A general strategy and a consolidated mechanism for low-methane hydrogenolysis of polyethylene over ruthenium

Polyethylene (PE) is one of the most environment-threatening plastic waste. Its Ru-catalyzed hydrogenolysis is rapid but produces too much methane. Here, in this study, low-density PE hydrogenolysis is performed at mild conditions and short times over Ru-doped zirconia catalysts (Ru-XZr, X = Ti, Nb, Ce, W, V, Mo, Fe) to determine low-methane catalysts. Methane is produced via direct terminal C-C scission and surface cascade of consecutive C-C scissions, with the latter sensitive to hydrogen availability and dominant in hydrogen-lean conditions. Reactivity studies, characterization and theory reveal that the most effective dopant oxides (W, V, and Mo) are intermediately reducible, as they store and supply extra hydrogen to Ru via reverse hydrogen spillover. This hydrogen readily hydrogenates and desorbs long alkyl surface intermediates that would otherwise produce cascade methane. Our proposed mechanism reconciles the low methane production achieved by increasing the hydrogen pressure or reducing the particle size and exposes the key selectivity descriptors.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

The role of catalyst acidity and microstructure on light olefin selectivity in polyethylene deconstruction in short contact time pulse Joule-heated reactors

The growing volume of plastics waste, compounded with a low recycling rate, has led to an alarming amount of plastics ending up in landfills or being incinerated. While pyrolysis offers a route for plastic waste deconstruction, its product distribution is often broad and poorly controlled due to unselective radical chemistry at high temperatures. We recently demonstrated that rapid pulse Joule-heated catalytic cracking over HZSM-5, combined with small fractions of steam, can achieve high selectivity (>80 %) toward C 2 -C 4 olefins, while significantly reducing coking compared to continuous Joule heating. Here, we investigate how acid catalyst properties, such as silica/alumina ratio, zeolite topology, and catalyst porosity, influence light olefin selectivity during polyethylene deconstruction via rapid pulse Joule heating. We demonstrate that silica-to-alumina ratios of ∼30 yield high light olefin selectivity, and small-pore zeolites favor light olefins at the expense of increased coke formation. To mitigate coking, we synthesize HZSM-5 nanosheets and hierarchical zeolites (MFI, FAU, and CHA). Furthermore, these catalysts achieve an ethylene selectivity of approximately 35 %, a twofold increase over prior catalytic pyrolysis. Additionally, co-feeding steam and incorporating hierarchical porosity reduce coke formation and enhance catalyst stability.

Catalytic cracking↗

A high throughput assay to detect enzymatic polyethylene oxidation

Biological plastics deconstruction and upcycling have emerged as sustainable alternatives to traditional recycling technologies for plastics waste. The discovery and engineering of efficient thermostable poly(ethylene terephthalate) (PET) hydrolases have made biological PET recycling possible at scale; however, enzymes for non-PET plastics, which account for approximately 70% of all plastics produced, remain largely undiscovered. To accelerate the discovery of such enzymes, we develop a high-throughput screen to detect initial polymer oxidation, specifically that of the C-H bond to an aldehyde. We test 4-hydrazino-7-nitro-2,1,3-benxoxadiozole hydrazine (NBD-H), which reacts with generated aldehydes to form a fluorescent hydrazone on plasma oxidized low-density polyethylene (LDPE) films. Hydrazone generation correlated well with the area of aldehyde peaks as measured by Fourier Transform Infrared Spectroscopy (FTIR) (R2 = 0.92). Moreover, we demonstrate that the probe reliably identifies LDPE-active dye decolorizing peroxidases (DyPs) that generate aldehydes on LDPE films (1.7 – 3.0 fold change relative to background), serving as an effective screen as demonstrated by receiver operating characteristic area under the curve of 0.95. Furthermore, this assay offers an LDPE oxidation screening platform that can be readily parallelized and automated for accelerated discovery of enzymes involved in polyolefin deconstruction.

biocatalysis↗

Polyethylene upcycling to fuels: Narrowing the carbon number distribution in n-alkanes by tandem hydropyrolysis/hydrocracking

