Rubber-toughened cyanate composites - Properties and toughening mechanism

Earlier work by Young et al. (1990) has shown that Dow experimental cyanate ester resin XU71787.02 is readily toughenable by rubber. A particularly effective rubber for this purpose is an experimental core-shell rubber which toughens the polymer by inducing shear yielding. This paper describes an investigation into the toughening mechanism in the corresponding carbon-fiber composite systems and the effect of fibers on composite properties. Resin-fiber interfacial shear strengths have been successfully correlated to the compressive strengths after impact and other key properties of composites based on rubber-toughened cyanate and several carbon fibers. The differences in the properties are explained by the difference in the functioning of the rubber particles during the fracture process.

Yang, P. C.↗

Oxidation of C/SiC Composites at Reduced Oxygen Partial Pressures

Carbon-fiber reinforced SiC (C/SiC) composites are proposed for leading edge applications of hypersonic vehicles due to the superior strength of carbon fibers at high temperatures (greater than 1500 C). However, the vulnerability of the carbon fibers in C/SiC to oxidation over a wide range of temperatures remains a problem. Previous oxidation studies of C/SiC have mainly been conducted in air or oxygen, so that the oxidation behavior of C/SiC at reduced oxygen partial pressures of the hypersonic flight regime are less well understood. In this study, both carbon fibers and C/SiC composites were oxidized over a wide range of temperatures and oxygen partial pressures to facilitate the understanding and modeling of C/SiC oxidation kinetics for hypersonic flight conditions.

Opila, Elizabeth J.↗

A review of issues and strategies in nondestructive evaluation of fiber reinforced structural composites

Techniques for quantitative assessment of the mechanical strength and integrity of fiber composites during manufacture and service and following repair operations are presented. Problems and approaches are discussed relative to acceptance criteria, calibrating standards, and methods for nondestructive evaluation of composites in strength-critical applications. Acousto-ultrasonic techniques provide the methods of choice in this area.

Vary, A.↗

Computational study of the effect of core–skin structure on the mechanical properties of carbon nanofibers

The effect of the core–skin structure on the mechanical properties of carbon nanofibers is investigated in large-scale molecular dynamics simulations of tensile deformation of carbon nanofibers with the core–skin and homogeneous structures. Contrary to an established notion of the deleterious effect of the skin layer on the strength of carbon fibers, the presence of a high-quality skin layer is found to increase both the Young’s modulus and tensile strength of the nanofiber. A detailed analysis of the fracture process indicates that the nanofiber strengthening is related to the ability of skin layer to suppress crack nucleation at the core–skin interface. Furthermore, the computational predictions suggest that the design of new approaches to carbon fiber manufacturing and processing leading to the generation of a high-quality skin layer while avoiding the introduction of structural defects at the core–skin interface may yield a significant enhancement of the mechanical properties of carbon fibers.

36 MATERIALS SCIENCE↗

Elevated temperature properties of boron/aluminum composites

The high temperature properties of boron/aluminum composites, fabricated by an air diffusion bonding technique utilizing vacuum-bonded monolayer tape are reported. Seventeen different combinations of matrix alloy, reinforcement diameter, reinforcement volume percent, angle-ply and matrix enhancement (i.e. titanium cladding and interleaves) were fabricated, inspected, and tested. It is shown that good to excellent mechanical properties could be obtained for air-bonded boron/aluminum composites and that these properties did not decrease significantly up to a test temperature of at least 260 C. Composites made with 8 mil B/W fiber show a much greater longitudinal strength dependence on volume percent fiber than composites made with 5.6 mil fiber. The addition of titanium caused difficulties in composite bonding and yielded composites with reduced strength.

Sullivan, P. G.↗

Laser Heated Oxide Fiber Growth Using Melt Modulation Technique

As a reinforcement for structural composites, single crystal alumina fibers offer low density, high modulus, and high creep resistance. In this study, the laser heated float zone approach was employed to grow c-axis Al2O3 continuous fibers of high purity and high strength. A new melt modulation technique, laser scanning, avoids the formation of surface induced ripples and allows the growth of 50 micro-m diameter sapphire fibers with strengths (approx. 7 GPa) significantly greater than either commercially available fibers grown by the edge-defined film growth process (approx. 2-3 GPa) or laboratory fibers grown by stationary laser heating (approx. 5 GPa). The present work suggests that surface striations are the predominant defects controlling the tensile strength of laser-scanned fibers at room temperature. Several possible mechanisms for inducing surface striations are systematically discussed for several oxide fiber compositions.

