Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Lithiation”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 397 records · Page 22

Understanding Stabilization in Nanoporous Intermetallic Alloy Anodes for Li-Ion Batteries Using Operando Transmission X-ray Microscopy

Tin-based alloying anodes are exciting due to their high energy density. Unfortunately, these materials pulverize after repetitive cycling due to the large volume expansion during lithiation and delithiation; both nanostructuring and intermetallic formation can help alleviate this structural damage. Here, these ideas are combined in nanoporous antimony–tin (NP-SbSn) powders, synthesized by a simple and scalable selective-etching method. The NP-SbSn exhibits bimodal porosity that facilitates electrolyte diffusion; those void spaces, combined with the presence of two metals that alloy with lithium at different potentials, further provide a buffer against volume change. This stabilizes the structure to give NP-SbSn good cycle life (595 mAh/g after 100 cycles with 93% capacity retention). Operando transmission X-ray microscopy (TXM) showed that during cycling NP-SbSn expands by only 60% in area and then contracts back nearly to its original size with no physical disintegration. The pores shrink during lithiation as the pore walls expand into the pore space and then relax back to their initial size during delithiation with almost no degradation. Importantly, the pores remained open even in the fully lithiated state, and structures are in good physical condition after the 36th cycle. The results of this work should thus be useful for designing nanoscale structures in alloying anodes.

25 ENERGY STORAGE↗

Visualization of lithium-ion transport and phase evolution within and between manganese oxide nanorods

Multiple lithium-ion transport pathways and local phase changes upon lithiation in silver hollandite are revealed via in situ microscopy including electron diffraction, imaging and spectroscopy, coupled with density functional theory and phase field calculations. Here, we report unexpected inter-nanorod lithium-ion transport, where the reaction fronts and kinetics are maintained within the neighbouring nanorod. Notably, this is the first time-resolved visualization of lithium-ion transport within and between individual nanorods, where the impact of oxygen deficiencies is delineated. Initially, fast lithium-ion transport is observed along the long axis with small net volume change, resulting in two lithiated silver hollandite phases distinguishable by orthorhombic distortion. As a result, a slower reaction front is observed, with formation of polyphase lithiated silver hollandite and face-centred-cubic silver metal with substantial volume expansion. Our results indicate lithium-ion transport is not confined within a single nanorod and may provide a paradigm shift for one-dimensional tunnelled materials, particularly towards achieving high-rate capability.

25 ENERGY STORAGE↗

Impact of dual-layer solid-electrolyte interphase inhomogeneities on early-stage defect formation in Si electrodes

While intensive efforts have been devoted to studying the nature of the solid-electrolyte interphase (SEI), little attention has been paid to understanding its role in the mechanical failures of electrodes. Here we unveil the impact of SEI inhomogeneities on early-stage defect formation in Si electrodes. Buried under the SEI, these early-stage defects are inaccessible by most surface-probing techniques. With operando full field diffraction X-ray microscopy, we observe the formation of these defects in real time and connect their origin to a heterogeneous degree of lithiation. This heterogeneous lithiation is further correlated to inhomogeneities in topography and lithium-ion mobility in both the inner- and outer-SEI, thanks to a combination of operando atomic force microscopy, electrochemical strain microscopy and sputter-etched X-ray photoelectron spectroscopy. Our multi-modal study bridges observations across the multi-level interfaces (Si/LixSi/inner-SEI/outer-SEI), thus offering novel insights into the impact of SEI homogeneities on the structural stability of Si-based lithium-ion batteries. Severe structural deformation during (de)lithiation is the main factor limiting the stability of Si anodes in Li-ion batteries. Here, a multi-modal approach is used to visualize these deformations in their early-stage and link them to inhomogeneities in the dual-layer solid-electrolyte interphase.

