Lithium battery cathode

A novel lithium battery cathode, a lithium ion battery using the same and processes and preparation thereof are disclosed. The battery cathode is formed by force spinning. Fiber spinning allows for the formation of core-shell materials using material chemistries that would be incompatible with prior spinning techniques. A fiber spinning apparatus for forming a coated fiber and a method of forming a coated fiber are also disclosed.

25 ENERGY STORAGE↗

Lithium battery cathode

A novel lithium battery cathode, a lithium ion battery using the same and processes and preparation thereof are disclosed. The battery cathode is formed by force spinning. Fiber spinning allows for the formation of core-shell materials using material chemistries that would be incompatible with prior spinning techniques. A fiber spinning apparatus for forming a coated fiber and a method of forming a coated fiber are also disclosed.

Bell, Nelson S.↗

Functionalized Embedded Monometallic Nickel Catalysts for Enhanced Hydrogen Evolution: Performance and Stability

Viable anionic exchange membrane (AEM) electrolysis for H 2 production requires highly active hydrogen evolution reaction (HER) catalysts that are also robust and cost-effective. Traditionally juxtaposition of two transition metals with one being more oxophilic is necessary for easier access to water in the inner Helmholtz plane as a source of protons in the crucial Volmer step for enhanced HER activity. However, they are prone to passivation at anodic potentials or deactivation via the formation of sub-surface metal hydrides at high cathodic overpotentials. Here we report a method of enabling close juxtaposition of Ni-Ni-oxide surfaces by functionalizing Ni-based catalysts via the careful thermal treatment of carbon-supported Ni nano-particles chelated with a select organic chelating compound referred to as cupferron. This functionalization results in an embedded Ni surface with a clear graphitic coating engendering long-term stability for passivation and subsurface hydride formation. The stability and activity of the functionalized Ni catalyst are demonstrated in half-cell RDE and full-cell AEM membrane-based hydrogen pump experiments. In the case of the latter, the functionalized Ni outperforms carbon-supported Pt.

25 ENERGY STORAGE↗

In-situ and in-operando analysis of voltage losses using sense wires for proton exchange membrane water electrolyzers

Proton exchange membrane water electrolyzer development requires understanding processes at the materials and interface levels to reach the required performance and lifetime targets for increasing market penetration. To achieve the required progress, it is critical to develop advanced in-situ diagnostics that allow observation of the changes that come with the reduction of catalyst loading combined with long-term intermittent operation. This work presents an internal voltage sensing method that enables observing internal voltage drops in an operating electrolyzer cell. It allows the total cell resistance to be separated into anode, CCM, and cathode resistance. The method is demonstrated by operating cells with different anode porous transport layers (PTLs). The changing properties of the PTLs result in significant variations of the resistances. Enhancing the PTL properties with a protective coating reduces the anode resistance significantly. In addition to these observations, the method enables a real-time monitoring of resistance related values that impact performance in water electrolyzers. Long-term experiments with the method allow us to gain insights into processes that occur during operation such as conditioning or degradation. The internal voltage sensing method presented in this study is a novel technique for diagnosing, analyzing, and optimizing water electrolyzers and other energy conversion devices.

42 ENGINEERING↗

Elucidating and Mitigating High-Voltage Degradation Cascades in Cobalt-Free LiNiO 2 Lithium-Ion Battery Cathodes

LiNiO 2 (LNO) is a promising cathode material for next-generation Li-ion batteries due to its exceptionally high capacity and cobalt-free composition that enables more sustainable and ethical large-scale manufacturing. However, its poor cycle life at high operating voltages over 4.1 V impedes its practical use, thus motivating efforts to elucidate and mitigate LiNiO 2 degradation mechanisms at high states of charge. Here, a multiscale exploration of high-voltage degradation cascades associated with oxygen stacking chemistry in cobalt-free LiNiO 2 , is presented. In this work, lattice oxygen loss is found to play a critical role in the local O3–O1 stacking transition at high states of charge, which subsequently leads to Ni-ion migration and irreversible stacking faults during cycling. This undesirable atomic-scale structural evolution accelerates microscale electrochemical creep, cracking, and even bending of layers, ultimately resulting in macroscopic mechanical degradation of LNO particles. By employing a graphene-based hermetic surface coating, oxygen loss is attenuated in LNO at high states of charge, which suppresses the initiation of the degradation cascade and thus substantially improves the high-voltage capacity retention of LNO. Overall, this study provides mechanistic insight into the high-voltage degradation of LNO, which will inform ongoing efforts to employ cobalt-free cathodes in Li-ion battery technology.

