Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “CORROSION PRODUCTS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 397 records · Page 22

Effects of impurities in coal-derived liquids on accelerated hot corrosion of superalloys

A Mach 0.3 burner rig was used to determine the effects of potential coal derived liquid fuel impurity combustion of products on hot corrosion in IN-100, IN-792, IN_738, U-700, Mar M-509, and 304 stainless steel. The impurities, added as aqueous solutions to the combustor, were salts of sodium, potassium, vanadium, molybdenum, tungsten, phosphorus, and lead. Extent of attack was determined by metal consumption and compared to the effects of sodium alone. Vanadium, molybdenum, tungsten, phosphorous, and lead in combination with sodium all resulted in increased attack as compared with sodium alone at some temperatures, apparently due in large part to the extension of the formation of liquid deposits. Varying the sodium-potassium ratio had little effect for ratios less than 1:3 for which reduced, but measurable, attack was observed.

Deadmore, D. L.↗

Measuring bio-oil upgrade intermediates and corrosive species with polarity-matched analytical approaches

Integrating biofuels with conventional petroleum products requires improvements in processing to increase blendability with existing fuels. This work demonstrates analysis techniques for more hydrophilic bio-oil liquids that give improved quantitative and qualitative description of the total acid content and organic acid profiles. To protect infrastructure from damage and reduce the cost associated with upgrading, accurate determination of acid content and representative chemical compound analysis are central imperatives to assessing both the corrosivity and the progress toward removing oxygen and acidity in processed biomass liquids. Established techniques form an ample basis for bio-liquids evaluation. However, early in the upgrading process, the unique physical phases and varied hydrophilicity of many pyrolysis liquids can render analytical methods originally designed for use in petroleum-derived oils inadequate. In this work, the water solubility of the organic acids present in bio-oils is exploited in a novel extraction and titration technique followed by analysis on the water-based capillary electrophoresis (CE) platform. The modification of ASTM D664, the standard for Total Acid Number (TAN), to include aqueous carrier solvents improves the utility of that approach for quantifying acid content in hydrophilic bio-oils. Termed AMTAN (modified Total Acid Number), this technique offers 1.2% relative standard deviation and dynamic range comparable to the conventional ASTM method. Furthermore, the results of corrosion product evaluations using several different sources of real bio-oil are discussed in the context of the unique AMTAN and CE analytical approaches developed to facilitate those measurements.

09 BIOMASS FUELS↗

Interplay between Catalyst Corrosion and Homogeneous Reactive Oxygen Species in Electrochemical Ozone Production

In this study, electrochemical ozone production (EOP), a six-electron water oxidation reaction, offers promising avenues for creating value-added oxidants and disinfectants. However, progress in this field is slowed by a dearth of understanding of fundamental reaction mechanisms. In this work, we combine experimental electrochemistry, spectroscopic detection of reactive oxygen species (ROS), oxygen-anion chemical ionization mass spectrometry, and computational quantum chemistry calculations to determine a plausible reaction mechanism on nickel- and antimony-doped tin oxide (Ni/Sb–SnO 2 , NATO), one of the most selective EOP catalysts. Antimony doping is shown to increase the conductivity of the catalyst, leading to improved electrochemical performance. Spectroscopic analysis and electrochemical experiments combined with quantum chemistry predictions reveal that hydrogen peroxide (H 2 O 2 ) is a critical reaction intermediate. We propose that leached Ni 4+ cations catalyze hydrogen peroxide into solution phase hydroperoxyl radicals ( • OOH); these radicals are subsequently oxidized to ozone. Isotopic product analysis shows that ozone is generated catalytically from water and corrosively from the catalyst oxide lattice without regeneration of lattice oxygens. Further quantum chemistry calculations and thermodynamic analysis suggest that the electrochemical corrosion of tin oxide itself might generate hydrogen peroxide, which is then catalyzed to ozone. The proposed pathways explain both the roles of dopants in NATO and its lack of stability. Our study interrogates the possibility that instability and electrochemical activity are intrinsically linked through the formation of ROS. In doing so, we provide the first mechanism for EOP that is consistent with computational and experimental results and highlight the central challenge of instability as a target for future research efforts.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Corrosion of 15th and early 16th century stained glass from the monastery of Batalha studied with external ion beam