25 ENERGY STORAGE↗

Effect of crystallite geometries on electrochemical performance of porous intercalation electrodes by multiscale operando investigation

Lithium-ion batteries are yet to realize their full promise because of challenges in the design and construction of electrode architectures that allow for their entire interior volumes to be reversibly accessible for ion storage. Electrodes constructed from the same material and with the same specifications, which differ only in terms of dimensions and geometries of the constituent particles, can show surprising differences in polarization, stress accumulation and capacity fade. Here, using operando synchrotron X-ray diffraction and energy dispersive X-ray diffraction (EDXRD), we probe the mechanistic origins of the remarkable particle geometry-dependent modification of lithiation-induced phase transformations in V2O5 as a model phase-transforming cathode. A pronounced modulation of phase coexistence regimes is observed as a function of particle geometry. Specifically, a metastable phase is stabilized for nanometre-sized spherical V2O5 particles, to circumvent the formation of large misfit strains. Spatially resolved EDXRD measurements demonstrate that particle geometries strongly modify the tortuosity of the porous cathode architecture. Greater ion-transport limitations in electrode architectures comprising micrometre-sized platelets result in considerable lithiation heterogeneities across the thickness of the electrode. These insights establish particle geometry-dependent modification of metastable phase regimes and electrode tortuosity as key design principles for realizing the promise of intercalation cathodes. Designing electrode architectures for Li-ion batteries that can be reversibly accessible for ion storage can be challenging. Using operando techniques the mechanistic origin of lithiation-induced phase transformations in a V2O5 model cathode is now clarified.

Luo, Yuting↗

Electrochemical characteristics of plasma-etched black silicon as anodes for Li-ion batteries

Nanostructured silicon as an anode material for Li-ion batteries is produced for the first time by inductively coupled plasma–plasma etching of Si wafers in the black silicon regime. The microscopic structure strongly resembles other types of nanostructured silicon, with a well-arranged nanostructure possessing a sufficient porosity for accommodating large volume expansion. Despite these features, however, a high first-cycle irreversible capacity loss and a poor cycle life are observed. The main reason for these poor features is the formation of a thick solid-electrolyte interphase (SEI) layer related to the surface condition of the pristine nanostructured black silicon (b-Si) electrode. Therefore, the cycle life of the b-Si electrode is heavily influenced by the constant reformation of the SEI layer depending upon the surface composition in spite of the presence of nanostructured Si. In the fast lithiation experiments, the nanostructure region of the b-Si electrode is detached from the Si substrate owing to the kinetics difference between the lithium ion diffusion and the electron injection and phase transformation in the nanostructured Si region. This means that more Si substrate is involved in lithiation at high current rates. It is therefore important to maintain balance in the chemical kinetics during the lithiation of nanostructured Si electrodes with a Si substrate.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effect of electrochemical cycling on microstructures of nanocomposite silicon electrodes using hyperpolarized 129 Xe and 7 Li NMR spectroscopy

The microstructural stability of composite electrodes during electrochemical cycling is critically important as it dictates the performance of Li-ion batteries. The issue becomes even more important for the high capacity alloying anode such as silicon that typically exhibits dramatic lithiation–delithiation-induced volume changes. The solid electrolyte interphase (SEI) layer formed on the active electrode surface has a profound effect on the overall microstructural stability of composite electrodes. An ideal SEI layer allows Li+ ions in and out of the electrode, but is an insulator to electrons, preventing the electrolyte from being further reduced. However, the SEI layers formed during initial lithiation may experience changes or degradation with subsequent cycling, adversely affecting the electrode performance. A combination of hyperpolarized 129 Xe and 7 Li nuclear magnetic resonance spectroscopies was applied to probe the microstructures of nanocomposite silicon electrodes at various stages of the lithiation–delithiation cycle. The results obtained from this study shed light on the degradation mechanism of nanocomposite Si electrodes upon electrochemical cycling and should prove useful in the effort to design more robust electrodes in the future.

