At least 379 records · Page 21

Use of aluminum as an oxidation barrier for titanium

A study is conducted of the use of aluminum coatings as oxidation retardants for Ti alloys, using room temperature normal emittance and spectral emittance as bases for the characterization of oxidation properties with and without the coatings. Thermal exposures were conducted in a thermogravimetric analysis apparatus in which specimen weight was continuously monitored. The results obtained indicate that the weight gains are proportional to the square root of the time for uncoated alloys and for 649 C-exposed aluminum-coated alloys. For the 704 C-exposed aluminum-coated alloys, weight gain exhibits a low rate for short and a high rate for long exposure times, implying that the 0.5-micron coating's protection decreases for long exposures at this temperature.

Unnam, J.↗

Correlations of norbornenyl crosslinked polyimide resin structures with resin thermo-oxidative stability, resin glass transition temperature and composite initial mechanical properties

PMR (polymerization of monomeric reactants) methodology was used to prepare 70 different polyimide oligomeric resins and 30 different unidirectional graphite fiber/polyimide composites. Monomeric composition as well as chain length between sites of crosslinks were varied to examine their effects on resin thermo-oxidative stability and glass transition temperature (Tg) of the cured/postcured resins. A linear correlation of decreasing 316 C resin weight loss/surface area versus (1) decreasing aliphatic content, or (2) increasing benzylic/aliphatic content stoichiometry ratio over a wide range of resin compositions was observed. An almost linear correlation of Tg versus molecular distance between the crosslinks was also observed. An attempt was made to correlate Tg with initial composite mechanical properties (flexural strength and interlaminar shear strength). However, the scatter in mechanical strength data prevented obtaining a clear correlation. Instead, only a range of composite mechanical properties was obtained at 25, 288, and 316 C. Perhaps more importantly, what did become apparent during the correlation study was (1) the PMR methodology could be used to prepare composites from resins containing a wide variety of monomer modifications, (2) that these composites almost invariably provided satisfactory initial mechanical properties as long as the resins formulated exhibited satisfactory processing flow, and (3) that PMR resins exhibited predictable rates of 316 C weight loss/surface area based on their benzylic/aliphatic stoichiometery ratio.

Alston, William B.↗

Theoretical performance of liquid ammonia, hydrazine and mixture of liquid ammonia and hydrazine as fuels with liquid oxygen biflouride as oxidant for rocket engines : I-mixture of liquid ammonia and hydrazine

Theoretical performance for mixture of 36.3 percent liquid ammonia and 63.7 percent hydrazine with liquid oxygen bifluoride as rocket propellant was calculated on assumption of equilibrium composition during expansion for a wide range of fuel-oxidant and expansios ratios. Parameters included were specific impulse, combustion-chamber temperature, nozzle exit temperature, composition mean molecular weight, characteristic velocity, coefficient of thrust and ratio of nozzle-exit area to throat area. For chamber pressure of 300 pounds per square inch absolute and expansion to 1 atmosphere, maximum specific impulse was 295.8 pound-seconds per pound. Five percent by weight of water in the hydrazine lowered specific impulse from about one to three units over a wide range of weight-percent fuel.

Huff, Vearl N↗

Effects of orbital exposure on RTV during the LDEF mission

Thermomechanical analysis (TMA), differential scanning calorimetry (DSC), and thermogravimetric analysis (TGA) were performed on samples of RTV 511 exposed on the Long Duration Exposure Facility (LDEF) mission for 6 years in orbit and unexposed RTV 511 control samples. Slices 20- to 400-microns thick were removed from the exposed surface down to a depth of 1,500 microns through the 3-mm thick samples. The TMA and DSC results, which arise from the entire slice and not just its surface, showed no significant differences between the LDEF exposed and the control samples. TMA scans were run from ambient to 500 C; results were compared by a tabulation of the onset temperatures for flow. DSC scans were run from ambient to 600 C; no endotherms or exotherms occurred over the range observed. What appear to be glass transition temperatures were compared for the samples as a function of section depth within the sample and between the exposed and control samples. The TGA scans from 25 to 900 C, which arise from the surface of the sample initially, showed a slight increase in the top most 105-micron slice (the exposed, discolored side) in the weight loss at 600 C in oxygen. This weight loss dropped to bulk values at the next slice below the top section, a mean depth of 258 microns. The control sample also showed an increase in weight loss as the top surface was approached, but the 600 C weight losses were very inconsistent. The LDEF RTV sample appears to be mechanically undamaged, with a surface layer which oxidizes slightly faster as a result of orbital exposure.

