Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Solid dissolution”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 379 records · Page 21

Li Morphology Evolution during Initial Cycles in a Gel Composite Polymer Electrolyte

Understanding and controlling lithium morphology evolution and lithium dendrite formation and growth during cycling is one of the key challenges for high-energy lithium metal batteries. This challenge applies to liquid electrolyte batteries as well as solid-state and semi-solid-state batteries. Our current knowledge about the evolution of the Li morphology is mostly obtained from liquid electrolyte-based studies in a Li–Li symmetrical cell configuration. The knowledge obtained in such conditions may not readily transfer into solid-state or semi-solid-state batteries. In this work, Li morphology evolution during initial cycling in a full cell configuration with the LiNi 0.6 Co 0.2 Mn 0.2 O 2 (NMC 622) cathode and a semi-solid-state gel composite electrolyte is monitored via post-mortem photographs and scanning electron microscopy at multiple length scales. The gel composite electrolyte contains a cross-linked poly(ethylene oxide)-based polymer electrolyte, ceramic fillers, and a liquid plasticizer. The results show that severe surface pitting occurs as early as the second stripping cycle. Pit formation and continuous dissolution during the stripping process are the main cause of the Li surface roughening and dendrite growth mechanism in the model gel composite electrolyte. Comparing Li dendrite growth mechanisms in liquid, polymer, and ceramic solid electrolytes, the dendrite growth mechanism observed in this model electrolyte resembles that of the liquid electrolyte the most. This study suggests that strategies to control Li morphology and prevent dendrite growth in a gel composite electrolyte should be similar to strategies applicable to liquid electrolytes.

25 ENERGY STORAGE↗

Cold sintering process of Li 1.5 Al 0.5 Ge 1.5 (PO 4 ) 3 solid electrolyte

Abstract The recently developed technique of cold sintering process (CSP) enables densification of ceramics at low temperatures, i.e., <300°C. CSP employs a transient aqueous solvent to enable liquid phase‐assisted densification through mediating the dissolution‐precipitation process under a uniaxial applied pressure. Using CSP in this study, 80% dense Li 1.5 Al 0.5 Ge 1.5 (PO 4 ) 3 (LAGP) electrolytes were obtained at 120°C in 20 minutes. After a 5 minute belt furnace treatment at 650°C, 50°C above the crystallization onset, Li‐ion conductivity was 5.4 × 10 −5 S/cm at 25°C. Another route to high ionic conductivities ~10 −4 S/cm at 25°C is through a composite LAGP ‐ (PVDF‐HFP) co‐sintered system that was soaked in a liquid electrolyte. After soaking 95, 90, 80, 70, and 60 vol% LAGP in 1 M LiPF 6 EC‐DMC (50:50 vol%) at 25°C, Li‐ion conductivities were 1.0 × 10 −4 S/cm at 25°C with 5 to 10 wt% liquid electrolyte. This paper focuses on the microstructural development and impedance contributions within solid electrolytes processed by (i) Crystallization of bulk glasses, (ii) CSP of ceramics, and (iii) CSP of ceramic‐polymer composites. CSP may offer a new route to enable multilayer battery technology by avoiding the detrimental effects of high temperature heat treatments.

Berbano, Seth S.↗

Generating porosity during olivine carbonation via dissolution channels and expansion cracks