Sayir, Ali↗

High temperature dynamic modulus and damping of aluminum and titanium matrix composites

Dynamic modulus and damping capacity property data were measured from 20 to over 500 C for unidirectional B/Al (1100), B/Al (6061), B/SiC/Al (6061), Al2O3/Al, SiC/Ti-6Al-4V, and SiC/Ti composites. The measurements were made under vacuum by the forced vibration of composite bars at free-free flexural resonance near 2000 Hz and at strain application below 0.000001. The damping of B/Al composites was found at all temperatures to be significantly greater than the damping of the Al2O3/Al and SiC/Ti composites, with little variation observed in the dynamic moduli of specimens having almost the same fiber content. It is concluded that on the practical level, the finding of a damping-strength correlation supports the use of composite damping measurements for the nondestructive evaluation of boron fiber strength in as-fabricated and heat-treated B/Al (6061) composites.

Dicarlo, J. A.↗

The effect of interface properties on nickel base alloy composites

This program was performed to assess the extent to which mechanical behavior models can predict the properties of sapphire fiber/nickel aluminide matrix composites and help guide their development by defining improved combinations of matrix and interface coating. The program consisted of four tasks: 1) selection of the matrices and interface coating constituents using a modeling-based approach; 2) fabrication of the selected materials; 3) testing and evaluation of the materials; and 4) evaluation of the behavior models to develop recommendations. Ni-50Al and Ni-20AI-30Fe (a/o) matrices were selected which gave brittle and ductile behavior, respectively, and an interface coating of PVD YSZ was selected which provided strong bonding to the sapphire fiber. Significant fiber damage and strength loss was observed in the composites which made straightforward comparison of properties with models difficult. Nevertheless, the models selected generally provided property predictions which agreed well with results when fiber degradation was incorporated. The presence of a strong interface bond was felt to be detrimental in the NiAI MMC system where low toughness and low strength were observed.

Groves, M.↗

The Effect of Matrix and Fiber Properties on Impact Resistance

The basic material properties which control impact damage are identified and testing techniques are assessed. It is demonstrated that static indentation tests can provide better information about failure processes than impact tests, and they are simpler to conduct. In thin and thick laminates, it was found that the matrix shear strength controls the onset of delamination damage and that the fiber strength controlled the penetration phase. In thin laminates, tough matrices do little to enhance impact resistance.

Elber, W.↗

Elucidating texture and grain morphology contributions to the micromechanical response of additively manufactured Inconel 625

Microstructural variation of additively manufactured (AM) metal components in comparison to wrought counterparts makes certification for critical applications a challenge. Microscale simulations leveraging modern computational tools may be used to supplement testing of AM microstructures, thus accelerating certification by reducing the number of experiments needed. However, as micromechanical response is closely tied to critical properties like fatigue-life and fracture, utilization of these simulations with macroscale experimental data alone is insufficient. One means to attain microscale experimental data is in situ diffraction data collected from synchrotron X-ray sources. In this work, such data were collected during in situ compression of AM Inconel 625 superalloy. Interpretation of experimental results was assisted by massive (8M element) complementary micromechanical simulations performed on sets of virtual microstructures generated using cellular automata. Together, micromechanical data from diffraction experiments and simulations were used to probe the effects of textured “track” microstructures generated during laser powder bed fusion and directional strength-to-stiffness on micromechanical response. Though fiber-averaged directional strength-to-stiffness ratios were expected to dominate given the high elastic anisotropy of the material, the combination of small variations in texture and specific grain configurations unique to AM microstructures lead to significant variability in micromechanical response after yield. The findings emphasize the importance of high-fidelity microstructural representation that captures key texture components and AM-specific morphology for property prediction of AM metals.

36 MATERIALS SCIENCE↗

Properties of M40J Carbon/PMR-II-50 Composites Fabricated with Desized and Surface Treated Fibers. Characterization of M40J Desized and Finished Fibers

To increase performance and durability of high temperature composites for potential rocket engine components, it is necessary to optimize wetting and interfacial bonding between high modulus carbon fibers and high temperature polyimide resins. It has been previously demonstrated that the electro-oxidative shear treatments used by fiber manufacturers are not effective on higher modulus fibers that have fewer edge and defect sites in the surface crystallites. In addition, sizings commercially supplied on most carbon fibers are not compatible with polyimides. This study was an extension of prior work characterizing the surface chemistry and energy of high modulus carbon fibers (M40J and M60J, Torray) with typical fluorinated polyimide resins, such as PMR-II-50. A continuous desizing system which utilizes environmentally friendly chemical- mechanical processes was developed for tow level fiber and the processes were optimized based on weight loss behavior, surface elemental composition (XPS) and morphology (FE-SEM) analyses, and residual tow strength of the fiber, and the similar approaches have been applied on carbon fabrics. Both desized and further treated with a reactive finish were investigated for the composite reinforcement. The effects of desizing and/or subsequent surface retreatment on carbon fiber on composite properties and performance including fiber-matrix interfacial mechanical properties, thermal properties and blistering onset behavior will be discussed in this presentation.