25 ENERGY STORAGE↗

Binder-Free Cnt Cathodes for Li-O 2 Batteries with More Than One Life

Li-O 2 batteries (LOB) performance degradation ultimately occurs through the accumulation of discharge products and irreversible clogging of the porous electrode during the cycling. Electrode binder degradation in the presence of reduced oxygen species can result in additional coating of the conductive surface, exacerbating capacity fading. Herein, a facile method to fabricate free-standing is established, binder-free electrodes for LOBs in which multi-wall carbon nanotubes form cross-linked networks exhibiting high porosity, conductivity, and flexibility. These electrodes demonstrate high reproducibility upon cycling in LOBs. After cell death, efficient and inexpensive methods to wash away the accumulated discharge products are demonstrated, as reconditioning method. The second life usage of these electrodes is validated, without noticeable loss of performance. These findings aim to assist in the development of greener high energy density batteries while reducing manufacturing and recycling costs.

25 ENERGY STORAGE↗

All Solid-State Li/LLZO/LCO Battery Enabled by Alumina Interfacial Coating

Li 7 La 3 Zr 2 O 12 (LLZO) garnet-type lithium-ion conductors are being investigated as a promising solid electrolyte for solid-state lithium batteries. To enable a functional all-solid-state configuration intensive investigations are needed to reduce the cathode/electrolyte interfacial resistance which contributes the most to cell performance loss. Among the commercial cathode materials investigated so far, LiCoO 2 (LCO) is one of the most stable with garnet electrolytes as only a superficial reaction has been detected between the two materials. However, even this minor reaction would block the Li-ion transport through the interface, resulting in deteriorated cell performance. In this work, we demonstrate that a thin aluminum oxide layer (5 nm) can be an effective interlayer to impede the formation of a harmful interphase and enable facile Li-ion transfer between LCO and the LLZO garnet. Room-temperature-sputtered LCO thin films were employed to form an interface with the garnet electrolyte and annealed at 800 °C to reveal the effect of the interfacial reaction on the Li-ion transfer across the interface. An aluminum oxide layer was then introduced between LCO and the garnet electrolyte by sputtering a metallic aluminum layer which is then annealed together with the upper LCO layer in oxygen, or by direct atomic layer deposition of the oxide. Compared to the LCO/LLZO/Li cells without an aluminum oxide interlayer, those with the interlayer exhibited improved performance, i.e., a stable discharge capacity of up to 90 mAh/(g LCO) at a C/10 rate, a rate capability up to 1.68C and a stable galvanostatic cycling at 0.1C for over 100 cycles with a discharge capacity fade rate of 0.15% per cycle. It was determined that aluminum diffused into the LCO layer after preventing the initial detrimental reaction between LCO and the LLZO garnet from happening during high temperature annealing, suggesting that the coating does not have to remain a physically blocking layer during cycling to function.

Electrochemistry↗

A novel polymeric lithicone coating for superior lithium metal anodes

Lithium metal (Li) is commonly regarded as the “holy grail” of rechargeable batteries and can serve as anodes for constituting various high-energy lithium metal batteries (LMBs). However, it suffers from two notorious issues: (1) continuous formation of inhomogeneous solid electrolyte interphase and (2) Li dendritic growth. Here, in this study, we developed a novel polymeric lithicone via a new molecular layer deposition (MLD) process, using lithium tert-butoxide (LTB) and hydroquinone (HQ) as precursors. We revealed that such an MLD process enabled the resultant LiHQ to grow linearly in a highly controllable and cyclic mode at a growth rate of 4 Å cycle −1 . Furthermore, its low process deposition temperature of 150 °C made it possible to practice high-quality coatings over Li anodes directly. We demonstrated that, very compellingly, this LiHQ coating could protect Li anodes from corrosion and dendritic growth. As a consequence, this LiHQ coating has enabled Li||Li symmetric cells an extremely long cyclability up to 8000 Li-plating/stripping cycles without failure. More excitingly, we demonstrated that, coupled with LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) cathodes, the LiHQ-modified Li anodes could help the resultant Li||NMC811 realize a much better capacity retention and much longer cyclability. Thus, this study represents a strategic route for developing commercializeable LMBs.