This paper reports the study of corrosion in two stained glass panels from the south aisle of Sta. Maria da Vitoria monastery, at Batalha (Portugal), one depicting the Last Supper (dated from 1508), and the other one showing a saint (c. 1450). These panels exhibit extensive corrosion with darkening phenomena that are an impediment to their correct visualization, a source of major concern both to conservators and curators. By using external micro-beam Particle Induced X-ray Emission (PIXE) and Particle Induced Gamma Emission (PIGE) spectrometry, the elemental compositions of large fragments were obtained, enabling the selection of representative corroded areas, from which elemental distribution maps were produced by scanning. Calcium and potassium rich structures were found - at the surface and inside cavities in the glass - that were identified as oxalates and carbonates, by Raman microscopy and micro-FTIR. The dark spots present in the glass surfaces were found to be Zn and Pb rich. These findings indicate that the corrosion observed was due not only to reactions with atmospheric water and CO{sub 2} but also with the oxalic acid secreted by micro-organisms. Furthermore, it did not result from reactions with atmospheric SO{sub 2} or acid rain. The information obtained is relevant for a better understanding of the corrosion processes and products formed on the surface of these panels and therefore for the proper planning of much needed adequate conservation-restoration actions and appropriate display conditions. - Research Highlights: {yields} Corrosion and darkening of stained glasses is of concern to conservators and curators. {yields} A multi-technique approach is of relevance to study stained glass corrosion. {yields} External beam PIXE-PIGE provide valuable insight on stained glass corrosion.

36 MATERIALS SCIENCE↗

The Effect of Kr-85 Decay to Rb-85 on Waste Forms - 17105

Krypton-85 (Kr-85) is a volatile radionuclide released during the reprocessing of used nuclear fuel (UNF). Prior to discharge of process off-gas streams to the environment, removal of Kr-85 is required to meet emission regulations. Once removed from the off-gas streams, Kr (containing stable Kr in addition to Kr-85) must be placed in storage until the Kr-85 has decayed to levels such that its potential release would meet regulatory guidelines. The current method of storage is high-pressure metal canisters. Historically, concerns have been expressed that the decay product of Kr-85, Rubidium-85 (Rb-85), could cause corrosion and weakening in the canisters that would ultimately lead to premature failure and release of Kr-85. Alternate methods and materials, such as matrix isolation in a vapor deposited metal and immobilization in zeolites, have been investigated as storage approaches for Kr. However, even these storage methods may become compromised due to the chemical effects of Rb-85 arising from the decay of Kr-85. A review was conducted of the available literature to examine topics relevant to the effects of Rb on the long-term storage of Kr-85, examine the source terms in the context of this concern, and suggest a path forward to resolve outstanding knowledge gaps. In the course of this analysis, several knowledge gaps were identified. Examples include: o The use of solid sorbents to potentially permit more Kr-85-bearing gas to be loaded into canisters, either at the pressures used in the current method or at significantly lower pressures. o A cost-to-benefit analysis is needed to ascertain the practicality of manufacturing waste forms for Kr-85 storage with solid sorbents. o The effects of radiation and chemical transmutation in solid sorbents or matrices for this application are virtually unknown. o Fundamental data are needed on corrosion rates and mechanisms as functions of Rb concentration, storage temperature, etc., for various storage approaches (e.g., as compressed gas or encapsulated in a getter material) and storage container materials. The present analysis focused on the available information regarding storage of Kr-85 in high-pressure containers. It was judged unlikely that such containers would be compromised by corrosion from the Rb decay product, especially if the Kr recovery operations result in a gas composition with very low oxygen content. However, this conclusion should be revisited based on preliminary data gathered from analysis of legacy Kr waste forms. These legacy waste forms are a result of experiments conducted at Idaho National Laboratory over 30 y ago and have been stored for more than three Kr-85 half-lives. Evaluation of these forms indicates significant corrosion, the cause of which has not been conclusively determined. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Thermophysical Properties and Corrosion Characterization of Low Cost Lithium Containing Nitrate Salts Produced in Northern Chile for Thermal Energy Storage

In recent years, lithium containing salts have been studied for thermal energy storage (TES) systems applications, because of their optimal thermophysical properties. In solar power plants, lithium is seen as a way to improve the properties of molten salts used today. Lithium nitrate is a good candidate for sensible heat storage, due to its ability to increase the salt mixture's working temperature range. In the present research, thermophysical properties characterization of lithium nitrate containing salts, produced in Chile, have been carried out. Corrosion evaluations of carbon and low chromium steels were performed at 390 degrees C for 1000 hours. Thermophysical properties of the salt mixtures, such as thermal stability and heat capacity, were measured before and after corrosion tests. Chemical composition of the salts was also determined and an estimation of Chilean production costs is reported. Results showed that purity, thermal stability and heat capacity of the salts were reduced, caused by partial thermal decomposition and incorporation of corrosion products from the steel.