The extensive use of plastics in modern life has resulted in a global waste crisis to the environment. Polyethylene (PE) is one of the most popular and hardest plastics to recycle because of its strong C(sp 3 )-C(sp 3 ) bonds. In this study, a tandem conversion process, i.e., hydropyrolysis and subsequent vapor-phase hydrocracking of primary intermediates (C n>5 alkenes and long-chain alkanes), was conducted via a two-step pressurized flow-through fixed-bed reactor over a CoAl 2 O 4 spinel-derived catalyst. The product distribution could be flexibly tuned by regulating operating parameters in the cascade fixed-bed reactor and Co/Al molar ratio in CoAl 2 O 4 spinel catalysts. Under optimal reaction conditions (0.2 MPa H 2 , 550 °C for hydropyrolysis in the 1st reactor, 300–325 °C for hydrocracking in the 2nd reactor, 20 s -1 of gas hourly space velocity), the maximum single-pass yields of gasoline (C 5 -C 12 ) and jet-fuel (C 8 -C 16 ) range n-alkanes reached 86.0 wt% and 68.1 wt%, respectively. The CoAl 2 O 4 spinel catalysts also gained high activity in degrading realistic post-consumer plastics such as linear low-, low-, and high-density PE, and a ~ 73.1 wt% gasoline yield and a ~ 54.7 wt% C 8 -C 16 yield were retained even after 3 cycles in-situ regeneration of deactivated CoAl 2 O 4 catalysts. This work provides an efficient and tunable approach to upcycle PE wastes into liquid fuels with an ideal carbon length.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Reduced-order condensed-phase kinetic models for polyethylene, polypropylene and polystyrene thermochemical recycling

Thermochemical recycling of plastic waste (PW) into chemicals and energy vectors requires coupling particle and reactor-scale simulations to accurate condensed phase pyrolysis mechanisms for each constituent. This work proposes a methodology to derive reduced-order condensed-phase kinetic models from validated semi-detailed kinetic mechanisms. Two types of kinetic models are obtained for polyethylene (PE), polypropylene (PP) and polystyrene (PS): reduced semi-detailed models and multi-step fully lumped ones. These families offer different compromises between accuracy and computational cost. The former employ 50–100 gas + liquid species and describe both the radical degradation and the detailed carbon distribution of the products. Conversely, the latter involves 5–10 species per polymer tracking only the main petroleum cuts. The kinetic mechanisms are complemented by the definition of thermochemical properties of gas, liquid, and solid-phase species, accounting for phase-transitions through pseudo-chemical reactions. Model validations are performed by comparison with experimental data and the original semi-detailed mechanisms in terms of mass loss, heat fluxes and product distribution profiles. The resulting CHEMKIN-like condensed-phase models are attached as Supplementary Material and as a GitHub repository. Extending the proposed approach to other polymers and coupling it with existing subsets in the CRECK kinetic framework (e.g., biomass, PVC, PET) offers a powerful tool to model thermochemical recycling of PW and biomass/PW mixtures.

kinetics↗

Improving the adhesion of glass/polypropylene (glass-PP) and high-density polyethylene (HDPE) surfaces by open air plasma treatment

The objective of this study was to investigate the bonding between glass reinforced polypropylene (glass-PP) and high-density polyethylene (HDPE) surfaces. As glass-PP and HDPE surfaces possess low surface energy inherently, atmospheric plasma treatment enhances the adhesion characteristics between the surfaces by increasing their surface energies. Both the materials were subjected to atmospheric/air plasma by varying parameters such as plasma intensity and number of treatments. Optimal plasma treatment conditions were determined based on the bond strength of the materials. Various characterization techniques such as FTIR (Fourier transform infrared spectroscopy), SEM (scanning electron microscopy), DSC (differential scanning calorimetry) and surface energy determination via wettability inks, were employed to understand the surface modification following plasma treatment. Furthermore, the effect of plasma treatment on glass-PP surface versus a neat polypropylene (neat PP) surface was characterized to understand and establish a baseline. Improvement in bond strength of glass-PP-HDPE panels was observed, GΙc (Mode 1 interlaminar fracture toughness) value of glass-PP- HDPE panels increased from 0.1 N/mm to 5.5 N/mm (after plasma treatment) whereas, the GΙc value of neat PP- HDPE panels increased from 0.4 N/mm to 2.8 N/mm (after plasma treatment). Enhancement in the surface energy of glass-PP and HDPE surfaces was observed, surface energy of glass-PP increased from 28 mN/m to 58 mN/m and the surface energy of HDPE surface increased from 28 mN/m to 72 mN/m.