Abstract. The olivine carbonation reaction, in which carbon dioxide is chemically incorporated to form carbonate, is central to the emerging carbon sequestration method using ultramafic rocks. The rate of this retrograde metamorphic reaction is controlled, in part, by the available reactive surface area: as the solid volume increases during carbonation, the feasibility of this method ultimately depends on the maintenance of porosity and the creation of new reactive surfaces. We conducted in situ dynamic X-ray microtomography and nanotomography experiments to image and quantify the porosity generation during olivine carbonation. We designed a sample setup that included a thick-walled cup (made of porous olivine aggregates with a mean grain size of either ∼ 5 or ∼ 80 µm) filled with loose olivine sands with grain sizes of 100–500 µm. The whole sample assembly was reacted with a NaHCO 3 aqueous solution at 200 °C, under a constant confining pressure of 13 MPa and a pore pressure of 10 MPa. Using synchrotron-based X-ray microtomography, the three-dimensional (3-D) pore structure evolution of the carbonating olivine cup was documented until the olivine aggregates became disintegrated. The dynamic microtomography data show a volume reduction in olivine at the beginning of the reaction, indicating a vigorous dissolution process consistent with the disequilibrium reaction kinetics. In the olivine cup with a grain size of ∼ 80 µm (coarse-grained cup), dissolution planes developed within 30 h, before any precipitation was observed. In the experiment with the olivine cup of ∼ 5 µm mean grain size (fine-grained cup), idiomorphic magnesite crystals were observed on the surface of the olivine sands. The magnesite shows a near-constant growth throughout the experiment, suggesting that the reaction is self-sustained. Large fractures were generated as the reaction proceeded and eventually disintegrated the aggregate after 140 h. Detailed analysis show that these are expansion cracks caused by the volume mismatch in the cup walls, between the expanding interior and the near-surface which keeps a nearly constant volume. Nanotomography images of the reacted olivine cup reveal pervasive etch pits and wormholes in the olivine grains. We interpret this perforation of the solids to provide continuous fluid access, which is likely key to the complete carbonation observed in nature. Reactions proceeding through the formation of nano- to micron-scale dissolution channels provide a viable microscale mechanism in carbon sequestration practices. For the natural peridotite carbonation, a coupled mechanism of dissolution and reaction-induced fracturing should account for the observed self-sustainability of the reaction.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Resupply Mechanism to a Contaminated Aquifer: A Laboratory Study of U(VI) Desorption from Capillary Fringe Sediments

Contaminated capillary fringe sediments are believed to function as long term source of U(VI) to Hanford’s 300 Area groundwater uranium plume that discharges to the Columbia River. The deep vadose zone at this site experiences seasonal water table elevation and water compositional changes in response to Columbia River stage. Batch and column desorption experiments of U(VI) were performed on two mildly contaminated sediments from this system that vary in hydrologic position to ascertain their U(VI) release behavior and factors controlling it. Solid phase characterization of the sediments was performed to identify mineralogic and chemical factors controlling U(VI) desorption. The desorption behavior of U(VI) was different from the two sediments in spite of similar chemical and textural characteristics, and non-carbonate mineralogy. Adsorption strength and sorbed U(VI) lability was higher in the near-river sediment 11D. Inland sediment 39B displayed low sorbed U(VI) lability (~ 10%) and measurable solid-phase carbonate content. Kinetic desorption was observed that was attributed to regeneration of labile U(VI) in 11D, and carbonate mineral dissolution in 39B. The desorption reaction was best described as an equilibrium surface complexation reaction. The noted differences in desorption behavior appear to result from U(VI) contamination and hydrologic history, as well as sediment carbonate content. Insights are provided on the dynamic adsorption/desorption behavior of contaminants in linked groundwater-river systems.

58 GEOSCIENCES↗

Sodium trithiocarbonate cathode for high-performance sodium–sulfur batteries

The high abundance and low cost of sodium and sulfur make room-temperature sodium-sulfur (RT Na-S) batteries an attractive technology compared to the current lithium-ion batteries for large-scale grid-storage applications. However, the commercialization of RT Na-S batteries is impeded by the slow kinetics of Na-S chemistry, severe sodium polysulfide shuttling, and uncontrollable growth of dendritic Na. Herein, sodium trithiocarbonate (Na 2 CS 3 ) is applied as a cathode material to facilitate concurrent improvement in both electrodes, leading to a high-rate performance with extended cycle life. The conductive characteristic of the carbon-sulfur resonance bond provides fast ion and electron transfer throughout the cathode, resulting in superior electrochemical reactivity. At the cathode, the presence of Na2CS3 forms an oligomer-structured layer to suppress the dissolution and shuttling of active materials. Meanwhile, when small portions of Na 2 CS 3 intermediates migrate to the anode, a stable solid electrolyte interphase (SEI) layer with uniform Na-ion flux is formed, enabling improved Na stripping and plating performance. A series of electrochemical and materials characterization, accompanied by density functional theory calculations demonstrate that Na 2 CS 3 is a promising candidate to realize high-rate performance long cycle life RT Na-S batteries.