Brower, William E., Jr.↗

The effect of simulated low earth orbit radiation on polyimides (UV degradation study)

UV degradation of polyimide films in air and vacuum were studied using UV-visible, ESR, FTIR, and XPS spectroscopies. The UV-visible spectra of polyimide films showed a blue shift in the absorption compared to Kapton. This behavior was attributed to the presence of bulky groups and kinks along the polymer chains which disrupt the formation of a charge transfer complex. The UV-visible spectra showed also that UV irradiation of polyimides result extensively in surface degradation, leaving the bulk of the polymer intact. ESR spectra of polyimides irradiated in vacuum revealed the formation of stable carbon-centered radicals which give a singlet ESR spectrum, while polyimides irradiated in air produced an asymmetric signal shifted to a lower magnetic field, with a higher g value and line width. This signal was attributed to oxygen-cenetered radicals of peroxy and/or alkoxy type. The rate of radical formation in air was two fold higher than for vacuum irradiation, and reached a plateau after a short time. This suggests a continuous depletion of radicals on the surface via an ablative degradation process. FTIR, XPS, and weight loss studies supported this postulate. An XPS study of the surface indicated a substantial increase in the surface oxidation after irradiation in air. The sharp increase in the C-O binding energy peak relative to the C-C peak was believed to be associated with an aromatic ring opening reaction.

Forsythe, John S.↗

The Effects of Fiber Surface Modification and Thermal Aging on Composite Toughness and Its Measurement

A detailed experimental study was conducted to establish the structure-property relationships between elevated temperature aging and fiber-matrix bonding, Mode 2 interlaminar fracture toughness, and failure modes of carbon fiber/PMR-15 composites. The fiber-matrix adhesion was varied by using carbon fibers with different surface treatments. Short beam shear tests were used to quantify the interfacial shear strength afforded by the use of the different fiber surface treatments. The results of the short beam shear tests showed that, for times up to 1000 hr, the aging process caused no changes in the bulk of the three composite materials that would degrade the shear properties of the material. Comparisons between the interlaminar shear strengths (ILSS) measured by the short beam shear tests and the GIIC test results, as measured by the ENF test, indicated that the differences in the surface treatments significantly affected the fracture properties while the effect of the aging process was probably limited to changes at the starter crack tip. The fracture properties changed due to a shift in the fracture from an interfacial failure to a failure within the matrix when the fiber was changed from AU-4 to AS-4 or AS-4G. There appears to be an effect of the fiber/matrix bonding on the thermo-oxidative stability of the composites that were tested. The low bonding afforded by the AU 1 fiber resulted in weight losses about twice those experienced by the AS 1 reinforced composites, the ones with the best TOS.

Bowles, Kenneth J.↗

Continued Advancement of Supported Liquid Membranes for Carbon Dioxide Control in Extravehicular Activity Applications

The development of a new, robust, portable life support system (PLSS) is a high priority for NASA in order to support longer and safer extravehicular activity (EVA) missions. One of the critical PLSS functions is maintaining the carbon dioxide (CO2) concentration in the suit at acceptable levels. Although the Metal Oxide (MetOx) canister has historically performed very well, it has a finite CO2 adsorption capacity. Therefore, the size and weight of the unit would have to be increased to extend EVA times. Consequently, new CO2 control technologies must be developed in order to meet mission objectives without increasing the size of the PLSS. Recent work has centered on sorbents that can be regenerated during the EVA; however, this strategy increases the system complexity and power consumption. A much simpler approach is to employ a membrane that vents CO2 to space and retains oxygen (O2). A membrane has many advantages over current technology: it is a continuous system with no limit on capacity, it requires no consumables, and it does not need any hardware to switch beds between absorption and regeneration. Unfortunately, conventional gas separation membranes do not have the needed selectivity for use in the PLSS. However, the required performance could be obtained with a supported liquid membrane (SLM), which consists of a microporous material filled with a liquid that selectively reacts with CO2 over O2. In a recently completed Phase II SBIR project, Reaction Systems, Inc. achieved the required CO2 permeance and selectivity with an SLM in a flat sheet configuration. This paper describes work to convert the SLM into a more compact form and to scale it up to handle more representative process flow rates.