42 ENGINEERING↗

Hydrogen from low-density polyethylene via nonthermal plasma: Effects of energy density and process parameters

Nonthermal plasma processes are promising for the modular valorization of plastic waste, especially into hydrogen and carbon materials, due to their high intensity, lack of reliance on catalysts or consumables, and suitability to be directly powered by electricity. We investigate the production of hydrogen from low-density polyethylene (LDPE) as a plastic waste model using streamer Dielectric Barrier Discharge (sDBD) plasma in nitrogen at atmospheric pressure. Here, we examine the effects of process energy density (energy input per unit of feedstock mass), feedstock mass, and plasma intensity (electric voltage) on plasma properties, hydrogen yield and energy efficiency via gas chromatography, optical emission spectroscopy, and electrical diagnostics, together with reactor-scale and nonlinear electric circuit modeling. The characteristic temperature of free electrons in the sDBD plasma is approximately 15000 K (1.3 eV), and that of gas species 10 times lower, demonstrating strong thermal non-equilibrium that can lead to molecular bond scission via charged species impact rather than direct heating. Experimental results show that higher energy density leads to greater hydrogen production and diminishing energy efficiency, and that higher plasma intensity and larger feedstock mass lead to greater hydrogen yield due to higher plasma temperatures and enhanced energy fluxes to the feedstock.

08 HYDROGEN↗

Effect of secondary gas-phase reactions (SGR) in pyrolysis of carbon feedstocks for anisotropic carbon materials production – 3: Modifying non-coking coal tar through co-pyrolysis of coal with linear low-density polyethylene and high-impact polystyrene

Herein, this work focuses on co-pyrolysis experiments of Utah Sufco coal with linear low-density polyethylene (LLDPE) and high-impact polystyrene (HIPS). These two plastic types have differing pyrolysis chemistries and have different hydrogen transfer behavior. Similar to earlier work in this series of papers, controlled secondary gas-phase reactions during pyrolysis were used to induce cracking and condensation reactions among the pyrolytic tar species. Co-pyrolysis tests were performed with feed plastic percentages ranging from 10-20 wt% and pyrolysis SGR temperatures ranging from 800-900°C. Analyses of the intermediate tar products showed that oxygen contents and aromaticity were substantially different, depending on the plastic, and resulting pitch softening points and mesophase contents also varied greatly depending on the starting plastic feedstock used. Most of the synergies observed in the co-pyrolysis results were negative, except for the oxygen content. Oxygen contents were higher than expected when LLDPE was used, resulting in reactive pitches with softening points > 350°C. On the other hand, oxygen contents were lower than expected when HIPS was used, resulting in less reactive pitches. Ultimately, only the HIPS/coal samples created at the SGR temperature of 900°C had reasonable softening points at or under 350°C, making them the only samples created in this work potentially suitable for mesophase pitch-based carbon fiber production. The success in creating fusible mesophase pitches from co-pyrolyzing HIPS with Utah Sufco coal is likely attributed to the fact that polystyrene is a stronger hydrogen acceptor rather than donor, which should facilitate more cracking rather than stabilizing tar oxygen functional groups, making the tar species ultimately less reactive during thermal conversion to mesophase pitch.

01 COAL, LIGNITE, AND PEAT↗

Recycled polyethylene and crumb rubber composites modified asphalt with improved aging resistance and thermal stability