25 ENERGY STORAGE↗

Leveraging Framework Instability: A Journey from Energy Storage to Drug Delivery

Amorphous pharmaceuticals often suffer from poor physical stability, which can negate their high solubility, fast dissolution rate, and better oral bioavailability vs. crystalline forms. This represents a major hurdle to processing, storage, and delivery of amorphous pharmaceuticals. Several approaches to addressing these problems have been pursued, but there is still a need for a general method for stabilizing the amorphous form. We describe a novel approach using a water-unstable metal-organic framework as a drug delivery vehicle that demonstrates improved amorphous form stability accompanied by remarkably enhanced solubility and a fast dissolution rate. This research project spanned eleven years from conception to realization and dissemination. With origins in understanding the stability or porous solids for energy storage materials, the work also highlights potential of basic science understanding to illuminate new areas of application.

Chemistry↗

Management of HL deposits for the D and D of UP1 reprocessing plant - retrieval and treatment scenarios - 15295

Built in 1958 on the Marcoule CEA site, the UP1 facility, was the 1. French industrial (500 t U / year) reprocessing plant based on the PUREX process. The plant, which has stopped operation in 1997, constitutes with its auxiliary workshop (vitrification workshop, glass canister storage), one of the largest and most challenging decommissioning project in France. In about 40 years of operation, various type of fuels elements such as metallic uranium, U-Al fuel rods, Phenix breeder elements or PWR fuel have been reprocessed, thereby requiring several plant and process adaptations. Resulting from these complex process chemistry and operation history, significant fouling of the chemical plant circuits and components has occurred. The fission product (FP) concentration process is particularly concerned. Preliminary investigation performed in 2010 in the evaporator's feeding tanks revealed the presence of significant amounts of sludge and dose rates as high as 250 Gy/h. Therefore a thorough investigation campaign, including visual inspection, volume quantification, deposits sampling, and radiological characterization of the components of this workshop has been initiated in 2013. Chemical analysis performed so far show that the solids are mainly composed of zirconium phosphates, 'MoZr' compounds and nitrate salt precipitates. But the presence of insoluble fines arising from the dissolution workshop and organic residues resulting from the TBP decomposition has also been evidenced in some of the tanks. The numerous constraints associated with the management of such highly active sludge, with Cs-137 specific activity ranging from 1 to 10 GBq/g, and a complex physico-chemical composition, lead CEA to investigate the implementation of an in situ conditioning treatment able to produce a waste package complying with existing evacuation routes and/or on-site storage facilities. The full paper presents an overview of the UP1 D and D project and then focuses on the possible dismantling scenarios for the FP concentration workshop, including the evaluation of different strategies for the highly active deposits management. The investigations and deposits characterization program will be developed so as the sampling methodologies that has been specifically tuned. In the light of the best actual knowledge of the deposits properties, the recovery and conditioning treatment scenarios will be exposed, considering, as a case study, the development of a specific vitrification tool to be implemented In Situ and specifically designed to match the requirements and constraints of the D and D project: adequately dimensioned, compact, flexible with respect to the feed composition, for a limited duration of use and designed to be dismantled. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Characterization of Tank 16H Annulus Samples Part II: Leaching Results

