A facile preparation and the luminescent properties of Eu{sup 3+}-doped Y{sub 2}O{sub 2}SO{sub 4} nanopieces
Graphical abstract: - Highlights: • Y{sub 2}O{sub 2}SO{sub 4}:Eu{sup 3+} nanopieces were prepared via electrospinning followed by calcination. • The photoluminescence of Y{sub 2}O{sub 2}SO{sub 4}:Eu{sup 3+} nanopieces were investigated. • The Y{sub 2}O{sub 2}SO{sub 4}:Eu{sup 3+} was compared to nanoribbons and commercial Y{sub 2}O{sub 3}:Eu{sup 3+}. • The potential applications of the nanopieces and the facile method are suggested. - Abstract: The europium(III)-doped yttrium oxysulfate (Y{sub 2}O{sub 2}SO{sub 4}:Eu{sup 3+}) nanopieces have been prepared via electrospinning followed by calcination at 1000 °C in mixed gas of sulfur dioxide and air. Based on the experimental results, a possible formation mechanism for the nanopieces is that the nanopieces are determined by the directing template of electrospun nanoribbons and the multilayer crystal structure of Y{sub 2}O{sub 2}SO{sub 4}. Besides, the nanopieces show excellent luminescent properties with emissions at 581, 589, 597, 653, 619, and 697 nm resulting from the {sup 5}D{sub 0} → {sup 7}F{sub J} (J = 0, 1, 2, 3, 4) transition of Eu{sup 3+}. The peaks of charge transfer and {sup 5}D{sub 0} → {sup 7}F{sub 2} transition of Eu{sup 3+} obviously have red shifts comparing to those of both Y{sub 2}O{sub 3}:Eu{sup 3+} nanoribbons and commercial Y{sub 2}O{sub 3}:Eu{sup 3+}. Moreover, the nanopieces exhibit stronger intensities than the Y{sub 2}O{sub 3}:Eu{sup 3+} in excitation and emission spectra. Concentration quenching in the nanopieces occurs when Eu{sup 3+} concentration is 11 mol%, indicating that the nanopieces have an optimum luminescent intensity under this doping concentration.