Wickham, David T.↗

The Effects of Fiber Surface Modification and Thermal Aging on Composite Toughness And its Measurement

A detailed experimental study was conducted to establish the structure-property relationships between elevated temperature aging and (I) fiber-matrix bonding, (2) Mode II interlaminar fracture toughness, and (3) failure modes of carbon fiber/PMR-15 composites. The fiber-matrix adhesion was varied by using carbon fibers with different surface treatments. Short beam shear tests were used to quantify the interfacial shear strength afforded by the use of the different fiber surface treatments. The results of the short beam shear tests definitely showed that, for aging times up to 1000 hr, the aging process caused no observable changes in the bulk of the three composite materials that---would degrade the shear properties of the material. Comparisons between the interlaminar shear strength (ILSS) measured by the short beam shear tests and the GII c test results, as measured by the ENF test, indicated that the differences in the surface treatments significantly affected the fracture properties while the effect of the aging process was probably limited to changes at the starter crack tip. The fracture properties changed due to a shift in the fracture from an interfacial failure to a failure within the matrix when the fiber was changed from AU-4 to AS-4 or AS-4G. There appears to be an effect of the fiber/matrix bonding on the thermo-oxidative stability of the composites that were tested. The low bonding afforded by the AU-4 fiber resulted in weight losses about twice those experienced by the AS-4 reinforced composites, the ones with the best TOS.

Bowles, Kenneth J.↗

Chemical, Structural, and Microstructural Changes in Metallic and Silicon-Based Coating Materials Exposed to Iodine Vapor

The chemical, structural and microstructural behavior of steels (304, 316 and A36), titanium-aluminum alloy (Ti-Al, (6Al-4V)), aluminum-magnesium alloy (Al-Mg, 6061), and coatings (Silcolloy and Dursan (SilcoTek Corporation)) were probed after exposure to iodine laminar flow. Exposures were carried out in a custom-built Iodine Vapor RIG (IVR) at 300 degrees C to an iodine laminar vapor flow of 1 mg min(exp. -1), carried by 145 mL-min(exp. -1) argon gas, for 5, 15 and 30 days. Samples were characterized before and after the experiment by gravimetric analysis, X-ray diffraction (XRD) and cross section electron microscopy analysis coupled with energy dispersive X-ray spectroscopy (EDS). All steels exposed for 30 days formed scales consisting mainly of metal (Cr, Fe, Ni) oxides showing different chemistry, microstructure and crystalline phases. Elemental iodine was only detected by EDS analysis in the scales of stainless steels 304 and 316. After 30 days, the Ti-Al exhibited no detectable scale, suggesting only a very thin film was formed. A scale consisting mainly of aluminum, iodine, and oxygen formed on the Al-Mg sample exposed to 30 days. Some pockets rich in magnesium, iodine and oxygen also formed in this Al-Mg alloy. Stainless steel 316, low carbon steel A36 and Ti-Al alloy coated with Silcolloy and stainless steel 304 coated with Dursan that were exposed for 30 days exhibited no oxidation. Stainless steel 304 coated with Silcolloy exposed for 30 days did not exhibit corrosion although the sample gained weight and the coating exhibited expansion. The weight gain per area performance of the materials exposed in iodine lamina flow containing oxygen at impurity level for 10, 15 and 30 days are reported from the lowest to the highest weight gain per area as follows: Steels: Less than 316 less than 304 less than A36; Ti-Al-Mg based alloys: Al-Mg less than Ti-Al: Considering the experimental uncertainties, no weight change was observed for Stainless steel 316, low carbon steel A36 and Ti-Al alloy coated with Silcolloy and stainless steel 304 coated with Dursan. The corrosion of the alloys is catalyzed by iodine in the presence of oxygen as impurity.

Costa, Gustavo C. C.↗

Miniature TOC Analyzer using Tunable Laser Spectroscopy and Combustion

Measurement of Total Organic Carbon (TOC) is an important tool on manned spaceflight missions for determining water quality. TOC quantification can be accomplished by oxidizing dissolved organic carbon to carbon dioxide (CO2) and analyzing the CO2 after volatilization. For human spaceflight applications, size, weight, and power need to be minimized while maintaining high sensitivity and accuracy. To this end, a tunable laser spectrometer tuned to measure CO2 was coupled to a miniature combustion reactor and the performance of the system for measuring the TOC was assessed. This combined system can be potentially reduced to around 1000 cm3 while offering the benefit afforded by combustion of converting all organics to CO2.