The closure of Tank 16H will require removal of material from the annulus of the tank. Samples from Tank 16H annulus were characterized and tested to provide information to evaluate various alternatives for removing the annulus waste. The analysis found all four annulus samples to be composed mainly of Si, Na, and Al and lesser amounts of other elements. The XRD data indicate quartz (SiO 2 ) and sodium aluminum nitrate silicate hydrate (Na 8 (Al 6 Si 6 O 24 )(NO 3 ) 2 .4H 2 O) as the predominant crystalline mineral phases in the samples. The XRD data also indicate the presence of crystalline sodium nitrate (NaNO 3 ), sodium nitrite (NaNO 2 ), gibbsite (Al(OH) 3 ), hydrated sodium bicarbonate (Na 3 H(CO 3 ) 2 .2H 2 O), and muscovite (KAl 2 (AlSi 3 O 10 )(OH) 2 ). Based on the weight of solids remaining at the end of the test, the water leaching test results indicate 20-35% of the solids dissolved after three contacts with an approximately 3:1 volume of water at 45°C. The chemical analysis of the leachates and the XRD results of the remaining solids indicate sodium salts of nitrate, nitrite, sulfate, and possibly carbonate/bicarbonate make up the majority of the dissolved material. The majority of these salts were dissolved in the first water contact and simply diluted with each subsequent water contact. The water leaching removed large amounts of the uranium in two of the samples and approximately 1/3 of the 99 Tc from all four samples. Most of the other radionuclides analyzed showed low solubility in the water leaching test. The oxalic acid leaching test result indicate approximately 34-47% of the solids in the four annulus samples will dissolve after three contacts with an approximately 3:1 volume of acid to solids at 45°C. The same sodium salts found in the water leaching test comprise the majority of dissolved material in the oxalic acid leaching test. However, the oxalic acid was somewhat more effective in dissolving radionuclides than the water leach. In contrast to the water leaching results, most constituents continued to dissolve during subsequent cycles of oxalic acid leaching. The somewhat higher dissolution found in the oxalic acid leaching test versus the water leaching test might be offset by the tendency of the oxalic acid solutions to take on a gel-like consistency. The filtered solids left behind after three oxalic acid contacts were sticky and formed large clumps after drying. These two observations could indicate potential processing difficulties with solutions and solids from oxalic acid leaching. The gel formation might be avoided by using larger volumes of the acid. Further testing would be recommended before using oxalic acid to dissolve the Tank 16H annulus waste to ensure no processing difficulties are encountered in the full scale process.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Beneficial effect of copper on pitting resistance of Ni-Cr-Fe alloys

This study examines the effect of copper alloying on pitting resistance in a model solid solution FCC Ni-13%Cr-10%Fe alloy through potentiodynamic and potentiostatic polarization in 0.1 M NaCl in conjunction with an analysis using first-principles competitive electro-chemisorption modeling. The pitting potential increased with increasing Cu content in the alloy. Furthermore, the extent of metastable pit growth was suppressed and the incubation time for metastable to stable pit transition increased with Cu content. The first-principles competitive adsorption calculations suggested that Cu alloying suppresses chloride ion adsorption on the alloy surface in a simulated pit environment, which inhibits active dissolution at the pit bottom, enhances proton adsorption, and thereby increases the local pH at the pit bottom. In conclusion, we propose that these two effects of Cu in solid solution combine to reduce pit stability and may act in addition to the enrichment of Cu on the corroding pit surface.

36 MATERIALS SCIENCE↗

Atomic-level studies of the depletion in reactive sites during clay mineral dissolution

Environmental weathering is typically viewed as a macroscopic phenomenon that is based on a number of competing atomic- or molecular-level processes. One important process is the release of metal or metalloid elements into solution at the water-rock interface. To both explain and predict environmental weathering, the atomic-level “reactive sites” on the surfaces of minerals must be characterized and quantified. Whether these sites are atomic in nature, represented by a chemical bond, or comprise a more complex assemblage of covalently or ionically linked atoms or molecules, the kinetic rate of atomic release (dissolution) depends on the available reactive surface. For one important class of materials, clay minerals, their reactive surface areas are a challenge to quantify as it is well recognized that there are two distinct types of surfaces: edge sites and basal planes1-3. Clay dissolution rates continuously decrease over time as reactive edge sites are preferentially depleted4. Changes in reactive surface area and the difficulties in quantifying this elusive variable have often been cited as one key reason for the complexity in developing accurate rate equations3,5,6. In this work, we demonstrate a solid-state nuclear magnetic resonance (SSNMR) method for counting the number of reactive surface sites on a defined quantity of a clay mineral. Using this SSNMR proxy7-9, changes in reactive surface area were monitored for a series of batch dissolution experiments of low-defect kaolinite KGa-1b at 21 ºC and pH 3 over the course of 80 days. While no changes (within error) were observed for specific surface area (as determined from BET gas isotherm data), the SSNMR proxy revealed decreases in the number of reactive surface sites per gram of kaolinite as a function of dissolution time. This observation can be tied to a concomitant decrease in the rates of release of Si and Al into solution. These results further highlight the need to account for changes in reactive surface area when developing and using dissolution rate models for clay minerals and other heterogeneous materials in the environment.

