroscopy study of the initial stages of rf magnetron sputter deposition of indium tin oxide on p-type Si substrate

The interface between indium tin oxide and p-type silicon is studied by in situ X-ray photoelectron spectroscopy (XPS). This is done by performing XPS without breaking vacuum after deposition of ultrathin layers in sequences. Elemental tin and indium are shown to be present at the interface, both after 2 and 10 s of deposition. In addition, the silicon oxide layer at the interface is shown to be composed of mainly silicon suboxides rather than silicon dioxide.

36 MATERIALS SCIENCE↗

Spark Plasma Sintering of SmS-Based Ceramic Targets for the Magnetron Sputtering

The results of studying the electric-spark plasma sintering of samarium monosulfide ceramics are presented. The dependence of the microstructure and phase composition of ceramics on the temperature of spark plasma sintering is studied on the basis of the data of scanning electron microscopy, energy dispersion X-ray microanalysis, and powder X-ray diffraction of synthesized samples. It is shown that a dense, nonporous ceramics, the phase composition of which is close to the composition of the initial powder, is formed at a sintering temperature of 1200°C.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Studies on Nd{sub x}In{sub 1−x}O{sub 3} semiconducting thin films prepared by rf magnetron sputtering

Neodymium-substituted indium oxide (Nd{sub x}In{sub 1−x}O{sub 3}, NIO) semiconducting thin films fabricated by rf sputtering were investigated. It was found that the incorporation of Nd atoms would lead to broadening the optical band gap, suppressing the grain growth, and reducing the free carrier concentration. The field-effect transistors with different NIO (5%, 15%, and 25% Nd concentration of the targets) channel layers exhibited similar electrical stability under positive gate-bias-stress, but the ones with 15% and 25% Nd concentration displayed much better stability under negative gate-bias-stress. Detailed studies showed that the content of |Nd3d{sub 5/2}{sup 5}4f{sup 4}O2p{sup −1}> electron configuration decreased as the Nd concentration increased, resulting in the reduction of holes during negative-bias-stress. And the reduction of the |Nd3d{sub 5/2}{sup 5}4f{sup 4}O2p{sup −1}> content as the Nd concentration increased was ascribed to less overlap between the metal and ligand orbitals arose from large lattice expansion.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Microstructure and chemical wet etching characteristics of AlN films deposited by ac reactive magnetron sputtering

The influence of the surface morphology of a molybdenum underlayer on the crystallinity and etchability of reactively sputtered c-axis oriented aluminum nitride thin films was investigated. Atomic force microscopy, scanning electron microscopy, transmission electron microscopy, high resolution x-ray diffraction, and defect selective chemical etching were used to characterize the microstructure of the Mo and AlN films. 1000 nm thick films of AlN with a full width at half maximum (FWHM) of the x-ray rocking curve ranging from 1.1 deg. to 1.9 deg. were deposited on 300 nm thick Mo underlayers with a FWHM of around 1.5 deg. The Ar pressure during the Mo deposition had a critical effect on the Mo film surface morphology, affecting the structure of the subsequently deposited AlN films and, hence, their wet etching characteristics. AlN films deposited on Mo sputtered at a relatively high pressure could not be etched completely, while AlN films deposited on low pressure Mo etched more easily. Postdeposition etching of the Mo surface in Ar rf discharge prior to deposition of the AlN film was found to influence the formation of AlN residuals that were difficult to etch. Optimal rf plasma etching conditions were found, which minimized the formation of these residuals.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Correlation of structure and hardness of rf magnetron sputtered silicon carbonitride films

Ternary nanocomposite silicon carbonitride (Si-C-N) ceramic coatings have shown potential for wear resistance, oxidation resistance, hardness, tunable band gap, and chemical inertness applications. A systematic investigation on the deposition of Si-C-N nanocomposite coatings by sputtering under varying deposition conditions such as chamber pressure, substrate temperature by structural, nanoindentation, and microstructural studies of optimized condition has been presented. Significant role of different deposition parameter on the mechanical and structural properties were observed. The structural characterizations of the coatings were carried out using Fourier transformed infra red (FTIR), transmission electron microscopy, Raman spectroscopy, and field emission scanning electron microscope. An increase in argon-nitrogen pressure in the range of 1-5 Pa led to lowering of particle size and surface smoothening and growth of hard phases of {beta}-C{sub 3}N{sub 4} and {beta}-Si{sub 3}N{sub 4}. An increase in substrate temperature from room temperature to 500 deg. C led to nucleation and growth of hard phases of {beta}-C{sub 3}N{sub 4} and Si{sub 3}N{sub 4} in the amorphous Si-C-N matrix. The nanoindentation studies showed the variation in hardness and Young's modulus from 8 to 22 GPa and from 100 to 240 GPa, respectively, dependent on the deposition conditions. The FTIR studies confirmed the presence of C-N, Si-N, Si-Si, Si-O, and Si-C in different films.