Crumb rubbers (CR) and recycled Polyethylene (PE) are commonly used as modifiers to improve the asphalt properties. However, the addition of these modifiers individually may result in phase separation of PE and inadequate degradation of CR, which may not simultaneously satisfy the rheological and aging resistance of the binder blends. In this study, a type of CR/PE composites manufactured through melt extrusion procedures was adopted for the improvement of the modified binder blends. The modified binder blends after short-term (RTFO) and long-term (PAV) aging were collected for dynamic shear rheometer and bending beam rheometer tests. FTIR tests were also used to quantify the aging resistance, while differential scanning calorimetry (DSC) and thermogravimetric analysis (TGA) were applied to evaluate the thermal behaviors of the binder blends. Optical microscopy tests were used to explore the modification mechanism and visualize the microstructures of original and PAV aged binder blends. Test results showed that CR/PE composites could significantly improve the aging resistance of the binder blends. The dispersed PE particles still interacted with each other and meanwhile worked with the diffused rubbery phase, which could form a similar TPEs network. The oxidation and high-temperature aging of such binder blends would strengthen the network that resisted the aging severity of the binder blends. Furthermore, it was also revealed that CR/PE modified asphalt could sustain more heat before a rapid degradation and the well-dispersed PE particles could interact with the diffused CR particles to form a network to resist aging.

02 PETROLEUM↗

Heterogeneous Diels–Alder tandem catalysis for converting cellulose and polyethylene into BTX

Producing biomass-derived aromatic hydrocarbons via controllable Diels–Alder reactions is a promising approach to recover energy and chemicals from waste streams. A tandem Diels–Alder catalysis consisting of SAPO-34 and Fe/HZSM-5 (stacked catalysis or mixed catalysis) was evaluated for thermochemical conversion of cellulose and polyethylene blends into benzene, toluene, and xylenes (BTX). Aromatization catalyst type significantly affected the activity of tandem catalysis, and the BTX obtained from the HZSM-5 stacked catalysis was ~2.3 times higher than that of the USY stacked one. An introduction of Fe active promoters into HZSM-5 increased the Lewis to Brønsted acid sites molar ratio (L/B) from 0.4 to 4.1. The comparison between Fe/HZSM-5 stacked catalysis and parent HZSM-5 single catalysis indicated that the former was more effective for BTX production, obtaining a nearly two-fold increase in yield with a high selectivity of 82.8%. A close proximity between Fe/HZSM-5 and SAPO-34 in the mixed catalysis increased the BTX enhancement to 1.8. A synergistic effect was provided by the coordination of Lewis and Brønsted acid sites in the Fe/HZSM-5 mixed catalysts for facilitating BTX generation, achieving a maximum of 25.9% at a Fe/HZSM-5 to SAPO-34 mass ratio of 1:1 with a theoretical L/B of 7.2. Finally, this work provides a sustainable strategy to produce biomass-derived aromatic hydrocarbons.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Techno-economic analysis and life cycle assessment for the catalytic hydrogenolysis and hydrocracking of polyethylene

Catalytic hydrogenolysis and hydrocracking are promising technologies for the conversion of polyolefin waste into hydrocarbons. Here, to explore the economic and environmental viability of these approaches, we conducted techno-economic analysis and life cycle assessment of polyethylene hydrogenolysis and hydrocracking processes that produce fuel-range products or olefins, respectively. Relative to primary production, the minimum selling price (MSP) of alkanes for linear-chain naphtha was estimated to be 1.8-fold higher, whereas branched-chain naphtha and propylene were shown to be cost competitive. Environmental impacts showed similar trends across scenarios, with propylene production by hydrocracking exhibiting greenhouse gas emissions comparable with conventional propylene due to relatively low hydrogen demand and high yield. Together, these results suggest that innovations in catalysis and reaction engineering will be required to make viable products that are scale matched with today's plastics, such as light olefins for closed-loop recycling.

09 BIOMASS FUELS↗

Indium tin oxide films deposited by thermionic-enhanced DC magnetron sputtering on unheated polyethylene terephthalate polymer substrate

Indium tin oxide thin films were deposited onto polyethylene terephthalate substrates via thermionic enhanced DC magnetron sputtering at low substrate temperatures. The structural, optical and electrical properties of these films are methodically investigated. The results show that compared with traditional sputtering, the films deposited with thermionic emission exhibit higher crystallinity, and their optical and electrical properties are also improved. Indium tin oxide films deposited by utilizing thermionic emission exhibit an average visible transmittance of 80% and an electrical resistivity of 4.5 x 10{sup -4} {Omega} cm, while films made without thermionic emission present an average visible transmittance of 74% and an electrical resistivity of 1.7 x 10{sup -3} {Omega} cm.