14 SOLAR ENERGY↗

Geochemical and Microbial Dynamics of Hydrogen in a Methane Storage Reservoir

Hydrogen has been identified as a flexible energy carrier with zero or negative emission across multiple energy systems, and existing natural gas infrastructure could be leveraged if hydrogen gas (H2) was blended with methane (CH4). For example, subsurface methane storage reservoirs could be slightly modified to also store hydrogen if a methane/hydrogen blend were injected. However, the compatibility of methane storage reservoirs to include H2 injection has not been fully demonstrated, and this could lead to geochemical and microbiological reactions that alter the reservoir and stored gas content. It is essential that we understand the impact of H2 gas on the biogeochemistry of subsurface storage reservoirs before deploying large-scale H2-CH4 storage, We collected produced fluid from two separate methane storage reservoirs in the Southwestern US. First, we completed a baseline analysis of the biogeochemistry through qPCR, 16S rRNA sequencing, metagenomic sequencing, and geochemical analysis. Each reservoir was found to have unique geochemical conditions and a unique microbial community structure, with Site 1 having a higher TDS and an abundance of Shewanella and Site 2 having a lower TDS and high abundance of Eubacterium and Acetobacterium. Next, we ran a series of high pressure, high temperature reactors under hydrogen storage conditions with the biological sample from one of the storage reservoirs and a 20% H2-80% CH4 gas blend for up to 7 days. Our results show a decrease of hydrogen by 5% in reactors as early as 1-3 days. Previous hydrogen storage work has linked subsurface microorganisms with methanogenesis hydrogen sulfide production, acid production, and microbial corrosion. Our results show minimal change in the fluid chemistry, with the exception of a decrease in dissolved sulfate concentrations. Taxonomic sequencing demonstrated the presence of microorganisms capable of iron redox, acid generation, and hydrogen sulfide production throughout the reactors, suggesting microbial hydrogen consumption may occur through various metabolic pathways. This work demonstrates that site-specific geochemistry and microbiology may impact the efficiency of hydrogen storage in methane storage reservoirs.

environmental microbiology↗

Analysis of the plugging of the systems autonomy demonstration project brassboard filters

A fine gray powder was clogging the brassboard filters. The powder appeared to be residue from a galvanic corrosive attack by ammonia of the aluminum and stainless steel components in the system. The corrosion was caused by water and chlorine that had entered into the system and combined with the ammonia. This combination made an electrolyte and a corrosive agent of the ammonia that attacked the metals in the system. The corroded material traveled through the system with the ammonia and clogged the filters. Key conclusions are: the debris collecting in the filters is a by-product of galvanic corrosion; the debris is principally corroded aluminum and stainless from the system; and galvanic corrosion occurred from water and chlorine that entered the system during normal and/or extreme operating and servicing conditions. Key recommendations are: use only one metal in the ammonia system-titanium, aluminum, or stainless steel; make the system as air-tight as possible (replace fittings with welded joints); and replace electron paramagnetic resonance (EPR) O-rings with neoprene O-rings, and do not use freon to clean system components.

Clay, John C.↗

Surface Studies of Ultra Strength Drilling Steel after Corrosion Fatigue in Simulated Sour Environment