36 MATERIALS SCIENCE↗

Electronic and optical properties of ScN and (Sc,Mn)N thin films deposited by reactive DC-magnetron sputtering

Scandium nitride (ScN) is a rocksalt semiconductor that has attracted significant attention from various researchers for a diverse range of applications. Motivated by the prospect of using its interesting electronic structure for optoelectronic and dilute magnetic semiconductor applications, we present detailed studies of the electronic transport and optical properties of ScN and its alloys with manganese nitride (MnN). Our results suggest (a) dilute manganese doping in ScN compensates for the high n-type carrier concentrations arising due to oxygen impurities and (b) an n-type to p-type carrier type transition occurs at a composition between 5.8% and 11% Mn on Sc sites. In terms of its optical properties, our analysis clearly indicates direct and indirect bandgap absorption edges of ScN located at 2.04 eV and 1.18 eV, respectively. In addition to the direct gap absorption edge, (Sc,Mn)N samples also show Mn-defect induced electronic absorption. Photoluminescence measurements at room temperature from ScN films exhibit a yellowish-green emission corresponding to direct gap radiative recombination. Direct gap recombination is not expected given the smaller indirect gap. A possible role of high excitation intensities in suppressing relaxation and recombination across the indirect bandgap is suspected. Raman spectroscopic and ellipsometric characterization of the dielectric permittivities of ScN and (Sc,Mn)N are also presented to assist in understanding the potential of ScN for optoelectronic applications.

36 MATERIALS SCIENCE↗

Size dependent optical properties of Si quantum dots in Si-rich nitride/Si{sub 3}N{sub 4} superlattice synthesized by magnetron sputtering

A spectroscopic ellipsometry compatible approach is reported for the optical study of Si quantum dots (QDs) in Si-rich nitride/silicon nitride (SRN/Si{sub 3}N{sub 4}) superlattice, which based on Tauc-Lorentz model and Bruggeman effective medium approximation. It is shown that the optical constants and dielectric functions of Si QDs are strongly size dependent. The suppressed imaginary dielectric function of Si QDs exhibits a single broad peak analogous to amorphous Si, which centered between the transition energies E{sub 1} and E{sub 2} of bulk crystalline Si and blue shifted toward E{sub 2} as the QD size reduced. A bandgap expansion observed by the TL model when the size of Si QD reduced is in good agreement with the PL measurement. The bandgap expansion with the reduction of Si QD size is well supported by the first-principles calculations based on quantum confinement.

36 MATERIALS SCIENCE↗

Potential for reactive pulsed-dc magnetron sputtering of nanocomposite VO{sub x} microbolometer thin films

Vanadium oxide (VO{sub x}) thin films were deposited by reactive pulsed-dc sputtering a metallic vanadium target in argon/oxygen mixtures with substrate bias. Hysteretic oxidation of the vanadium target surface was assessed by measuring the average cathode current during deposition. Nonuniform oxidization of the target surface was analyzed by Raman spectroscopy. The VO{sub x} film deposition rate, resistivity, and temperature coefficient of resistance were correlated to oxygen to argon ratio, processing pressure, target-to-substrate distance, and oxygen inlet positions. To deposit VO{sub x} in the resistivity range of 0.1–10 Ω-cm with good uniformity and process control, lower processing pressure, larger target-to-substrate distance, and oxygen inlet near the substrate are useful.

36 MATERIALS SCIENCE↗

Growth, electrical, and optical properties of nanocrystalline VO{sub 2} (011) thin films prepared by thermal oxidation of magnetron sputtered vanadium films

Nanocrystalline vanadium dioxide (VO{sub 2}) thin films were prepared on glass substrates at different deposition temperatures by oxidizing sputtered vanadium films. Atomic force microscope, x-ray diffraction, and Raman scattering were employed to characterize the films. It was confirmed that low deposition temperature resulted in improving oxygen atom diffusion and VO{sub 2} nanograin growth in the thermal oxidation process. Investigation of the electrical properties revealed that the amplitude of semiconductor-metal transition and transition temperature decreased, whereas the Hall mobility and carrier concentration increased as the deposition temperature elevated. Optical investigations were carried out in the ultraviolet-visible-near-infrared region. Narrow optical band gaps were observed in these films.