58 GEOSCIENCES↗

Yttria-Stabilized Zirconia Aided Electrochemical Investigation on Ferric Ions in Mixed Molten Calcium and Sodium Chlorides

Electrolytic reduction of dissolved iron oxide to metal iron in molten salts with an inert anode is an alternative short route for steelmaking without CO{sub 2} emissions. A novel and simple integrated yttria-stabilized zirconia (YSZ) cell was constructed from a YSZ tube with a closed end. The YSZ tube played multiple functions, including the container for the molten salts, the solid electrolyte membrane in the O{sup 2−}|YSZ|Pt|O{sub 2} (air) reference electrode (RE), and the solid electrolyte membrane between the working and counter electrodes (WE and CE). Electrochemical behavior of ferric ions (Fe{sup 3+}) that were formed by dissolution of 0.5 wt pct Fe{sub 2}O{sub 3} in the molten CaCl{sub 2}-NaCl eutectic mixture was investigated on a Pt WE at 1273 K by various electrochemical techniques including cyclic voltammetry, linear scan voltammetry, square wave voltammetry, chronopotentiometry, chronoamperometry, and potentiostatic electrolysis. Analysis of the mechanism of electrode reactions was further assisted by scanning electron microscopy, energy dispersive X-ray spectroscopy, and X-ray diffraction. Some electrochemical parameters were obtained, including the number of exchanged electrons and the diffusion coefficient of ferric ions in the mixed molten salts. The results from various electrochemical techniques are in good agreement with each other, and show that the electrochemical reduction of Fe{sup 3+} to Fe in the molten salt mixture could be a single three-electron transfer step and diffusion-controlled reaction that was also possibly reversible. This work may form the foundation for extraction of iron and alloys from molten salts and also provide a stable O{sup 2−}|YSZ|Pt|O{sub 2} (air) RE with wide applicability for investigation on electrochemical properties of other electroactive metal oxides in molten salts.

36 MATERIALS SCIENCE↗

Enabling Solar Water Oxidation by BiVO 4 in Strongly Acidic Solutions

The oxygen evolution reaction (OER) is paired with various electrochemical and photoelectrochemical reduction reactions used for fuel and chemical production. As there is a strong interest in performing many of these reduction reactions in strongly acidic solutions to increase the reaction rate, efficiency, or selectivity, there is also a great interest in enabling efficient and stable OER in strongly acidic solutions. In this study, we report stable photoelectrochemical OER (POER) of a BiVO 4 photoanode in 0.1 M HNO 3 (pH 1). This was achieved by using Nb 2 O 5 as a protection layer. While Nb 2 O 5 was rarely used as a protection layer for photoelectrodes in the past, we show its excellent capability to suppress both the chemical and photoelectrochemical dissolution of BiVO 4 at pH 1. After stabilizing BiVO 4 with a Nb 2 O 5 protection layer, we added Co 2+ ions to the electrolyte as an OER catalyst to enhance the POER. We found that Co (aq) 2+ can serve as a homogeneous OER catalyst without being deposited as a CoO x solid catalyst on Nb 2 O 5 . When we performed the POER using unprotected BiVO 4 with Co (aq) 2+ under the same condition, although POER was enhanced, the enhancement could not be sustained due to the chemical dissolution of BiVO 4 . After the POER, we found that a Co 3+ -containing OER catalyst was deposited on the bare BiVO 4 surface. This result suggested that the use of Co 2+ ions as a homogeneous catalyst was possible due to the inertness of the Nb 2 O 5 surface toward the adsorption or deposition of Co ions. This study enabling stable POER of BiVO 4 in 0.1 M HNO 3 using the combination of a Nb 2 O 5 protection layer and Co (aq) 2+ as a homogeneous OER catalyst provides promising possibilities for acidic POER and OER.