36 MATERIALS SCIENCE↗

Rate-dependent phase transition of high density polyethylene

Quasi-static and dynamic tension tests are conducted on a widely used semicrystalline polymer, high density polyethylene (HDPE), to explore the strain rate effects on phase transition. HDPE exhibits considerable strain-rate hardening. In situ , high-speed x-ray diffraction demonstrates a martensitic transformation from the orthorhombic to monoclinic phase during both loading conditions. However, compared to quasi-static loading, the phase transition occurs at a lower bulk strain but higher stress under dynamic loading (strain rate 5100 s –1 ), suggesting strain-rate-accelerated phase transition dynamics. Furthermore, evolutions of lattice strain with bulk stress indicate different roles of amorphous and crystalline phases in deformation under different strain rates.

36 MATERIALS SCIENCE↗

Structural and antibacterial properties of NSAID-loaded ultra-high molecular weight polyethylene

Peri-articular delivery of pain medication in joint arthroplasty has the potential to address post-operative pain and decrease the use of systemic opioids. Additionally, the sustained release from a delivery vehicle may be especially impactful in the initial post-operative period when pain is most severe. We recently described a novel approach for the sustained intra-articular delivery of an analgesic (bupivacaine) from an ultra-high molecular weight polyethylene (UHMWPE) bearing surface. A secondary but very significant effect of incorporating bupivacaine in UHMWPE was its antibacterial effect against Staphylococcal species, which are associated with the majority of periprosthetic joint infections. Here, we report on the structure, properties, elution characteristics and antibacterial properties of UHMWPE loaded with the non-steroidal anti-inflammatory drug (NSAID) — tolfenamic acid. We showed that 6 wt% drug loading was optimal for eluting clinically relevant intra-articular and systemic concentrations, for maintaining mechanical properties at a clinically relevant level, and for providing anti-colonization potential against low risk (planktonic) and high risk (biofilm forming) Staphylococcal species. We determined the osteoblast response to the tolfenamic acid-loaded UHMWPE to evaluate the cytotoxicity profile of this novel material. Tolfenamic acid-loaded UHMWPE has the potential to be used as a part of multimodal pain management therapy following arthroplasty and may provide prophylaxis for periprosthetic infection.

36 MATERIALS SCIENCE↗

A New Polyethylene Scattering Law Determined Using Inelastic Neutron Scattering

Monte Carlo neutron transport codes such as MCNP rely on accurate data for nuclear physics cross-sections to produce accurate results. At low energy, this takes the form of scattering laws based on the dynamic structure factor, S (Q, E). High density polyethylene (HDPE) is frequently employed as a neutron moderator at both high and low temperatures, however the only cross-sections available are for T =300 K, and the evaluation has not been updated in quite some time. In this paper we describe inelastic neutron scattering measurements on HDPE at 5 and 300 K which are used to improve the scattering law for HDPE. We describe the experimental methods, review some of the past HDPE scattering laws, and compare computations using these models to the measured S (Q, E). The total cross-section is compared to available data, and the treatment of the carbon secondary scatterer as a free gas is assessed. We also discuss the use of the measurement itself as a scattering law via the 1 phonon approximation. We show that a scattering law computed using a more detailed model for the Generalized Density of States (GDOS) compares more favorably to this experiment, suggesting that inelastic neutron scattering can play an important role in both the development and validation of new scattering laws for Monte Carlo work.

Lavelle, Christopher M↗

Quantitative analysis of changes in antioxidant in crosslinked polyethylene (XLPE) cable insulation material exposed to heat and gamma radiation