The Unites States predicted 60% growth in energy demand by 2030 makes oil and natural gas primary target fuels for energy generation. The fact that the peak of oil production from shallow wells (< 5000 m) is about to be reached, thereby pushing the oil and natural gas industry into deeper wells. However, drilling to depths greater than 5000 m requires increasing the strength-to weight ratio of the drill pipe materials. Grade UD-165 is one of the ultra- high yield strength carbon steels developed for ultra deep drilling (UDD) activities. Drilling UDD wells exposes the drill pipes to Cl{sup -}, HCO{sub 3}{sup -}/CO{sub 3}{sup 2-}, and H{sub 2}S-containig corrosive environments (i.e., sour environments) at higher pressures and temperatures compared to those found in conventional wells. Because of the lack of synergism within the service environment, operational stresses can result in catastrophic brittle failures characteristic for environmentally assisted cracking (EAC). Approximately 75% of all drill string failures are caused by fatigue or corrosion fatigue. Since there is no literature data on the corrosion fatigue performance of UD-165 in sour environments, research was initiated to better clarify the fatigue crack growth (FCGR) behavior of this alloy in UDD environments. The FCGR behavior of ultra-strength carbon steel, grade UD-165, was investigated by monitoring crack growth rate in deaerated 5%NaCl solution buffered with NaHCO{sub 3}/Na{sub 2}CO{sub 3} and in contact with H{sub 2}S. The partial pressure of H{sub 2}S (p{sub H2S}) was 0.83 kPa and pH of the solution was adjusted by NaOH to 12. The fatigue experiments were performed at 20 and 85 C in an autoclave with surface investigations augmented by scanning electron microscopy (SEM) and energy dispersive x-ray (EDX) spectroscopy. In this study, research focused on surface analyses supported by the fatigue crack growth rate measurements. Fig. 1 shows an SEM micrograph of the crack that propagated from the notch in the solution at 20 C. Accumulation of the corrosion products is visible along the crack. The EDX chemical analysis near the crack tip found iron, sulfur and oxygen in the passive layer. The surface of the sample after the fatigue test in the sour environment at 85{sup o}, Fig. 2, C looks different from that fatigued surface at 20 C. The crack propagates across the passive film that covers the surface fairly uniformly. Some spallation of the passive film is observed near the notch. The EDX chemical analysis of the passive film near the crack tip identified mainly iron, carbon and oxygen. It appears that temperature plays a very important role in formation of the passive film. This may be associated with different solubility of H{sub 2}S in the solution, which will be further studied.

03 NATURAL GAS↗

Investigation of electrochemical migration on Sn-0.7Cu-0.3Ag-0.03P-0.005Ni solder alloy in HNO{sub 3} solution

Current issue in lead-free solder in term of its reliability is still under investigation. This high impact research attempts to investigate the electrochemical migration (ECM) on Sn-0.7Cu-0.3Ag-0.03P-0.005Ni solder alloy by Water Drop Test (WDT) in different concentration of HNO{sub 3} solution. The concentration of HNO{sub 3} solution used in this research was 0.05, 0.10, 0.50 and 1M. Optical Microscope (OM), Field Emission Scanning Electron Microscope (FESEM) and Energy Dispersive X-Ray Analysis (EDX) were carried out in order to analysis the ECM behavior based on the growth of dendrite formation after WDT. In general, the results demonstrated that dendrite growth is faster in higher concentration compared with low concentration of HNO{sub 3}. The concentration of HNO{sub 3} solution used has a strong correlation with Mean-Time-To-Failure (MTTF). As the concentration of HNO{sub 3} increases, the MTTF value decreases. Based on the MTTF results the solder alloy in 1M HNO{sub 3} solution is most susceptible to ECM. SnO{sub 2} forms as a corrosion by-product in the samples proved by EDX analysis. The solder alloy poses a high reliability risk in microelectronic devices during operation in 1M HNO{sub 3} solution.

36 MATERIALS SCIENCE↗

Underground Architecture and Layout for the Belgian High-Level and Long-Lived Intermediate-Level Radioactive Waste Disposal Facility- 12116

The underground architecture and layout of the proposed Belgian high-level (HLW) and long-lived, intermediate-level radioactive wastes (ILW-LL) disposal system (repository) is mainly based on lessons learned during the development and 30-year-long operation of an underground research laboratory (URL) ('HADES') located adjacent to the city of Mol at a depth of 225 m in a 100-m-thick, Tertiary clay formation; the Boom clay. The following main operational and safety challenges are addressed in the proposed architecture and layout: 1. Following excavation, the underground openings needed to be promptly supported to minimize the extent of the excavation damaged zone (EDZ). 2. The size and unsupported stand-up time at tunnel crossings/intersections also needed to be minimized to minimize the extent of the related EDZ. 3. Steel components had to be minimized to limit the related long-term (post-closure) corrosion and hydrogen production. 4. The shafts and all equipment had to go down through a 180-m-thick aquifer and handle up to 65-Ton payloads. 5. The shaft seals had to be placed in the underlying clay layer. The currently proposed layout minimizes the excavated volume based on strict long-term-safety criteria and optimizes operational safety. Operational safety is further enhanced by a remote-controlled waste-package-handling system transporting the waste packages from their respective surface location down to their respective disposal location with no intermediate operation. The related on-site preparation and thenceforth use of cement-based, waste package- transportation containers are integral operational-safety components. In addition to strengthening the waste packages and providing radiation protection, these containers also provide long-term corrosion protection of the internal 'primary' steel packages. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Fission Product and Actinide Distribution in the SiC Layer of Fissioned Triso Fuel Particles