25 ENERGY STORAGE↗

Enigmatic Moisture Effects on Al2O3 Scale and TBC Adhesion

Alumina scale adhesion to high temperature alloys is known to be affected primarily by sulfur segregation and reactive element additions. However, adherent scales can become partially compromised by excessive strain energy and cyclic cracking. With time, exposure of such scales to moisture can lead to spontaneous interfacial decohesion, occurring while the samples are maintained at ambient conditions. Examples of this Moisture-Induced Delayed Spallation (MIDS) are presented for NiCrAl and single crystal superalloys, becoming more severe with sulfur level and cyclic exposure conditions. Similarly, delayed failure or Desk Top Spallation (DTS) results are reviewed for thermal barrier coatings (TBCs), culminating in the water drop failure test. Both phenomena are discussed in terms of moisture effects on bulk alumina and bulk aluminides. A mechanism is proposed based on hydrogen embrittlement and is supported by a cathodic hydrogen charging experiment. Hydroxylation of aluminum from the alloy interface appears to be the relevant basic reaction.

Smialek, James L.↗

Evaluation of thermal sprayed metallic coatings for use on the structures at Launch Complex 39

The current status of the evaluation program is presented. The objective was to evaluate the applicability of Thermal Sprayed Coatings (TSC) to protect the structures in the high temperature acid environment produced by exhaust of the Solid Rocket Boosters during the launches of the Shuttle Transportation System. Only the relatively low cost aluminum TSC which provides some cathodic protection for steel appears to be a practical candidate for further investigation.

Welch, Peter J.↗

Micro cavity fission chamber radiation detection system

A radiation detector to monitor the neutron flux of a nuclear reactor or other high-radiation environment, that can withstand the high temperatures and radiation fields of such environment, is provided. A small dielectric substrate with a low neutron-activation cross section is provided. The substrate is coated with a neutron conversion material, such as uranium oxide or thorium oxide. One or more substrates form a micro-sized detection cavity that is filled with a detection gas. A voltage is provided across anode and cathode wires in the detection cavity. A neutron absorbed in the conversion material may release reaction products into the gas, causing ionization of the gas which then produces a current or voltage signal. The small detector volume minimizes energy deposition into the detection gas by competing particles such as gamma rays, fast electrons, and beta particles, and therefore minimizes false counts while retaining large signals from neutron interactions.

McGregor, Douglas S.↗

Atomic- and Molecular-Scale Interphase Engineering for High-Performance Solid-State Batteries

Solid-state batteries (SSBs) promise a decisive advance beyond conventional Li-ion systems, yet their development remains constrained by persistent solid–solid interfacial instabilities that degrade performance and durability. Interfaces between solid electrolytes and both cathodes and Li metal often exhibit poor wettability, limited physical contact, and high charge–transfer resistance, leading to chemical decomposition, mechanical failure, and impedance growth. Overcoming these limitations requires interphase engineering with atomic-scale precision—capabilities that conventional coating methods cannot reliably deliver. Atomic layer deposition (ALD) and molecular layer deposition (MLD) uniquely meet this need by enabling ultrathin, conformal, and composition-tunable films that stabilize reactive surfaces, suppress parasitic reactions, and regulate Li-metal morphology. Importantly, this Perspective highlights ALD/MLD systems that have already demonstrated effectiveness in liquid-electrolyte cells and discusses how these validated strategies can be deliberately translated to solid-state architectures. By grounding future directions in experimentally proven concepts rather than speculative hypotheses, we outline how atomic- and molecular-scale design principles can accelerate the development of robust, high-performance SSB technologies.

atomic and molecular layer deposition↗

Electrodes and lithium ion cells with high capacity anode materials

High capacity silicon based anode active materials are described for lithium ion batteries. These materials are shown to be effective in combination with high capacity lithium rich cathode active materials. Supplemental lithium is shown to improve the cycling performance and reduce irreversible capacity loss for at least certain silicon based active materials. In particular silicon based active materials can be formed in composites with electrically conductive coatings, such as pyrolytic carbon coatings or metal coatings, and composites can also be formed with other electrically conductive carbon components, such as carbon nanofibers and carbon nanoparticles. Additional alloys with silicon are explored.