Catalysts↗

Hydrogen trapping at neutron irradiation produced defects in recrystallized alpha annealed Zircaloy-4 - 2016-0060

Hydrogen is absorbed into zirconium alloy-clad fuel elements and structural components as a result of water-side corrosion in both pressurized water reactor (PWR) and boiling water reactor (BWR) environments. Increasing hydrogen concentrations in the zirconium alloy affect both its mechanical properties and dimensional stability. It is well known that hydrogen can diffuse relatively rapidly through zirconium base alloys (in relation to the lifetime of the components) in response to solid solution concentration, temperature, and stress gradients. Migration of hydrogen within a component through its life must be considered to reliably predict the performance of the component through life and even post-service life. Many of the physical properties needed to describe this process, such as the solubility of hydrogen in zirconium alloys, diffusion coefficients of hydrogen through zirconium alloys, and the Soret effect within zirconium alloys, already have been published. Many of these measurements have been made outside of the reactor core environment on nonirradiated zirconium alloys. This paper presents in-reactor, isothermal hydrogen diffusion data that show an effect of the in-reactor radiation environment on the final measured hydrogen concentrations. Samples used are similar to the hydrogen diffusion couples used by several investigators in the past to measure the hydride dissolution solvus as a function of temperature. The experimental results are interpreted on the basis of a physical model for hydrogen trapping that hypothesizes that hydrogen in solid solution in the zirconium lattice comes into thermodynamic equilibria with the hydride phase as well as into a steady-state equilibrium with trapping at irradiation-induced defects within the lattice. In agreement with the model, the irradiation effect on final measured concentrations is seen to be a decreasing function of the irradiation temperature between ∼271 deg. C and 354 deg. C, with any effect essentially eliminated by an irradiation temperature of 354 deg. C. (authors)

36 MATERIALS SCIENCE↗

Small-scale Assessment of Simplified Ceramic Waste Form Processing

The feasibility of directly processing glass-bonded sodalite ceramic waste form materials by heating a mixture of Zeolite 4A, chloride salt, and sodium borosilicate binder glass was demonstrated by generating laboratory-scale materials. This direct processing method eliminates pre-setting the moisture content of the Zeolite 4A, eliminates the step of occluding salt in the prepared Zeolite 4A prior to processing, and can be conducted using larger particle sizes of crushed Zeolite 4A and crushed borosilicate glass than those called for in the current method. These simplifications are expected to facilitate material transfer and handling in a hot cell or controlled atmosphere environment and be more readily implemented at large scale than the current method. Most materials made to assess these simplifications were directly processed at 925 °C for two hours in an argon atmosphere glovebox, but one material was processed at 925 °C for four hours and one material was processed at 880 °C for two hours. Sodalite was generated and became microencapsulated by the binder glass in all materials. The microstructures were uniform throughout each product, were similar in all products, and were similar to the microstructures of materials made previously using the pressureless consolidation or hot isostatic pressing methods. Various formulations showed the efficiency of sodalite generation was not sensitive to the salt-to-Zeolite 4A ratio or salt-to-glass mass ratio, although a greater relative mass of glass is required to encapsulate sodalite generated from large particles of aggregated Zeolite 4A. The upper limit of salt loadings that can be effectively processed remains to be determined. The effectiveness of direct processing provided new insights into the conversion mechanism. The salt was likely dissolved into the glass that transported NaCl into the Zeolite 4A aggregates and sodalite was generated in situ as NaCl migrated from the outside of the aggregate inward. Other salt cations (e.g., potassium, strontium, cesium, and probably lithium) remain dissolved in the glass encapsulating the zeolite/sodalite domains. When the glass solidifies during cooling, small halite inclusion phases form in glass within sodalite domains and large mixed salt inclusions form in glass surrounding the sodalite due to the low solubility of chloride in the (solid) glass. Other salt cations were oxidized during processing and formed inclusions in the bulk glass (e.g., neodymium). Initial degradation tests show the dissolution behavior of directly processed CWF (SCWF) materials is similar to CWF materials made using different methods.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