Tri-structural Isotropic (TRISO) encapsulated fuel particles are used in next generation high-temperature gas-cooled nuclear reactors. The integrity of the fuel over a wide range of temperatures is integral to the safety of an operating nuclear reactor. It has been observed that fission products are released at high temperatures that simulate hypothesized accident scenarios. The particles under study were from the AGR-1 fuel development and qualification program. They consist of an enriched UCO fuel kernel surrounded by a dense carbon buffer layer (100 {mu}m), an inner pyrolytic carbon (IPyC) layer (40 {mu}m), a silicon carbide (SiC) layer (35 {mu}m), and an outer pyrolytic carbon (OPyC) layer (40 {mu}m). The SiC layer acts as the main diffusion barrier to fission products, but has been demonstrated to fail due to release of Ag through intact particles and local corrosion from metallic fission products such as Pd. In this work, we use transmission electron microscopy and diffraction techniques to study the structure and dispersion of release products within the SiC of TRISO particles as a function of annealing temperature used to simulate margin temperatures for in-reactor accident scenarios. In order to improve our understanding of fission product retention as a function of temperature, we have the unique opportunity to examine irradiated, fissioned TRISO particles to study post-irradiation effects on these materials. This data will contribute to current models used to predict the behavior of fission products in the SiC layer of TRISO fuels.

07 ISOTOPE AND RADIATION SOURCES↗

Elucidating the Transition of 3D Morphological Evolution of Binary Alloys in Molten Salts with Metal Ion Additives

Molten salts serve as effective high-temperature heat transfer fluids and thermal storage media used in a wide range of energy generation and storage facilities, including concentrated solar power plants, molten salt reactors and high-temperature batteries. However, at the salt–metal interfaces, a complex interplay of charge-transfer reactions involving various metal ions, generated either as fission products or through corrosion of structural materials, takes place. Simultaneously, there is a mass transport of ions or atoms within the molten salt and the parent alloys. The precise physical and chemical mechanisms leading to the diverse morphological changes in these materials remain unclear. Here, to address this knowledge gap, this work employed a combination of synchrotron X-ray nanotomography and electron microscopy to study the morphological and chemical evolution of Ni-20Cr in molten KCl-MgCl 2 , while considering the influence of metal ions (Ni 2+ , Ce 3+ , and Eu 3+ ) and variations in salt composition. Our research suggests that the interplay between interfacial diffusivity and reactivity determines the morphological evolution. The summary of the associated mass transport and reaction processes presented in this work is a step forward toward achieving a fundamental comprehension of the interactions between molten salts and alloys. Overall, the findings offer valuable insights for predicting the diverse chemical and structural alterations experienced by alloys in molten salt environments, thus aiding in the development of protective strategies for future applications involving molten salts.

36 - MATERIALS SCIENCE↗

Effects of Variations in Salt-Spray Conditions on the Corrosion Mechanisms of an AE44 Magnesium Alloy

The understanding of how corrosion affects magnesium alloys is of utmost importance as the automotive and aerospace industries have become interested in the use of these lightweight alloys. However, the standardized salt-spray test does not produce adequate corrosion results when compared with field data, due to the lack of multiple exposure environments. This research explored four test combinations through three sets of cycles to determine how the corrosion mechanisms of pitting, intergranular corrosion, and general corrosion were affected by the environment. Of the four test combinations, Humidity-Drying was the least corrosive, while the most corrosive test condition was Salt Spray-Humidity-Drying. The differences in corrosivity of the test conditions are due to the various reactions needed to cause corrosion, including the presence of chloride ions to cause pit nucleation, the presence of humidity to cause galvanic corrosion, and the drying phase which trapped chloride ions beneath the corrosion by-products.