Lopez, Herman A.↗

Enhanced Light Outcoupling from OLEDs Fabricated on Novel Low-Cost Patterned Plastic Substrates of Varying Periodicity

OLEDs continue to make strides in display applications, but their commercial utilization in solid-state lighting (SSL) is lagging. An ongoing challenge, in particular for manufacturing, is the need for enhanced efficiency and hence the necessity to increase in an inexpensive approach the extraction of the light generated inside the OLED into the forward (viewing) hemisphere. In conventional OLEDs fabricated on a transparent flat anode coated on glass, the external quantum efficiency (EQE) is only ~20%. About 50% of the light is lost to internal waveguiding in the high refractive index (RI) organic + ITO anode layers and to surface plasmon polaritons (SPPs) at the organic/metal cathode interface. Another ~30% of the light is externally waveguided in the substrate to its edges. While extraction of the externally waveguided light is commonly addressed by adding a microlens array (MLA) or a scattering layer at the substrate’s air-side, light outcoupling increases by only ~1.6-1.7x (vs up to 2.5x in improving from ~20% to ~50%). The use of a hemispherical lens or an index matching fluid (IMF) at the substrate/photodetector (PD) interface increases the outcoupling by at least 2x; these approaches however, are not viable industrially, and even a MLA is sometimes undesirable due to its non-planar, scattering structure. In multi-stack tandem OLEDs, where the metal cathode is far from the emitting zone(s), the impact of photons loss to SPPs decreases. Our project addressed the ~50% loss to the internally waveguided light and SPPs. We evaluated OLEDs fabricated on patterned or planarized plastic substrates manufactured in a cost-effective approach compatible with a roll-to-roll (R2R) process. The OLEDs were either (i) patterned to various degrees depending on the pitch a and height or depth h of the pattern features or (ii) planar, with a pattern buried under a flat high RI planarization layer. We demonstrated that the outcoupling from green patterned OLEDs reaches ~50% by mitigating plasmon–related loss and internal waveguiding, even without the addition of a MLA, a hemispherical lens, or IMF. Simulations conducted in parallel with the experimental effort demonstrated how diffraction by conformally corrugated OLEDs increases the outcoupling to >60%. Structures with varying pitch values were also simulated indicating that combining domains of varying pitch could increase outcoupling to 55-60%. Experimentally, we additionally assessed the role a and h in determining not only the OLED efficiencies, but also their structural properties, i.e., the uniformity and conformality throughout the OLED stack. As planar OLEDs are preferred over corrugated devices, we studied different patterns in plastic substrates that were planarized by a high RI formulation. Planar green OLEDs on such structures showed enhanced efficiencies with EQEs larger than 60% with the addition of an IMF (to extract the substrate mode) at the substrate/Si PD interface. White OLEDs showed EQEs of 45.5%. Plastic substrates are currently less attractive than glass substrates due to drawbacks such as permeability to water vapor and oxygen, and in some cases thermal instability. Plastic substrates however, are flexible and easy to handle unlike thin flexible glass, and once transparent thin barrier films are available, they will become more attractive; they are already of interest in medical applications. Importantly, as it is easy to generate various patterns in different plastic materials, they provide excellent means for assessing and optimizing enhancing extracting structures. Such structures can also be transferred to glass substrates with some process modifications. The technical effectiveness and economic feasibility of the project lie in the patterning of the extracting plastic substrates in an approach that is scalable to R2R manufacturing. R2R processes are of drastically lower-cost than batch or single-unit fabrication. The patterned plastic can be a part of an integrated substrate either plastic or glass, which includes also a MLA or a planar layer with embedded scattering particles, as well as a conductive metal mesh/electrode design. SSL is environmentally-friendly and as OLED SSL becomes more efficient it will reduce electricity consumption, and hence lighting cost, as well as produce less expensive attractive lighting fixtures. Our university-industry collaboration is hence of major benefit to the public as it demonstrates the feasibility of manufacturing optimized extracting substrates for highly efficient OLEDs for SSL in a future R2R process, which would drastically reduce the manufacturing cost and increase production in the USA. Moreover, newly developed methods by our team allow low-cost roll manufactured substrates to be transferred to flexible or rigid glass substrates, which solves the plastic substrate barrier issues, and when combined with device encapsulation will increase the OLEDs’ environmental stability.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Constructing stable interface layer for boosting high-voltage cycling performance of single-crystal Ni-rich cathodes