Winiberg, Frank↗

Comparison of Graphite Fabric Reinforced PMR-15 and Avimid N Composites After Long Term Isothermal Aging at Various Temperatures

Extensive effort is currently being expended to demonstrate the feasibility of using high-performance, polymer-matrix composites as engine structural materials over the expected operating lifetime of the aircraft, which can extend from 18,000 to 30,000 hr. The goal is to develop light-weight, high-strength, and high-modulus materials for use in higher temperature sections of advanced 21 st century aircraft propulsion systems. To accomplish this goal, it is necessary to pursue the development of thermal and mechanical durability models for graphite-fiber-reinforced, polymer-matrix composites. Numerous investigations have been reported regarding the thermo-oxidative stability (TOS) of the polyimide PMR-15 (1-5). A significant amount of this work has been directed at edge and geometry effects, reinforcement fiber influences, and empirical modeling of high-temperature weight loss behavior. It is yet to be determined if the information obtained from the PMR-15 composite tests is applicable to other polyimide-matrix composites. The condensation-curing polymer Avimid N is another advanced composite material often considered for structural applications at high temperatures. Avimid N has better thermo-oxidative stability than PMR-15 (6), but the latter is more easily processed. The most comprehensive study of the thermo-oxidative stability of Avimid N neat resin and composites at 371 (infinity)C is found in Salin and Seferis (7). The purposes of the work described herein were to compare the thermal aging behavior of these two matrix polymers and to determine the reasons for and the consequences of the difference in thermal durability. These results might be of some use in improving future polymer development through the incorporation of the desirable characteristics of both polyimides.

Bowles, Kenneth J.↗

Advances in direct oxidation methanol fuel cells

Fuel cells that can operate directly on fuels such as methanol are attractive for low to medium power applications in view of their low weight and volume relative to other power sources. A liquid feed direct methanol fuel cell has been developed based on a proton exchange membrane electrolyte and Pt/Ru and Pt catalyzed fuel and air/O2 electrodes, respectively. The cell has been shown to deliver significant power outputs at temperatures of 60 to 90 C. The cell voltage is near 0.5 V at 300 mA/cm(exp 2) current density and an operating temperature of 90 C. A deterrent to performance appears to be methanol crossover through the membrane to the oxygen electrode. Further improvements in performance appear possible by minimizing the methanol crossover rate.

Surampudi, S.↗

Monitoring Damage Accumulation in Ceramic Matrix Composites Using Electrical Resistivity

The electric resistance of woven SiC fiber reinforced SiC matrix composites were measured under tensile loading conditions. The results show that the electrical resistance is closely related to damage and that real-time information about the damage state can be obtained through monitoring of the resistance. Such self-sensing capability provides the possibility of on-board/in-situ damage detection and accurate life prediction for high-temperature ceramic matrix composites. Woven silicon carbide fiber-reinforced silicon carbide (SiC/SiC) ceramic matrix composites (CMC) possess unique properties such as high thermal conductivity, excellent creep resistance, improved toughness, and good environmental stability (oxidation resistance), making them particularly suitable for hot structure applications. In specific, CMCs could be applied to hot section components of gas turbines [1], aerojet engines [2], thermal protection systems [3], and hot control surfaces [4]. The benefits of implementing these materials include reduced cooling air requirements, lower weight, simpler component design, longer service life, and higher thrust [5]. It has been identified in NASA High Speed Research (HSR) program that the SiC/SiC CMC has the most promise for high temperature, high oxidation applications [6]. One of the critical issues in the successful application of CMCs is on-board or insitu assessment of the damage state and an accurate prediction of the remaining service life of a particular component. This is of great concern, since most CMC components envisioned for aerospace applications will be exposed to harsh environments and play a key role in the vehicle s safety. On-line health monitoring can enable prediction of remaining life; thus resulting in improved safety and reliability of structural components. Monitoring can also allow for appropriate corrections to be made in real time, therefore leading to the prevention of catastrophic failures. Most conventional nondestructive evaluation (NDE) techniques such as ultrasonic C-scan, x-ray, thermography, and eddy current are limited since they require structural components of complex geometry to be taken out of service for a substantial length of time for post-damage inspection and assessment. Furthermore, the typical NDE techniques are useful for identifying large interlaminar flaws, but insensitive to CMC materials flaws developed perpendicular to the surface under tensile creep conditions. There are techniques such as piezoelectric sensor [7,8], and optical fiber [9,10] that could be used for on-line health monitoring of CMC structures. However, these systems involve attaching an external sensor or putting special fibers in CMC composites, which would be problematic at high temperature applications.