ADVANCED OXIDATION: OXALATE DECOMPOSITION TESTING WITH OZONE

At the Savannah River Site (SRS), oxalic acid is currently considered the preferred agent for chemically cleaning the large underground Liquid Radioactive Waste Tanks. It is applied only in the final stages of emptying a tank when generally less than 5,000 kg of waste solids remain, and slurrying based removal methods are no-longer effective. The use of oxalic acid is preferred because of its combined dissolution and chelating properties, as well as the fact that corrosion to the carbon steel tank walls can be controlled. Although oxalic acid is the preferred agent, there are significant potential downstream impacts. Impacts include: (1) Degraded evaporator operation; (2) Resultant oxalate precipitates taking away critically needed operating volume; and (3) Eventual creation of significant volumes of additional feed to salt processing. As an alternative to dealing with the downstream impacts, oxalate decomposition using variations of ozone based Advanced Oxidation Process (AOP) were investigated. In general AOPs use ozone or peroxide and a catalyst to create hydroxyl radicals. Hydroxyl radicals have among the highest oxidation potentials, and are commonly used to decompose organics. Although oxalate is considered among the most difficult organic to decompose, the ability of hydroxyl radicals to decompose oxalate is considered to be well demonstrated. In addition, as AOPs are considered to be 'green' their use enables any net chemical additions to the waste to be minimized. In order to test the ability to decompose the oxalate and determine the decomposition rates, a test rig was designed, where 10 vol% ozone would be educted into a spent oxalic acid decomposition loop, with the loop maintained at 70 C and recirculated at 40L/min. Each of the spent oxalic acid streams would be created from three oxalic acid strikes of an F-area simulant (i.e., Purex = high Fe/Al concentration) and H-area simulant (i.e., H area modified Purex = high Al/Fe concentration) after nearing dissolution equilibrium, and then decomposed to {le} 100 Parts per Million (ppm) oxalate. Since AOP technology largely originated on using ultraviolet (UV) light as a primary catalyst, decomposition of the spent oxalic acid, well exposed to a medium pressure mercury vapor light was considered the benchmark. However, with multi-valent metals already contained in the feed, and maintenance of the UV light a concern; testing was conducted to evaluate the impact from removing the UV light. Using current AOP terminology, the test without the UV light would likely be considered an ozone based, dark, ferrioxalate type, decomposition process. Specifically, as part of the testing, the impacts from the following were investigated: (1) Importance of the UV light on the decomposition rates when decomposing 1 wt% spent oxalic acid; (2) Impact of increasing the oxalic acid strength from 1 to 2.5 wt% on the decomposition rates; and (3) For F-area testing, the advantage of increasing the spent oxalic acid flowrate from 40 L/min (liters/minute) to 50 L/min during decomposition of the 2.5 wt% spent oxalic acid. The results showed that removal of the UV light (from 1 wt% testing) slowed the decomposition rates in both the F & H testing. Specifically, for F-Area Strike 1, the time increased from about 6 hours to 8 hours. In H-Area, the impact was not as significant, with the time required for Strike 1 to be decomposed to less than 100 ppm increasing slightly, from 5.4 to 6.4 hours. For the spent 2.5 wt% oxalic acid decomposition tests (all) without the UV light, the F-area decompositions required approx. 10 to 13 hours, while the corresponding required H-Area decompositions times ranged from 10 to 21 hours. For the 2.5 wt% F-Area sludge, the increased availability of iron likely caused the increased decomposition rates compared to the 1 wt% oxalic acid based tests. In addition, for the F-testing, increasing the recirculation flow rates from 40 liter/minute to 50 liter/minute resulted in an increased decomposition rate, suggesting a better use of ozone.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