Increasing demand for electric vehicles (EVs) worldwide and the requirements for environmental protection have greatly promoted the development of low-Co, Ni-rich layered cathodes due to their high energy density, reasonable cost, and less environmental pollution. Nevertheless, serious performance degradation and safety concerns resulting from structural/interfacial instability under high operating voltages (≥4.3 V) have greatly hindered its commercialization. Herein, we propose a feasible surface modification strategy by introducing a multifunctional Li 2 SiO 3 (LSO) coating layer onto the surface of Co less single-crystalline LiNi 0.63 Co 0.07 Mn 0.3 O 2 (NCM) to solve the above challenges. Additionally, the uniform Li 2 SiO 3 coating layer has a unique three-dimensional (3D) ion diffusion channel, which greatly promotes the transmission of Li + and alleviates interfacial stress accumulation. Equally important, the electrochemically inert Li 2 SiO 3 coating layer has a stable structure framework with strong Si-O bonds, which inhibit anisotropic particle volume expansion and the occurrence of side reactions during long-term cycling. As a consequence, LSO modified NCM exhibits greatly improved electrochemical properties even at harsh testing conditions and achieves capacity retention of 79.1% after 200 cycles at 25°C within 2.95-4.5 V in half cells. Furthermore, it provides an outstanding capacity retention of 94.7% after 300 cycles at 25°C within 2.95-4.4 V when tested in pouch full cells.

25 ENERGY STORAGE↗

Sulfur and Moisture Effects on Alumina Scale and TBC Spallation

It has been well established that a few ppmw sulfur impurity may segregate to the interface of thermally grown alumina scales and the underlying substrate, resulting in bond degradation and premature spallation. This has been shown for NiAl and NiCrAl-based alloys, bare single crystal superalloys, or coated superalloys. The role of reactive elements (especially Y) has been to getter the sulfur in the bulk and preclude interfacial segregation. Pt additions are also very beneficial, however a similar thermodynamic explanation does not apply. The purpose of the present discussion is to highlight some observations of these effects on Rene'142, Rene'N5, PWA1480, and PWA1484. For PWA1480, we have mapped cyclic oxidation and spallation in terms of potential sulfur interfacial layers and found that a cumulative amount of about one monolayer is sufficient to degrade long term adhesion. Depending on substrate thickness, optimum performance occurs if sulfur is reduced below about 0.2-0.5 ppmw. This is accomplished in the laboratory by hydrogen annealing or commercially by melt-fluxing. Excellent 1150 C cyclic oxidation is thus demonstrated for desulfurized Rene'142, Rene'N5, and PWA1484. Alternatively, a series of N5 alloys provided by GE-AE have shown that as little as 15 ppmw of Y dopant was effective in providing remarkable scale adhesion. In support of a Y-S gettering mechanism, hydrogen annealing was unable to desulfurize these alloys from their initial level of 5 ppmw S. This impurity and critical doping level corresponds closely to YS or Y2S3 stoichiometry. In many cases, Y-doped alloys or alloys with marginal sulfur levels exhibit an oxidative sensitivity to the ambient humidity called Moisture-Induced Delayed Spallation (MIDS). After substantial scale growth, coupled with damage from repeated cycling, cold samples may spall after a period of time, breathing on them, or immersing them in water. While stress corrosion arguments may apply, we propose that the underlying cause is related to a hydrogen embrittlement reaction: Al alloy + 3 H2O = Al(OH)3 + 3H(+) + 3e(-). This mechanism is derived from an analogous moisture-induced hydrogen embrittlement mechanism originally shown for Ni3Al and FeAl intermetallics. Consequently, a cathodic hydrogen charging technique was used to demonstrate that electrolytic de-scaling occurs for these otherwise adherent alumina scales formed on Y-doped Rene'N5, in support of hydrogen effects. Finally, some TBC observations are discussed in light of all of the above. Plasma sprayed 8YSZ coatings, produced on PWA1484 without a bond coat, were found to survive more than 1000 1-hr cycles at 1100 C when desulfurized to below 0.1 ppmw. At higher sulfur (1.2 ppmw) levels, moisture sensitivity and delayed TBC failure, referred to as Desk Top Spallation, occurred at just 200 hr. Despite a large degree of scatter, a factor of 5 in life improvement is indicated for desulfurized samples in cyclic furnace tests, confirming the beneficial effect of low sulfur alloys on model TBC systems. (DTS and moisture effects are also observed on commercially applied PVD 7YSZ coatings on Rene'N5+Y with Pt-aluminide bond coats). These types of catastrophic failure were subverted on the model system by segmenting the substrate into a network of 0.010 high ribs, spaced in. apart, prior to plasma spraying. No failures occurred after 1000 cycles at 1150 C or after 2000 cycles at 1100 C, even after water immersion. The benefit is described in terms of elasticity models and a critical buckling stress.

