Friction pull plug welding: top hat plug design

Friction Pull Plug Welding is a solid state repair process for defects up to one inch in length, only requiring single sided tooling, or outside skin line (OSL), for preferred usage on flight hardware. The most prevalent defect associated with Friction Pull Plug Welding (FPPW) was a top side or inside skin line (ISL) lack of bonding. Bonding was not achieved at this location due to the reduction in both frictional heat and welding pressure between the plug and plate at the end of the weld. Thus, in order to eliminate the weld defects and increase the plug strength at the plug `top` a small `hat` section is added to the pull plug for added frictional heating and pressure.

Coletta, Edmond R.↗

Welding Development: Marshall Space Flight Center

This paper presents the basic understanding of the friction stir welding process. It covers process description, pin tool operation and materials, metal flow theory, mechanical properties, and materials welded using the process. It also discusses the thermal stir welding process and the differences between thermal stir and friction stir welding. MSFC weld tools used for development are also presented.

Ding, Jeff↗

Elastic-Plastic Fracture Mechanics Analysis of Critical Flaw Size in ARES I-X Flange-to-Skin Welds

NASA's Ares 1 Upper Stage Simulator (USS) is being fabricated from welded A516 steel. In order to insure the structural integrity of these welds it is of interest to calculate the critical initial flaw size (CIFS) to establish rational inspection requirements. The CIFS is in turn dependent on the critical final flaw size (CFS), as well as fatigue flaw growth resulting from transportation, handling and service-induced loading. These calculations were made using linear elastic fracture mechanics (LEFM), which are thought to be conservative because they are based on a lower bound, so called elastic, fracture toughness determined from tests that displayed significant plasticity. Nevertheless, there was still concern that the yield magnitude stresses generated in the flange-to-skin weld by the combination of axial stresses due to axial forces, fit-up stresses, and weld residual stresses, could give rise to significant flaw-tip plasticity, which might render the LEFM results to be non-conservative. The objective of the present study was to employ Elastic Plastic Fracture Mechanics (EPFM) to determine CFS values, and then compare these values to CFS values evaluated using LEFM. CFS values were calculated for twelve cases involving surface and embedded flaws, EPFM analyses with and without plastic shakedown of the stresses, LEFM analyses, and various welding residual stress distributions. For the cases examined, the computed CFS values based on elastic analyses were the smallest in all instances where the failures were predicted to be controlled by the fracture toughness. However, in certain cases, the CFS values predicted by the elastic-plastic analyses were smaller than those predicted by the elastic analyses; in these cases the failure criteria were determined by a breakdown in stress intensity factor validity limits for deep flaws (a greater than 0.90t), rather than by the fracture toughness. Plastic relaxation of stresses accompanying shakedown always increases the calculated CFS values compared to the CFS values determined without shakedown. Thus, it is conservative to ignore shakedown effects.

Chell, G. Graham↗

Assessment of the LC-2 Prelaunch Fatigue Spectra of the CM-to-SM Flange Weld

The pad stay and rollout components of the Ares I-X life cycle can generate cyclic stress oscillations to the vehicle that could initiate and grow fatigue cracks from weld defects. The Ares I-X Project requested that a study be performed to determine if stabilization of the vehicle is required to reduce the stresses that could initiate and grow fatigue cracks at the flange-to-skin weld of the Command Module (CM) and Service Module (SM) interface. A fatigue crack growth analysis was conducted that used loads (LC-2) and stress analyses developed by the Ares I-X Project and utilized material data and analysis methods developed by a critical initial flaw size (CIFS) analysis conducted by NASA Engineering and Safety Center (NESC) for the Upper Stage Simulator (USS) of the Ares I-X vehicle. A full CIFS analysis for the CM-to-SM flange-to-skin weld was not performed because the full flight spectrum was not provided and was not necessary to answer the question posed by the Ares I-X Project. Instead, an approach was developed to determine if the crack growth due to the pad stay and rollout components of the flight spectrum would adversely influence the CIFS. The approach taken used a number of conservative assumptions that eliminated the need for high-fidelity analyses and additional material testing, but still provided a bounding solution for the uncertainties of the problem. The results from this analysis indicate that the LC-2 pad stay and rollout spectrum components would not produce significant fatigue crack growth on the CM-to-SM flange-to-skin weld. Thus, from a fatigue crack growth standpoint, no stabilization is required to reduce the LC-2 pad stay and rollout cyclic stresses on the CM-to-SM flange-to-skin weld.