TCCR Operational Summary and Optimization for Tank 9 Processing - 20314

Savannah River Remediation (SRR) manages and operates the liquid waste facilities at Savannah River Site (SRS) for the Department of Energy (DOE). Stored liquid waste is a complex mixture of insoluble solids (sludge) and soluble salts in an alkaline solution. SRR has deployed the Tank Closure Cesium Removal (TCCR) system, a tank-side ion exchange process, to remove radioactive cesium from salt waste and enable onsite disposal of the resulting decontaminated salt solution as low-level waste at the Saltstone facilities. The TCCR system consists of two prefilters, four ion exchange (IX) columns, one resin trap, and a ventilation system. The IX process uses a form of inorganic crystalline silicotitanate (CST), which has a high affinity for cesium and other alkali metals, strontium, and actinides. This process is currently deployed utilizing salt feed from Tank 10, with future plans to dissolve solid salt in Tank 9 and transfer the salt solution to Tank 10 for processing through TCCR. The feed for TCCR must be created from salt-cake in Tank 10 through a dissolution process. Once enough salt has been dissolved, a qualification process is entered. This process characterizes the feed and ensures the cesium loading on the columns will not cause boiling of waste within the columns during or after processing. Once the batch has been qualified, salt waste is fed to the TCCR system through a transfer pump in the center of the tank. The waste is filtered through a set of two shielded, dead-end prefilters that prevent solids buildup in the columns. The filtered salt solution then travels to the shielded IX columns, which can be operated individually or in series, where the cesium is sorbed on the CST media. The decontaminated salt solution (DSS) then travels through a resin trap and out of the module to Tank 11. TCCR has successfully processed approximately 795,000 L of Tank 10H radioactive salt waste over two batches to date. There has not yet been a system induced shutdown. The prefilters performed as expected with only minor degradation in recovery of differential pressure after a backflush sequence. The time between backflushes decreased as each batch reached the end of processing. The hydraulics in the IXCs mostly performed as expected at all flow rates, except for one IXC that will be further investigated during Batch 3 processing. The TCCR system has shown some opportunities for more efficient processing during the length of the demonstration so far. For future processing of material from Tank 9H through Tank 10H and the TCCR unit, TCCR 1A will implement changes to the prefilters and the IXCs. The prefilters will have an increased surface area and a new filter media in an effort to increase time between filter swaps and improve backwashing cleaning capability. The IXCs will have a reduced diameter to allow for increased heat transfer out of the column and increased loading of Cs-137. Additionally, a new form of CST with an increased kinetic performance is being investigated for use during TCCR 1A operation. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Absence of Nanostructuring in NaPb m SbTe m+2 : Solid Solutions with High Thermoelectric Performance in the Intermediate Temperature Regime

Thermoelectric devices directly convert heat into electrical energy and are highly desired for emerging applications in waste heat recovery. Currently, PbTe based compounds are the leading thermoelectric materials in the intermediate temperature regime (~800 K); however, integration into commercial devices has been limited. This is largely because the performance of PbTe, which is maximized ~900 K, is too low over the temperatures of interest for most potential commercial applications (generally under 600 K). Improving the low temperature performance of PbTe based materials is therefore critical to achieve usage outside of existing niche applications. Here, we provide an in-depth study of the cubic NaPb m SbTe m+2 system of compounds (m = 1-20) and report that it is an excellent class of low- to medium-temperature thermoelectrics when m = 10-20. Here, we show that the as-cast polycrystalline ingots exhibit degenerate p-type conduction and high maximum ZTs of 1.2-1.4 at 650 K when m = 6-20. Because the ingots are found to be extremely brittle, we utilize spark plasma sintering (SPS) to prepare more mechanically robust samples, and surprisingly, find that SPS results in an undesired change in charge transport toward n-type behavior. We show this unanticipated transition from p-type behavior as ingots to n-type after SPS is due to dissolution of secondary phases that are present in the ingots into the primary matrix during the SPS process, resulting in a transformation from an inhomogeneous state to a solid solution without any observable evidence of nanoscale precipitation. This is in sharp contrast to the seemingly similar AgPb m SbTe m+2 (LAST) system, which is heavily nanostructured. The SPSed NaPb m SbTe m+2 is doped p-type by tuning the cation stoichiometry, i.e., Na 1+x Pb m-x Sb 1-y Te m+2 . The optimized compounds have very low lattice thermal conductivities of 1.1-0.55 W·m -1 ·K -1 over 300-650 K, which enhances the low intermediate temperature performance and gives rise to maximum ZT values up to 1.6 at 673 K as well as an excellent ZT avg of 1.1 over 323-673 K for m = 10, 20, making Na 1+x Pb m-x Sb 1-y Te m+2 among the highest performing PbTe-based thermoelectrics under 650 K.

Electrical conductivity↗