Martin, Holly J.↗

Rethinking PCMI Failures Under Transient Conditions

Under PCMI conditions, the cladding strain is driven by either pellet swelling during normal operation or pellet thermal expansion in transients. The loading in PCMI is displacement controlled because friction between the pellet and the cladding results in a strain compatibility at the pellet/cladding interface. Failure is known to occur under PCMI loading conditions during operation when normal power changes result in release of iodine (and other fission products) causing stress corrosion cracking where the crack-propagation rate is dependent upon the cladding stress but slow relative to strictly mechanical failures. Failures after normal power changes are often referred to as failure by pellet-cladding interaction or PCI to distinguish it from PCMI. Such failures are considered displacement-controlled failures, as noted above, and occur with limited plastic strain. This is different to what is typically thought of as PCMI failure under transient conditions, either Anticipated Operational Occurrences (AOOs) or Reactivity Insertion Accidents (RIAs), which is generally assumed to occur once the cladding reaches a mechanical strain limit. But there are two features in the typical PCMI failure in an RIA that are not consistent with the PCMI assumptions. The first is the ductile shear failure feature in cross section and the second is a large crack opening post failure (e.g., see OI-11 failure in NSRR program). The ductile feature is indicative of a plastic instability that requires very large local strains, and the large crack opening must be the result of a release of energy, both of which are not expected if stress in the cladding was only driven by thermal expansion in the pellet. It is concluded that there must be a mechanism (likely related to rod internal pressure) that eliminates strain compatibility between the pellet and cladding – allowing strain localization to occur in what are known as PCMI transient failures. In some sense, these PCMI failures may actually be early burst failures that occur when thermal expansion causes uniform strains greater than a defined limit and fission gas pressure eliminate the strain compatibility

Cantonwine, Paul↗

Aluminum Clad Spent Nuclear Fuel Task 4: Performance of Aluminum SNF in Dry Storage Experiment Test Plan

This document presents the activities to be performed in support of understanding the performance of aluminum spent nuclear fuel (ASNF) in dry storage. These activities will visually examine and acquire baseline samples of as-irradiated ATR fuel assembly components to determine fuel condition and the morphology of the aluminum oxyhydroxides present on the fuel external surfaces. Because the boehmite phase of oxyhydroxide is projected to be a significant contributor to radiolytic hydrogen production and general corrosion, being able to quantify its presence is of major importance to long term storage of aluminum spent nuclear fuel. Baseline samples will be taken from irradiated end adapters, removed from ATR SNF elements, stored in the ATR Canal. These will be transferred to Idaho National Laboratory (INL) Materials and Fuels Complex (MFC) to perform non-destructive and destructive testing to determine the degree of hydration of the wet-stored aluminum components prior to drying and air storage. Examination of the dry stored SNF at Idaho Nuclear Technology and Engineering Center (INTEC) in CPP-603 Irradiated Fuel Storage Facility (IFSF) will allow the opportunity to identify gross degradation and as conditions permit, sample the surface oxide on fueled and un-fueled portions of the stored assemblies. The information resulting from analysis of the ATR Canal samples will be used to support validation of surrogate samples prepared under Task 6, sample surrogate preparation, and used in Task 1, oxyhydroxide layer behavior and chemistry, Task 2, oxide layer radiolytic gas generation, and Task 5, oxide layer response to drying. Surface oxide samples collected from SNF in IFSF dry storage will SNF dry storage prediction modeling from Task 3, sealed and vented system episodic breathing and gas generation prediction.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Composite structural armor for combat vehicle applications

Several projects that have demonstrated the advantages of using thick composite armor technology for structural applications in armored combat vehicles are discussed. The first involved composite cargo doors for the Marine Corps LVTP-7 amphibious landing vehicle. Another was a demonstration composite turret that offered a weight reduction of 15.5 percent. The advantages of this composite armor compared to metallic armors used for combat vehicle hull and turret applications are reduced weight at equal ballistic protection; reduced back armor spall; excellent corrosion resistance; reduced production costs by parts consolidation; and inherent thermal and acoustic insulative properties. Based on the encouraging results of these past programs, the Demonstration Composite Hull Program was started in September 1986. To demonstrate this composite armor technology, the Army's newest infantry fighting vehicle, the Bradley Fighting Vehicle (BFV), was selected as a model. A composite infantry fighting vehicle, designated the CIFV for this program, has been designed and fabricated and is currently undergoing a 6000 mile field endurance test. The CIFV demonstration vehicle uses the BFV engine, transmission, suspension, track and other equipment.

Haskell, William E., III↗