36 MATERIALS SCIENCE↗

Electronic structure and electrical transport in ternary Al-Mg-B films prepared by magnetron sputtering

Nanostructured ternary Al-Mg-B films possess high hardness and corrosion resistance. In the present work, we study their electronic structure and electrical transport. The films exhibit semiconducting characteristics with an indirect optical-bandgap of 0.50 eV, as deduced from the Tauc plots, and a semiconductor behavior with a Fermi level of {approx}0.24 eV below the conduction band. Four-probe and Hall measurements indicated a high electrical conductivity and p-type carrier mobility, suggesting that the electrical transport is mainly due to hole conduction. Their electrical properties are explained in terms of the film nanocomposite microstructure consisting of an amorphous B-rich matrix containing AlMgB{sub 14} nanoparticles.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Characterizations of Binary FeCr (AISI 430) Thin Films Deposited from a Single Magnetron Sputtering Under Easy Controllable Deposition Parameters

A series of 50-nm binary FeCr martensitic thin films were sputtered from a single source made of commercial AISI 430 ferritic stainless steel under the deposition rates gradually increased from 0.03 to 0.11 nm/s with 0.02 nm/s steps at stationary condition. And, under 0.09 nm/s deposition rate, a second series of the films were also deposited under the rotation speed of their substrates which was chosen at 0, 25, and 45 rpm. As far as we are concerned, this study is the first investigation of properties of the thin films produced from AISI 430. The atomic Fe content in the films increased from 79.3 to 98.6% while atomic Cr content decreased from 20.5 to 1.2% with the increase of deposition rate from 0.03 to 0.11 nm/s. According to compositional analysis, the Fe content increased while Cr content decreased with increasing deposition rate. The reason for this may be attributed to the relatively different bond energy/melting point of metals which have different contents sputtered from source material since this physical parameter is very significant for the sputtering process. And, the Fe content in the films decreased from 84.9 to 79.2 at. % while the Cr content increased from 14.9 to 20.6 at. % when the increase of rotation speed of substrate. The crystal structure of all films was observed to have a body-centered tetragonal phase and the intensity of (110) peak varied with the atomic Fe content. The surface observations of films performed by a scanning electron microscope exposed that the number of surface grains increased with the increase of deposition rate and decreased with the increase of rotation speed. According to surface roughness analysis done by an atomic force microscope, the roughness of the film surfaces increased as the deposition rate increased. And, the roughness of the film surfaces decreased as the rotation speed increased. This has been consistent with the grain size and roughness parameters. Thus, increasing deposition rate and decreasing rotation speed of the substrate caused an increase in grain size and roughness parameters. The magnetic measurements of the films achieved, by a vibrating sample magnetometer at room temperature, displayed that the saturation magnetization, M{sub s}, values increased from 820.1 to 1700.4 emu/cm{sup 3}, the remanence magnetization, M{sub r}, values increased from 293 to 817 emu/cm{sup 3}, and the coercivity, H{sub c}, value also increased from 38 to 107 Oe with the increasing of deposition rate. It is also seen that the magnetic easy axis are in the film plane due to the shape anisotropy. With the increase rotation speed, the values of M{sub s} and M{sub r} increased and the H{sub c} decreased. It was seen that variation of Fe content in the films influences the M{sub s} values and the H{sub c} values are consistent with the surface properties. It was concluded that the deposition rate and the rotation speed of the substrate play a considerable role on the structural and related magnetic properties of the sputtered FeCr thin films, and the properties of the films can be easily controlled by changing production parameters.

36 MATERIALS SCIENCE↗

Structural and superconducting properties of Nb 3 Sn films grown by multilayer sequential magnetron sputtering

Nb 3 Sn thin films are fabricated by sequential sputtering followed by annealing at 850–1200°C in vacuum. The effects of the annealing temperature and time on the formation of Nb 3 Sn were examined. The film crystal structure, morphology, surface topography and composition were distinguished by X-ray diffraction, field-emission scanning electron microscopy, atomic force microscopy, and energy dispersive X-ray spectroscopy analysis. The superconducting properties of the films were characterized by measuring the surface resistivity by the four-point probe method. The highest critical temperature T c = 17.86 K was observed for the Nb 3 Sn films annealed at 950°C for 3 h. When the films were annealed above 1000°C for 3 h, Sn evaporation resulted in a Nb-rich film, degrading the superconducting performance. Annealing at 1200°C for 3 h resulted in evaporation of Sn leaving less than 1% Sn on the surface, as detected by energy dispersive spectroscopy, and for that film a T c of 7.9 K was observed.

36 MATERIALS SCIENCE↗