36 MATERIALS SCIENCE↗

Electrochemical Dilatometry of Si-Bearing Electrodes: Dimensional Changes and Experiment Design

The severe volumetric changes in Si particles during the Li (de)alloying process cause expansion and contraction of the electrodes, which along with excessive electrolyte reduction and solid electrolyte interphase formation brings about rapid decay in cell capacity. In this work, we use operando electrochemical dilatometry to quantify the (de)lithiation-induced expansion/contraction of Si-based and graphite-rich electrodes during electrochemical cycling. We evaluate the relationship between electrode capacity and dilation and observe that by increasing the Si contribution to the electrode capacity, the swelling is aggravated upon lithiation. For silicon-rich anodes, the electrode dilation can be higher than 300%, and the expansion profile consists of a combination of slow swelling at low lithiation followed by an accelerated increase at higher lithium contents. We investigate how electrode properties, such as porosity, affect the dilation profile and quantify the irreversible expansion of the electrodes. Finally, we discuss some of the challenges associated with the dilatometry technique and suggest experimental approaches for obtaining consistent and reliable data.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Inactive Overhang in Silicon Anodes

Li-ion batteries contain excess anode area to improve manufacturability and prevent Li plating. These overhang areas in graphite electrodes are active but experience decreased Li + flux during cycling. Over time, the overhang and the anode portions directly opposite to the cathode can exchange Li + , driven by differences in local electrical potential across the electrode, which artificially inflates or decreases the measured cell capacity. Here, we show that lithiation of the overhang is less likely to happen in silicon anodes paired with layered oxide cathodes. The large voltage hysteresis of silicon creates a lower driving force for Li + exchange as lithium ions transit into the overhang, rendering this exchange highly inefficient. For crystalline Si particles, Li + storage at the overhang is prohibitive, because the low potential required for the initial lithiation can act as thermodynamic barrier for this exchange. We use micro-Raman spectroscopy to demonstrate that crystalline Si particles at the overhang are never lithiated even after cell storage at 45 °C for four months. Because the anode overhang can affect the forecasting of cell life, cells using silicon anodes may require different methodologies for life estimation compared to those used for traditional graphite-based Li-ion batteries.

25 ENERGY STORAGE↗

Recent Developments in Lithium-Manganese-Nickel Oxide Electrochemistry: The Alchemy of LiMn 0.5 Ni 0.5 O 2

Efforts have been underway for some time at Argonne National Laboratory to design structurally integrated and stabilized lithium-manganese-nickel-oxide cathode materials. The goal has been to find a cobalt-free, high-capacity cathode for a Li-ion battery that is competitive, both cost- and energy-wise, with lithium-nickel-manganese-cobalt-oxide (NMC) and lithium-iron-phosphate (LFP) products. This brief synopsis highlights the remarkable alchemy of LiMn 0.5 Ni 0.5 O 2 resulting from its well-known, slightly disordered layered structure and the recently discovered lithiated spinel phase and totally disordered rock-salt configurations. All three arrangements share a structurally compatible cubic-close-packed oxygen array. The lithiated spinel and layered components provide an intersecting network of two- and three-dimensional channels that facilitate Li + -ion transport, while a minor amount of an extensively disordered rock-salt component likely serves to enhance the structural and electrochemical stability of the electrode. The synopsis also encompasses the historical development of lithiated spinel electrode materials and structurally integrated systems.

Thackeray, Michael M. [Argonne National Laboratory↗

Electrochemical Properties of Electrodes Derived from NaTi 3 O 6 OH·2H 2 O in Sodium and Lithium Cells

Materials derived from the layered compound NaTi 3 O 6 OH·2H 2 O, also known as “sodium nonatitanate” or NNT, have recently been found to undergo reversible sodium or lithium intercalation processes at very low potentials. While practical discharge capacities in lithium cells can be above 200 mAh/g, making them of interest for high-energy applications, the presence of mobile sodium in the materials complicates the cycling behavior. A simple ion-exchange process prior to incorporation in electrochemical cells removes all sodium ions, producing the lithiated form of the material. The lithiated material (LNT) performs similarly to NNT in lithium cells, although coulombic inefficiencies are somewhat higher. A comparison is made between the behavior of NNT in sodium cells and that of NNT and the lithiated analog in lithium cells.