Dawicke, David S.↗

Fatigue Crack Growth in Peened Friction Stir Welds

Friction stir welding induces residual stresses that accelerates fatigue crack growth in the weld nugget. Shot peening over the weld had little effect on growth rate. Laser peening over the weld retarded the growth rate: Final crack growth rate was comparable to the base, un-welded material. Crack tunneling evident from residual compressive stresses. 2195-T8 fracture surfaces were highly textured. Texturing makes comparisons difficult as the material system is affecting the data as much as the processing. Material usage becoming more common in space applications requiring additional work to develop useful datasets for damage tolerance analyses.

Forth, Scott C.↗

Pin Tool Geometry Effects in Friction Stir Welding

In friction stir welding (FSW) there is significant evidence that material can take one of two different flow paths when being displaced from its original position in front of the pin tool to its final position in the wake of the weld. The geometry of the pin tool, along with the process parameters, plays an important role in dictating the path that the material takes. Each flow path will impart a different thermomechanical history on the material, consequently altering the material microstructure and subsequent weld properties. The intention of this research is to isolate the effect that different pin tool attributes have on the flow paths imparted on the FSWed material. Based on published weld tool geometries, a variety of weld tools were fabricated and used to join AA2219. Results from the tensile properties and microstructural characterization will be presented.

Querin, J. A.↗

Advanced Welding Applications

Some of the applications of advanced welding techniques are shown in this poster presentation. Included are brief explanations of the use on the Ares I and Ares V launch vehicle and on the Space Shuttle Launch vehicle. Also included are microstructural views from four advanced welding techniques: Variable Polarity Plasma Arc (VPPA) weld (fusion), self-reacting friction stir welding (SR-FSW), conventional FSW, and Tube Socket Weld (TSW) on aluminum.

Ding, Robert J.↗

Large Spun Formed Friction-Stir Welded Tank Domes for Liquid Propellant Tanks Made from AA2195: A Technology Demonstration for the Next Generation of Heavy Lift Launchers

Improving structural efficiency while reducing manufacturing costs are key objectives when making future heavy-lift launchers more performing and cost efficient. The main enabling technologies are the application of advanced high performance materials as well as cost effective manufacture processes. This paper presents the status and main results of a joint industrial research & development effort to demonstrate TRL 6 of a novel manufacturing process for large liquid propellant tanks for launcher applications. Using high strength aluminium-lithium alloy combined with the spin forming manufacturing technique, this development aims at thinner wall thickness and weight savings up to 25% as well as a significant reduction in manufacturing effort. In this program, the concave spin forming process is used to manufacture tank domes from a single flat plate. Applied to aluminium alloy, this process allows reaching the highest possible material strength status T8, eliminating numerous welding steps which are typically necessary to assemble tank domes from 3D-curved panels. To minimize raw material costs for large diameter tank domes for launchers, the dome blank has been composed from standard plates welded together prior to spin forming by friction stir welding. After welding, the dome blank is contoured in order to meet the required wall thickness distribution. For achieving a material state of T8, also in the welding seams, the applied spin forming process allows the required cold stretching of the 3D-curved dome, with a subsequent ageing in a furnace. This combined manufacturing process has been demonstrated up to TRL 6 for tank domes with a 5.4 m diameter. In this paper, the manufacturing process as well as test results are presented. Plans are shown how this process could be applied to future heavy-lift launch vehicles developments, also for larger dome diameters.

Stachulla, M.↗

Laser Beam Welding Benchmark Experiments Performed in Reduced Gravity and Vacuum

Laser beam welding (LBW) is affected by the extreme temperatures, reduced pressure, and reduced gravity present in space environments. Gravity and pressure especially influence its melt pool and solidification dynamics. A compact, modular vacuum chamber adaptable to flight platforms from parabolic to orbital currently hosts an experiment to investigate the combined influence of reduced gravity and pressure on LBW. A swappable cartridge contains a rotating platen on which customizable workpieces can be welded under vacuum, greatly increasing experimental throughput. Instrumentation includes weld and thermal cameras observing the process, thermocouples placed on workpieces, accelerometers, and vacuum sensors. Experimental data gathered during the welding process will be combined with post-flight nondestructive evaluation, metallography, and mechanical testing to provide validation datasets for computational modeling. Phase I of this effort involves a parabolic flight campaign in low gravity while an anticipated Phase II would proceed to in-space demonstration to access extended duration microgravity.