Allred, Ronald E.↗

The tensile failure modes of metal-matrix composite materials

The strengths of individual boron fibers extracted from various as-received and thermally fatigued aluminum alloy matrix materials were measured. The results are described in terms of a Weibull distribution, and strengths of composites fabricated from these fibers are calculated in terms of lower and upper bounds. Tests conducted on composite specimens indicated that strengths approaching the upper bounds can be achieved in composites fabricated by normal diffusion bonding techniques. Cyclic temperature changes effectively reduced the strength values toward the lower bounds. It was concluded that this effect resulted from the degradation of the strength of the fiber-matrix bond.

Wright, M. A.↗

Resistance welding graphite-fiber composites

High-strength joints are welded in seconds in carbon-reinfored thermoplastic beams. Resistance-welding electrode applies heat and pressure to joint and is spring-loaded to follow softening material to maintain contact; it also holds parts together for cooling and hardening. Both transverse and longitudinal configurations can be welded. Adhesive bonding and encapsulation are more time consuming methods and introduce additional material into joint, while ultrasonic heating can damage graphite fibers in composite.

Lamoureux, R. T.↗

Experimental and analytical investigation of the fracture processes of boron/aluminum laminates containing notches

Experimental results for five laminate orientations of boron/aluminum composites containing either circular holes or crack-like slits are presented. Specimen stress-strain behavior, stress at first fiber failure, and ultimate strength were determined. Radiographs were used to monitor the fracture process. The specimens were analyzed with a three-dimensional elastic-elastic finite-element model. The first fiber failures in notched specimens with laminate orientation occurred at or very near the specimen ultimate strength. For notched unidirectional specimens, the first fiber failure occurred at approximately one-half of the specimen ultimate strength. Acoustic emission events correlated with fiber breaks in unidirectional composites, but did not for other laminates. Circular holes and crack-like slits of the same characteristic length were found to produce approximately the same strength reduction. The predicted stress-strain responses and stress at first fiber failure compared very well with test data for laminates containing 0 deg fibers.

Johnson, W. S.↗

Metal clad aramid fibers for aerospace wire and cable

High strength light weight metal clad aramid fibers can provide significant weight savings when used to replace conventional metal wire in aerospace cable. An overview of metal clad aramid fiber materials and information on performance and use in braided electrical shielding and signal conductors is provided.

Tokarsky, Edward W.↗

Compression After Impact Strength Comparison of Rohacell Foam and Aluminum Honeycomb Core Sandwich Structure

This Technical Memorandum is a follow-on study to a previous one1 that examined the compression after impact (CAI) strength of carbon fiber sandwich structure with aluminum honeycomb core and Rohacell foam core with barely visible impact damage (BVID). In this current study a wider range of impact energies were utilized and the CAI strength assessed with these different damage severity levels. This was done to provide a more complete database for the two types of sandwich structure tested in these studies. In addition, the honeycomb sandwich specimens were tested with both the ‘L’ and ‘W’ directions aligned with the axis of compression loading. As in the study examining CAI strength with BVID1, the results were normalized by the mass of the sandwich structure. The results showed that the CAI strength did differ depending on the orientation of the core during testing and that when tested in the W-direction, the honeycomb core sandwich structure had about the same CAI strength as the foam core sandwich structure when normalized by the mass of the sandwich structures.

Sandwich Structure↗

Comparison of the compressive strengths for stitched and toughened composite systems

The compression strength of a stitched and a toughened matrix graphite/epoxy composite was determined and compared to a baseline unstitched untoughened composite. Two different layups with a variety of test lengths were tested under both ambient and hot/wet conditions. No significant difference in strength was seen for the different materials when the gage lengths of the specimens were long enough to lead to a buckling failure. For shorter specimens, a 30 percent reduction in strength from the baseline was seen due to stitching for both a 48-ply quasi-isotropic and a (0/45/0/-45/90/-45/0/45/0)s laminate. Analysis of the results suggested that the decrease in strength was due to increased fiber misalignment due to the stitches. An observed increasing strength with decreasing gage length, which was seen for all materials, was explained with a size effect model. The model assumed a random distribution of flaws (misaligned fibers). The toughened materials showed a small increase in strength over the baseline material for both laminates presumably due to the compensating effects of a more compliant matrix and straighter fibers in the toughened material. The hot/wet strength of the stitched and baseline material fell 30 percent below their ambient strengths for shorter, nonbuckling specimen, while the strength of the toughened matrix material only fell 20 percent. Video images of the failing specimen were recorded and showed local failures prior to global collapse of the specimen. These images support the theory of a random distribution of flaws controlling composite failure. Failed specimen appearance, however, seems to be a misleading indication of the cause of failure.

Reeder, James R.↗