Quantitative analysis of the antioxidant poly(1,2-dihydro-2,2,4-trimethylquinoline) (pTMQ) was conducted on pristine, thermally-aged, and gamma radiation-aged commercial cross-linked polyethylene-(XLPE-)based cable insulation material aged at temperatures 60, 90, and 115?°C, with gamma radiation exposure dose rates of 0, 120, 300, and 540?Gy/h for 15 days. The quantification of antioxidant was performed using pyrolysis gas chromatography-mass spectrometry (Py-GCMS). Oxidation induction time (OIT) was measured using differential scanning calorimetry (DSC) and correlation was made between the quantified depletion of antioxidant and measured OIT. It was observed that, in the case of isothermal aging, the quantity of antioxidant and OIT decreased with increasing gamma radiation dose. In the case of samples exposed to the same gamma radiation dose, the quantity of antioxidant and OIT were observed to decrease with increasing aging temperature. Depletion in the quantity of antioxidant relative to that in the pristine material ranged from 7 to 93% for differently aged samples. The measured decline in OIT ranged from 0 to 80%. Change in the quantity of antioxidant in the material was observed to follow the same trend as the change in OIT when the samples were aged under various conditions. The observations are explained in terms of the reaction between the antioxidant and free radicals created during exposure of the samples to thermal and gamma radiation.

Pyrolysis gas chromatography-mass spectroscopy, an↗

Aging mechanisms of filled cross-linked polyethylene (XLPE) cable insulation material exposed to simultaneous thermal and gamma radiation

Thermal and simultaneous thermal and gamma radiation aging experiments were conducted on an industry grade cross-linked polyethylene (XLPE) cable insulation material, which is a composite material with XLPE as polymer matrix and various additives and fillers. Reverse engineering was conducted to identify and quantify the material composition given that this information was not revealed by the cable manufacture. Samples were then aged at temperatures of 60, 90, and 115 °C, exposed to gamma radiation for total doses of 0 to 324 kGy, and at dose rates of 0 to 540 Gy/h. Aging mechanisms were studied using various materials characterization techniques including pyrolysis gas chromatography mass spectrometry (Py-GCMS), differential scanning calorimetry (DSC), nuclear magnetic resonance spectroscopy (NMR), and gel-fraction tests. Results show that the flame-retardant components were decomposed into smaller molecules when the material was exposed to gamma radiation, while no changes were observed when the samples were aged thermally without gamma radiation. With exposure to gamma radiation, the crystalline phase of the XLPE were damaged by gamma radiation introducing defects in the crystals, resulting in smaller and less perfect crystals. The dominance of chain scission or chain reformation process largely depends on the chain mobility, which is decided by the aging temperature. Chain scission was seen to dominate when the material was exposed to gamma radiation at 60 °C. Chain cross-linking slightly dominated when the material was exposed to gamma radiation at 90 °C and became more dominant with exposure to gamma radiation at 115 °C. No significant change to the XLPE polymer matrix was observed when the samples were exposed to thermal aging without gamma radiation. Finally, antioxidant is more effective in protecting the XLPE polymer matrix under thermal aging, but less effective with sample exposure to gamma radiation.

38 RADIATION CHEMISTRY, RADIOCHEMISTRY, AND NUCLEA↗

Direct comparison of gamma, electron beam and X-ray irradiation doses on characteristics of low-density polyethylene, polypropylene homopolymer, polyolefin elastomer and chlorobutyl rubber medical device polymers

There is a growing need for increased efficiency in the sterilization of single use medical devices and other products that contain polymer components. Gamma radiation is widely used for devices suited for radiation sterilization; however, safety, throughput and cobalt-60 source availability are challenging the prospect of relying on gamma radiation to meet the anticipated needs of the industry. Use of electron beam (e-beam) and X-rays as alternatives to gamma for radiation sterilization have been hampered in part by a concern that these modalities may adversely affect polymer integrity and performance relative to the gamma method, for which the industry has had much more experience. To address this concern, the effects of sterilization-relevant doses of ebeam, X-ray and gamma radiation were directly compared using common medical device polymers found in two prototypical commercial devices currently sterilized using cobalt-60 gamma irradiation. The Becton, Dickinson and Company (BD) Vacutainer™ Plus tube contains low-density polyethylene and chlorobutyl rubber components, while the BD Vacutainer™ Push Button Blood Collection Set contains polypropylene homopolymer and polyolefin elastomer components. Injection-molded samples prepared from the polymers used in these products were exposed to target doses of 15, 35, 50 and 80 kGy using gamma, e-beam and X-ray radiation. Changes in coloration, tensile properties and hardness were measured for each condition, and the effects of e-beam and X-ray irradiation compared with the effects of gamma irradiation on these properties. Both e-beam and X-ray appear as viable alternatives to gamma irradiation for sterilization of the polymers tested.