in-space welding↗

Topical. Permanent Low-Earth Orbit Testbed for Welding and Joining: A Path Forward for the Commercialization of Space

NASA, defense, academia, and commercial space companies seek to develop orbital manufacturing to enhance mission capabilities. In-space welding and joining are needed for space-based manufacturing. We propose a permanent low-earth orbital welding and joining testbed for scientific study of relevant physical phenomena and development of welding and joining processes to technical maturity. Such data will enable integrated computational materials engineering(ICME)to elucidate the underlying physical and metallurgical processes needed to achieve critical space welding and joining operations.

In-space manufacturing↗

Automatic reel controls filler wire in welding machines

Automatic reel on automatic welding equipment takes up slack in the reel-fed filler wire when welding operation is terminated. The reel maintains constant, adjustable tension on the wire during the welding operation and rewinds the wire from the wire feed unit when the welding is completed.

Millett, A. V.↗

System maintains constant penetration during fusion welding

Servo system senses variations in fusion welding process, and adjusts the control parameters to compensate for them. The system assumes a correlation between uniform weld penetration and temperature gradients near the molten puddle. It senses weld properties and makes adjustments to travel speed and weld current.

Cook, G.↗

Gage monitors quality of cross-wire resistance welds

Gage nondestructively monitors the quality of cross-wire resistance welds during the welding operation. The gage gives a dial indication of the relative embedment of the cross wires during the actual welding operation. A direct relationship exists between the depth of embedment and both weld strength and consistency.

Etzel, J.↗

Nondestructive assessment of penetration of electron-beam welds

Empirical method correlates penetration of an electron-beam weld with external measurements of the weld. Empirical polygon accurately confirms full-penetration welds while a second, larger polygon provides for penetration of welds near the tip.

Harmon, T. J.↗

Behavior of Ti-5Al-2.5Sn ELI titanium alloy sheet parent and weld metal in the presence of cracks at 20 K

Through- and surface-cracked specimens of two thicknesses were tested in uniaxial tension. Surface-cracked specimens were generally found to be stronger than through-cracked specimens with the same crack length. Apparent surface-crack fracture toughness calculated using the Anderson modified Irwin equation remained relatively constant for cracks as deep as 90 percent of the sheet thickness. Subcritical growth of surface cracks was investigated. Comparison of chamber and open air welds showed chamber welds to be slightly tougher. Both methods produced welds with toughness that compared favorably with that of the parent metal. Weld efficiencies were above 94 percent.

Sullivan, T. L.↗

Influence of restraint and thermal exposure on welds in T-111 and ASTAR-811C

The notched-tensile, tensile, and bend properties of GTA welds in T-111 and ASTAR-811C sheet were determined following a wide range of thermal exposures in order to define changes in ductility and mechanical property behavior due to weld aging response. No notch sensitivity or unusual tensile response was noted for any of the conditions evaluated. An aging response was noted for the bend ductile-brittle transition temperature determinations on both T-111 and ASTAR-811C welds. A tentative explanation for the observed response of each alloy is presented. In addition, the interrelationship of mechanical and chemical factors leading to underbead cracking in T-111 was investigated. The problem was shown to be amenable primarily to chemical solutions, such as alloy compositional changes. This was demonstrated by the improved performance of ASTAR-811C over T-111 in plate weld studies. Only modest success was achieved using procedural techniques as a means of eliminating underbead cracking.

Gold, R. E.↗

Improved TIG weld joint strength in aluminum alloy 2219-T87 by filler metal substitution

The results of an investigation on weld joint characteristics of aluminum alloy 2219-T87 are given. Five different alloys were utilized as filler material. The mechanical properties of the joints were determined at ambient and cryogenic temperatures for weldments in the as-welded condition and also, for weldments after elevated temperature exposures. Other evaluations included hardness surveys, stress corrosion susceptibility, and to a limited extent, the internal metallurgical weld structures. The overall results indicate that M-943 filler weldments are superior in strength to weldments containing either the standard 2319 filler or fillers 2014, 2020, and a dual wire feed consisting of three parts 2319 and one part 5652. In addition, no deficiencies were evident in M-934 filler weldments with regard to ductility, joint strength after elevated temperature exposure, weld hardness, metallographic structures, or stress corrosion susceptibility.

Poorman, R. M.↗