36 MATERIALS SCIENCE↗

Mechanistic Analysis of Mechano-Electrochemical Interaction in Silicon Electrodes with Surface Film

High-capacity anode materials for lithium-ion batteries, such as silicon, are prone to large volume change during lithiation/delithiation which may cause particle cracking and disintegration, thereby resulting in severe capacity fade and reduction in cycle life. In this work, a stochastic analysis is presented in order to understand the mechano-electrochemical interaction in silicon active particles along with a surface film during cycling. Amorphous silicon particles exhibiting single-phase lithiation incur lower amount of cracking as compared to crystalline silicon particles exhibiting two-phase lithiation for the same degree of volumetric expansion. Rupture of the brittle surface film is observed for both amorphous and crystalline silicon particles and is attributed to the large volumetric expansion of the silicon active particle with lithiation. The mechanical property of the surface film plays an important role in determining the amount of degradation in the particle/film assembly. A strategy to ameliorate particle cracking in silicon active particles is proposed.

25 ENERGY STORAGE↗

Lithium-Ion Cathode/Coating Pairs for Transition Metal Containment

Formany lithium-ion cathode materials, transitionmetal (TM) dissolution into the electrolyte contributes to cell degradation. Cathode coatings can limit TM dissolution by containing TMs in cathode materials. We perform density functional theory calculations to evaluate cathode/coating pairs for TM containment, specifically focusing on reactive stability of coating/cathode pairs as well as TM solubility in the coating materials. We consider stability and containment of materials at both synthesis and operating conditions. We find that many cathode/coating pairs are reactive when lithiated, while other cathode-coating pairs are stable when lithiated but become reactive following delithiation. Of all the coatings that we considered, Li 3 PO 4 occupies a unique chemical position, in that its coatings on oxide cathode materials maintained equilibrium under both lithiated and delithiated conditions. Furthermore, for oxide cathode materials, the Li 3 PO 4 coatings exhibit low TM solubilities across all cathode states of charge. Our results demonstrate that Li 3 PO 4 is a promising candidate for stable coatings on oxide cathode materials to limit TM dissolution into the electrolyte.

25 ENERGY STORAGE↗

Measuring Li + inventory losses in LiCoO 2 /graphite cells using Raman microscopy

Here, the contribution from loss of Li + inventory to capacity fade is described for slow rates (C/10) and long-term cycling (up to 80 cycles). It was found through electrochemical testing and ex-situ Raman analysis that at these slow rates, the entirety of capacity loss up to 80 cycles can be explained by loss of Li + inventory in the cell. The Raman spectrum of LiCoO 2 is sensitive to the state of lithiation and can therefore be leveraged to quantify the state of lithiation for individual particles. With these Raman derived estimates, the lithiation state of the cathode in the discharged state is compared to electrochemical data as a function of cycle number. High correlation is found between Raman quantifications of cycleable lithium and the capacity fade. Additionally, the linear relationship between discharge capacity and cell overpotential suggests that the loss of capacity stems from an impedance rise of the electrodes, which based on Li inventory losses, is caused by SEI formation and repair.

25 ENERGY STORAGE↗

Review of the Stability/Capacity Trade-off in Silver Hollandite Lithium Battery Cathodes

ABSTRACT Highly detailed structural characterization is required to understand the discharge mechanism in order to effectively investigate α-MnO 2 structured lithium battery cathode materials. This paper discusses recent findings which elucidate the lithiation mechanism of silver-hollandite, Ag x Mn 8 O 16 . For Ag 1.2 Mn 8 O 16 , the structure is not significantly perturbed during the first 2 equivalents of lithiation and the electrochemistry is highly reversible. Upon 4 equivalents of lithiation, the structure becomes highly distorted, in correlation with capacity fade observed over 40 cycles. Notably, regarding capacity fade, modifications to Ag/Mn ratio are less impactful than modifications to the α-MnO 2 crystallite size. This is shown in comparisons of two materials with the same stoichiometry (Ag 1.4 Mn 8 O 16 ) and differing crystallite size (10 and 15 nm).