Smith, Craig E.↗

X-ray photoelectron spectroscopy study of nickel and nickel-base alloy surface alterations in simulated hot corrosion conditions with emphasis on eventual application to turbine blade corrosion

Research on the high temperature oxidation and Na2SO4 induced hot corrosion of some nickel base superalloys was accomplished by using ESCA to determine the surface composition of the oxidized or corroded samples. Oxidation was carried out at 900 or 1000 C in slowly flowing O2 for samples of B-1900, NASA-TRW VIA, 713C, and IN-738. Oxidation times ranged from 0.5 to 100 hr. Hot corrosion of B-1900 was induced applying a coating of Na2SO4 to peroxidized samples, the heating to 900 C in slowly flowing O2. For oxidized samples, the predominant type of scale formed by each superalloy was determined, and a marked surface enrichment of Ti was found in each case. For corroded samples, the transfer of significant amounts of material from the oxide layer to the surface of the salt layer was observed to occur long before the onset of accelerating weight-gain. Changes in surface composition were observed to coincide with the beginning of accelerating corrosion, the most striking of which was a tenfold decrease in the sulfur to sodium ration and an increase in the Cr(VI) ratio.

Mateescu, G. D.↗

High modulus rare earth and beryllium containing silicate glass compositions

Glass compositions having a Young's modulus of at least 16 million psi and a specific modulus of at least 110 million inches consisting essentially of approximately, by weight, 20 to 43% SiO2, 8 to 21% Al2O3, 4 to 10% BeO, 27 to 58% of at least one oxide selected from a first group consisting of Y2O3, La2O3, Nd2O3, Ce2O3, Ce2O3, and the mixed rare earth oxides, and 3 to 12% of at least one oxide selected from a second group consisting of MgO, ZrO2, ZnO and CaO are described. The molar ratio of BeO to the total content of the first group oxides is from 1.0 to 3.0.

Bacon, J. F.↗

PMR Resin Compositions For High Temperatures

Report describes experiments to identify polymer matrix resins suitable for making graphite-fiber laminates used at 700 degree F (371 degree C) in such applications as aircraft engines to achieve higher thrust-to-weight ratios. Two particular high-molecular-weight formulations of PMR (polymerization of monomer reactants) resins most promising. PMR compositions of higher FMW exhibit enhanced thermo-oxidative stability. Formation of high-quality laminates with these compositions requires use of curing pressures higher than those suitable for compositions of lower FMW.

Vannucci, Raymond D.↗

Development of Protective Coatings for Chromium-Base Alloys

Chromium alloy sheet was clad with 5 to 10-mil-thick oxidation-resistant nickel-base alloy foils. Specimens also contained 1/2 to 1-mil-thick intermediate layers of platinum, tungsten, and/or W-25Re. Cladding was done by the isostatic hot gas-pressure bonding,.process. The clad chromium-alloy specimens were cyclic oxidation tested at 2100 F and 2300 F for up to 200 hours to determine the effectiveness of these metal claddings in protecting the chromium alloy Cr-5W from oxidation and contamination. Cladding systems consisting of 5-mil-thick Ni-20Cr-20W modified with 3 to 5 weight percent aluminum and containing a 1 /2-mil tungsten diffusion barrier demonstrated potential for long-time service at temperatures as high as 2300 F.

English, J. J.↗

Moisture-Induced Delamination Video of an Oxidized Thermal Barrier Coating

PVD TBC coatings were thermally cycled to near-failure at 1150 C. Normal failure occurred after 200-300 1-hr cycles with only moderate weight gains (0.5 mg/cm2). Delamination and buckling was often delayed until well after cooldown (desktop spallation), but could be instantly induced by the application of water drops, as shown in an accompanying video-recording. Moisture therefore plays a primary role in delayed desktop TBC failure. Hydrogen embrittlement is proposed as the underlying mechanism.

Smialek, James L.↗