Smialek, James L.↗

Enabling fast-charging of lithium-ion batteries through printed electrodes

It has been well recognized that introducing secondary porous networks (SPNs) into the electrodes can effectively improve the electrochemical performance of lithium-ion batteries (LIBs), especially under fast-charging operations. However, the process complexity and high cost limit the commercial success of advanced electrodes with SPNs. To address this issue, we developed a facile screen-printing process to produce structured graphite electrodes with SPNs. The experimental results demonstrated that, by tuning the diameter and center-to-center (C2C) distance of emulsion dots on the stencil screen, the pore diameters and C2C pore distances of SPNs in screenprinted electrodes can be precisely controlled in the range of 100 mu m to 1 mm and 100 mu m to 3 mm respectively. In addition, the SPNs with hexagonal and square-shape pore alignments have also been imprinted onto the electrode coatings through adjusting the patterns of screen stencils. Used as anodes, the printed graphite electrodes demonstrated significantly reduced overpotential and voltage fluctuation under fast-charging operations from 2C to 6C. Coupled with LiNi 0.6 Mn 0.2 Co 0.2 O 2 (NMC622) cathodes, the full cells with printed graphite anodes exhibited an unprecedently stable performance with almost no capacity decay up to 170 cycles when charged to 80 % SOC at 2C. Observations from electron microscopy showed plated lithium undetectable at the surface of printed graphite electrodes after numerous cycles. The electrochemical analysis on the voltage evolution during the cell rest period indicated the significantly delayed onset of lithium plating in the presence of printed graphite electrodes. In conclusion, all these results suggest that the significantly improved cell performance is associated with the shortened Li-ion diffusion distance, reduced polarization and suppressed Li plating in the printed electrodes with patterned SPNs.

25 ENERGY STORAGE↗

Detection of a Cobalt-Containing Interphase at the Li 6 PS 5 Cl-NMC111 Interface by In Situ μ XANES and EIS

Sulfide electrolyte all-solid-state lithium batteries (ASLBs) with uncoated Li-Ni x Mn y Co 1–x–y O 2 (NMC) cathodes suffer from a large capacity loss during initial cycling and an increase in cell impedance. Decomposition reactions are known to occur at the Li 6 PS 5 Cl-NMC111 interface due to incompatibility between the two materials. If a stabilizing coating is applied to the NMC, it delivers full capacity during initial charge. However, the loss in capacity during discharge still occurs. The interface was studied by μ XANES and through EIS analysis. A chemically-formed interphase was detected by μ XANES, evident from reduction of Co at an uncoated NMC particle surface. This interphase was produced by decomposition at rest. To study the effect of the interphase on electrochemically active surface area, piecewise in situ EIS was performed and the data was modeled using a transmission line model (TLM). The charge transfer resistance R CT was used to estimate the volume specific active surface area (a act ). The median value for a act was 296 cm –1 , a factor of 7.5 lower than the theoretical value of 2216 cm –1 . This provided evidence of a lower electrochemically active surface area in the ASLB.

36 MATERIALS SCIENCE↗