energy storage (including batteries and capacitors↗

The Science of Battery Degradation

This report documents work that was performed under the Laboratory Directed Research and Development project, Science of Battery Degradation. The focus of this work was on the creation of new experimental and theoretical approaches to understand atomistic mechanisms of degradation in battery electrodes that result in loss of electrical energy storage capacity. Several unique approaches were developed during the course of the project, including the invention of a technique based on ultramicrotoming to cross-section commercial scale battery electrodes, the demonstration of scanning transmission x-ray microscopy (STXM) to probe lithium transport mechanisms within Li-ion battery electrodes, the creation of in-situ liquid cells to observe electrochemical reactions in real-time using both transmission electron microscopy (TEM) and STXM, the creation of an in-situ optical cell utilizing Raman spectroscopy and the application of the cell for analyzing redox flow batteries, the invention of an approach for performing ab initio simulation of electrochemical reactions under potential control and its application for the study of electrolyte degradation, and the development of an electrochemical entropy technique combined with x-ray based structural measurements for understanding origins of battery degradation. These approaches led to a number of scientific discoveries. Using STXM we learned that lithium iron phosphate battery cathodes display unexpected behavior during lithiation wherein lithium transport is controlled by nucleation of a lithiated phase, leading to high heterogeneity in lithium content at each particle and a surprising invariance of local current density with the overall electrode charging current. We discovered using in-situ transmission electron microscopy that there is a size limit to lithiation of silicon anode particles above which particle fracture controls electrode degradation. From electrochemical entropy measurements, we discovered that entropy changes little with degradation but the origin of degradation in cathodes is kinetic in nature, i.e. lower rate cycling recovers lost capacity. Finally, our modeling of electrode-electrolyte interfaces revealed that electrolyte degradation may occur by either a single or double electron transfer process depending on thickness of the solid-electrolyte-interphase layer, and this cross-over can be modeled and predicted.

25 ENERGY STORAGE↗

Final Technical Report: Application of in situ Neutron Diffraction to Understand the Mechanism of Phase Transitions

In this research, phase transitions in the bulk electrodes for Li-ion batteries were investigated using neutron diffraction (ND) as well as neutron imaging techniques. The objectives of this research is to design of a novel in situ electrochemical cell to obtain Rietveld refinable neutron diffraction experiments using small volume electrodes of various laboratory/research-scale electrodes intended for Li-ion batteries. This cell is also to be used to investigate the complexity of phase transitions in Li(Mg) alloy electrodes, either by diffraction or by neutron imaging, which occur under electrochemical lithiation and delithiation, and to determine aspects of phase transition that enable/limit energy storage capacity. Additional objective is to investigate the phase transitions in electrodes made of etched micro-columns of silicon and investigate the effect of particle/column size on phase transitions and nonequilibrium structures. An in situ electrochemical cell was designed successfully and was used to study the phase transitions under in-situ neutron diffraction in both the electrodes (anode/cathode) simultaneously in graphite/LiCoO 2 and in graphite/LiMn 2 O 4 cells each with two cells. The diffraction patterns fully validated the working of the in situ cell. Additional experimental were performed using the Si micro-columnar electrodes. The results revealed new lithiation phenomena, as evidenced by mosaicity formation in silicon electrode. These experiments were performed in Vulcan diffractometer at SNS, Oak Ridge National Laboratory. In parallel, the spatial distribution of Li during lithiation and delithiation processes in Li-battery electrodes were investigated. For this purpose, neutron tomographic imaging technique has been used for 3D mapping of Li distribution in bulk Li(Mg) alloy electrodes. It was possible to observe the phase boundary of Li(Mg) alloy indicating phase transition from Li-rich BCC β-phase to Li-lean α-phase. These experiments have been performed at CG-1D Neutron Imaging Prototype Station at SNS.

25 ENERGY STORAGE↗